• Title/Summary/Keyword: lead free piezoelectric ceramics

Search Result 169, Processing Time 0.022 seconds

Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Ta,Sb)O3 Ceramics Manufactured Using Columbite Methods with Calcination Temperature (Columbite법으로 제조된 (Na,K,Li)(Nb,Ta,Sb)O3 세라믹스의 하소온도에 따른 유전 및 압전 특성)

  • Ra, Cheol-Min;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.3
    • /
    • pp.159-163
    • /
    • 2016
  • In this paper, in order to develop optimum composition ceramics with excellent piezoelectric properties, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.823}Sb_{0.08}Ta_{0.037})O_3+0.3wt%Bi_2O_3+0.4wt%Fe_2O_3$ lead-free piezoelectric ceramics were synthesized by conventional soild-state method. The calcination temperature of columbite precursors were fabricated at temperature range from $950^{\circ}C$ to $1,150^{\circ}C$ and sintering aids with low melting point were added to densify these ceramics. Effect of calcination temperature on dielectric and piezoelectric properties of ceramics were investigated. the ceramics with B-site columbite precursors at temperature of $1,100^{\circ}C$ obtained the optimal values of $d_{33}=272$ [pC/N], $k_p=0.51$, $Q_m=102$, ${\varepsilon}_r=978$.

Effect of Ta Doping on Piezoelectric Properties of Lead-Free (K0.5Na0.5)NbO3 Ceramics ((K0.5Na0.5)NbO3 세라믹스의 압전 특성에 대한 Ta 도핑 효과)

  • Kang, Jin-Kyu;Lee, Yong-Hui;Heo, Dae-Jun;Lee, Hyun-Young;Dinh, Thi Hinh;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.5
    • /
    • pp.292-296
    • /
    • 2014
  • We investigated the effect of Ta doping on the dielectric and piezoelectric properties of lead-free $(K_{0.5}Na_{0.5})NbO_3$ ceramics prepared using a conventional ceramic processing. X-ray diffraction analysis revealed that Ta was perfectly substituted into Nb-sites in the range of 0 to 20 at%. As Ta content in the KNN increased, the sinterability of KNN ceramics was significantly degraded while the Ta doping enhanced the piezoelectric constant $d_{33}$, planar mode piezoelectric coupling coefficient ($k_p$), and electromechanical quality factor ($Q_m$). The highest values for $d_{33}$, $k_p$, and $Q_m$ was found to be 156 pC/N, 0.37, and 155, respectively.

A Study on Improving the Characteristics of Lead-free Piezoelectric Ceramic Materials Applicable to IT and BT Converged Products (IT와 BT 융복합 제품에 적용 가능한 무연압전세라믹소재의 특성 개선에 관한 연구)

  • Seongjun Yun;Joonsoo Bae
    • Journal of Korean Society of Industrial and Systems Engineering
    • /
    • v.47 no.3
    • /
    • pp.86-94
    • /
    • 2024
  • In this study, an attempt was made to approximate the main characteristic values of Bi0.5(Na0.78K0.22)0.5TiO3 (= BNKT) depending on the content of Fe2O3 additives, aiming to approach the values of lead(Pb) piezoelectric ceramic materials (PZT). Specifically, when the piezoelectric coefficient (d33) value of lead(Pb) piezoelectric ceramic material (PZT polycrystalline ceramic powder) is 300[pC/N] or higher, it is applied for hard purposes such as ultrasonic welding machines and cleaning machines, and when it exceeds 330[pC/N], it is applied for soft purposes like piezoelectric sensors. In this study, research and development were conducted for devices with a piezoelectric coefficient (d33) of 300[pC/N] or more for actuators. For this purpose, K+ exceeding 0.02 to 0.12 mol% was added to (Na0.78K0.22)0.5Bi0.5TiO3 to analyze structural changes due to K+ excess, and (Na0.78K0.22)0.5Bi0.5TiO3 + 8mol% K2CO3 Ti4+ was substituted with Fe3+ to manufacture lead-free piezoelectric materials. As a result, ceramics with Fe3+ substitution at x = 0.0075 yielded an average value of d33 = 315[pC/N]. Furthermore, for ceramics with Fe3+ substitution at x = 0.0075, the average values of maximum polarization (Pmax), residual polarization (Prem), and coercive field (Ec) were found to be 39.63 μC/cm2, 30.45 μC/cm2, and 2.50 kV/mm, respectively. The reliable characteristic values obtained from the research results can be applied to linear actuator components (such as the zoom function of mobile cameras, LDM for skin care, etc.) and ultrasonic vibration components.

Microstructure and Piezoelectric Properties of Low Temperature Sintering (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics (저온소결 (Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 미세구조 및 압전특성)

  • Lee, Kab-Soo;Yoo, Ju-Hyun;Lee, Jie-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.4
    • /
    • pp.205-209
    • /
    • 2016
  • In this paper, piezoelectric ceramics with the composition of $(Na_{0.525}K_{0.4425}Li_{0.0375})(Nb_{0.8975}Sb_{0.065}Ta_{0.0375})O_3+0.3wt%\;CoO+x\;CuO$ ($0.005{\leq}x{\leq}0.025$) (abbreviated to NKL-NST) were fabricated for ultrasonic sensor application. The effects of CuO addition and sintering on the microstructure and the piezoelectric properties of the NKL-NST ceramics were systematically studied. Excellent piezoelectric properties such as electromchanical coupling $factor(k_p)=0.415$, piezoelectric constant $(d_{33})=166pC/N$ and piezoelectric figure of merit $d_{{33}*}g_{33}=5.47pm^2/N$ were obtained from the 2.5 mol% CuO doped NKL-NST+0.3 wt%CoO ceramics sintered at $1,000^{\circ}C$ for 3 h.

Piezoelectric and Ferroelectric Properties of $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}Ba_xTiO_3$ Lead-Free Piezoelectric Ceramics (비납계 $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}Ba_xTiO_3$ 압전 세라믹의 압전-유전특성)

  • Lee, Dae-Su;Jeong, Soon-Jong;Kim, Min-Su;Park, Eun-Cheol;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.271-271
    • /
    • 2006
  • The structural, dielectric and piezoelectric properties of $[Bi_{1-x}(Na_{0.7-x}K_{0.2}Li_{0.1})]_{0.5}BaxTiO_3$ (BNKLBxT) ceramics were studied for the compositional range, x = 0-0.08. The samples were prepared by conventional sintering technique. The result of X-ray diffraction (XRD) suggest that $Ba^{2+}$ diffuse into the $[Bi(Na_{0.7}K_{0.2}Li_{0.1})]_{0.5}TiO_3$ (BNKLT) lattices to form a solid solution with a single phase perovskite structure. The ceramic show excellent piezoelectric and ferroelectric properties, and optimum properties measured are as follows: piezoelectric constant $d_{33}=230pC/N$, planar electromechanical coupling factor $k_p\;=\;40.3%$, remanent polarization $P_r\;=\;30\;{\mu}C/cm^2$, and coercive field $E_c\; =\;2.5\;kV/mm$, respectively.

  • PDF

Electrical Properties of lead free (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics with MnO2 Addition (MnO2 첨가량에 따른 비납계 (Na,K,Li)(Nb,Sb,Ta)O3 세라믹스의 전기적특성)

  • Lee, Seung-Hwan;Nam, Sung-Pill;Lee, Dong-Hyun;Lee, Sung-Gap;Lee, Sang-Chul;Lee, Young-Hie
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.60 no.4
    • /
    • pp.801-804
    • /
    • 2011
  • Electrical properties and microstructure were investigated on the effects of $MnO_2$ and the lead-free $(Na_{0.44}K_{0.52}Li_{0.04})(Nb_{0.83}Sb_{0.07}Ta_{0.1})O_3$ ceramics with the addition of $MnO_2$ were fabricated by a conventional mixed oxide method. A gradual change in the crystal and microstructure was observed with the increase of $MnO_2$ addition. For the NKN-LST-xmol%$MnO_2$ sintered at $1100^{\circ}C$, bulk density increased with the addition of $MnO_2$ and showed maximum value at addition 1.0mol% of $MnO_2$. Curie temperature of the NKN-LST ceramics slightly decreased with adding $MnO_2$. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased below 0.25mol% of $MnO_2$ addition, which might be due to the increase in density. The high piezoelectric properties = 145 pC/N, electromechanical coupling factor = 0.421 and dielectric constant = 2883 were obtained for the NKN-LST-0.25mol%$MnO_2$ sintered at $1100^{\circ}C$ for 4h.

Structural, Dielectric and Field-Induced Strain Properties of La-Modified Bi1/2Na1/2TiO3-BaTiO3-SrZrO3 Ceramics

  • Hussain, Ali;Maqbool, Adnan;Malik, Rizwan Ahmed;Zaman, Arif;Lee, Jae Hong;Song, Tae Kwon;Lee, Jae Hyun;Kim, Won Jeong;Kim, Myong Ho
    • Korean Journal of Materials Research
    • /
    • v.25 no.10
    • /
    • pp.566-570
    • /
    • 2015
  • $Bi_{0.5}Na_{0.5}TiO_3$ (BNT) based ceramics are considered potential lead-free alternatives for $Pb(Zr,Ti)O_3$(PZT) based ceramics in various applications such as sensors, actuators and transducers. However, BNT-based ceramics have lower electromechanical performance as compared with PZT based ceramics. Therefore, in this work, lead-free bulk $0.99[(Bi_{0.5}Na_{0.5})_{0.935}Ba_{0.065}]_{(1-x)}La_xTiO_3-0.01SrZO_3$ (BNBTLax-SZ, with x = 0, 0.01, 0.02) ceramics were synthesized by a conventional solid state reaction The crystal structure, dielectric response, degree of diffuseness and electric-field-induced strain properties were investigated as a function of different La concentrations. All samples were crystallized into a single phase perovskite structure. The temperature dependent dielectric response of La-modified BNBT-SZ ceramics showed lower dielectric response and improved field-induced strain response. The field induced strain increased from 0.17%_for pure BNBT-SZ to 0.38 % for 1 mol.% La-modified BNBT-SZ ceramics at an applied electric field of 6 kV/mm. These results show that La-modified BNBT-SZ ceramic system is expected to be a new candidate material for lead-free electronic devices.

Effect of Excess CuO on the Sintering Behavior and Piezoelectric Properties of Bi0.5(Na0.82K0.18)0.5TiO3 Ceramics (Bi0.5(Na0.82K0.18)0.5TiO3 세라믹스의 소결거동 및 압전 특성에 대한 과잉의 CuO 첨가 효과)

  • Kang, Jin-Kyu;Jang, Hyun-Deok;Heo, Dae-Jun;Lee, Hyun-Young;Ahn, Kyoung-Kwan;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.6
    • /
    • pp.372-376
    • /
    • 2014
  • We investigated the effect of excess CuO on the sintering behavior, ferroelectric, and piezoelectric properties of lead-free $Bi_{0.5}(Na_{0.82}K_{0.18})_{0.5}TiO_3$ (BNKT) ceramics. The addition of excess CuO was found to greatly contribute to the densification and grain growth, however, excess CuO over 3 mol% was precipitated at grain boundaries after sintering. BNKT with 1~2 mol% CuO in excess sintered at $975^{\circ}C$ showed piezoelectric properties comparable to those of unmodified BNKT sintered at $1,175^{\circ}C$. These results seem meaningful for its application to low cost multilayer actuators (MLAs) because low firing ceramics make it possible to apply less expensive base metals to the inner electrode of MLAs.

Dielectric and Piezoelectric Characteristics of $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ Ceramics with the amount of $MnO_2$ addition ($MnO_2$ 첨가에 따른 $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Yoo, Ju-Hyun;Kim, In-Sung;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.172-173
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_3$-0.05Li$(Sb_{0.8}Nb_{0.2})O_3$ + $Ag_2O$ + x wt% $MnO_2$ were investigated as a function of the amount of $MnO_2$ addition in order to improve dielectric and piezoelectric properties of Lead-free piezoelectric ceramics. With increasing the amount of $MnO_2$ addition, density and electromechanical coupling factor $(k_p)$ increased up to 0.3wt.% $MnO_2$ and decreased above 0.3wt.% $MnO_2$. At the sintering temperature of 1020 $^{\circ}C$, Electromechanical coupling factor $(k_p)$, density, dielectric constant $({\varepsilon}r)$ and mechanical quality factor $(Q_m)$ of composition ceramics with 0.4wt% $Ag_2O$ addition showed the optimal value of 0.431, 4.33 g/$cm^3$, 820 and 119, respectively.

  • PDF