• Title/Summary/Keyword: layer deposition

Search Result 2,816, Processing Time 0.031 seconds

The stable e-beam deposition of metal layer and patterning on the PDMS substrate (PDMS 기판상에 금속층의 안정적 증착 및 패터닝)

  • Baek, Ju-Yeoul;Kwon, Gu-Han;Lee, Sang-Hoon
    • Journal of Sensor Science and Technology
    • /
    • v.14 no.6
    • /
    • pp.423-429
    • /
    • 2005
  • In this paper, we proposed the fabrication process of the stable e-beam evaporation and the patterning of metals layer on the polydimethylsiloxane (PDMS) substrate. The metal layer was deposited under the various deposition rate, and its effect to the electrical and mechanical properties (e.g.: adhesion-strength of metal layer) was investigated. The influence of surface roughness to the adhesion-strength was also examined via the tape test. Here, we varied the roughness by changing the reactive ion etching (RIE) duration. The electrode patterning was performed through the conventional photolithography and chemical etching process after e-beam deposition of $200{\AA}$ Ti and $1000{\AA}$ Au. As a result, the adhesion strength of metal layer on the PDMS surface was greatly improved by the oxygen plasma treatment. The e-beam evaporation on the PDMS surface is known to create the wavy topography. Here, we found that such wavy patterns do not effect to the electrical and mechanical properties. In conclusion, the metal patterns with minimum $20{\mu}m$ line width was produced well via the our fabrication process, and its electrical conductance was almost similar to the that of metal patterns on the silicon or glass substrates.

Electrodeposition of Copper on AZ91 Mg Alloy in Cyanide Solution

  • Nguyen, Van Phuong;Park, Min-Sik;Yim, Chang Dong;You, Bong Sun;Moon, Sungmo
    • Journal of Surface Science and Engineering
    • /
    • v.49 no.3
    • /
    • pp.238-244
    • /
    • 2016
  • Copper electrodeposition on AZ91 Mg alloy was studied in views of preferential deposition on ${\alpha}$- or ${\beta}$- phases and how to achieve uniform deposition over the entire surface on ${\alpha}$- and ${\beta}$-phases in a cyanide solution. The inhomogeneous microstructure of AZ91 Mg alloy, particularly ${\alpha}$- and ${\beta}$-phases, was found to result in non-uniform deposition of zincate layer, preferential deposition of zincate on ${\beta}$-phases, which leads to non-uniform growth of copper layer during the following electrodeposition process. The preferential depositions of zincate can be attributed to higher cathodic polarizations on the ${\beta}$-phases. Pin-hole defects in the copper electrodeposit were observed at the center of large size ${\beta}$-phase particles which is ascribed to gas bubbles formed at the ${\beta}$-phases. The activation of AZ91 Mg alloy in hydrofluoric acid solution was used to obtain uniform growth of zincate layer on both the ${\alpha}$- and ${\beta}$-phases. By choosing an optimum activation time, a uniform zincate layer was obtained on the AZ91 Mg alloy surface and thereby uniform growth of copper was obtained in a cyanide copper electroplating solution.

Effect of Metal Ni Atomic Layer Deposition Coating on Ni/YSZ, Anode of Solid Oxide Fuel Cells (SOFCs) (고체산화물 연료전지의 Anode인 Ni/YSZ에 Ni 원자층 증착 코팅의 효과)

  • Kim, Jun Ho;Mo, Su In;Park, Gwang Seon;Kim, Hyung Soon;Kim, Do Heyoung;Yun, Jeong Woo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.1
    • /
    • pp.61-66
    • /
    • 2022
  • This study is to increase the surface area and maximize the effect of the catalyst by coating a nanometersized metal catalyst material on the anode layer using atomic layer deposition (ALD) technology. ALD process is known to produce uniform films with well-controlled thickness at the atomic level on substrates. We measured the performance by coating metals (Ni) on Ni/YSZ, which is the most widely known anode material for solid oxide fuel cells. ALD coatings began to show a decrease in cell performance over 3 nm coatings.

Assessment Corrosion and Bioactive Behavior of Bioglass Coating on Co-Cr-Mo Alloy By Electrophoretic Deposition For Biomedical Applications

  • Areege K. Abed;Ali. M. Mustafa;Ali M. Resen
    • Corrosion Science and Technology
    • /
    • v.23 no.3
    • /
    • pp.179-194
    • /
    • 2024
  • A layer-by-layer coating was produced using electrophoretic deposition for a HA/Al2O3 coating layer and a bioglass coating layer on Co-Cr-Mo alloy with a roughness of 0.5 ㎛ (400 emery paper SiC). The corrosion behaviour was analyzed by assessing the coating layers' exceptional corrosion resistance, which outperformed the substrate. Cr ion release test using AAS was carried out, indicating that factional graded coating inhibited ion release from the uncoated substrate to coated sample. The porosity was expressed as a percentage, representing the extent of imperfections on the surface of all coatings. These imperfections fell within an acceptable range of 1% to 3%. The roughness of the coated surface was measured using atomic force microscopy, which revealed an excellent roughness value of 3.32 nm. Tape test technique for adhesion revealed that the removal area of the substrate coating layer varied by 11.92%. X-ray diffraction analysis confirmed the presence of all coating material peaks and verified phases of the deposited coating layers. These findings provided evidence that the coating composition remains unaffected by the electrophoretic deposition process. The bioactivity was assessed by immersion in a simulated bodily fluid, which revealed the formation of HCA during a period of 5 days.

The Organic-Inorganic Hybrid Encapsulation Layer of Aluminium Oxide and F-Alucone for Organic Light Emitting Diodes

  • Gwon, Deok-Hyeon;Seong, Myeong-Mo
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.374-374
    • /
    • 2012
  • Nowadays, Active Matrix Organic Light-Emitting Diodes (AM-OLEDs) are the superior display device due to their vivid full color, perfect video capability, light weight, low driving power, and potential flexibility. One of the advantages of AM-OLED over Liquid Crystal Display (LCD) lies in its flexibility. The potential flexibility of AM-OLED is not fully explored due to its sensitivity to moisture and oxygen which are readily present in atmosphere, and there are no flexible encapsulation layers available to protect these. Therefore, we come up with a new concept of Inorganic-Organic hybrid thin film as the encapsulation layer. Our Inorganic layer is Al2O3 and Organic layer is F-Alucone. We deposited these layers in vacuum state using Atomic Layer Deposition (ALD) and Molecular Layer Deposition (MLD) techniques. We found the results are comparable to commercial requirement of 10-6 g/m2 day for Water Vapor Transmission Rate (WVTR). Using ALD and MLD, we can control the exact thin film thickness and fabricate more dense films than chemical or physical vapor deposition methods. Moreover, this hybrid encapsulation layer potentially has both the flexibility of organic layers and superior protection properties of inorganic layer.

  • PDF

Characteristics of Thin Films Fabricated by Using the Layer-by-Layer Sputtering and Evaporation Method (순차 스퍼터 법과 증발 법으로 제작한 박막의 특성)

  • Cheon, Min-Woo;Park, Yong-Pil;Kim, Jeong-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.571-574
    • /
    • 2003
  • The thin films fabricated by using the layer-by-layer sputtering was compared with the thin film fabricated by using the evaporation method. Re-evaporation in the form of Bi atoms or $Bi_2O_3$ molecules easily bring out the deficiency of Bi atoms in thin film due to the long sputtering time of the layer-by-layer deposition. On the other hand, the respective atom numbers corresponding to BiSrCaCuO phase is concurrently supplied on the film surface in the evaporation deposition process and leads to BiSrCaCuO phase formation. Also, it is cofirmed that by optimizing the deposition condition, each single phase of the Bi2201 phase and the Bi2212 phase can be fabricated, the sticking coefficient of Bi element is clearly related to the changing of substrate temperature and the formation of the Bi2212 phase.

  • PDF

Effect of Structure Change in Second-Generation Superconducting Wire Stabilization Layer on Resistivity Characteristics (2세대 초전도 선 안정화 층 구조변화가 비저항 특성에 미치는 영향)

  • Ban, Sang-Jae;Du, Ho-Ik;Jeong, Hyun-Gi;Doo, Seung-Gyu;Yang, Sung-Chae
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.2
    • /
    • pp.172-177
    • /
    • 2022
  • The quench voltage of the second-generation superconducting wire is affected by the resistivity characteristics of the stabilization layer. The specific resistance of the stabilization layer can be changed by the deposition process using RF magnetron sputtering. In this paper, a thin film made of a homogeneous material (Ag) and a dissimilar material (Cu) was deposited on the stabilization layer of the second-generation superconducting wire through RF magnetron sputtering. We found that the specific resistance was reduced by increasing the thickness of the stabilization layer. The reduction in the resistivity of the stabilization layer led to a decrease in the quench voltage of the second-generation superconducting wire. We suggest that various characteristic changes of the second-generation superconducting wire can be expected through the successful change in the resistivity of the stabilization layer of the proposed deposition process.

Optimizing the Plasma Deposition Process Parameters of Antistiction Layers Using a DOE (Design of Experiment) (실험 계획법을 이용한 점착방지막용 플라즈마 증착 공정변수의 최적화 연구)

  • Cha Nam-Goo;Park Chang-Hwa;Cho Min-Soo;Park Jin-Goo;Jeong Jun-Ho;Lee Eung-Sug
    • Korean Journal of Materials Research
    • /
    • v.15 no.11
    • /
    • pp.705-710
    • /
    • 2005
  • NIL (nanoimprint lithography) technique has demonstrated a high potential for wafer size definition of nanometer as well as micrometer size patterns. During the replication process by NIL, the stiction between the stamp and the polymer is one of major problems. This stiction problem is moi·e important in small sized patterns. An antistiction layer prevents this stiction ana insures a clean demolding process. In this paper, we were using a TCP (transfer coupled plasma) equipment and $C_4F_8$ as a precursor to make a Teflon-like antistiction layer. This antistiction layer was deposited on a 6 inch silicon wafer to have nanometer scale thicknesses. The thickness of deposited antistiction layer was measured by ellipsometry. To optimize the process factor such as table height (TH), substrate temperature (ST), working pressure (WP) and plasma power (PP), we were using a design of experimental (DOE) method. The table of full factorial arrays was set by the 4 factors and 2 levels. Using this table, experiments were organized to achieve 2 responses such as deposition rate and non-uniformity. It was investigated that the main effects and interaction effects between parameters. Deposition rate was in proportion to table height, working pressure and plasma power. Non-uniformity was in proportion to substrate temperature and working pressure. Using a response optimization, we were able to get the optimized deposition condition at desired deposition rate and an experimental deposition rate showed similar results.

Optical and electrical property of Indium-doped ZnO (IZO) grown by Atomic Layer Deposition (ALD) using Et2InN(TMS)2 as In precursor and H2O oxidant

  • Jo, Yeong-Jun;Jang, Hyo-Sik
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.421.1-421.1
    • /
    • 2016
  • We studied indium-doped zinc oxide (IZO) film grown by atomic layer deposition (ALD) as transparent conductive oxide (TCO). A variety of TCO layer, such as ZnO:Al (AZO), InSnO2(ITO), Zn (O,S) etc, has been grown by various method, such as ALD, chemical vapor deposition (CVD), sputtering, laser ablation, sol-gel technique, etc. Among many deposition methods, ALD has various advantages such as uniformity of film thickness, film composition, conformality, and low temperature deposition, as compared with other techniques. In this study, we deposited indium-doped zinc oxide thin films using diethyl[bis(trimethylsilyl)amido]indium [Et2InN(TMS)2] as indium precursor, DEZn as zinc precursor and H2O as oxidant for ALD and investigated the optical and electrical properties of IZO films. As an alternative, this liquid In precursor would has several advantages in indium oxide thin-film processes by ALD, especially for low resistance indium oxide thin film and high deposition rate as compared to InCp, InCl3, TMIn precursors etc. We found out that Indium oxide films grown by Et2InN(TMS)2 and H2O precursor show ALD growth mode and ALD growth window. We also found out the different growth rate of Indium oxide as the substrate and investigated the effect of the substrate on Indium oxide growth.

  • PDF

HIGH-THROUGHPUT PROCESS FOR ATOMIC LAYER DEPOSITION

  • Shin, Woong-Chul;Choi, Kyu-Jeong;Baek, Min;Kim, Mi-Ry
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2009.11a
    • /
    • pp.23.2-23.2
    • /
    • 2009
  • Atomic layer deposition (ALD)have been proven to be a very attractive technique for the fabrication of advanced gate dielectrics and DRAM insulators due to excellent conformality and precise control of film thickness and composition, However, one major disadvantages of ALD is its relatively low deposition rate (throughput) because the deposition rate is typically limited by the time required for purging process between the introduction of precursors. In order to improve its throughput, many efforts have been made by commercial companies, for example,the modification reactor and development of precursors. However, any promising solution has not reported to date. We developed a new concept ALD system(Lucida TM S200) with high-throughput. In this process, a continuous flow of ALD precursor and purging gas are simultaneously introduced from different locations in the ALD reactor. A cyclic ALD process is carried out by moving the wafer holder up and down. Therefore, the time required for ALD reaction cycle is determined by speed of the wafer holder and vapor pressure of precursors. We will present the operating principle of our system and results of deposition.

  • PDF