The surface of nano-kenaf containing cellulose fibers was treated with alkali (NaOH) and their effects on the physical properties of the polypropylene (PP) composite were investigated. The treatment of alkali on the fibers increased the melt flow index (M.I.), elongation%, and impact strength, while it decreased the tensile strength, flexural modulus and heat deflection temperature (HDT) of the compound compared to the untreated one. It seemed the alkali treatment on the nano-kenaf fiber changed the character of the fiber due to removal of impurities and chemicals on the surface and resulted in decreased interfacial adhesion between the nano-fiber surface and the PP matrix and changed the character of the PP.
Au/PDMS membranes are widely used to fabricate strain sensors which can detect input signals. An interfacial adhesion between metal films and polydimethylsiloxane (PDMS) substrates is one of the important factors determining the performance of strain sensors, in terms of robustness, reliability, and sensitivity. Here, we fabricate Au/PDMS membranes with (3-mercaptopropyl) trimethoxysilane (MPTMS) treatment. PDMS membranes were fabricated by spin-coating and the thickness was controlled by varying the spin rates. Au electrodes were deposited on the PDMS membrane by metal sputtering and the thickness was controlled by varying sputtering time. Owing to the MPTMS treatment, the interfacial adhesion between the Au electrode and the PDMS membrane was strengthened and the membrane was highly transparent. The Au electrode, fabricated with a sputtering time of 50 s, had the highest gauge factor at a maximum strain of ~0.7%, and the Au electrode fabricated with a sputtering time of 60 s had the maximum strain range among sputtering times of 50, 60, and 120 s. Our technique of using Au/PDMS with MPTMS treatment could be applied to the fabrication of strain sensors.
Kim, Hong-Un;Bang, Yun-Hyuk;Choi, Soo-Myung;Lim, Kyung-Hee
Journal of the Korean Applied Science and Technology
/
v.23
no.4
/
pp.290-299
/
2006
This article investigated to polymer-clay nanocomposite, especially in interfacial respect clay structure, its dispersion into polymer matrix, and clay modification is studied. The cationic exchange of surfactants with clay gallery results in preparing organo-clay capable of compatiblizing to monomer or polymer and increasing interlayer adhesion energy due to expansion of interlayer spacing. The orientation of surfactant in clay gallery is affected by chemical structure and charge density of clay, and interlayer spacing and volume is increased with alkyl chain length of surfactant, or charge density of clay. Also, the interaction between clay and polymer in preparing polymer-clay nanocomposite is explained thermodynamically. In the future, the study and development of polymer-clay nanocomposite is paid attention to the interfacial adhesion, clay dispersion within polymer, mechanism of clay intercalation or exfoliation.
In this study, wasted stone powders (WSP) obtained from sludge and Wasted Tire Chips (WTC) as fillers have been used to formulate polymer hybrid composites based on Unsaturated Polyester (UPE) resin. To further enhance not only the interfacial bond between the inorganic filler and the polymer matrix, but also the filler dispersion by wetting the particulate surfaces to uniformly spread the resin during the mixing, silane coupling agent[${\gamma}$-methacryloxy propyl trimethoxy silane (${\gamma}$-MPS)] was used. The influences of organic recycled fillers contents and the concentrations of coupling agent in polymer hybrid composite formulations have been investigated from a mechanical and microstructural point o view through Mercury Porosimeter and SEM.
In this work, an Ar+ beam was irradiated on carbon fiber surfaces to improve the interfacial shear strength (IFSS) of the resulting composites using an ion assisted reaction (IAR) method h single fiber pull-out test was executed to investigate the basic characteristics of the single Carbon fiber/matrix interface. Based on Greszczuk's geometrical model, the debonding force for pull-out of the fiber from the resins was discussed with the applied ion beam energy as a result, it was known that an ion beam treatment produced the functional groups on fiber surface and etching lines along the fiber axis direction, resulting in increasing the adhesion forces between fibers and matrix, which caused the improvement of the IFSS in a composite system. And, it was also found that the maximum IFSS was shown at 0.8 keV ion beam energy in this system.
Among the next-generation solar cells, organic solar cells using organic materials are a key energy production device for the future energy generation devices, and have recently been receiving a lot of attention with rapid growth. To improve the efficiency of organic solar cells, interfacial engineering technology has been widely applied. In particular, it is widely used to improve device efficiency through energy level control by using interface engineering on the anode and cathode, which are positive electrodes, and to ultimately utilize interface engineering for tandem organic solar cells to derive excellent electrical and optical performance to produce high-performance devices. In this article, we will summarize and introduce recent research trends on interfacial engineering used in organic solar cells, and discuss the method of manufacturing high-performance organic solar cells.
In this study, the Johnson-Kendall-Roberts (JKR) theory was combined with the instrumented indentation technique (IIT) to evaluate work of adhesion and modulus of elastomeric polymer. Indentation test was used to obtain the load-displacement data for contacts between Tungsten Carbide indenter and elastomeric polymer. And the JKR contact model, contrived to take viscoelastic effects of polymer into account, was applied to compensate the contact area and the elastic modulus which Hertzian contact model would underestimate and overestimate, respectively. Besides, we could obtain the thermodynamic work of adhesion by considering the surface energy in this contact model. In order to define the relation between JKR contact area and applied load without optical measuring of contact area, we used the relation between applied load and contact stiffness by examining the correlation between JKR contact area and stiffness through dimensional analysis with 14 kinds of elastomeric polymer. From this work, it could be demonstrated that the interfacial work of adhesion and elastic modulus of compliant polymer can be obtained from a simple instrumented indentation testing without area measurement, and provided as the main algorithm of compliant polymer characterization.
A copper based leadframe was oxidized in brown-oxide forming solution, then the growth characteristics of brown oxide and the effect of brown-oxide formation on the adhesion strength of leadframe to epoxy molding compound (EMC) were studied by using sandwiched double cantilever beam (SDCB) specimens. The brown oxide is composed of fine acicular CuO, and its thickness increased up to ~150 nm within 2 minutes and saturated. Bare leadframe showed alomost no adhesion to EMC, while once the brown-oxide layer formed on the Surface of leadframe, the adhesion strength increased up to ~80 J/$\m^2$ within 2 minutes. Correlation between oxide thickness, $\delta$ and the adhesion strength in terms of interfacial fracture toughness, $G_{c}$ was linear. Considering the above results, we might conclude that the main adhesion mechanism of brown-oxide treated leadframe to EMC is mechanical interlocking, in which fine acicular CuO plays a major role.e.
Kim, Gahui;Lee, Jina;Park, Se-hoon;Park, Young-Bae
Journal of the Microelectronics and Packaging Society
/
v.27
no.1
/
pp.37-43
/
2020
The effects of O2 plasma pre-treatment and post-annealing conditions on the interfacial adhesion of Ti thin film and WPR dielectric were investigated using 90° peel test for fan-out wafer level packaging (FOWLP) redistribution layer (RDL) applications. Peel strength between Ti film and WPR dielectric decreased from 8.9±1.3 g/mm to 2.7±0.9 g/mm for variation of O2 plasma pre-treatment time from 30s to 300s, which is closely related to C-O-C or C=O bonds breakage at the WPR dielectric surface due to excessive plasma pre-treatment conditions. During post-annealing at 150℃, the peel strength abruptly decreased from 0 h to 24 h, and then maintained constant until 100 h, which is also mainly due to the damage of WPR dielectric which is weak to high temperature. Therefore, the optimum plasma pre-treatment conditions on the surface of dielectric is essential to interfacial reliability of FOWLP RDL.
Kim, Dong-Kyu;Kim, Kwan-Woo;Han, Woong;Song, Bhumkeun;Oh, Sang-Yub;Bang, Yun Hyuk;Kim, Byung-Joo
Applied Chemistry for Engineering
/
v.27
no.5
/
pp.472-477
/
2016
We studied the effects of anodic oxidation treatments of carbon fibers on interfacial adhesion of the carbon fibers-reinforced epoxy matrix composites with various current densities. The surface of treated carbon fibers was characterized by atomic force microscope (AFM), field emission-scanning electron microscope (FE-SEM), Fourier transform infrared spectroscopy (FT-IR), and X-ray photoelectron spectroscopy (XPS). The interlaminar shear strength (ILSS) of the composites was determined by a short beam shear test. This result showed that both the roughness and oxygen group of the carbon fibers surface increased in proportion to the current density. After anodic-oxidation-treated, the ILSS also increased as a function of the current density. In addition, the proportional relationship between ILSS and phenolic hydroxyl group was confirmed. The ILSS of the CF-2.0 sample increased by 4% compared to that of the CF-AS sample, because the anodic oxidation treatment increased the oxygen group and roughness on the carbon fibers surface, which leading to the improvement of the interfacial adhesion of the carbon fibers-reinforced epoxy matrix composites. Among these, the phenolic hydroxyl group which has the proportional relationship with ILSS is found to be the most important factor for improving the interfacial adhesion of the carbon fibers-reinforced epoxy matrix composites.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.