• 제목/요약/키워드: hydroxyapatite (HAP)

검색결과 147건 처리시간 0.026초

Nano-Hydroxyapatite Modified by Grafting Polylactide and its Tissue Engineering Application

  • Zhuang, Xiuli;Zhang, Peibiao;Qiu, Xueyu;Chen, Xuesi;Jing, Xiabin
    • 한국고분자학회:학술대회논문집
    • /
    • 한국고분자학회 2006년도 IUPAC International Symposium on Advanced Polymers for Emerging Technologies
    • /
    • pp.182-182
    • /
    • 2006
  • PLLA grafted Hydroxyapatite / polylactide (g-HA/PLA) composites were prepared by three grafting methods. The modified particles (p-HA) were dispersed more uniformly in the PLLA matrix than pure n-HA. The p-HA/PLLA composites exhibited better mechanical properties and thermal stability than the n-HA/PLLA composites. The composites also demonstrated improved cell compatibility due to the good biocompatibility of the HAP nanoparticles and the more uniform distribution of the PLLA-grafted HAP nanoparticles on the film surface. All of these results indicated that the p-HAP/PLLA nano-composites might have a promising medical application in bone repair and in bone tissue-engineering.

  • PDF

dPAO SBR 입상슬러지의 형태학적 특성 (Morphological Characteristics of Granular Sludge in dPAO SBR)

  • 유태욱;이한샘;윤금희;윤주환
    • 한국물환경학회지
    • /
    • 제29권4호
    • /
    • pp.497-503
    • /
    • 2013
  • The morphological characteristics of granules, which were generated in lab-scale sequencing batch reactor (SBR) for simultaneous nitrogen and phosphorus removal with denitrifying phosphorus accumulating organism (dPAO) were identified. Granular sludge was fully developed in the anaerobic-anoxic (An-Ax) SBR after 180 days of SBR operation. The average diameter of granular sludge was 2.2 mm and rod-type organisms dominated in the granules. In addition, about 1.0 mm of white precipitate was observed in the core of the granule, and the material was confirmed that it is very similar to hydroxyapatite $(HAP;\;Ca_5(PO_4)_3(OH))$ by X-ray diffraction) analysis.

생물학적 축산분뇨처리시설에서 인 회수의 가능성 평가 (Feasibility of Phosphorus Recovery from Biological Livestock Wastewater Treatment Plant)

  • 안조환;김장호;민성재
    • 한국물환경학회지
    • /
    • 제32권4호
    • /
    • pp.343-348
    • /
    • 2016
  • A chemical sequencing batch reactor was operated to test the feasibility of nutrient recovery from a biological livestock wastewater treatment plant. Both phosphate and ammonia could be successfully recovered as magnesium ammonium phosphate (MAP) crystals. The contents of TP and TN in the recovered MAP crystals were 26.2% and 4.0%, respectively. Zn, Cr and Ti were identified in the crystals, but the contents remained below the Korean standard for an organic fertilizer. Chemical analyses confirmed that the MAP crystals could be useful phosphate fertilizers. On the other hand, the results of physical analyses using an X-ray diffractometer and an energy dispersive X-ray spectrometer strongly suggested that crystalline materials like magnesium potassium phosphate (KMP) and hydroxyapatite (HAP) were also formed during the MAP crystallization, depending on the availability of K+ and Ca2+.

Synthesis and Sinterability of Hydroxyapatite from Fishery by-products

  • Wibisono, Yusuf;Dwijaksara, Ni Luh Bella;Widayatno, Wahyu Bambang;Wismogroho, Agus Sukarto;Amal, Muhamad Ikhlasul;Rochman, Nurul Taufiqu;Nishimura, Toshiyuki;Noviyanto, Alfian
    • 한국세라믹학회지
    • /
    • 제55권6호
    • /
    • pp.570-575
    • /
    • 2018
  • Hydroxyapatites (HAps) were synthesized using the powdered waste of fishery products, i.e., fish scales and crab shells, as starting materials. HAp was synthesized by a wet-chemistry method followed by calcination at 600 and $800^{\circ}C$. Calcined crabshell powder revealed a single HAp phase and fine powder, while calcined fish-scale powder showed a ${\beta}-TCP$ secondary phase, even at the higher calcination temperature. Dense HAp pellets were obtained from the crab-shell powder by spark plasma sintering at $1000^{\circ}C$ for 10 min under applied pressures of 40 and 80 MPa in a vacuum state, giving sample densities of 2.93 and $3.06g/cm^3$, respectively. The estimated grain size of HAp was $448{\pm}96$ and $283{\pm}59nm$ for applied pressures of 40 and 80 MPa, respectively. In contrast, the HAp obtained using the pressureless sintering technique showed excessive grain growth without further densification.

석회계 입상알칼리재의 용출특성과 이를 이용한 인 결정화공정의 적용성 (Elution characteristics of lime-based granular alkaline material and applicability of phosphorus crystallization processes)

  • 장향연;박나리;장여주;안광호;임현만;김원재
    • 상하수도학회지
    • /
    • 제31권6호
    • /
    • pp.577-586
    • /
    • 2017
  • One of the major sources causing eutrophication and algal blooms of lakes or streams is phosphorus which comes from point and nonpoint pollution sources. HAP (hydroxyapatite) crystallization using granular alkaline materials can achieve the decrease of phosphorus load from wastewater treatment plants and nonpoint pollution control facilities. In order to induce HAP crystal formation, continuous supply of calcium and hydroxyl ions is required. In this research, considering HAP crystallization, several types of lime-based granular alkaline materials were prepared, and the elution characteristics of calcium and hydroxyl ions of each were analyzed. Also, column tests were performed to verify phosphorus removal efficiencies of granular alkaline materials. Material_1 (gypsum+cement mixed material) achieved the highest pH values in the column tests consistently, also, Material_2 (gypsum+slag mixed material) and Material_3 (calcined limestone material) achieved over pH 9.0 for 240 hours (10 days) and proved the efficiencies of long-term ion supplier for HAP crystallization. In the column tests using Material_3, considerable pH increase and phosphorus removal were carried out according to each linear velocity and filtration depth. T-P removal efficiencies were 87.0, 84.0, 68.0% and those of PO4-P 100.0, 97.0, 80.0% for linear velocity of 1.0, 2.5, 5.0 m/hr respectively. Based on the column test results, the applicability of phosphorus removal processes for small-scale wastewater treatment plants and nonpoint pollution control facilities was found out.

혼합물분석을 통해 최적화된 TiO2/HAP/Ge 촉매를 이용한 Lincomycin 제거특성 연구 (A Study on Characteristics of Lincomycin Degradation by Optimized TiO2/HAP/Ge Composite using Mixture Analysis)

  • 김동우;장순웅
    • 한국지반환경공학회 논문집
    • /
    • 제15권1호
    • /
    • pp.63-68
    • /
    • 2014
  • 본 연구에서는 UV-A 조사를 통해 titanium dioxide($TiO_2$), hydroxyapatite(HAP)와 germanium(Ge)의 다양한 복합촉매를 통한 항생제(lincomycin, LM)의 광촉매 제거를 조사하였다. 우선, 다양한 복합촉매의 향상된 광촉매능을 비교하였고, 도출된 제거효율은 $TiO_2/HAP/Ge$ > $TiO_2/Ge$ > $TiO_2/HAP$ 순으로 관찰되었다. $TiO_2/HAP/Ge$의 조성은 반응표면법의 하나인 혼합물분석(mixture analysis)에 기초하여 통계적 방안이 수행되었다. 각 인자별 6개의 조건을 포함하도록 설정한 독립변수 $TiO_2(X_1)$, HAP($X_2$)와 Ge($X_3$)의 LM($Y_1$)과 TOC($Y_2$) 제거에 대한 영향을 살펴보았다. 분산분석(ANOVA)의 회귀분석항은 유의한 p값(p<0.05)과 높은 결정계수 값($R^2$ of $Y_1=99.28%$ and $R^2$ of $Y_2=98.91%$)을 나타냈다. 등고선도와 반응곡선을 통해 UV-A 조사조건에서 $TiO_2$/HAP/Ge 조성에 따른 LM의 제거를 나타냈다. TOC($Y_2$) 제거를 기준으로 도출된 최적조성비는 코드화 값으로 $X_1=0.6913$, $X_2=0.2313$$X_3=0.0756$으로 나타났다. 실제 적용에 따른 비교 실험 결과는 LM과 TOC의 평균제거율이 각각 99.2%와 49.3%로 나타나 모델의 예측과 잘 부합하였다.

마이크로파-수열 합성법을 이용한 나노 수산화아파타이트 합성과 특성평가 (Characterization and Synthesis of Nano-Sized Hydroxyapatite Powder by Microwave-Hydrothermal Method)

  • 한재길;이치우;이병택
    • 한국세라믹학회지
    • /
    • 제43권2호
    • /
    • pp.126-130
    • /
    • 2006
  • Nano-sized hydroxyapatite (HAp) powders were synthesized by a microwave-hydrothermal method using $H_3PO_4\;and\;Ca(OH)_2$ as starting materials. The applied microwave powers and mole ratio of Ca/P were served as powerful factors in the synthesis of calcium phosphate. In the case of relatively low microwave power of 450 Wand Ca/P ratio of 1.57, the mixed calcium phosphate compounds were detected in the synthesized powders. But in the case of running at 550 Wand 1.67(Ca/P), the synthesized powder showed the monophase of HAp having two kinds of morphologies. One was a needle shape with $5\~15\;nm$ in width and $20\~50\;nm$ in length, and the other was a spherical shape of $10\~40\;nm$ in diameter.

Development of Multi-sample Loading Device for TEM Characterization of Hydroxyapatite Nanopowder

  • Lee, Jong-Moon;Kim, Jung-Kyun;Jeong, Jong-Man;Kim, Jin-Gyu;Lee, Eunji;Kim, Youn-Joong
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권3호
    • /
    • pp.788-792
    • /
    • 2013
  • A shortcoming of using transmission electron microscopy (TEM) for structural analysis via electron diffraction is the relatively large error of the measurements as compared to X-ray diffraction. To reduce these errors, various internal standard methods from earlier studies have been widely used. We developed a new device to facilitate the application of internal standard methods in preparation of TEM grids used for nanopowder analysis. Through the application of a partial mask on the TEM grid, both the internal standards and the research materials can be loaded on the same grid. Through this process, we conducted a TEM analysis that compared synthetic hydroxyapatite (HAp) nanopowder to bone apatite from a bovine femur. We determined that the accuracy of the d-spacing measurements of the HAp and bone powders could be improved to better than 1% after statistical treatments of the experimental data. By applying a quarter mask, we loaded four different nanoparticles on a single TEM grid, with one section designated for the internal standard.

미세기공함유 유리의 제조 및 특성 (Preperation and Properties of Fine Porous Glass)

  • 채수진;박만규;강원호
    • 한국산학기술학회논문지
    • /
    • 제10권3호
    • /
    • pp.476-481
    • /
    • 2009
  • 판유리 폐기물과 hydroxyapatite를 사용하여 미세기공 함유 다공성유리를 제조하여 미세기공의 형태와 기계적 강도를 평가하였다. 발포제의 함량은 7%이상 함유시 기공이 조대하여지고 불균질하게 형성되었으며, $3{\sim}5%$ 함유시 발포 열처리온도 $830{\sim}840^{\circ}C$에서 $10{\mu}m$전후의 균일한 기공크기를 생성하였다. 기공성유리의 압축강도 및 곡강도는 각각 $18kg/cm^2$, $8kg/cm^2$를 나타내었다.

Hydroxyapatite 소결체의 가소제 첨가에 따른 특성 (Properties of hydroxyapatite sintered body added with plasticizer)

  • 류수착;김재규;김승현
    • 한국결정성장학회지
    • /
    • 제29권4호
    • /
    • pp.167-172
    • /
    • 2019
  • HAp의 성형성과 열처리를 용이하게 하는 유기가소제를 사용하여 첨가량에 따른 강도(MPa)와 경도(Hv), 수축율(%) 및 생물학적 특성 중 항균력을 측정하였다. 가소제의 첨가량이 증가할수록 기계적 특성인 압축강도와 굽힘강도, 경도 등이 증가하였으나 가소제의 첨가량이 7%를 넘을 경우 오히려 기계적 특성이 감소하였다. 이는 허용치 이상의 가소제의 첨가는 성형 시 균열을 발생시키고 이러한 균열은 소결 시 내부에 미세균열 및 산화 시 기공의 발생을 촉진시켜 기계적 특성의 감소를 유발한다. 항균성 측정 결과 가소제 첨가량 에 관계없이 균은 검출되지 않았으며 우수한 항균력을 발휘하였다.