CuAlNi 형상기억합금의 결정립 미세화에 따른 시효효과 (The Effect of Ageing on Grain Refinement of CuAlNi Shape Memory Alloy)

  • 양권승;박창선;장우양
    • 열처리공학회지
    • /
    • 제8권1호
    • /
    • pp.65-74
    • /
    • 1995
  • This research was performed to investigate the effect of ageing on grain refinement of 82wt%Cu-13.5wt%Al-4.5wt%Ni-0.1wt% misch metal alloy with ageing temperature and time. The results obtained in this study are as follows; The variation of transformation temperature with ageing temperature had very influence on ageing time at $300^{\circ}C$. But it had not influence on ageing time at $100^{\circ}C$. The variation of transformation temperature after second reversed transformation cycle was not occured in martensitic phase ageing, but $M_s$ point was appeared equally with third reversed transformation cycle in parent phase ageing. The variation of $M_s$ point was not nearly with ageing time at $100^{\circ}C$ ageing temperature. But it was decreasing with ageing time at $300^{\circ}C$ ageing temperature and $A_s$ point was increasing with ageing time. Structure of parent phase ageing was being M18R martensitic and N2H martensitic phase. It was found that ${\alpha}$ and ${\gamma}_2$ phase were created by ageing of long time at $300^{\circ}C$ ageing temperature.

  • PDF

ECAP 강가공에 의한 마그네슘 AZ31합금의 결정립 미세화 및 미세조직 불안정성 (Grain Refinement and Microstructural Instability of an AZ31 Mg Alloy by Severe Plastic Deformation Using ECA Pressing)

  • 김호경;정강;현창용
    • 열처리공학회지
    • /
    • 제17권3호
    • /
    • pp.139-145
    • /
    • 2004
  • Equal channel angular pressing (ECAP) technique had been adapted to the Mg alloy (AZ31) for achieving effective grain refinement through severe deformation. The average grain size of $2.5{\mu}m$ could be obtained after 4 passes. The stability of the ECAPed structure at elevated temperatures was examined by annealing the ECAPed materials over a wide range of temperature between 473 and 748 K. The average activation energy, Q, for static grain growth of 1, 2 and 3 passes was 33.7 kJ/mole (=0.25QL, activation for lattice diffusion). The abnormally low Q value in the lower temperature range may indicate that grain growth occurs in the unrecrystallized microstructure where non-equilibrium grain boundaries containing a large number of extrinsic dislocations exist. The yield stresses of the ECAPed alloys decreased whereas the elongations increased after the ECAP process. These results should be related to the modification of texture for easier slip on basal plane.

Structural Characterization of the (TEX)$Sr_2Co_0.5Nb(Ta)_0.5O_4$(/TEX) and (TEX)$Sr_3CoNb(Ta)O_7$(/TEX)

  • 조한상;;류광현;유철현
    • Bulletin of the Korean Chemical Society
    • /
    • 제21권7호
    • /
    • pp.679-684
    • /
    • 2000
  • The Sr2Co0.5Nb(Ta)0.5O4 and Sr3CoNb(Ta)O7 compounds, both with Ruddlesden-Popper structures, have been synthesized by the ceramic method at $1150^{\circ}C$ under atmospheric pressure. The crystallographic structure of the compounds was assigned to the tetr agonal system with space group 14/mmm by X-ray diffraction(XRD) Rietveld refinement. The reduced lattice volume and lattice parameters increased as the Ta with 5d substitutes for the Nb with 4d in the compounds. The Co/Nb(Ta)O bond length has been determined by X-ray absorption spectroscopic(EXAFS/XANES) analysis and the XRD refinement. The CoO6,octahedra were tetragonally distorted by elongation of Co-O bond along the c-axis. The magnetic measurement shows the compounds Sr2Co0.5Nb(Ta)0.5O4 and Sr3CoNb(Ta)O7 have paramagnetic properties and the Co ions with intermediate spin sates between high and low spins in D4h symmetry. All the compounds showed semiconducting behavior whose electrical conductivity increased with temperature up to 1000 K. The electrical conductiviy increased and the activation energy for the conduction decreased as the number of perovskite layers increased in the compounds with chemical formula An+1BnO3n+1.

SUS304합금의 마찰접합특성 평가 (Evaluation of the Friction Welding Properties on SUS304 Alloy)

  • 김영규;송국현;정준기;하태권
    • 소성∙가공
    • /
    • 제33권3호
    • /
    • pp.193-199
    • /
    • 2024
  • The friction welding characteristics of stainless steels, mainly used in energy and chemical plant industries due to its excellent corrosion resistance and high strength, was evaluated in this study. Friction welding was introduced and conducted at a rotation speed of 2,000 RPM, friction pressure of 30 MPa, burn-off length of 5 mm and upset pressure of 110 ~ 200 MPa on rod typed specimens. The grain boundary characteristics distributions such a grain size, shape, misorientation angle and kernel average misorientation of the welds were clarified by electron backscattering diffraction method. The application of friction welding on SUS304 alloy resulted in a significant refinement of the grain size in the weld zone (5.11 mm) compared to that of the base material (48.09 mm). The mechanical properties of the welds, on the other hand, appeared to be relatively low or similar to those of the base material, which were mainly caused by dislocation density in the initial material and grain refinement in the welds.

ZnO와 PbO가 Sr-페라이트의 자기적 특성에 미치는 영향 (Effects of ZnO and PbO on the Magnetic Properties of Sr-ferrite)

  • 김정훈;김동엽;김동진;정완배;오재현
    • 한국세라믹학회지
    • /
    • 제28권6호
    • /
    • pp.471-477
    • /
    • 1991
  • Effects of ZnO, PbO and SiO2 on the grain growth and magnetic properties of Sr-ferrite were investigated. (1) Addition of ZnO to Sr-ferrite increased remanence, but decreased coercivity and maximum energy product. (2) Addition of PbO up to 0.5 wt% increased (B$.$H)max of Sr-ferrite, but addition more than 0.5 wt% decreased (B$.$H)mzx (3) SiO2 addition to the 0.5 wt% PbO doped Sr-ferrite decreased remanence and increased coercivity. The coercivity increase in due to the grain refinement effect of SiO2. But addition of SiO2 more than 0.5 wt% invoked a decrease of coercivity and (B$.$H)max of Sr-ferrite due to abnormal grain growth. Sr-ferrite magnet having maximum energy product of 3.7MGOe was fabricated by using the roasting product of Pyrrhotite.

  • PDF

LOCAL CONVERGENCE OF THE SECANT METHOD UPPER $H{\ddot{O}}LDER$ CONTINUOUS DIVIDED DIFFERENCES

  • Argyros, Ioannis K.
    • East Asian mathematical journal
    • /
    • 제24권1호
    • /
    • pp.21-25
    • /
    • 2008
  • The semilocal convergence of the secant method under $H{\ddot{o}}lder$ continuous divided differences in a Banach space setting for solving nonlinear equations has been examined by us in [3]. The local convergence was recently examined in [4]. Motivated by optimization considerations and using the same hypotheses but more precise estimates than in [4] we provide a local convergence analysis with the following advantages: larger radius of convergence and finer error estimates on the distances involved. The results can be used for projection methods, to develop the cheapest possible mesh refinement strategies and to solve equations involving autonomous differential equations [1], [4], [7], [8].

  • PDF

용해도 차이를 이용한 질산망간 용액의 정제 (Refinement of the manganese nitrate solution prepared by leaching the reduced Ferromanganeses dust with nitric acid.)

  • 조영근;송영준;이계승;신강호;김형석;김윤채;조동성
    • 자원리싸이클링
    • /
    • 제12권1호
    • /
    • pp.33-40
    • /
    • 2003
  • 약 90%의 $Mn_3$$O_4$를 함유하는 고탄소폐로망간을 중저탄소폐로망간으로 제조하는 과정의 bag filter에 채집된 분진에는 소량의 Na, K, Fe, Si, Ca, Mg등의 불순물이 함유된다. 환원배소로 망간을 MnO의 상태로 만든 분진을 질산으로 침출하여 고농도 망간 침출액을 조제하고, 조제된 침출액에서 불순물을 제거하기 위한 기초실험을 하였다. 침출액중의 철 성분은 침출액의 pH를 4 이상으로 하여 수산화철 침전을 생성시킨 다음 여과에 의해 제거하므로써 여액 내의 잔류농도가 수ppm 이하가 되도록 하였고, 이 때 규소성분도 수산화철과 함께 공침시켜 10ppm 이하로 제거하였다. 4N의 질산을 사용하는 경우 질산 $1ell$ 대하여 환원된 분진 150g을 첨가하면 침출액의 pH가 4이상으로 되어 철과 규소 성분이 제거된 Mn농도가 약 10%인 침출액을 조제 할 수 있었다. 그리고 Ca 와 Mg를 옥살산염 형태로 침전시켜 제거할 목적으로 수행한 단일 옥살산염 수용액에서의 Mn과 Ca, Mg의 용해 및 침전 특성 조사에서는 수용액의 온도가 높을수록 반응속도가 빨라져 Mg의 제거에 유리하며, pH가 낮을수록 고농도의 Mn용액을 얻을 수 있으며 이 때 용액내의 Ca/Mn 및 Mg/Mn은 pH에 관계없이 일정하였다.

$Re(≡NC_6H_5)(DPPE)CI_3$화합물의 합성 및 구조 (Preparation and Structure of $Re(≡NC_6H_5)(DPPE)CI_3$, $[DPPE=Ph_2PCH_2CH_2PPh_2]$)

  • 박병규;정건수
    • 한국결정학회지
    • /
    • 제6권2호
    • /
    • pp.93-97
    • /
    • 1995
  • Re(≡NC6H5)(PPh3)2CI3 화합물이 1,2-bis(diphenylphosphino)ethane (DPPE)와 반응하여 fac-Re(≡NC6H5)(DPPE)CI3이 되었다. 이 생성물의 구조를 1H-NMR, 원소분석, 그리고 X-ray 회절법으로 규명하였다. 이 생성물은 단사정계로 (Pc, a=11.083(3)Å, b=10.930(1)Å, c=14.081(2)Å, β=108.37(2)°, Z=2) 결정화되었다. 최소자승법으로 구조를 정밀화한 결과 신뢰도는 R(wR2)=0.0254(0.0607)이였다.

  • PDF

결정립크기와 집합조직제어를 통한 마그네슘 합금의 기계적 성질 개선 (Improvement of Mechanical Properties of Mg alloys through Control of Grain Size and Texture)

  • 김우진;이종범;김우영;정하국;박종덕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.57-58
    • /
    • 2006
  • The effects of lowering ECAP temperature during ECAP process and Post-ECAP annealing on microstructure, texture and mechanical properties of the AZ31 alloys have been investigated in the present study. The as-extruded materials were ECAP processed to 2 passes at 553K prior to subsequent pressing up to 6 passes at 523K or 493K. When this method of lowering ECAP temperature during ECAP was used, the rods could be successfully deformed up to 6 passes without any surface cracking. Grain refinement during ECAP process at 553K might have helped the material to endure further straining at lower deformation temperatures probably by increasing the strain accommodation effect by grain boundary sliding, causing stress relaxation. Texture modification during ECAP has a great influence on the strength of Mg alloys because HCP metals have limited number of slip systems. As slip is most prone to take place on basal planes in Mg at room temperature, the rotation of high fraction of basal planes to the directions favorable for slip as in ECAP decreases the yield stress appreciably. The strength of AZ31 Mg alloys increases with decrease of grain size if the texture is constant though ECAP deformation history is different. A standard positive strength dependence on the grain size for Mg alloys with the similar texture (Fig. 1) supports that the softening of ECAPed Mg alloys (a negative slope) typically observed despite the significant grain refinement is due to the texture modification where the rotation of basal planes occurs towards the orientation for easier slip. It could be predicted that if the original fiber texture is restored after ECAP treatment yielding marked grain refinement, yield stress as high as 500 MPa will be obtained at the grain size of ${\sim}1{\mu}m$. Differential speed rolling (DSR) with a high speed ratio between the upper and lower rolls was applied to alter the microstructure and texture of the AZ31 sheets. Significant grain refinement took place during the rolling owing to introduction of large shear deformation. Grain size as small as $1.4{\mu}m$ could be obtained at 423K after DSR. There was a good correlation between the (0002) pole intensity and tensile elongation. This result indicates that tensile ductility improvement in the asymmetrically rolled AZ31 Mg alloys is closely related to the weakening of basal texture during DSR. Further basal texture weakening occurred during annealing after DSR. According to Hall-Petch relation shown in Fig. 1, the strength of the asymmetrically rolled AZ31 is lower than that of the symmetrically rolled one when compared at the same grain size. This result was attributed to weakening of fiber texture during DSR. The DSRed AZ31, however, shows higher strength than the ECAPed AZ31 where texture has been completely replaced by a new texture associated with high Schmid factors.

  • PDF

인접 화소를 이용한 개선된 움직임 보상 (Improved Motion Compensation Using Adjacent Pixels)

  • 서정훈;김정필;이영렬
    • 방송공학회논문지
    • /
    • 제15권2호
    • /
    • pp.280-289
    • /
    • 2010
  • H.264/AVC 표준은 영상간의 시간적 중복성(Temporal Redundancy)을 줄여 부호화 효율을 높이는 인터예측 방법을 사용한다. 하지만, 영상에서 발생할 수 있는 지역적인 밝기 변화를 효율적으로 부호화 할 수 없기 때문에, 화질의 열화가 발생하여 부호화 효율이 떨어지는 문제점을 지니고 있다. 본 논문은 지역적인 밝기 변화를 인접화소 및 움직임벡터 재조정을 이용하여 효율적으로 부호화 할 수 있는 방법을 제안한다. 제안하는 방법은, H.264/AVC와 비교하여 0.01 ~ 0.21dB의 BD-PSNR (Bj$\o$ntegaard Delta Peak Signal-to-noise) 이득을 얻을 수 있었다.