  • An experimental study is carried out to estimate the way of applying the granulated blast furnace slag[GBFS] to the lean concrete base of concrete pavement. According to the test results, this application seems promising. For this application, mixing percent of GBFS ranging from 30 to 50 is recommendable at this stage. And performance of base mixed with GBFS is greatly affected by the curing and placing condition. As long as all requirements for application of GBFS to the base is satisfied, better performance is expected.

  • PDF

고로슬래그 미분말을 활용한 콘크리트포장 린콘크리트 보조기층 시험 적용 (Experimental Application of the Ground Granulated Blast-Furnace Slag to the Lean Concrete Subbase Course)

  • 류명찬;유태석;엄주용;김대영;손진군
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회 논문집(II)
    • /
    • pp.1091-1094
    • /
    • 2000
  • An experimental study is carried out to estimate the way of applying the granulated blast furnace slag[GBFS] to the lean concrete subbase of concrete pavement. According to the test results, this application seems promising. For this application, mixing percent of GBFS ranging from 30 to 45 is recommendable at this stage. Expected benefits using GGBFS in the field of concrete pavement include reduced shrinkage crack, reduced pavement thickness, and extended service life.

순환골재 용출수를 활용한 고로슬래그 미분말 혼입 모르터의 강도특성 (A Study on the Hydration Property of Mortar with Balst Furnace Slag using Water Eluted from Recycled Coarse Aggregates)

  • 신상엽;정의창;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.81-82
    • /
    • 2012
  • The purpose of this study is the hydration properties of motar using Blast-Furnace Slag(BFS) with water elured from recycled coarse aggregate. The results of the experiment show that the water eluted from recycled coarse aggregate mixed with blast furnace slag has comparatively higher hydration activity than the mortar not mixed with one in early-age mortar causing the calcium hydroxide in the recycled coarse aggregate to work on as a stimulus to the hydration of ground granulated blast furnace slag. BFS mixed with the eluting water the hydration reaction was a promotion.

  • PDF

고로슬래그미분말의 입도와 양생방법에 따른 모르터 물성에 관한 연구 (A Study on the Properties of Mortar With Particle Size of Blast Furnace Slag Powder and Curing Methods)

  • 김승진;박유진;조재우;김영근;김대영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.191-194
    • /
    • 1999
  • Recently in Korea, may workers have reported the effects of the granulated blast furnace slag[BFS] of high fineness on the strength development of slag cement. We have studied the effect of slag fineness on the strength development of mortar with curing conditions, in order to get the basic data of high strength concrete using BFS. In this paper, we discussed the effects of slag fineness and porosity of mortar and the reaction of slag in hardened slag cement.

  • PDF

플라이애쉬 및 고로슬래그를 사용한 고성능콘크리트의 특성 (The properties of High Performance Concrete Using Fly Ash and Blast-Furnace Slag)

  • 이승한;정용욱;박정준
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.275-280
    • /
    • 1998
  • In this study, to increase fluidity and resistance of segregation of materials, the effect of each of the materials, which have effects on high performance concrete from investigating the properties of strength and drying shrinkage of high performance concrete made by the basic mix proportion used fly-ash and ground granulated blast-furnace slag after hardening, has been checked. By the results of this experiment, fluidity on W/C=34% was satisfied within slump-flow 65$\pm$5cm and U-type self-compacting difference 5cm. On the properties of strength, high performance concrete produced compressive strength over 400kg/$\textrm{cm}^2$ in 28days when powder was replaced by 40% of fly-ash and 60% of ground granulated blast-furnace slag. And compressive strength was taken over 600kg/$\textrm{cm}^2$ equal to non-replacement in 91days. Also, the length change of concrete with the addition of fly-ash was smaller than that without it. Therefore, it may be effective on the decrease of drying shrinkage volume.

  • PDF

응결시간과 겉보기 활성화 에너지를 이용한 고로슬래그 콘크리트의 압축강도 예측에 관한 연구 (Prediction of Compressive Strength Using Setting Time and Apparent Activation Energy of Blast Furnace Slag Concrete)

  • 김한솔;양현민;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2021년도 가을 학술논문 발표대회
    • /
    • pp.101-102
    • /
    • 2021
  • The compressive strength of concrete is greatly affected by the temperature inside the concrete at the initial age immediately after pouring. The apparent activation energy of cement and the setting time of concrete are major factors influencing the development of compressive strength of concrete. This study measured the apparent activation energy and setting time according to the change in W/B for each mixing rate of Ground Granulated Blast-Furnace Slag (GGBFS). And after calculating the compressive strength prediction model, the accuracy of the prediction model was evaluated by comparing the predicted compressive strength and the compressive strength.

  • PDF

Effect of curing temperature on the properties of ground granulated blast furnace slag-cement bentonite slurry

  • Kim, Taeyeon;Lee, Bongjik;Hong, Seongwon
    • Geomechanics and Engineering
    • /
    • 제29권3호
    • /
    • pp.237-247
    • /
    • 2022
  • To investigate the curing temperature effect on the engineering properties of ground granulated blast furnace slag-cement bentonite (GGBS-CB) slurry for cutoff walls, the laboratory experiments including the setting time, unconfined compressive strength, and permeability tests were carried out. The mixing procedure for GGBS-CB slurry was as follows: (1) montmorillonite-based bentonite slurry was first fabricated and hydrated for four hours, and (2) cement or GGBS with cement was added to the bentonite slurry. The dosage range of GGBS was from 0 to 90 % of cement by mass fraction. The GGBS-CB slurry specimens were cured and stored in environmental chamber at temperature of 14±1, 21±1, 28±1℃ and humidity of 95±2% until target days. The highest average temperature of three seasons in South Korea was selected and used for the tests. The experimental results indicated that in early age (less than 28 days) of curing the engineering properties of GGBS-CB slurry were primarily affected by the curing temperature, whereas the replacement ratio of GGBS became a main factor to determine the properties of the slurry as the curing time increased.

고로슬래그를 사용한 건식 및 습식 재생 잔골재 모르타르의 물리적 특성에 관한 연구 (A Study on the Physical Properties of Recycled Fine Aggregate (by Dry and Wet Type Production formula) Mortar Using Blast Furnace Slag)

  • 심종우;이세현;서치호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.501-504
    • /
    • 2006
  • Recycled aggregate mortar contains plenty of calcium hydroxide to improve the strength of blast furnace slag, although the surface mortar made of recycled aggregate deteriorates adhesion to cement paste and blast furnace slag has a low initial strength. Therefore, this study assumes that the combination with both recycled aggregate and blast furnace slag will produce a better performance. The results of the experiment show that dry mortar made of recycled aggregate provides with higher strength than wet mortar does at the 3-day and 7-day age, while lower at the 28-day age. It indicates that a large amount of cement mortar made of dry recycled aggregate has deteriorated adhesion strength. The mixes with 30% and 50% of blast furnace slag and 50% and 75% of recycled aggregate provide with much better strength at the 7-day age, although they usually have latent hydraulic property at the 28-day age. It indicates that calcium hydroxide($Ca(OH){_2}$) in recycled aggregate has affected ground granulated blast furnace slag.

  • PDF

고로슬래그 미분말을 혼입한 순환골재 콘크리트의 압축강도 및 동결융해 저항성 (Compressive Strength and Resistance to Freezing and Thawing of Recycled Aggregate Concrete Containing Ground Granulated Blast Furnace Slag)

  • Bae, Suho;Jeon, Juntai
    • 한국재난정보학회 논문집
    • /
    • 제9권4호
    • /
    • pp.469-475
    • /
    • 2013
  • 이 연구의 목적은 고로슬래그 미분말을 혼입한 순환골재 콘크리트의 압축강도 및 동결융해 저항성을 평가하는 것이다. 이를 위하여 순환골재 대체율에 따라 고로슬래그 미분말 혼입률을 변수로 콘크리트 공시체를 제작한 후 이들의 압축강도 및 동결융해 저항성을 평가하였다. 고로슬래그 미분말 20% 혼입한 순환골재 콘크리트의 재령 28일 압축강도는 플레인 콘크리트보다 훨씬 우수하였고, 동결융해 300 사이클 시험 결과, 콘크리트의 공기량을 4~6% 유지하였을 때, 순환골재 대체율 및 고로슬래그 미분말 혼입률이 동결융해 저항성에 미치는 영향은 거의 없는 것으로 나타났다.