• 제목/요약/키워드: dynamic ductile fracture

검색결과 36건 처리시간 0.018초

동적하중 하에서의 강도적 불균질부를 갖는 용접이음재의 강도 및 파괴 특성 (Characteristics of Strength and Fracture in Strength Mismatched Joint by Dynamic Loading)

  • 안규백;;;방한서
    • Journal of Welding and Joining
    • /
    • 제21권6호
    • /
    • pp.55-63
    • /
    • 2003
  • Welded joint generally has heterogeneity of strength, material, and fracture toughness and it is important to understand the characteristics of material strength and fracture of welded joint considering heterogeneous effect. Characteristics of strength and fracture of an undermatched joint under dynamic loading was studied by round-bar tension tests and thermal elastic-plastic analyses in this paper. The strength and fracture of the undermatched joints should be evaluated based on the effects of the strain rate and the temperature including temperature rise during the dynamic loading. The differences of fracture characteristics like such as ductile-to-brittle transition behavior are well precisely explained from the stress-strain distribution obtained by numerical analysis.

가스배관의 재질등급 및 충격에너지에 따른 연속연성파괴 거동분석 (Dynamic Ductile Fracture Analysis of Natural Gas Pipelines on the Basis of Material Grade and Charpy V-Notch Impact Energy)

  • 정효태;최병학;이영진;이정화;홍기용;백종현;김우식
    • 한국가스학회지
    • /
    • 제16권5호
    • /
    • pp.35-40
    • /
    • 2012
  • 가스배관 종류 및 사용 환경에 따른 거시적 파괴거동 평가해석을 위하여 1) 가스배관의 특성 및 환경에 따른 파괴거동 변화의 컴퓨터해석과 2) Battelle Two-Curve Method를 이용한 연속연성파괴거동 평가해석을 수행하였다. 새로운 사용환경의 가스와 오일의 배관계획이 진행되면서, 개선된 성능, 신뢰성, 그리고 경제성을 위한 재료가 요구되고 있다. 여기서 제시되는 연속연성파괴 해석은 높은 배관압력, 큰 배관직경과 같은 배관 특성의 변화와 천연가스와 같이 다양한 성분을 함유하는 가스, 수소가스, 액화 이산화탄소 등과 같이 다양한 수송매체의 변화를 수용하기 위한 배관시스템에서 고려하여야 할 중요한 기술요소이다.

동적하중하에서의 강도적 불균질재의 연성크랙 발생한계의 해석적 검토 - 강도적 불균질 및 동적부하의 영향에 의한 연성크랙 발생조건 (제 2 보) - (Analytical Examination of Ductile Crack Initiation with Strength Mismatch under Dynamic Loading - Criterion for Ductile Crack Initiation Effect of Strength Mismatch and Dynamic Loading (Report 2) -)

  • 안규백;;;방한서
    • Journal of Welding and Joining
    • /
    • 제21권7호
    • /
    • pp.49-58
    • /
    • 2003
  • It has been well known that ductile fracture of steel is accelerated by triaxiality stresses. The characteristics of ductile crack initiation in steels are evaluate quantitatively using two-parameter criterion based on equivalent plastic strain and stress triaxiality. Recently, the characteristics of critical crack initiation of steels are quantitatively estimated using the two-parameter, that is, equivalent plastic strain and stress triaxiality, criterion. This study is paid to the fundamental clarification of the effect of geometrical heterogeneity and strength mismatching, which can elevate plastic constraint due to heterogeneous plastic straining, and loading rate on critical condition to initiate ductile crack using two-parameter. Then, the crack initiation testing were conducted under static and dynamic loading. To evaluate the stress/strain state in the specimens especially under dynamic loading, thermal elastic-plastic dynamic FE-analysis considering the temperature rise was used. The result showed that the critical global strain to initiate ductile fracture in specimens with strength mismatch under various loading rate cu be estimated based on the local criterion, that is two-parameter criterion obtained on homogeneous specimens under static tension, by mean of FE-analysis taken into account accurately both strength mismatch and dynamic loading effects on stress/strain behavior.

CO2 배관의 연속연성파괴 분석 (Analysis on Dynamic Ductile Fracture of Transportation Pipeline for Carbon Dioxide Capture and Storage System)

  • 정효태;최병학;김우식;백종현
    • 한국가스학회지
    • /
    • 제18권3호
    • /
    • pp.13-19
    • /
    • 2014
  • 이산화탄소 포집 및 저장 시스템(CCS, Carbon dioxide Capture and Storage system)의 수송배관에 대한 연속연성파괴(DDF, Dynamic Ductile Fracture)를 연구하기 위하여 Battlle Two Curve법(BTCM)으로 CCS수송배관의 연속연성파괴거동을 해석하여 천연가스 수송배관의 연속연성파괴거동과 비교하였다. 또한, $CO_2$배관에서의 배관두께 및 사용온도에 따른 연속연성파괴 민감도를 분석함으로써 연속연성파괴에 대한 사용기준을 해석하였다. 우리나라 기후조건에 따른 $CO_2$배관두께와 수송압력 사용기준을 분석하였으며, 상온의 경우에는 기존의 천연가스용 배관을 $CO_2$배관으로 사용하기 위해서는 배관두께가 7mm이상이어야 하고 수송압력은 54bar이하이어야 함을 해석하였다.

EFFECT OF STRENGTH MISMATCH AND DYNAMIC LOADING ON THE DUCTILE CRACK INITIATION FROM NOTCH ROOT

  • An, Gyn-Baek;Yoshida, Satoshi;Ohata, Mitsuru;Toyoda, Masao
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.145-150
    • /
    • 2002
  • It has been well known that ductile fracture of steels is accelerated by triaxial stresses. The characteristics of ductile crack initiation in steels are evaluated quantitatively using two-parameters criterion based on equivalent plastic strain and stress triaxiality. It has been demonstrated by authors using round-bar specimens with circumferential notch in single tension that the critical strain to initiate ductile crack from specimen center depends considerably on stress triaxiality, but surface cracking of notch root is in accordance with constant strain condition. In order to evaluate the stress/strain state in the specimens, especially under dynamic loading, a thermal, elastic-plastic, dynamic finite element (FE) analysis considering the temperature rise due to plastic deformation has been carried out. This study provides the fundamental clarification of the effect of strength mismatching, which can elevate plastic constraint due to heterogeneous plastic straining, loading mode and loading rate on critical condition to initiate ductile crack from notch root using equivalent plastic strain and stress triaxiality based on the two-parameter criterion obtained on homogeneous specimens under static tension. The critical condition to initiate ductile crack from notch root for strength mismatched bend specimens under both static and dynamic loading would be almost the same as that for homogeneous tensile specimens with circumferential sharp notch under static loading.

  • PDF

강도적 불균질을 갖는 구조물의 동적하중하에서의 연성크랙 발생조건 (Criterion for ductile crack initiation with strength mismatch under dynamic loading)

  • 안규백;일본명;일본명;방한서;일본명
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2003년도 추계학술발표대회 개요집
    • /
    • pp.179-181
    • /
    • 2003
  • The present study focuses on the effect of geometrical discontinuity, strength mismatch, which can elevate plastic constraint due to heterogeneous plastic straining, and loading rate on the ductile crack initiation using two-parameter criterion. Fracture initiation testing has been conducted under static and dynamic loading using circumferentially notched round-bar specimens. In order to evaluate the stress/strain state in the specimens, especially under dynamic loading, a thermal elastic-plastic dynamic finite element (FE) analysis considering the temperature rise due to plastic deformation has been carried out.

  • PDF

Numerical Ductile Tearing Simulation of Circumferential Cracked Pipe Tests under Dynamic Loading Conditions

  • Nam, Hyun-Suk;Kim, Ji-Soo;Ryu, Ho-Wan;Kim, Yun-Jae;Kim, Jin-Weon
    • Nuclear Engineering and Technology
    • /
    • 제48권5호
    • /
    • pp.1252-1263
    • /
    • 2016
  • This paper presents a numerical method to simulate ductile tearing in cracked components under high strain rates using finite element damage analysis. The strain rate dependence on tensile properties and multiaxial fracture strain is characterized by the model developed by Johnson and Cook. The damage model is then defined based on the ductility exhaustion concept using the strain rate dependent multiaxial fracture strain concept. The proposed model is applied to simulate previously published three cracked pipe bending test results under two different test speed conditions. Simulated results show overall good agreement with experimental results.

Application of cohesive zone model to large scale circumferential through-wall and 360° surface cracked pipes under static and dynamic loadings

  • Moon, Ji-Hee;Jang, Youn-Young;Huh, Nam-Su;Shim, Do-Jun;Park, Kyoungsoo
    • Nuclear Engineering and Technology
    • /
    • 제53권3호
    • /
    • pp.974-987
    • /
    • 2021
  • This paper presents ductile fracture simulation of full-scale cracked pipe for nuclear piping materials using the cohesive zone model (CZM). The main objective of this study is to investigate the applicability of CZM to predict ductile fracture of cracked pipes with various crack shapes and under quasi-static/dynamic loadings. The transferability of the traction-separation (T-S) curve from a small-scale specimen to a full-scale pipe is demonstrated by simulating small- and full-scale tests. T-S curves are calibrated by comparing experimental data of compact tension specimens with finite element analysis results. The calibrated T-S curves are utilized to predict the fracture behavior of cracked pipes. Three types of full-scale pipe tests are considered: pipe with circumferential through-wall crack under quasistatic/dynamic loadings, and with 360° internal surface crack under quasi-static loading. Computational results using the calibrated T-S curves show a good agreement with experimental data, demonstrating the transferability of the T-S curves from small-scale specimen.

유효 $K_{1d}$ 산정을 위한 샬피 충격시험편의 노치형상에 관한 연구 (An Evaluation of Notch Shpae for Estimation of Available $K_{1d}$ by Instrumented Charpy Impact Test)

  • 우창기;강동명;이하성
    • 한국자동차공학회논문집
    • /
    • 제7권6호
    • /
    • pp.135-143
    • /
    • 1999
  • This investigation evaluates effects of notch depth, fatigue precrack length and side groove in impact specimen for estimation of a valid K1d by instrumented Charpy impact test. Specimen material is 6005-T6. for notch depth 2.0mm and 2.5mm specimens or within about 2mm fatigue precrack length with notch depth 2.0mm and 2.5mm specimens or within about 2mm fatigue precrack length with notch depth 2.0mm , dynamic fracture toughness [$K_{1d,(1)}$] obtained by crack initiation load($P_m$) should be used. Dynamic fracture toughness of side grooved specimens are overestimated to that of standard impact specimen about 15 %-20%. It is confirmed that the formula of dynamic fracture toughness obtained by impact absorbed energy is inappropriate for ductile materials.

  • PDF

강도적 불균질재의 노치 표면에서의 연성크랙 발생 거동 (Behavior of ductile crack initiation with strength mismatch from notch root)

  • 안규백;대연윤;방한서;풍전정남
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.246-248
    • /
    • 2004
  • It has been well known that ductile fracture of steels is accelerated by triaxial stresses. The characteristics of ductile crack initiation in steels are evaluated quantitatively using two-parameters criterion based on equivalent plastic strain and stress triaxiality. This study provides the fundamental clarification of the effect of strength mismatching, which can elevate plastic constraint due to heterogeneous plastic straining, loading mode and loading rate on critical condition to initiate ductile crack from notch root using equivalent plastic strain and stress triaxiality based on the two-parameter criterion obtained on homogeneous specimens under static tension. The critical condition to initiate ductile crack from notch root for strength mismatched bend specimens under both static and dynamic loading would be almost the same as that for homogeneous tensile specimens with circumferential sharp notch under static loading.

  • PDF