Study of Surface Reaction and Gas Phase Chemistries in High Density C4F8/O2/Ar and C4F8/O2/Ar/CH2F2 Plasma for Contact Hole Etching

  • Kim, Gwan-Ha
    • Transactions on Electrical and Electronic Materials
    • /
    • v.16 no.2
    • /
    • pp.90-94
    • /
    • 2015
  • In this study, the characterizations of oxide contact hole etching are investigated with C4F8/O2/Ar and CH2F2/C4F8/O2/ Ar plasma. As the percent composition of C4F8 in a C4F8/O2/Ar mixture increases, the amount of polymer deposited on the etched surface also increases because the CxFy polymer layer retards the reaction of oxygen atoms with PR. Adding CH2F2 into the C4F8/O2/Ar plasma increases the etch rate of the oxide and the selectivity of oxide to PR. The profile of contact holes was close to 90°, and no visible residue was seen in the SEM image at a C4F8/(C4F8+O2) ratio of 58%. The changes of chemical composition in the chamber were analyzed using optical emission spectroscopy, and the chemical reaction on the etched surface was investigated using X-ray photoelectron spectroscopy.

Optimization of a-IGZO Thin-Film Transistors for OLED Applications

  • Chung, Hyun-Joong;Yang, Hui-Won;Kim, Min-Kyu;Jeong, Jong-Han;Ahn, Tae-Kyung;Kim, Kwang-Suk;Kim, Eun-Hyun;Kim, Sung-Ho;Im, Jang-Soon;Choi, Jong-Hyun;Park, Jin-Seong;Jeong, Jae-Kyeong;Mo, Yeon-Gon;Kim, Hye-Dong
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2008.10a
    • /
    • pp.1097-1100
    • /
    • 2008
  • We demonstrate that the performance of amorphous indium-gallium-zinc-oxide (IGZO) thin-film transistors (TFT) can be optimized by controlling the interfaces between IGZO and sandwiching insulators and by proper deposition of IGZO layer. Specifically, contact and channel resistances are decreased by reducing IGZO bulk resistance and optimizing dry-etch process, respectively. Field-effect mobility ($\mu_{FE}$) and subthreshold gate swing (S) are further enhanced by fine-tuning IGZO deposition condition.

  • PDF

$\mu$CP Process Technology for Nanopattern Implementation (나노패턴 구현을 위한 $\mu$CP 공정기술)

  • 조정대;신영재;김광영
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.624-627
    • /
    • 2003
  • Microcontact printing (uCP) of alkanethiols on gold was the first representative of soft-lithography processes. This is an attempt to enhance the accuracy of classical to a precision comparable with optical lithography, creating a low-cost, large-area, and high-resolution patterning process. Microcontact printing relies on replication of a pattered PDMS stamp from a master to form an elastic stamp that can be inked with a SAM solution(monolayer -forming ink) using either immersion inking or contact inking. The inked PDMS stamp is then used to print a pattern that selectively protects the gold substrate during the subsequent etch.

  • PDF

A novel self-aligned offset gated polysilicon thin film transistor without an additional offset mask (오프셋 마스크를 이용하지 않는 새로운 자기 정합 폴리 실리콘 박막 트랜지스터)

  • 민병혁;박철민;한민구
    • Journal of the Korean Institute of Telematics and Electronics A
    • /
    • v.32A no.5
    • /
    • pp.54-59
    • /
    • 1995
  • We have proposed a novel self-aligned offset gated polysilicon TFTs device without an offset mask in order to reduce a leakage current and suppress a kink effect. The photolithographic process steps of the new TFTs device are identical to those of conventional non-offset structure TFTs and an additional mask to fabricate an offset structure is not required in our device due to the self-aligned process. The new device has demonstrated a lower leakage current and a better ON/OFF current ratio compared with the conventional non-offset device. The new TFT device also exhibits a considerable reduction of the kink effect because a very thin film TFT devices may be easily fabricated due to the elimination of contact over-etch problem.

  • PDF

Analysis of Chemical and Morphological Changes of Phenol Formaldehyde-based Photoresist Surface caused by O2 Plasma

  • Shutov, D.A.;Kang, Seung-Youl;Baek, Kyu-Ha;Suh, Kyung-Soo;Min, Nam-Ki;Kwon, Kwang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.5
    • /
    • pp.211-214
    • /
    • 2007
  • Chemical and morphological changes of phenol formaldehyde-based photoresist after $O_2$ radiofrequency(RF) plasma treatment depending on exposure time and source power were investigated. It was found that etch rate of photoresist sharply increased after discharge turn on and reached a limit with increase in plasma exposure time. Contact angle measurements and X-ray photoelectron spectroscopy(XPS) analysis showed that the surface chemical structure become nearly constant after 15 sec of the treatment. Atomic force microprobe(AFM) measurements were shown that surface roughness was increased with plasma exposure time.

A Study on Pattern Formation of Ultra Definition Display Panel Applying Phosphoric Acid (인산을 적용한 Ultra Definition 디스플레이 패널의 패턴 형성에 관한 연구)

  • Kim, Min-Su;Cho, Ur Ryong
    • Journal of the Semiconductor & Display Technology
    • /
    • v.13 no.3
    • /
    • pp.13-19
    • /
    • 2014
  • Phosphoric acid was used as etching agent instead of conventional peroxide - based chemicals for forming pattern of ultra definition display. Etchant was synthesized by mixing etching agent, oxidation agent, buffer solution, and additive into solvent, deionized water. Thicknesses of copper, main metal of ultra definition display, for etching, were 10,000 and $30,000{{\AA}}$. Etch stop of good low skew for proper pattern formation has been occurred at the content ratio of phosphoric acid 60 - 64%, nitric acid 4 - 5%, additive(potassium acetate) 1 - 3%. Buffer solution(acetic acid) decreased the metal contact angle $63.07^{\circ}$ to $42.49^{\circ}$ for benefiting pattern formation. Content variations on four components (phosphoric acid, nitric acid, acetic acid, potassium acetic acid) of the etchant with storage time were within 3 wt% after 24 hrs of etching work.

Efficient Shadow-Test Algorithm for the Simulation of Dry Etching and Topographical Evolution (건식 식각 공정 시뮬레이션을 위한 효율적인 그림자 테스트 알고리즘과 토포그래피 진화에 대한 연구)

  • Kwon, Oh-Seop;Ban, Yong-Chan;Won, Tae-Young
    • Journal of the Korean Institute of Telematics and Electronics D
    • /
    • v.36D no.2
    • /
    • pp.41-47
    • /
    • 1999
  • In this paper, we report 3D-simulations of a plasma etching process by employing cell-removal algorithm takes into account the mask shadow effect os well as spillover errors. The developed simulator haas an input interface to take not only an analytic form but a Monte Carlo distribution of the ions. The graphic user interface(GUI) was also built into the simulator for UNIX environment. To demonstrate the capability of 3D-SURFILER(SURface proFILER), we have simulated for a typical contact hole structure with 36,000($30{\times}40{\times}30$) cells, which takes about 20 minutes with 10 Mbytes memory on sun ultra sparc 1. as an exemplary case, we calculated the etch profile during the reactive ion etching(RIE) of a contact hole wherein the aspect ratio is 1.57. Furthermore, we also simulated the dependence of a damage parameter and the evolution of topography as a function of the chamber pressure and the incident ion flux.

  • PDF

Simultaneous Transfer and Patterning of CVD-Grown Graphene with No Polymeric Residues by Using a Metal Etch Mask

  • Jang, Mi;Jeong, Jin-Hyeok;Trung, T.Q.;Lee, Nae-Eung
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.642-642
    • /
    • 2013
  • Graphene, two dimensional single layer of carbon atoms, has tremendous attention due to its superior property such as high electron mobility, high thermal conductivity and optical transparency. Especially, chemical vapor deposition (CVD) grown graphene has been used as a promising material for high quality and large-scale graphene film. Unfortunately, although CVD-grown graphene has strong advantages, application of the CVD-grown graphene is limited due to ineffective transfer process that delivers the graphene onto a desired substrate by using polymer support layer such as PMMA(polymethyl methacrylate). The transferred CVD-grown graphene has serious drawback due to remaining polymeric residues generated during transfer process, which induces the poor physical and electrical characteristics by a p-doping effect and impurity scattering. To solve such issue incurred during polymer transfer process of CVD-grown graphene, various approaches including thermal annealing, chemical cleaning, mechanical cleaning have been tried but were not successful in getting rid of polymeric residues. On the other hand, lithographical patterning of graphene is an essential step in any form of microelectronic processing and most of conventional lithographic techniques employ photoresist for the definition of graphene patterns on substrates. But, application of photoresist is undesirable because of the presence of residual polymers that contaminate the graphene surface consistent with the effects generated during transfer process. Therefore, in order to fully utilize the excellent properties of CVD-grown graphene, new approach of transfer and patterning techniques which can avoid polymeric residue problem needs to be developed. In this work, we carried out transfer and patterning process simultaneously with no polymeric residue by using a metal etch mask. The patterned thin gold layer was deposited on CVD-grown graphene instead of photoresists in order to make much cleaner and smoother surface and then transferred onto a desired substrate with PMMA, which does not directly contact with graphene surface. We compare the surface properties and patterning morphology of graphene by scanning electron microscopy (SEM), atomic force microscopy(AFM) and Raman spectroscopy. Comparison with the effect of residual polymer and metal on performance of graphene FET will be discussed.

  • PDF

Influence of Wet Chemistry Damage on the Electrical and Structural Properties in the Wet Chemistry-Assisted Nanopatterned Ohmic Electrode (Wet chemistry damage가 Nanopatterned p-ohmic electrode의 전기적/구조적 특성에 미치는 영향)

  • Lee, Young-Min;Nam, Hyo-Duk;Jang, Ja-Soon;Kim, Sang-Mook;Baek, Jong-Hyub
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.150-150
    • /
    • 2008
  • 본 연구에서는 Wet chemistry damage가 Nanopatterned p-ohmic electrode에 미치는 영향을 연구하였다. Nanopattern은 Metal clustering을 이용하여, P-GaN와 Ohmic형성에 유리한 Pd을 50$\AA$ 적층한 후 Rapid Thermal Annealing방법으로 $850^{\circ}C$, $N_2$분위기에서 3min열처리를 하여 Pd Clustering mask 를 제작하였다. Wet etching은 $85^{\circ}C$, $H_3PO_4$조건에서 시간에 따라 Sample을 Dipping하는 방법으로 시행하였다 Ohmic test를 위해서 Circular - Transmission line Model 방법을 이용하였으며, Atomic Force Microscopy과 Parameter Analyzer로 Nanopatterned GaN surface위에 형성된 Ni/ Au Contact에서의 전기적 분석과, 표면구조분석을 시행하였다. AFM결과 Wet처리시간에 따라서 Etching형상 및 Etch rate이 영향을 받는 것이 확인되었고, Ohmic test에서 Wet chemistry처리에 의한 Tunneling parameter와 Schottky Barrier Height가 크게 증/감함을 관찰하였다. 이러한 결과들은 Wet처리에 의해서 발생된 Defect가 GaN의 표면과 하부에서 발생되며, Deep acceptor trap 및 transfer거동과 밀접한 관련이 있음을 확인 할 수 있었다. 보다 자세한 Transport 및 Wet chemical처리영향에 관한 형성 Mechanism은 후에 I-V-T, I-V, C-V, AFM결과 들을 활용하여 발표할 예정이다.

  • PDF

Fabrication of Superhydrophobic Micro-Nano Hybrid Structures by Reactive Ion Etching with Au Nanoparticle Masks (나노입자 마스크를 이용하여 제작한 초소수성 마이크로-나노 혼성구조)

  • Lee, C.Y.;Yoon, S.B.;Jang, G.E.;Yun, W.S.
    • Journal of the Korean Vacuum Society
    • /
    • v.19 no.4
    • /
    • pp.300-306
    • /
    • 2010
  • Superhydrophobic micro-nano hybrid structures were fabricated by reactive ion etching of hydrophobic polymer micro patterns using gold nanoparticles as etch masks. Micro structures of perfluoropolyether bisurethane methacrylate (PFPE) were prepared by soft-lithographic technique using polydimethylsiloxane (PDMS) molds. Water contact angles on the surfaces of various PFPE micro structures and corresponding micro-nano hybrid structures were compared to examine the effects of micro patterning and nanostructure formation in the manifestation of superhydrophobicity. The PFPE micro-nano hybrid structures exhibited a very stable superhydrophobicity, while the micro-only structures could not reach the superhydrophobicity but only showed the unstable hydrophobicity.