Compressive behaviour of circular steel tube-confined concrete stub columns with active and passive confinement

  • Nematzadeh, Mahdi;Hajirasouliha, Iman;Haghinejad, Akbar;Naghipour, Morteza
    • Steel and Composite Structures
    • /
    • 제24권3호
    • /
    • pp.323-337
    • /
    • 2017
  • This paper presents the results of a comprehensive experimental investigation on the compressive behaviour of steel tube-confined concrete (STCC) stub columns with active and passive confinement. To create active confinement in STCC columns, an innovative technique is used in which steel tube is laterally pre-tensioned while the concrete core is simultaneously pre-compressed by applying pressure on fresh concrete. A total of 135 STCC specimens with active and passive confinement are tested under axial compression load and their compressive strength, ultimate strain capacity, axial and lateral stress-strain curves and failure mode are evaluated. The test variables include concrete compressive strength, outer diameter to wall thickness ratio of steel tube and prestressing level. It is shown that applying active confinement on STCC specimens can considerably improve their mechanical properties. However, applying higher prestressing levels and keeping the applied pressure for a long time do not considerably affect the mechanical properties of actively confined specimens. Based on the results of this study, new empirical equations are proposed to estimate the axial strength and ultimate strain capacity of STCC stub columns with active and passive confinement.

Experimental and analytical investigations of CFFT columns with and without FRP bars under concentric compression

  • Khan, Qasim S.;Sheikh, M. Neaz;Hadi, Muhammad N.S.
    • Steel and Composite Structures
    • /
    • 제30권6호
    • /
    • pp.591-601
    • /
    • 2019
  • This research study investigates experimentally and analytically the axial compressive behaviour of Concrete Filled Fiber Reinforced Polymer Tube (CFFT) columns with and without Fiber Reinforced Polymer (FRP) bars. The experimental program comprises five circular columns of 204-206 mm outer diameter and 800-812 mm height. All columns were tested under concentric axial compressive loads. It was found that CFFT columns with and without FRP bars achieved higher peak axial compressive loads and corresponding axial deformations than conventional steel reinforced concrete (RC) column. The contribution of FRP bars was about 12.1% of the axial compressive loads carried by CFFT columns reinforced with FRP bars. Axial load-axial deformation ($P-{\delta}$) curves of CFFT columns were analytically constructed, which mapped well with the experimental $P-{\delta}$ curves. Also, an equation was proposed to predict the axial compressive load capacity of CFFT columns with and without FRP bars, which adequately considers the contributions of the circumferential confinement provided by FRP tubes and lower ultimate strength of FRP bars in compression than in tension.

Axial compressive behavior of concrete-encased CFST stub columns with open composite stirrups

  • Ke, Xiaojun;Ding, Wen;Liao, Dingguo
    • Advances in concrete construction
    • /
    • 제12권5호
    • /
    • pp.399-409
    • /
    • 2021
  • The existing method to improve the coordination performance of the inner and outer parts of concrete-encased concrete-filled steel tube (CFST) composite columns by increasing the volume-stirrup ratio causes difficulties in construction due to over-dense stirrups. Thus, this paper proposes an open polygonal composite stirrup with high strength and high ductility CRB600H reinforced rebar, and seventeen specimens were constructed, and their axial compressive performance was tested. The main parameters considered were the volume-stirrup ratio, the steel tube size, the stirrup type and the stirrup strength. The test results indicated: For the specimens restrained by open octagonal composite stirrups, compared with the specimen of 0.5% volume-stirrup ratio, the compressive bearing capacity increased by 14.6%, 15.7% and 21.5% for volume-stirrup ratio of 0.73%, 1.07% and 1.61%, respectively. For the specimens restrained by open composite rectangle stirrups, compared with the specimen of 0.79% volume-stirrup ratio, the compressive bearing capacity increased by 7.5%, 6.1%, and -1.4% for volume-stirrup ratio of 1.12%, 1.58% and 2.24%, respectively. The restraint ability and the bearing capacity of the octagonal composite stirrup are better than other stirrup types. The specimens equipped with open polygonal composite stirrup not only had a higher ductility than those with the traditional closed-loop stirrup, but they also had a higher axial bearing capacity than those with an HPB300 strength grades stirrup. Therefore, the open composite stirrup can be used in practical engineering. A new calculation method was proposed based on the stress-strain models for confined concrete under different restrain conditions, and the predicted value was close to the experimental value.

유공위치 변경에 따른 RC기둥의 내력변화에 관한 실험적 연구 (Stress Change Varying with Hole Place of RC Column)

  • 손기상
    • 한국안전학회지
    • /
    • 제21권2호
    • /
    • pp.70-79
    • /
    • 2006
  • many plumbing system are needed in the ceiling of the building as it becomes advanced more and more. This leads to make effective space between ceiling level and slab less. Also, piping system is not suitably arranged and operated if it is bent around the columns which they are a lot. But this system can be more effective if it passes through the columns directly. Most people think that those columns should not be damaged with such as holes. But actually this is existed in a hotel building in switzerland. This study is to fing out how much capacity the columns become damaged and low using model size of $20cm{\times}30cm$ rectangular section, and 160cm long, in the structural test. it's compressive strength is focused on $240kg/cm^{2}$ design strength, commonly used in korea. Compressive test for them was done at Hanyang University using UTM one thousand tone(1000t) capacity. Variable numbers for the study are one hole of dia 3cm with distance 20cm or 40cm, two holes of dia 3cm with 20cm and 40cm distance, one hole of dia 5cm with distance 20cm and 40cm, two holes of dia 5cm with 20cm and 40cm distance, me eccentric hole with 20cm and 40cm distance, Normal(without hole). two test specimens of each variable are made for the test. ED5H20 capacity was 16.7% decreased, compared to normal one. While ED5H40 distant 40cm from the end of column top showed 19.5% capacity decrease, compared to normal one. Strain of ED5H20 diameter 5cm, in distance of 20cm form the top of the column was less 5% than the one of diameter 3cm. Finally, conclusions are that in case of hole diameter 3cm, located at 20cm from the end of the column top, capacity was decreased down to 3, percent only compared to the same diameter hole with 20cm distant from the end of it.

Numerical and experimental analysis on the axial compression performance of T-shaped concrete-filled thin-walled steel

  • Xuetao Lyu;Weiwei Wang;Huan Li;Jiehong Li;Yang Yu
    • Steel and Composite Structures
    • /
    • 제50권4호
    • /
    • pp.383-401
    • /
    • 2024
  • The research comprehensively studies the axial compression performance of T-shaped concrete-filled thin-walled steel tubular (CTST) long columns after fire exposure. Initially, a series of tests investigate the effects of heating time, load eccentricity, and stiffeners on the column's performance. Furthermore, Finite Element (FE) analysis is employed to establish temperature and mechanical field models for the T-shaped CTST long column with stiffeners after fire exposure, using carefully determined key parameters such as thermal parameters, constitutive relations, and contact models. In addition, a parametric analysis based on the numerical models is conducted to explore the effects of heating time, section diameter, material strength, and steel ratio on the axial compressive bearing capacity, bending bearing capacity under normal temperature, as well as residual bearing capacity after fire exposure. The results reveal that the maximum lateral deformation occurs near the middle of the span, with bending increasing as heating time and eccentricity rise. Despite a decrease in axial compressive load and bending capacity after fire exposure, the columns still exhibit desirable bearing capacity and deformability. Moreover, the obtained FE results align closely with experimental findings, validating the reliability of the developed numerical models. Additionally, this study proposes a simplified design method to calculate these mechanical property parameters, satisfying the ISO-834 standard. The relative errors between the proposed simplified formulas and FE models remain within 10%, indicating their capability to provide a theoretical reference for practical engineering applications.

콘크리트의 전단마찰 내력에 대한 횡보강근 및 압축응력의 영향 (Effect of Shear Reinforcement and Compressive Stress on the Shear Friction Strength of Concrete)

  • 황용하;양근혁
    • 콘크리트학회논문집
    • /
    • 제28권4호
    • /
    • pp.419-426
    • /
    • 2016
  • 이 연구에서는 다양한 콘크리트를 갖는 전단계면에서의 전단마찰거동에 대한 횡보강근 및 압축응력의 영향을 평가하였다. 12개 직접전단실험체로부터 균열진전, 전단하중-상대 미끄러짐 관계, 균열발생시 전단응력, 최대전단내력 및 횡보강근의 전단저항력 등이 측정되었다. 실험결과 동일 전단하중에서 상대 미끄러짐 제어에 대한 횡보강근 배근형상 및 콘크리트 압축강도의 영향은 미미하였다. 작용 압축응력의 증가와 함께 콘크리트의 전단전달력을 증가하는 반면, 횡보강근의 전단전달력은 감소하였는데, 횡보강근의 전단저항은 배근형태에 의해 영향을 받지 않았다. AASHTO-LRFD, Mattock 및 Hwang and Yang의 모델은 콘크리트의 전단마찰내력을 과소평가하였다. 반면, Hwang and Yang의 모델은 실험결과와의 비교에 대한 평균과 표준편차 값이 각각 1.02과 0.23으로서 기존 모델에 비해 다양한 변수의 영향을 적절히 고려하면서 콘크리트의 전단마찰내력을 잘 예측하였다.

긴 세장한 R/C 벽체의 연성능력 (Ductility Capacity of Slender-Wind R/C Walls)

  • 홍성걸
    • 한국지진공학회:학술대회논문집
    • /
    • 한국지진공학회 2000년도 춘계 학술발표회 논문집 Proceedings of EESK Conference-Spring
    • /
    • pp.202-212
    • /
    • 2000
  • This study investigates the ductility capacity of slender-wide reinforced concrete walls under predominant flexural moment loading. The experimental work for this study aims to provide design guidelines for bar detailing in critical regions under compressive stress in particular in case of slender-wide RC walls. According to the experimental observation the Bernoulli hypothesis of linear strain distribution is no longer valid and the ultimate compressive strain of concrete is significantly reduced, It is postulated that the nonlinear strain distribution causes the concentrated compressive stressed region and hence the premature crushing failure at the toe of walls. The reduced ultimate strain and nonlinear strain distribution need transverse reinforcement for confinement and more realistic models for the strength and displacement estimation of slender-wide RC wall.

  • PDF

고강도 콘크리트 기둥의 2계 거동에 관한 실험적 연구 (Experiments on Second -Order Behavior of High Strength Concrete Columns)

  • 김진근;양주경
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1992년도 가을 학술발표회 논문집
    • /
    • pp.167-172
    • /
    • 1992
  • To analyze the effects compressive strength of concrete and longitudinal steel ratio on second-order moment of columns, 30tied rein reinforced concrete columns with hinged ends were tested. The 80mm square cross section was used and the amount of eccentricity was 24mm. The compressive strengths of column specimens with slenderness ratios of 10, 60, and 100were 250, 648 and 880kg/$\textrm{cm}^2$, and the longitudinal steel ratios were 1.98%(4-D6) and 3.95%(8-D6). The ratio of ultimate load capacity to that of short column with the same eccentricity (Pu/Pn) was much decreased at high slenderness ratio with increasing the compressive strength of concrete. And the lateral displacement of slender column at the ultimate load was decreased as the strength was increased. These are due to that at high slenderness ratio the load capacity and behavior of column are affected by flexural rigidity. And, it was also found that with increasing steel ratio, the value of Pu/Pn and the lateral displacement at the ultimate load were larger for the same slenderness ratio.

  • PDF

고성능 철근콘크리트 보의 휨강도 및 연성능력에 관한 실험적 연구 (An Experimental Study on the Flexural Strength and Ductility Capacity of Reinforced High Performance Concrete Beams)

  • 김용부;고만영;김상우
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.501-506
    • /
    • 1998
  • This paper is an experimental study on the flexural strength and ductility capacity of reinforced high performance concrete beams with the concrete which has compressive strength of 600~700kg/$\textrm{cm}^2$, slump value of 20~25cm and slump-flow value of 60~70cm. Total 8 beams with different tensile reinforcement ratio and pattern of loading were tested. Form the results of reinforced high performance concrete beams, the equivalent stress block parameters proposed by MacGregor et al. or New Zealand code are recommended to use. Also, an extreme fiber concrete compressive strain of reinforced high performance concrete beams are distributed 0.0033~0.0048. In reinforced high performance concrete beams, reinforcement ratio in order to insure curvature ductility index 2 and 4 propose by ACI code should be less than those of reinforced normal strength concrete beams.

  • PDF

탄소섬유판으로 횡보강된 콘크리트 압축부재의 구조거동에 관한 실험적 연구 (An Experimental Study on the Structural Behavior of Reinforced Concrete Compressive Members Rehabilitated with Carbon Fiber Laminate)

  • 이희경;김성철;유성훈;김중구;정란
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.679-684
    • /
    • 1997
  • In this study, compressive strengths of reinforced concrete compression members rehabilitated with C.F.L. were analyzed from the test. Test parameters are spacing, spliced length, and section area of rehabilitation material. Displacement, failure load were measured during test. The failure mode and ultimate load were analyzed from these measured data. Test result shows that closer spacing of C.F.L. is more effective. strengthening with 1-ply C.F.L. is more effective than that of specimen with 2-ply C.F.L. The compressive capacity of specimen spliced ($\pi$.D)/2 shows almost similar strength to that of non-spliced specimen. The ultimate load carrying capacity of specimen strengthened with C.F.L. is increased to 1.11~1.68 times of that of non-rehabilitation specimen.

  • PDF