주석 및 아연 박막이 코팅된 베어링 표면의 구름 저항 거동에 대한 실험적 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Coated by Pure Tin and Zinc Films)

  • 양승호;공호성;윤의성;김대은
    • Tribology and Lubricants
    • /
    • 제14권1호
    • /
    • pp.1-6
    • /
    • 1998
  • An experimental study was performed to discover the tribological behaviors of pure tin and zinc coated 52100 bearing steel. Pure tin coatings ranging from 30 nm to 30,000 nm and pure zinc coatings ranging from 500 nm to 52,000 nm were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the effect of coating thickness on the tribological rolling behavior. Results showed that the existence of optimum film thickness which revealed minimum rolling resistance was discovered for tin and zinc coating. The compatibility of coating material to iron showed no significant effect on the rolling resistance behavior. The hardness of coating material revealed significant influence to the rolling resistance behavior.

주석 및 아연 박막이 코팅된 베어링 표면의 구름 저항 거동에 대한 실험적 고찰 (An Experimental Study on the Rolling Resistance of Bearing Surfaces Covered by Pure Tin and Zinc Films)

  • 양승호;공호성;윤의성;김대은
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1997년도 제26회 추계학술대회
    • /
    • pp.51-58
    • /
    • 1997
  • An experimental study was performed to discover the tribological behaviors of pure tin and zinc coated 52100 bearing steel. Pure tin coatings ranging from 30 nm to 30,000 nm and pure zinc coatings ranging from 500 nm to 52,000 nm were produced by a thermal evaporation coating method. Experiments using a thrust ball bearing-typed rolling test-rig were performed for the investigations of the effect of coating thickness on the tribological rolling behavior. Results showed that the existence of optimum film thickness which revealed minimum rolling resistance was discovered for tin and zinc coating. The compatibility of coating matehal to iron showed no significant effect on the rolling resistance behavior. The hardness of coating material revealed significant influence to the rolling resistance behavior.

  • PDF

STS316 용사코팅의 마모거동에 미치는 작용하중 및 미끄럼속도의 영향 (Effect of Applied Load and Sliding Speed on Wear Behavior of Thermally Sprayed STS316 Coating)

  • 이재홍;김영식
    • 동력기계공학회지
    • /
    • 제18권5호
    • /
    • pp.74-79
    • /
    • 2014
  • This article aims at investigating the effect of applied load and sliding speed on wear behavior of thermally spraryed STS316 coating. STS316 coatings were fabricated by flame spray process according to optimal parameters on steel substrates. Dry sliding wear tests were performed on STS316 coating using four different applied load as 10, 15, 20 and 25 N and four different sliding speed as 15, 30, 45 and 60 rpm. Wear behavior on worn surface was investigated using scanning electron microscope(SEM) and energy disperive X-ray spectroscopy(EDS). The dominant wear mechanism of STS316 coating under low applied load and sliding speed was oxidation on worn surface. However, under high applied load and sliding speed the principal wear mechanism was abrasion on oxidation film and damage of oxidation film.

레이저 다이오드 Mirror면의 Anti-Reflection 코팅 박막 제작 및 특성 분석 (The Manufacture and Properties Analysis of Anti-Reflection Coating Thin Film of Laser Diode Mirror)

  • 기현철;김선훈;김상택;김효진;김회종;홍경진;민용기;조재철;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 광주전남지부
    • /
    • pp.103-106
    • /
    • 2006
  • Semiconductor laser diode has a reflective facet in a both-ends side fundamentally. Laser performance for improving, Anti-Reflection and High-reflection coating on the facet of semiconductor laser diode. To prevent internal feedback from both facets for realizing superluminescent diode and reducing the reflection-induced intensity noise of laser diode, it's key techniques are AR/HR coatings. In the study AR coating film were manufactured by Ion-Assisted Deposition(IAD) system. Then manufactured coating film measurement electrical properties(L-I-V, Se, Resistor) and Optical properties (wavelength FFP)

  • PDF

스핀코팅 및 급속열처리 공정을 통해 형성된 Y2O3:Eu3+ 박막의 발광특성 (Luminescent Properties of Y2O3:Eu3+ Thin Film Through Spin-coating and Rapid Thermal Annealing Process)

  • 박재홍;정용석
    • 반도체디스플레이기술학회지
    • /
    • 제23권1호
    • /
    • pp.88-91
    • /
    • 2024
  • The europium doped yttrium oxide (Y2O3:Eu3+) thin film was formed on a Si substrate by the conventional spin-coating process followed by rapid thermal annealing (RTA) treatment. The spinning profiles such as rotation speed, acceleration and holding times were controlled during the spin-coating process for the best condition of the Y2O3:Eu3+ thin film. The RTA treatment was conducted for several temperature in order to crystallize the spin coated film. The Y2O3:Eu3+ thin film presented best performance in the conditions of 4000 rpm, 30 s and 10 s of rotation speed, acceleration time and holding time, respectively, at a fixed RTA temperature of 900 ℃.

  • PDF

A theoritical study on spin coating technique

  • Tyona, M.D.
    • Advances in materials Research
    • /
    • 제2권4호
    • /
    • pp.195-208
    • /
    • 2013
  • A comprehensive theory of the spin coating technique has been reviewed and the basic principles and parameters controlling the process are clearly highlighted, which include spin speed, spin time, acceleration and fume exhaust. The process generally involves four stages: a dispense stage, substrate acceleration stage, a stage of substrate spinning at a constant rate and fluid viscous forces dominate fluid thinning behaviour and a stage of substrate spinning at a constant rate and solvent evaporation dominates the coating thinning behaviour. The study also considered some common thin film defects associated with this technique, which include comet, striation, chucks marks environmental sensitivity and edge effect and possible remedies.

New Diffuser Film Using Coating Technology for LCD Backlight

  • Hwang, Hee-Nam;Choi, Woong-Hyun;Lee, Ki-Ho;Kim, In-Sun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2004년도 Asia Display / IMID 04
    • /
    • pp.1066-1067
    • /
    • 2004
  • New diffuser film for LCD backlight is developed. A diffuser film was manufactured through coating UV curable monomer on a plastic film. The diffuser layer coated on plastic film showed excellent optical transmittance.

  • PDF

1,2-Bis(2,4-dimethyl-5-phenyl-3-thienyl)-3,3,4,4,5,5-hexafluoro-1-cyclopentene을 사용한 유-무기 혼성 광 변색 코팅 막의 제조 및 특성 (Preparation and Characterization of Photochromic Organic-Inorganic Hybrid Coating Using 1,2-Bis(2,4-dimethyl-5-phenyl-3-thienyl)3,3,4,4,5,5-hexafluoro-1-cyclopentene)

  • 이창호;이상구;이종대
    • 폴리머
    • /
    • 제36권1호
    • /
    • pp.16-21
    • /
    • 2012
  • 광 변색 물질로 1,2-bis(2,4-dimethyl-5-phenyl-3-thienyl)-3,3,4,4,5,5-hexafluoro-1-cyclopentene(BTHFC)를 사용하는 유-무기 혼성 코팅막이 금속 알콕사이드인 tetramethoxysilane(TMOS), 다양한 실란 커플링제, 그리고 용매와 같은 다양한 반응 조건하에서 제조되었다. 제조된 코팅 막 중에서 상대적으로 비극성인 실린 커플링제를 사용한 경우, 광 변색 유기물인 BTHFC는 우수한 흡광도 및 소색속도를 나타내었다. 더욱이 용매 THF 존재 하에서 TMOS와 methacryloyloxypropyltrimethoxysilane(MPTMS)의 몰 비가 1:1로 하여 제조되었을 때 흡광도와 소색속도는 크고 빠른 것을 알 수 있었다. 연필강도는 TMOS의 함량이 증가할수록 증가한 반면, 투과도는 상대적으로 감소하였다.

졸겔법에 의한 알루미나 박막의 제조 및 특성(II);코팅용 알루미나 졸의 합성 및 박막 제조 (Preparation and Characterization of Alumina Thin Film by Sol-Gel Method (II); Synthesis of Alumina Sol for Coating and Preparation of Coating Films)

  • 이재호;최세영
    • 한국세라믹학회지
    • /
    • 제31권8호
    • /
    • pp.911-919
    • /
    • 1994
  • As the study for preparation of single-layer anti-reflective coating on glass, the conditions of synthesis of sol for coating and of reproducible coating procedure were investigated. In case of water-based sol, coating was impossible because of poor wettability of sol. The Substitution of solvent with ethanol improved the wettability of sol on the glass surface, and optimum amount of ethanol for substitution was 70 vol%. Maximum specific surface area and total pore volume of water-based sol were 268.7$m^2$/g and 0.315 cc/g, but after substitution, those values increased to 404.1 $m^2$/g and 0.376 cc/g, respectively. The upper limit withdrawl speed of coating in order to get clean coated films without aggregations or stains was 7 cm/min. In case of addition of 0.1 mol HNO3 and substitution with 70 vol% ethanol and heat-treatment at 40$0^{\circ}C$ for 1 hour, thin film with thickness of 94 nm was obtained at withdrawl speed of 4 cm/min. The thickness of thin film was independent of drying time.

  • PDF

옥외 청동문화재 보존을 위한 BTA 방청 피막의 특성에 미치는 코팅 조건의 영향 (Influence of Coating Process on Properties of BTA (Benzotriazole) Coating Film for Outdoor Bronze Artifacts Conservation)

  • 심규태;유영란;권용혁;김영식
    • 대한금속재료학회지
    • /
    • 제47권10호
    • /
    • pp.652-659
    • /
    • 2009
  • Many ancient and historical artifacts were made by copper and its alloys. In the case of outdoor exposure artifacts, the surface could be suffered from corrosion and tarnish by the reaction with its environment. In order to preserve the artifacts, surface treatment would be needed and BTA coating has been usually applied to tin-bronze. This paper dealt with the evaluation of the properties of BTA coated film using a linear polarization method and AC impedance measurement. On the base of corrosion rate and film resistance for the specimen formed by coating process, optimum coating conditions are as follows; 3 cycles brushing or 3 cycles spraying coatings for natural dried process and 1 cycle brushing coating or 5 cycles spraying coating for hot-air dried process.