• Title/Summary/Keyword: bar splice

Search Result 82, Processing Time 0.024 seconds

Evaluation on Stiffness of High-strength Mortar-filled Sleeve Bar Splice Under Cyclic Loading (반복하중이 작용하는 고강도 모르타르 충전식 슬리브 철근이음에 대한 강성 평가)

  • Kim, Hyong Kee;Chung, Goo Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.1
    • /
    • pp.85-93
    • /
    • 2013
  • In order to make a more reasonable evaluation on the stiffness of the high-strength mortar-filled sleeve bar splices under cyclic loading, we investigated and analyzed the existing experiment data of 106 full-sized reinforcing bar splices with test variables such as compressive strength of mortar, development length of reinforcement and sleeve type, etc. The following were found: 1) If mortar and the reinforcement development length with $f_{g^*}$(L/d) of more than 340 is used, the cast iron sleeve bar splices for SD350 and SD400 will have the stiffness of higher than A class of the AIJ code. 2) If mortar and the reinforcement development length with $f_{g^*}$(L/d) of more than 400 is used, the cast iron sleeve splices and pipe sleeve splices for SD500 will have the stiffness of higher than A class of the AIJ code.

Cyclic testing of weak-axis column-tree connections with formation of plastic hinge at beam splice

  • Oh, Keunyeong;Chen, Liuyi;Hong, Sungbin;Yang, Yang;Lee, Kangmin
    • Earthquakes and Structures
    • /
    • v.8 no.5
    • /
    • pp.1039-1054
    • /
    • 2015
  • The purpose of this study was to evaluate the seismic performance of weak-axis column-tree type connections used in steel moment frames. These connections are composed of a shop-welded and fieldbolted steel structure and can improve welding quality. On this basis, column-tree type connections are widely used in steel moment resisting frames in Korea and Japan. In this study, splices designed with a semirigid concept regarding the seismic performance of column-tree connections were experimentally evaluated. The structures can absorb energy in an inelastic state rather than the elastic state of the structures by the capacity design method. For this reason, the plastic hinge might be located at the splice connection at the weak-axis column-tree connection by reducing the splice plate thickness. The main variable was the distance from the edge of the column flange to the beam splice. CTY series specimens having column-tree connections with splice length of 600 mm and 900 mm were designed, respectively. For comparison with two specimens with the main variable, a base specimen with a weak-axis column-tree connection was fabricated and tested. The test results of three full-scale test specimens showed that the CTY series specimens successfully developed ductile behavior without brittle fracture until 5% story drift ratio. Although the base specimen reached a 5% story drift ratio, brittle fracture was detected at the backing bar near the beam-to-column connection. Comparing the energy dissipation capacity for each specimen, the CTY series specimens dissipated more energy than the base specimen.

Development of Staggered Grip Type Coupling for Improving the Workability in Reinforcing Bar (철근공사 작업성 향상을 위한 엇물림 그립 타입의 이음장치 개발)

  • Woo, Jong-Yeol;Hong, Seong-Wook;Yang, Jin-Kook;Park, Seung-Hwan
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.05a
    • /
    • pp.295-297
    • /
    • 2013
  • Reinforcing bar coupling method has a variety of ways including lap-splice method. However, there are problems that need to be improved in terms of constructability, economics analysis. We should be improved about the problems of the existing methods. Accordingly, this study were developed a new type of staggered grip type reinforcing bar coupling. The proposed method show the following effects than existing methods. First, this method can be reduce time through improved workability. Second, increasing safety through the slip removal. Third, improving economic efficiency by reduce the manufacturing costs.

  • PDF

Capacity and Length of Compression Lap Splice in Unconfined Concrete of 100MPa and Less Compressive Strength (횡보강근이 없는 100 MPa 이하 콘크리트의 철근 압축이음 강도와 이음길이)

  • Chun, Sung-Chul;Lee, Sung-Ho;Oh, Bo-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.5
    • /
    • pp.659-666
    • /
    • 2010
  • Although the compression splice needs not be longer than the tension slice due to existence of end bearing, current design codes impose a longer compression lap splice than a tension lap splice in high strength concrete. Hence, new criteria for the compression lap splice including the effects of concrete strength need to be sought for economical design involving ultra-high strength concrete. An experimental study has been conducted with column specimens in concrete strength of 80 and 100 MPa. Test results show that the splice strength can be evaluated to be proportional to square root of compressive strength of concrete. Bar stress developed by end bearing is not affected by splice length and is expressed with a function of the square root of concrete strength. Mean value of stresses developed by end bearing is 16.5 square root of $f_{ck}$. The stresses developed by bond in compression splices are nearly identical to those in tension splices and, therefore, strength increment of compression splices is attributed to end bearing only. From regression analysis of 58 tests, a design equation is proposed for compression lap splice in 40 to 100 MPa of compressive strength of concrete. By the proposed equation, the anomaly of lap lengths in tension and compression is got rid of. In addition, the equation has a reliability equivalent to those of the specified strengths of materials.

An Experimental Study of Tension Properties on New Developed Up-Set Coupler (Up-Set Coupler 이음철근의 인장특성에 대한 실험적 연구)

  • Sim, Jong-Sung;Park, Cheol-Woo;Kang, Tae-Sung;Kim, Tae-Soo
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.5
    • /
    • pp.109-115
    • /
    • 2008
  • As structures are getting super-rise and large-sized, introducing the construction methods such as prefabrication of bar-meshes and complex method are being actively discussed to pursue the high quality of reinforced concrete, the simplification of field works, and the reduction of duration, as well as the study on how to connect reinforcing rods, which occurs while applying the same methods, is in progress Also, the pressure welded joint is a kind of method that heats the ends of reinforced bars locally and joint them, and after the pressure welding, the vulnerable part in the reinforced bar occur. Thus, in the construction field, the throughout quality control is necessary because of the delayed duration and the lowered construct ability. In this study, of the traditional lap splice method and the mechanical splice one, the screw coupler, we tried to look into through experiments the prefabrication method of bar-meshes, a typical joint method usually used for the joint parts for PSC structures applying the reinforced bar with its big diameter, and a newly-developed up-set coupler method. And we also examined the characteristic of tensile.

Flexural Behavior of Concrete Beams Reinforced with Lap Spliced FRP Bar (겹이음된 FRP 보강근으로 보강된 콘크리트 보의 휨거동)

  • Oh, Hongseob
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.13 no.1 s.53
    • /
    • pp.186-194
    • /
    • 2009
  • This is a part of the extensive ongoing investigation being carried out by author to develop appropriate design procedure of the concrete member reinforced with FRP rebars instead of conventional steel rebars. This study presents the experimental results of a research programme to assess the structural characteristics of spliced rebar in reinforced concrete members with FRP reinforcement. The test variables are the diameter of FRP rebar and the embedment length. The development length (ld) was calculated according to the ACI 440 for FRP rebars in concrete. A total of 14 concrete beams reinforced with spliced FRP rebars and 4 reference beams reinforced with non-spliced FRP rebars were tested. The effects of bar size (10, 13, 16 and 19 mm) and splice length (from 0.72 to 1.58ld) on the bond strength were empirically evaluated. The test results indicate that a modification factor of 1.3 and 1.6 is relatively sufficient for the bond development length of glass FRP rebars in order to achieve an adequate tension lap splice length.

Effect of Flexural Performance on U-Shaped Precast Concrete Beams with Noncontact Lapped Splice (비접촉 겹침 이음된 프리캐스트 U형 보의 휨성능에 미치는 효과)

  • Ha, Sang-Su;Kim, Seung-Hun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.6
    • /
    • pp.119-128
    • /
    • 2008
  • In this study, new moment-resisting precast concrete beam-column joint is proposed for moderate seismic regions. It has the connection reinforcing bars, penetrated the joint and lap-spliced with the bottom bars of precast U-shaped PC beam. To evaluate the performance for noncontact lapped splice, experimental and analytical works were conducted. Major variables for tests are the length of lap, the diameter of connection reinforcing bars, and the distance between lapped bars. Analytic research was performed nonlinear finite element method. Analytic research focused on crack pattern, load-deflection curve, comparison of internal force, evaluation of ductility strains of reinforcement bar. Results of experimental and analytical works show that the these variables has much influence on flexural strength and ductility, and joint behavior.

A Development of Small-diameter Composite Helical Spring Structure for Reinforcement of Fiber Splice (광섬유 융착 부위 중접용 미소 직경 복합재료 스프링 구조물 개발)

  • 윤영기;정승환;이우일;이병호;윤희석
    • Composites Research
    • /
    • v.16 no.2
    • /
    • pp.26-32
    • /
    • 2003
  • Optical fibers, for splice, are stripped of their plastic coatings with a plastic stripper and cut off at the end. Therefore, stripped fibers often receive accidental damages and sustain small flaws or cracks. As a result, the breaking strength of a fiber splice made under normal conditions is reduced to about 0.4∼1 ㎏ on the average, nearly one-tenth of the fiber's strength. This makes it necessary to reinforce the splice. One of the most practical and reliable methods for optical fiber splicing is fusion splicing, comprising the steps of tripping the plastic coatings from the two fiber ends to be splice, placing the two bare fiber ends in an end-to-end position, and of fusion splicing, such as are fusion. Generally, steel bar (SB) sleeve is used to reinforce this fusion-splicing region. However, this type of sleeve has a critical defect to keep optical lose after bent by a sudden load. New type of composite spring (CS) sleeve is developed to make up for the weak points in the SB sleeve. This sleeve has an effect on restoration to the original state after eliminating the bending load. The optical spectrum analyzes results show the availability of reinforcement for the fusion splicing optical fiber using small diameter composite springs under the various loading conditions.

An Evaluation of Lap Splice Length of Epoxy Coated Reinforcements Using Beam-End Test (보-단부 시험을 이용한 에폭시 도막 철근의 겹침 이음길이 평가)

  • Kim, Jee-Sang;Kang, Won Hyeak
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.2
    • /
    • pp.175-182
    • /
    • 2020
  • The application of epoxy coated reinforcements is increased as a means to prevent a corrosion of reinforcements embedded in reinforced concrete structures, However, epoxy coating may reduce the bond capacity between concrete and reinforcement, which results a longer development length and lap splice length. This paper aims to the possibility of modification in lap splice length from reduction of basic development length which was confirmed using a direct pull out test. Total 36 beam specimens were tested to compare the lap splice properties of normal and epoxy coated reinforcements with beam-end test for various lap lengths and diameters of reinforcements. According to the results on failure modes, deformations, and crack widths of this experiments, the modification factor of 1.2 should be used, though the direct bond capacity is assured through direct pull out test.