A new kind of 'All Ceramic Crown' could be manufactured by making improvements in the manufacturing technique for the current 'All Ceramic Crown' which does not use a special ceramic but rather a general one as a substitute. If we use the manufacturing technique for the 'All Ceramic Crown', metal coping and core are not produced. The effects of the new manufacturing technique for the 'All Ceramic Crown' are as follows: First. We do not need to use new material or special machinery or tools. Second. We can use general machinery and tools. Third. Using the basic 'All Ceramic Technique', we anticipate improvement in learning in our students. Forth. We can save effort, materials and time. Fifth. The technique also has advantages for esthetic 'temporary crown'.
Kim, Chong-Hyun;Park, Young-Bum;Kim, Sung-Tae;Lee, Keun-Woo
The Journal of Korean Academy of Prosthodontics
/
v.49
no.2
/
pp.152-160
/
2011
Purpose: The aim of this study was to evaluate the volumetric change of teeth after preparation for various designs and margin locations through Micro CT analysis (Skyscan 1076: SKYSCAN, Konitch, Belgium). Materials and methods: The 36 artificial teeth were used to determine reduction volume of upper central incisor. According to the restorative design these 36 teeth were divided into 4 groups and according to the marginal location each group was divided into 3 subgroups. The volume of unprepared teeth was obtained by using Micro CT and the volume of prepared teeth was obtained in the same method. The CT scanned images before and after preparation were superimposed. Results: The volume difference was significantly increased as follows: traditional laminate veneer < full laminate veneer < all ceramic crown < metal ceramic crown. One-way ANOVA and Tukey multiple comparison analyses were used to analyze the data in this study. In each group the volume difference was significantly increased as follows: 1 mm above CEJ < CEJ < 1 mm below CEJ (P<.05). The % volume difference of all ceramic crown and metal ceramic crown was 31 - 48% and that of laminate veneer was 14 - 30%. The volume difference of the traditional laminate veneer was 1/3 of that of metal ceramic crown. The full laminate (1 mm below CEJ) and all ceramic crown (1 mm above CEJ) showed a similar volume difference. Metal ceramic crown showed 13.7% more volume difference than all ceramic crown. Conclusion: There exists the difference in volumetric change according to designs of restoration and margin locations of preparation.
In this study, We tried to find out the fracture strength of zirconia coping all ceramic crown and collarless porcelain fused gold alloy crown as the compared group. Each of the collarless porcelain fused gold crown and zirconia all ceramic crown has been produced specimen 10 each. And after pasting them on the steel jig, it had load given at porcelain incisal edge by 130$^{\circ}$ and measured fracture strength by Universal Testing Machine and then We have results from that. 1. The average value of fracture strength suggested 950.49 N at collarless porcelain fused gold alloy crown, 656.81 N at zirconia coping all ceramic crown. 2. Fractured pattern showed that the whole of labial part was exposed in collarless porcelain fused gold crown, but porcelain of margin part did not show fracture in advance. In the practice, the concern that collarless might cause fracture strength to be weaken does not matter, we concluded zirconia all ceramic crown made fracture that only a part of labial porcelain was fractured. The combination of zirconia all ceramic crown and turned out to be excellent.
Purpose: The purpose of this study was to compare the fracture strength of the zirconia monolithic all-ceramic crowns according to the thickness(0.5 mm, 0.8 mm, 1.1 mm) and IPS Empress II ceramic crown of 1.5 mm thickness. Material and method: Eight crowns for each of 3 zirconia crown groups were fabricated using CAD/CAM system(Kavo, Germany) and eight Empress II crowns were made from silicone mold and wax pattern. Each crown group was finished in accordance with the specific manufacturer s instruction. All crowns were luted to the metal dies using resin cement and mounted on the testing jig in a universal testing machine. The load was directed at the center of crown with perpendicular to the long axis of each specimen until catastrophic failure occurred. Analysis of variance and Tukey multiple comparison test(p<.05) were applied to the data. Results and Conclusion: 1. The fracture strength of the zirconia monolithic all-ceramic crown was higher thickness increased(p<.05). 2 The fracture strength of 1.1 mm thickness zirconia monolithic all-ceramic crown was higher than the fracture strength of 1.5 mm thickness IPS Empress II crown(p<.05). 3. The fracture strength of 0.5 mm thickness zirconia monolithic all-ceramic crown exceeded maximum occlusal forces.
Purpose: To investigate the influence of crown margin design on the stress distribution and to localize critical sites in maxillary canine under functional loading by using three dimensional finite element analysis. Materials and Methods: The bite force of 100 N, 150 N, and 200 N was applied with an angulation of $45^{\circ}$ to the longitudinal axis of tooth. Six models were restored with IPS e.max (Ivoclar Vivadent, Schaan, Liechtenstein) with a different margin design. With lingual ledge and various thicknesses, three different core ceramics were designed in each model. Result: In the core ceramic, the maximum tensile stresses were found at the labiocervical region. In the veneering ceramic the maximum tensile stresses were found at the area where the force was applied in all models. Conclusion: Shoulder and chamfer margin types are acceptable for all-ceramic rehabilitations. A ledge on the core ceramic at cervical region may affect the strength of all-ceramic crowns.
Purpose: The purpose of this study was to compare the fracture strength of the zirconia monolithic all-ceramic crowns according to the thickness (0.5mm, 0.8mm, 1.1mm) and metal-ceramic crowns (1.0mm, 1.5mm) Material and method: Twelve crowns for each of 3 zirconia crown groups were fabricated using CAD/CAM system (Kavo, Germany) and twelve crowns for each of 2 metal-ceramic crown groups were made by the conventional method. All crowns were luted to the metal dies using resin cement. Half of the specimens were exposed to thermocycling ($5-55^{\circ}C$, 1 Hz) and cyclic loading (300,000 cycles, 50N). Subsequently, all crowns were mounted on the testing jig in a universal testing machine. The load was directed at the center of crown with perpendicular to the long axis of each specimen until catastrophic failure occurred. Analysis of variance and Tukey multiple comparison test (P<.05) were used for statistical analysis of all groups, and paired t-test (P<.05) was followed for statistical comparison between each groups' fracture load before and after cyclic loading. Results: 1. The fracture strength of the zirconia monolithic crowns and the metal-ceramic crown increased as thickness increased (P<.05). 2. The cyclic loading and thermocycling significantly decreased the fracture strength of the zirconia monolithic crowns (P<.05). 3. The standard deviation of fracture strength of the zirconia monolithic crowns was very low. Conclusion: The fracture strength of the zirconia monolithic crowns for the posterior area tends to be higher with thickness increased and 0.8mm or over in thickness is recommended to have similar or over the fracture strength of metal-ceramic crowns.
The purpose of this study was to compare the fracture strengths and the fracture patterns of several hybrid-ceramic crowns and metal-ceramic crown. Ten crowns were constructed for each group according to the manufacturer's instruction. Removable template of silicone rubber impression material was used for standardization of each crowns. Each crown was cemented on a metal die with hybrid glass ionomer cement. All crowns cemented were stored in distilled water, $36^{\circ}C$ for 24 hours prior to loading in an universal testing machine. The load was directed at 130 degrees the long axis of metal die. The fracture strengths were measured and the fracture patterns were observed. The following results were obtained from this study 1. The mean fracture strengths of $Artglass^{(R)}$, $Sculpture^{(R)}$ and $Targis^{(R)}$ were $57.5{\pm}9.5Kgf,\;62.7{\pm}12.2Kgf$ and $60.2{\pm}10.1Kgf$ respectively. There was no significant difference among each hybrid ceramic crown group. 2. The toad required to fracture hybrid-ceramic crowns was significantly smaller than metal-ceramic crowns($131.7{\pm}22.0Kgf$). 3. In the metal-ceramic crowns, labial porcelain detached partially from porcelain-metal junction of proximal side by load. 4. Hybrid-ceramic crowns showed a simple fracture pattern that fracture line began at the loading area and extended through proximal surface, perpendicular to the margin. The crown was separated into two parts of labial side and lingual side. Above results revealed that three kinds of the hybrid-ceramic crowns used in this study must have careful application in clinical use since the strength of hybrid-ceramic crown was lower(about 1/2) than that of metal-ceramic crown.
Journal of the Korean Academy of Esthetic Dentistry
/
v.11
no.1
/
pp.11-15
/
2002
The black triangle is a common clinical finding in aged people with gingival recessions. Among other prosthetic treatment molalities such as composite resin filling and laminate venners, the all ceramic restoration procedure can lead to most successful result. With improved bonding strength and ceramic properties, the tooth preparation design for all-ceramic crown can be modified to minimize the reduction of sound tooth structure without loosing properties of conventional preparation design. Case selection is an important factor in acheiving succesful prosthesis. In this case report, the leucite reinforced pressable ceramic, $Authentic^{TM}$ [Ceramay, Germany] was used to fabricate the prosthesis.
This investing was carried out to evaluate the alteration of stress distribution on teeth and esthetic crowns. Analyzing the stress distribution by the two-dimensional finite element methods, a model of lower 1st molar according to the porcelain fused metal crown an the porcelain fused glass ceramic core crown and the all glass ceramic crown. 1. The pattern of stress distribution showed no apparent differences. 2. The greatest von Mises values were concentrated around the central fossa of all esthetic crowns. The greatest Maximum principle value were concentrated around the interface between the base of esthetic crown and the abutment tooth. It was found that the apatite glass ceramic could be applicable for use in dental crown prosthesis.
Purpose: In this study, we tried to compare marginal accuracy when produce ceramic crown using all ceramic materials and existent metal-ceramic system. Material and methods: All-ceramic systems were E-max (Ivoclar/Vivadent, Lichtenstein), Lava(3M, U.S.A.) and Wol-ceram(Teamziereis, Germany). Metal-ceramic system(PFG) was composed of Au-Pt alloy (Metalor, Switzerlandand) and overlying ceramic(D-sign, Ivoclar/Vivadent, Lichtenstein). We fabricated metal master die with upper diameter of 7.95mm, bottom diameter of 9.00mm, height of 5.00mm, and taper of $6^{\circ}$. All ceramic system used 0.5mm thickness ceramic coping, while metalceramic system used 0.3 thickness metal coping. By adding dentin and enamel ceramics on each coping, a crown with a proximal thickness of 1.0 mm and occlusal thickness of 2.0mm was fabricated. Pressure of 2kg was applied for 10 seconds on each crown with static load compressor. Before and after cementation, we measured the marginal gap at 4 points of each crown using optical microscope. The data was analyzed using a Student's t test and repeated-measures of analyses of variance(ANOVA) followed by a Bonferroni test. A p value<0.05 was considered significant. Results: As experiment results, marginal accuracy of wol-ceram and Lava is no good when compared with marginal accuracy of PFG. But marginal accuracy of E.max is good when compared with PFG. This result showed not significant. The marginal accuracy of E.max is good when compared with marginal accuracy of wol-ceram and Lava. Conclusion: The marginal accuracy of E.max is very good when compared with marginal accuracy of another group.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.