실내 가속부식시험을 통한 해양 강관합성 말뚝의 방식 기법 수명 평가 (Evaluation of Life Time for Anti-Corrosive Methods for Marine Steel Sheet by Cyclic Corrosion Test)

  • 박종원;이종구;이경황;김진홍;정문경;이주형
    • Corrosion Science and Technology
    • /
    • 제8권6호
    • /
    • pp.243-250
    • /
    • 2009
  • When a steel sheet pipe applied to marine environment, an anti-corrosive coating should be treated to obtain long-term life-time for steels, especially, splash zone. Although anti-corrosive property of coatings is required to be tested in real marine environment, it is difficult because of long test time such as 20 years or more time. Therefore, we used cyclic corrosion tester in a laboratory, which has similar conditions with salt-dry-wet process such as real marine environment. Anti-corrosive properties of the coatings and two steels were tested their anti-corrosive properties under cyclic corrosion test conditions(KS D ISO 14993) and the results were compared with estimate life-time in real marine environment. According to cyclic corrosion test, accelerated corrosive factor of each anti-corrosive coating was investigated accelerated corrosive factor from impedance with EIS method. Accelerated corrosive factor of type SS400 carbon steel and A690 was also investigated their accelerated corrosive factor from the regression curves of weigh loss results. One of the anti-corrosive coatings showed about 50 years life-time compared with standard sample life-time. Carbon steel SS400 showed from 0.1 mm/yr to 0.06 mm/yr as its corrosion rate.

급속 촉진 탄산화 시험을 통한 플라이애쉬 콘크리트의 탄산화 특성 연구 (A Study on the Carbonation Characteristics of Fly Ash Concrete by Accelerated Carbonation Test)

  • 최성;이광명;정상화;김주형
    • 콘크리트학회논문집
    • /
    • 제21권4호
    • /
    • pp.449-455
    • /
    • 2009
  • 최근 각종 산업화에 따른 탄산가스 배출량의 증가는 철근콘크리트구조물의 탄산화를 촉진시켜 구조물의 내 구성을 저하시키고 있다. 이미 선진 각국에서는 탄산가스 증가량을 고려하여 철근콘크리트구조물의 탄산화에 관한 안 전 관리 대책을 마련하고 있지만 현재까지도 실 구조물의 탄산화를 정확하게 예측하기 어렵고 탄산화 측정하기 위해서 는 많은 시간과 노력이 소요된다. 최근에 개발된 급속 촉진 탄산화 시험은 대기 중 $CO_2$농도를 100%로 하여 보다 신속 하게 탄산화 시험 결과를 제공할 수 있다. 본 논문에서는 플라이애쉬 콘크리트의 탄산화 특성을 알아보기 위하여 기존 에 주로 사용된 촉진 탄산화 시험과 급속 촉진 탄산화 시험에 의한 탄산화 결과를 비교, 분석하였다. 또한 장기재령에 서 플라이애쉬 콘크리트의 탄산화 특성을 알아보기 위하여 급속 촉진 탄산화 시험을 이용하여 재령 180일의 콘크리트 시편의 탄산화 실험을 수행하였다. 그 결과 플라이애쉬 콘크리트는 초기재령에서 탄산화에 다소 취약하였지만, 장기재 령에서는 OPC에 비하여 탄산화 저항성이 향상됨을 알 수 있었다.

Mg(OH)2 혼입 시멘트 페이스트의 탄산화 저항성에 관한 실험적 연구 (An experimental study on carbonation resistance of Mg(OH)2 mixed cement paste)

  • 진정심;이윤수;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 춘계 학술논문 발표대회
    • /
    • pp.165-166
    • /
    • 2017
  • Corrosion of reinforcement is the main factors affecting the durability of reinforced concrete in the world which lead to the failure of structures of reinforced concrete buildings. In this research, mixed brucite(Mg(OH)2) into ordinary portland cement paste in ratio of 5, 10 and 15% as a kind of CO2 fixation material. Samples were exposed to an accelerated carbonation enslavement of 20% CO2 concentration, 60% relative humidity, and a temperature of 20℃ until tested at 3d, 7d, 14d and 28d. After 28d CO2 accelerated curing, in the paste containing MH megnesian calcite was found by XRD and SEM-EDX. Meanwhile, paste containing Mg(OH)2 exhibit the better pore distribution than ordinary portland cement paste and relatively good compressive strength.

  • PDF

유압 피스톤 펌프의 수명 예측 연구 (A Study on Life Prediction of Hydraulic Piston Pump)

  • 김경수;이지환;강명철;유범상
    • 한국군사과학기술학회지
    • /
    • 제21권5호
    • /
    • pp.607-613
    • /
    • 2018
  • Hydraulic systems are widely used in the field of defense, construction machinery, agricultural machinery, and general industries, due to various advantages such as quick response speed and precision control. The defense equipments such as light rescue vehicle is operated in very harsh environments, so hydraulic components used in defense equipment are required to have very high reliability. In particular, hydraulic piston pump is very important component in a hydraulic systems, so life prediction of pump is essential. Therefore, in this study, we analyze the potential failure and the main failure mode of the hydraulic piston pump for the light rescue vehicle through the FMEA analysis, and predict the life of the pump by the accelerated life test considering the usage conditions.

중장비용 우레탄 도료 내후성 가속시험 (Accelerated Weathering Test of Urethane Paint for Heavy Construction Equipment)

  • 김대용;김영준
    • 한국신뢰성학회지:신뢰성응용연구
    • /
    • 제1권2호
    • /
    • pp.79-93
    • /
    • 2001
  • Recently, new aspects of paints such as a beautiful appearance, use of environmentally friendly paints, etc., in addition to the superior performance of paints have been requested for industrial paints including the paints for heavy construction equipment and others. Particularly, the quality of appearance of coating affects the sales of heavy construction equipment. And the necessity for the paints to have a superior weather-proof property without changing the luster or color even after long-time exposure to the open air is emphasized. The change in the surface color and luster of the paint due to the natural environment progresses very slowly, and it takes a long time to verify material properties when developing new paints. In order to improve such methods, weathering tests are performed in many laboratories as a test for accelerating aging of coating, and the lifetime of the products is estimated through evaluation of the weathering (environment-proof) quality of paints. However, not a great deal of research activity has been conducted up to the present time since the interrelationship between the actual results of testing and field data is different for each paint and it takes a long time to study relevant materials. Therefore, introduced in the present study is the estimation of the change in the quality of appearance of coating in the field through the accelerated aging test among the cases of improvement of the quality of appearance of the urethane paint for heavy construction equipment.

  • PDF

고도수처리 환경에 노출된 에폭시 수지계 방수/방식재의 침식 저항성 평가에 관한 실험적 연구 (An Experimental Study on the Deteriorative Resistance of Epoxy Resin Waterproofing Phase under Advanced Water and Wastewater Treatment)

  • 오상근;장성주;김영삼;양승도
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.59-62
    • /
    • 2002
  • Recently, advanced system for water and wastewater treatment is introduced and operated because of water pollution and etc. One of this System makes use of O3(Ozone) for water and wastewater treatment. In airtight concrete structure, waterproofing phase as well as water are affected by strong oxidative O3 in the long-term. For this reason, material stability against O3 is examined. Consequently, the purpose of this study is to find out material stability an object of epoxy resin by way of accelerated O3 testing.

  • PDF

고화매트의 내구성 향상을 위한 시스템 개선의 실험적 연구 (An Experimental Study on Solidifying Mat of System Improving for Durability Improving)

  • 홍성록;이정윤;김영삼;박헌일;조병영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.108-109
    • /
    • 2014
  • The purpose of this study is to enhance durability of solidifying mat. solidifying mat excellent mechanical properties of geotextile. multi-layer coating system is applied to the mat and the chloride ions penetration resistance, chemical resistance, accelerated carbonation test were evaluated by testing the durability. Durability test results are as follows. chloride ions penetration resistance results are coated mat is approximately 70 % lower than plain. chemical resistance test results are coated mat no discoloration. accelerated carbonation test results are coated mat is approximately 90 % lower than the plain.