Study on Wear Characteristics of Lubricants with Nano-diamond Additives (나노다이아몬드가 첨가된 윤활제의 마모 특성 연구)

  • Kim, Seung Taek;Kim, Seung Mok;Park, Tae Hee;Lee, JungSeok;Lee, YoungZe
    • Tribology and Lubricants
    • /
    • v.30 no.5
    • /
    • pp.291-294
    • /
    • 2014
  • Multiple additives can help improve the performance of generally used lubricants. These additives include MoS2, cadmium, chloride, indium, sulfide, and phosphide, which are harmful to both humans and the environment. Thus, researchers in this industry have been trying to reduce the use of these additives by finding alternatives. Nanodiamonds are one of these candidates. Nanodiamond particles are very hard, chemically stable, and highly heat-conductive. This research involved uniformly dispersing nanodiamond particles in marine engine oils via a matrix synthesis method at various concentrations (0, 0.1, 0.3, 0.5, and 1.0 wt). Friction and wear tests involved constant loads on ball-on-disk specimens, where the ball was AISI 51200 steel, the disk was AISI 1020 steel, and the sliding speed was 0.217 m/s. The lowest wear occurred at a suitable concentration of nanodiamonds (0.3 wt). However, excessive amounts of nanodiamonds caused them to act as abrasive debris because of their hardness, which increased the wear amount. The friction coefficient decreased as the nanodiamond concentration increased because their octagonal, almost spherical shape caused them to act as rolling contact elements between two surfaces.

Effect of Nitrogen Ion Implantation on Wear Behavior of Biocompatible Ti Implant (질소이온 주입이 생체적합성 티타늄 임플란트의 마모특성에 미치는 영향)

  • Byeon, Eung-Seon;Kim, Dong-Su;Lee, Gu-Hyeon;Jeong, Yong-Su
    • 연구논문집
    • /
    • s.30
    • /
    • pp.137-145
    • /
    • 2000
  • Since the concept of osseointegration was introduced, titanium and titanium-based alloy materials have been increasingly used for bone-anchored metal in oralmaxillofacial and orthopedic reconstruction. Successful osseointegration has been attributed to biocompatibility and surface condition of metal implant among other factors. Although titanium and titanium alloys have an excellent over the metal ion release and biocompatibility, considerable controversy has developed over the metal ion and wear debris in vivo and vitro. In this study, nitrogen ion implantation technique was used to improve the corrosion resistance and wear property of titanium materials, ultimately to enhance the tissue reaction to titanium implants As ion implantation energy was increased, projected range of nitrogen ion the Ti substrate was gradually increased. Under condition of constant ion energy. atomic concentration of nitrogen was also increased with ion doses. The friction in Hank's solution was increased with ion doses. The friction coefficient of ion implanted specimens in HanK's solution was increased from 0.39, 0.47 to 0.52, 0.65 respectively under high energy and ion dose conditions. As increasing ion energies and ion dose, amount of wear was reduced.

  • PDF

Wear properties of (Ti$_{1-x}$Cr$_{x}$)N coatings deposited by ion-plating method (이온 플레이팅법으로 제조한 (Ti$_{1-x}$Cr$_{x}$)N 박막의 마모특성에 관한 연구)

  • 이광희;박찬홍;이정중
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.2
    • /
    • pp.125-134
    • /
    • 2001
  • ($Ti_{1-x}$ $Cr_{x}$ )N coatings were deposited by an ion-plating method in a reactor with two separate metal sources, Ti and Cr. Ti was evaporated using an electron beam, while Cr evaporation was carried out by resistant heating. The Ti and Cr concentrations in the coatings were controlled by the Ti and Cr evaporation ratio. The coating hardness increased with increasing the Cr content(x) and showed a maximum value of 6,000 HK at around x=0.8. The critical load of the coatings, measured by the scratch test, was around 30 N. The wear resistance properties of the ($Ti_{1-x}$$Cr_{ x}$)N coatings were evaluated using a CSEM pin-on-disk type tribometer. A Cr-steel ball as well as a SiC ball, which had hardness values of 590 HK and 2,600 HK respectively, were used as the pin. After the wear test, the surface morphology, roughness and the concentration of the coatings were investigated, with the main focus being on the effect of wear debris and the transferred layer on the wear behavior.

  • PDF

Foreign Body Reaction after Implantation of a Device for Intervertebral Assisted Motion

  • Seo, Jun-Yeong;Ha, Kee-Yong;Kim, Young-Hoon;Ahn, Joo-Hyun
    • Journal of Korean Neurosurgical Society
    • /
    • v.59 no.6
    • /
    • pp.647-649
    • /
    • 2016
  • The device for intervertebral assisted motion (DIAM) is a dynamic implant that consists of a silicone bumper enveloped by a polyethylene terephthalate (PET) fiber sack. Silicone and PET were used because of their biological inertness, but repetitive motion of the spine can cause wear on the implant nonetheless. The purpose of this study is to report a case of foreign body reaction (FBR) against a DIAM. A 72-year-old female patient presented with lower back pain and both legs radiating pain. She had undergone DIAM implantation at L4-5 for spinal stenosis 5 years previously. The intervertebral disc space of L4-5, where the DIAM was inserted, had collapsed and degenerative scoliosis had developed due to left-side collapse. MRI showed L3-4 thecal sac compression and left L4-5 foraminal stenosis. The patient underwent removal of the DIAM and instrumented fusion from L3 to L5. During surgery, fluid and granulation tissue were evident around the DIAM. Histopathology showed scattered wear debris from the DIAM causing chronic inflammation due to the resulting FBR. A FBR due to wear debris of a DIAM can induce a hypersensitivity reaction and bone resorption around the implant, causing it to loosen.

Wear behaviors of HVOF spray coating of Co-alloy T800

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Park, Bong-Kyu;Youn, Suk-Jo;Back, Nam-Ki;Chun, Hui-Gon
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.16 no.3
    • /
    • pp.121-126
    • /
    • 2006
  • HVOF thermal spray coating of Co-alloy T800 is progressively replacing the classical hard coatings such as chrome plating because of the very toxic $Cr^{6+}$ ion known as carcinogen causing lung cancer. For the study of the possibility of replacing of chrome plating, the wear properties of HVOF Co-alloy T800 coatings are investigated using the reciprocating sliding tester both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$. The possibility as durability improvement coating is studied for the application to the high speed spindles vulnerable to frictional heat and wear. Wear mechanisms at the reciprocating sliding wear test are studied for the application to the systems similar to the sliding test such as high speed spindles. Wear debris and frictional coefficients of T800 coatings both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$ are drastically reduced compared to those of non-coated surface of parent substrate Inconel 718. This study shows that the coating is recommendable for the durability improvement coatings on the surfaces vulnerable to frictional heat. The sliding surfaces are weared by the mixed mechanisms such as oxidative wear, abrasion by the sliding ball slurry erosion by the mixture of solid particles and small drops of the melts and semi-melts of the attrited particles cavitation by the relative motions among the coating, sliding ball, the melts and semi-melts. and corrosive wear. The oxide particles and the melts and semi-melts play roles as solid and liquid lubricant reducing the wear and friction coefficient.

A Study on the Friction and Wear Properties of Tribaloy 800 Coating by HVOF Thermal Spraying

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Song, Ki-Oh;Back, Nam-Ki;Chun, Hui-Gon;Hwang, Soon-Young
    • Journal of the Korean institute of surface engineering
    • /
    • v.39 no.5
    • /
    • pp.240-244
    • /
    • 2006
  • Tribaloy 800 (T800) powder is coated on the Inconel 718 substrate by the optimal High Velocity Oxy-Fuel (HVOF) thermal spray coating process developed by this laboratory. For the study of the possibility of replacing of the widely used classical chrome plating, friction, wear properties and sliding wear mechanism of coatings are investigated using reciprocating sliding tester both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C). Both at room temperature and at $538^{\circ}C$, friction coefficients and wear debris of coatings are drastically reduced compared to those of non-coated surface of Inconel 718 substrate. Friction coefficients and wear traces of both coated and non-coated surfaces are drastically reduced at higher temperature of $538^{\circ}C$ compared with those at room temperature. At high temperature, the brittle oxides such as $CoO,\;Co_3O_4,\;MoO_2,\;MoO_3$ are formed rapidly on the sliding surfaces, and the brittle oxide phases are easily attrited by reciprocating slides at high temperature through complicated mixed wear mechanisms. The sliding surfaces are worn by the mixed mechanisms such as oxidative wear, abrasion, slurry erosion. The brittle oxide particles and melts and partial-melts play roles as solid and liquid lubricant reducing friction coefficient and wear. These show that the coating is highly recommendable for the durability improvement coating on the surfaces vulnerable to frictional heat and wear.

The Lubricant Effect of Oxidation and Wear Products of HVOF Co-alloy T800 Powder Coating

  • Cho, Tong Yul;Yoon, Jae Hong;Kim, Kil Su;Song, Ki Oh;Youn, Suk Jo;Chun, Hui Gon;Hwang, Soon Young
    • Corrosion Science and Technology
    • /
    • v.6 no.4
    • /
    • pp.159-163
    • /
    • 2007
  • Micron size Co-alloy 800 (T800) powder is coated on the high temperature, oxidation and corrosion resistant super alloy Inconel 718 substrate by the optimal high velocity oxy-fuel (HVOF) thermal spray coating process developed by this laboratory. For the study of durability improvement of high speed spindle operating without lubricants, friction and sliding wear behaviors of the coatings are investigated both at room and at an elevated temperature of $1000^{\circ}F(538^{\circ}C)$. Friction coefficients, wear traces and wear debris of coatings are drastically reduced compared to those of non-coated surface of Inconel 718 substrate both at room temperature and at $538^{\circ}C$. Friction coefficients and wear traces of both coated and non-coated surfaces are drastically reduced at higher temperature of $538^{\circ}C$ compared with those at room temperature. At high temperature, the brittle oxides such as CoO, $Co_{3}O_{4}$, $MoO_2$ and $MoO_3$ are formed rapidly on the sliding surfaces, and the brittle oxide phases are easily attrited by reciprocating slides at high temperature through oxidation and abrasive wear mechanisms. The brittle solid oxide particles, softens, melts and partial-melts play roles as solid and liquid lubricants reducing friction coefficient and wear. These show that the coating is highly recommendable for the durability improvement coating on the machine component surfaces vulnerable to frictional heat and wear.

The properties and wear behavior of HVOF spray coating layer of Co-alloy powder

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Back, Nam-Ki;Chun, Hui-Gon
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.16 no.6
    • /
    • pp.273-277
    • /
    • 2006
  • High velocity of oxy-fuel (HVOF) thermal spray coating is progressively replacing the other classical hard coatings such as chrome plating and ceramic coating by the classical methods, since the very toxic $Cr^{6+}$ ion is well known as carcinogen causing lung cancer, and the ceramic coatings are brittle. Co-alloy T800 powder is coated on the Inconel 718 substrates by the HVOF coating procesess developed by this laboratory. For the study of the possibility of replacing of chrome plating, the wear properties of HVOF Co-alloy T800 coatings are investigated using the reciprocating sliding tester with a counter sliding SUS 304 ball both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$. The possibility as durability improvement coating is studied for the application to the high speed spindles vulnerable to frictional heat and wear. Wear mechanisms at the reciprocating sliding wear test are studied far the application to the systems similar to the sliding test such as high speed spindles. Wear debris and frictional coefficients of T800 coatings both at room and at an elevated temperature of $538^{\circ}C$ are drastically reduced compared to those of non-coated surface of Inconel 718 substrates. Wear traces and friction coefficients of both coated and non-coated surfaces are drastically reduced at a high temperature of $538^{\circ}C$ compared with those at room temperature. These show that the coating is highly recommendable far the durability Improvement coating on the surfaces vulnerable to frictional heat and wear.

Effect of environment on the tribological behavior of Si-incorporated diamond-like carbon films (실리콘이 첨가된 다이아몬드상 카본 필름의 트라이볼로지적 특성에 미치는 환경변화의 영향)

  • 양승호;공호성;이광렬;박세준;김대은
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.42-48
    • /
    • 1999
  • An experimental study was performed to discover the effect of environment on the tribological behavior of Si-incorporated diamond-like carbon(Si-DLC) film slid on a steel ball. The films were deposited on Si(100) wafers from radio-frequency glow discharge of mixtures of benzene and dilute silane gases. Experiments using a ball-on-disk test-rig was performed under vacuum, dry air and ambient air conditions. It was observed that coefficient of friction was decreased as the environmental condition changes from vacuum, to dry air. It was also observed that the coefficient of friction decreased with increasing silicon concentration in the film. Chemical analyses of debris suggested that the low and stable friction coefficient is closely related to the silicon rich oxide debris and the rolling action.

  • PDF

Distortion of the Bottom Surface in Micro Cavity Machining Using MEDM (미세 캐비티 방전 가공에서 바닥면 형상 왜곡)

  • 임종훈;류시형;제성욱;주종남
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.20 no.12
    • /
    • pp.191-197
    • /
    • 2003
  • As mechanical components are miniaturized, the demand on micro die and mold is increasing. Micro mechanical components usually have high hardness and good conductivity. So micro electrical discharge machining (MEDM) is an effective way to machine those components. In micro cavity fabrication using MEDM, it is observed that the bottom surface of cavity is distorted. Electric charges tend to be concentrated at the sharp edge. At the center of the bottom surface, debris can not be drawn off easily. These two phenomena make the bottom surface of the electrode and workpiece distort. As machining depth increases, the distorted shape of electrode approaches hemisphere. This process is affected by capacitance and the size of electrode. By using a smaller electrode than the desired cavity size and appropriate tool movement, bottom shape distortion can be prevented.