• Title/Summary/Keyword: WT1

Search Result 6,265, Processing Time 0.028 seconds

Carbon Nanotube/Nafion Composites for Biomimetic Artificial Muscle Actuators

  • Lee, Se-Jong;Yoon, Hyun-Woo;Lee, Deuk-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.4 s.299
    • /
    • pp.198-201
    • /
    • 2007
  • Multi-walled carbon nanotube (M-CNT)/Nafion nanocomposites were prepared by solution casting to elucidate the effect of M-CNT addition, from 0 to 7 wt%, on the viscoelastic behavior of the composites. The M-CNT bundles induced by the Nafion polymer were determined to be uniformly distributed for the 1 wt% M-CNT/Nafion nanocomposites. The 1 wt% M-CNT/Nafion composite exhibited the highest blocking stress of 2.3 kPa due to its high elastic modulus of 0.485 GPa. From a dynamic mechanical analysis, the 1 wt% M-CNT had the highest storage and loss moduli compared with the other samples in all frequency and temperature ranges. From the storage modulus data, the M-CNT loaded composites had similar $T_g$ values near $120^{\circ}C$. The glass transition temperatures of the M-CNT loaded composites were $120^{\circ}C$ (1 wt%), $117^{\circ}C$ (3 wt%), $117^{\circ}C$ (5 wt%), and $135^{\circ}C$ (7 wt%), suggesting that the effect of the M-CNTs on the Nafion film begins at 1 wt%. Thus, it has been concluded that the 1 wt% M-CNT disported composite is attractive for actuator applications.

Geochemical Composition of Volcanic Ash from Historical Eruptions of Mt. Baekdu, Korea (역사시대에 분화한 백두산 화산재의 화학 성분)

  • Yun, Sung-Hyo;Koh, Jeon Seon;Chang, Cheolwoo
    • The Journal of the Petrological Society of Korea
    • /
    • v.27 no.1
    • /
    • pp.37-47
    • /
    • 2018
  • Volcanic ash samples of historical eruptions from Mt. Baekdu were analyzed for major oxides, trace and rare earth elements by a variety of analytical techniques. The results indicate that the ashes consist of approximately 58.8~71.1 wt.% $SiO_2$, 9.6~16.8 wt.% $Al_2O_3$, 4.5~6.9 wt.% $Fe_2O_{3t}$, 0.1~1.7 wt.% MgO, 0.3~1.6 wt.% CaO, 5.2~6.3 wt.% $Na_2O$, 4.3~5.9 wt.% $K_2O$ and less than 1.2 wt.% $TiO_2$. Thirty two trace metals including Ba, Cu, Cr. Co, Ni, Sr, V, Zn, and Zr were analyzed. The ashes can be divided two groups: group A(1 ka Millennium pumice, 1668 and $190{\underline{3}}$ pumice) and group B(1702 pumice) according to the relative enrichment of HREEs. The abundances of heavy metals such as Cu, Co, Mn, and Zn were relatively low. As compared to the Sakurajima volcanic ash, Baekdusan volcanic ash has low concentrations of Y, Nb, Pb, U, Sc, V, Ni and Cu and high concentrations of Zr, Ba, Hf, Cr, Co, Zn and rare-earth (except Eu).

Separation of $H_2$ and $N_2$ by PDMS-NaYZeolite Composite Membranes (PDMS-NaYZeolite 막에 의한 수소-질소 분리에 관한 연구)

  • Ha, Jung-Im;Kang, Tae-Beom
    • Membrane Journal
    • /
    • v.20 no.1
    • /
    • pp.47-54
    • /
    • 2010
  • The PDMS-NaYzeolite composite membranes were prepared by adding 1~40 wt% NaYzeolite to PDMS. In order to investigate the characteristics of these membranes, we used the analytical methods such as FT-IR, $^1H$-NMR, and SEM. The permselectivity of $H_2$ and $N_2$ gases through the composite membranes was studied as a function of NaYzeolite contents. The permeability and selectivity ($H_2/N_2$) of PDMS membrane increased as the gas permeation pressure increased. The permeability of the PDMS-NaYzeolite composite membranes increased when 1~10 wt% NaYzeolite was added, and then decreased at higher wt% as NaYzeolite content increased. The selectivity ($H_2/_2$) of PDMS-NaYzeolite composite membranes decreased when 1~2 wt% NaYzeolite was added, and then increased as NaYzeolite content increased. As the $H_2$ permeability increased, the selectivity ($H_2/N_2$) of PDMS-NaYzeolite composite membranes decreased at 0~2 wt% and 10~40 wt% NaYzeolite contents, increased at 2~10 wt% NaYzeolite content.

Mechanical properties of bamboo-epoxy composites a structural application

  • Biswas, Sandhyarani
    • Advances in materials Research
    • /
    • v.1 no.3
    • /
    • pp.221-231
    • /
    • 2012
  • In this study, the physical and mechanical properties of bamboo fiber reinforced epoxy composites were studied. Composites were fabricated using short bamboo fiber at four different fiber loading (0 wt%, 15 wt%, 30 wt% and 45 wt%). It has been observed that few properties increases significantly with respect to fiber loading, however properties like void fraction increases from 1.71% to 5.69% with the increase in fiber loading. Hence, in order to reduce the void fraction, improve hardness and other mechanical properties silicon carbide (SiC) filler is added in bamboo fiber reinforced epoxy composites at four different weight percentages (0 wt%, 5 wt%, 10 wt% and 15 wt%) by keeping fiber loading constant (45 wt%). The significant improvement of hardness (from 46 to 57 Hv) at 15 wt%SiC, tensile strength (from 10.48 to 13.44 MPa) at 10 wt% SiC, flexural strength (from 19.93 to 29.53 MPa) at 5 wt%SiC and reduction of void fraction (from 5.69 to 3.91%) at 5 wt%SiC is observed. The results of this study indicate that using particulate filled bamboo fiber reinforced epoxy composites could successfully develop a composite material in terms of high strength and rigidity for light weight applications compared to conventional bamboo composites. Finally, SEM studies were carried out to evaluate fibre/matrix interactions.

Hydrogen Storage Properties of Zr-Based AB2-x Mx Metal Hydrides Made by Hydriding Combustion Synthesis (HCS) (자전연소합성법으로 제조한 Zr계 AB2-x Mx 금속수소화물의 수소저장특성)

  • Hur, Tae Hong;Han, Jeong Seb;Kim, Jin Ho
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.3
    • /
    • pp.256-262
    • /
    • 2012
  • This study investigated the hydrogen storage properties of Zr-Based $AB_{2-x}M_x$ metal hybride made by HCS (Hydriding Combustion Synthesis). The materials were prepared by HCS 80 wt% $AB_2$-15 wt% Mg-5 wt% Mm, HCS 80 wt% $AB_2$-20 wt% Mg and pure Zr-Based $AB_2$, These materials were activated at 298 K under 20 bar. Both HCS 80 wt% $AB_2$-20 wt% Mg and HCS 80 wt% $AB_2$-15 wt% Mg-5 wt% Mm were absorbed within 1 minute. In the case of the $AB_2$, it was perfectly absorbed within 6 minutes. Then, the materials were evaluated to obtain P-C-T (Pressure-Composition-Temperature) curves at 298K. As a result, the hydrogen storage capacity of HCS 80 wt% $AB_2$-20 wt% Mg, HCS 80 wt% $AB_2$-15 wt% Mg-5 wt% Mm and pure Zr-Based $AB_2$ were determined to be 1.2, 1.6 and 1.74 wt%, respectively. The activation energy and rate controlling step were calculated by the Johnson-Mehl Avrami equation. The activation energies of HCS 80 wt% $AB_2$-20 wt% Mg, HCS 80 wt% $AB_2$-15 wt% Mg-5 wt% Mm and pure Zr-Based $AB_2$ were 26.91, 20.45, and 60.41 kJ/mol, respectively. Also, the values of ${\eta}$ in the Johnson-Mehl Avrami equation for HCS 80 wt% $AB_2$-20 wt% Mg, HCS 80 wt% $AB_2$-15 wt% Mg-5 wt% Mm and pure Zr-Based $AB_2$ are 0.60, 0.51, and 0.44. So, the rate controlling steps which indicate hydrogen storage mechanism are an one dimensional diffusion process.

Two-step Acid Hydrolysis Method for Producing Fermentable Sugar from Lignocellulosic Biomass (발효당 생산을 위한 목질계 바이오매스의 2단 산당화)

  • Park, Jang Han;Kim, Jun Seok
    • Korean Chemical Engineering Research
    • /
    • v.54 no.1
    • /
    • pp.1-5
    • /
    • 2016
  • For obtain fermentable sugar, we conducted acid hydrolysis with lignocellulosic biomass without enzyme. The lignocellulosic biomass used pinus rigida and Palm residues (EFB; empty fruit bunches). In the acid hydrolysis, we consider the hydrolysis condition to reduce a denatured sugar. So this study was conducted 2-step acid hydrolysis. First-step hydrolysis used high concentration (72 wt%) sulfuric acid at $80^{\circ}C$. At the condition, we obtained 11.49 wt%, 32 wt% glucose conversion for pinus rigida and EFB. After the step, the liquor was dilute until 9~15 wt% acid concentration and conducted second hydrolysis at $50{\sim}120^{\circ}C$. In the second hydrolysis, we obtained maximum glucose conversion (pinus rigida 86.8 wt% (39 g/L) and EFB 95.3 wt% (32.4 g/L)) at 9 wt% acid concentration and $120^{\circ}C$ for 80 min. All samples through the process are analyzed on the basis of mass balance.

Lightweight Porcelain using GHM(Glass Hollow Microsphere) (유리질 중공체 GHM(Glass Hollow Microsphere)을 활용한 자기의 경량화)

  • Kim, Geun-Hee;Choi, Hyo-Sung;Pee, Jae-Hwan;Cho, Woo-Seok;Kim, Kyeong-Ja
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.1
    • /
    • pp.74-79
    • /
    • 2011
  • The pore generation technology using GHM (Glass Hollow Microsphere) was studied in order to reduce the weights of porcelain. In this study, we verify the property of modified slurry by adding GHM. The modified slurry was prepared by adding 1.0~2.5 wt%(K1), 1.0~6.0 wt%(K37) of GHM to the slurry for porcelain. The slurry viscosity were stable inside a content range of 1.0~2.5 wt%(K1), 1.0~6.0 wt%(K37). However, the viscosity of modified slurry increased more than 3.0 wt%(K1) and 6.5 wt%(K37). The formed specimen by slip casting was fired at $1229^{\circ}C$, $1254^{\circ}C$. As the amount of GHM content increased, the weight decreased and the addition of 1.0~2.5 wt%(K1), 1.0~6.0 wt%(K37) of GHM resulted in a weight drop of 30%(K1) and 25(K37). However, when the GHM content increased, the strength decreases over 70%. This is caused by the presence of a large volume of surface defects (pores) and defects from the agglomeration of GHM.

Influence of Water Temperature on Egg Development of Surf clam, Spisula sachalinensis (북방대합, Spisula sachazinensis의 난 발생에 미치는 수온의 영향)

  • 이정용;장윤정;김영신;최윤희;장영진
    • Journal of Aquaculture
    • /
    • v.15 no.1
    • /
    • pp.39-42
    • /
    • 2002
  • Water temperature, at which Spisula sachdinensis egg successfully completed development ranges from 10 to $25^{\circ}C$. Within this range, the development duration is reduced with increasing temperature. The relationships between temperature (WT, $^{\circ}C$) and the required time (t: hour) from egg to each developmental stage are described as follows: 2-cell : 1/t = 0.0554 WT -0.3769; 8-cell : 1/t = 0.0210 WT -0.1142; Morula : 1/t = 0.0125WT -0.0712; Trochophore : 1/t = 0.0039 WT -0.0203; D-shaped larva : 1/t = 0.0024W T -0.0108. Biological minimum temperature for the egg development is 5.5$^{\circ}C$.

Improvement of Hydrogen Storage Properties of Mg by Addition of NbF5 via Mechanical Milling under H2

  • Kwak, Young Jun;Song, Jiyoung;Mumm, Daniel R.
    • Korean Journal of Materials Research
    • /
    • v.23 no.10
    • /
    • pp.562-567
    • /
    • 2013
  • A 90 wt% Mg-10 wt% $NbF_5$ sample was prepared by mechanical milling under $H_2$ (reactive mechanical grinding). Its hydriding and dehydriding properties were then examined. Activation of the 90 wt% Mg-10 wt% $NbF_5$ sample was not required. At n=1, the sample absorbed 3.11 wt% H for 2.5 min, 3.55 wt% H for 5 min, 3.86 wt% H for 10 min, and 4.23 wt% H for 30 min at 593K under 12 bar $H_2$. At n=1, the sample desorbed 0.17 wt% H for 5 min, 0.74 wt% H for 10 min, 2.03 wt% H for 30 min, and 2.81 wt% H for 60 min at 593K under 1.0 bar $H_2$. The XRD pattern of the 90 wt% Mg-10 wt% $NbF_5$ after reactive mechanical grinding showed Mg, ${\beta}-MgH_2$ and small amounts of ${\gamma}-MgH_2$, $NbH_2$, $MgF_2$ and $NbF_3$. The XRD pattern of the 90 wt% Mg-10 wt% $NbF_5$ dehydrided at n=3 revealed Mg, ${\beta}-MgH_2$, a small amount of MgO and very small amounts of $MgH_2$ and $NbH_2$. The 90 wt% Mg-10 wt% $NbF_5$ had a higher initial hydriding rate and a larger quantity of hydrogen absorbed for 60 min than the 90 wt% Mg-10 wt% MnO and the 90 wt% Mg-10 wt% $Fe_2O_3$, which were reported to have quite high hydriding rates and/or dehydriding rates. The 90 wt% Mg-10 wt% $NbF_5$ had a higher initial dehydriding rate (after an incubation period) and a larger quantity of hydrogen desorbed for 60 min than the 90 wt% Mg-10 wt% MnO and the 90 wt% Mg-10 wt% $Fe_2O_3$.

Fundamental Study on Recycling as Construction Material of Dredged Harbor Soil Mixed with Clay and Glass Frit (점토와 유리프리트를 혼합한 항만준설토의 건축자재 재활용에 관한 기초연구)

  • Im, Dong-Su;Kim, Kyung-Nam;Cho, Yeon-Bae;Park, Joon-Seok
    • Journal of the Korean Applied Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.575-585
    • /
    • 2013
  • This research was performed to evaluate the recycling feasibility as a construction material of dredged harbor soil mixed with clay and glass frit. Concentration of heavy metals of the dredged soil from D harbor was severly high, showing Zn of 526.0~13,150.1 mg/kg. The dredged soil was maily composed of 48.30 wt% $SiO_2$, 16.60 wt% $Al_2O_3$, 10.10 wt% CaO, 7.75 wt% $Fe_2O_3$. The clay and the glass frit contained 70.82 wt% $SiO_2$ and $Al_2O_3$ 18.78 wt%, and 71.75 wt% $SiO_2$, 13.99 wt% CaO, 8.51 wt% $Na_2O$, respectively. After adding 10~40 wt% to the clay and sintering them at $1,000^{\circ}C$ or $1,100^{\circ}C$, the compressive strength of the sintered specimens showed $132.6{\sim}178.5kgf/cm^2$ or $581.2{\sim}793.7kgf/cm^2$, respectively. In case of SC46 with the addition 40 wt% of the dredged soil to the clay, the compressive strength ($793.7kgf/cm^2$) of specimen sintered at $1,100^{\circ}C$ was over 5 times higher than that at $1,000^{\circ}C$. The specimen mixed with 40 wt% of dredged soil, 60 wt% of clay and 1 wt% of glass frit satisfied the 1st grade standard for clay brick by KS L 4201. The results of all specimens by Korean Standard Leaching Test also satisfied the standard criteria.