• 제목/요약/키워드: Uniaxial Compression Test

검색결과 282건 처리시간 0.029초

종이의 단축압축 표준시험법 개발

  • 김형진;엄기증;이태주;고승태;유영정
    • 한국펄프종이공학회:학술대회논문집
    • /
    • 한국펄프종이공학회 2007년도 추계학술발표논문집
    • /
    • pp.325-330
    • /
    • 2007
  • Uniaxial tensile test are generally much simpler than uniaxial compressive test. Uniaxial compressive test is experimentally more difficult because of the low buckling resistance of a sheet of paper. In order to avoid buckling, many researchers have applied various lateral restraint techniques to investigate paper uniaxial compression behavior. Adding unnecessary force to inhibit compressive deformation of the sheet is unwanted, but sufficient force must be used to inhibit buckling. This study has been carried out to develop new uniaxial compressive standard test method without exerting unnecessary force to paper specimen to prevent buckling.

  • PDF

입자결합모델을 이용한 횡방향 변형률 제어 하에서의 암석의 일축 및 삼축압축시험의 수치적 모사 (Numerical Simulation of Radial Strain Controlled Uniaxial and Triaxial Compression Test of Rock Using Bonded Particle Model)

  • 이창수;권상기;전석원
    • 터널과지하공간
    • /
    • 제21권3호
    • /
    • pp.216-224
    • /
    • 2011
  • 본 연구에서는 Class II 거동에 대해 입자결합모델을 이용하여 수치해석적인 방법으로 살펴보았으며, 횡방향 변형률 제어 압축시험을 수치해석적으로 모사할 수 있는 방법을 제시하였다. 수치해석에서 사용된 미시변수는 스웨덴 Aspo Hard Rock Laboratory에서 수행한 일축압축시험을 이용하여 결정하였다. 제시된 수치해석 기법을 이용해 Aspo 암석의 Class II 거동을 효과적으로 모사할 수 있었으며, 수치해석의 결과는 실험실 시험 결과와 잘 일치하였다.

대구지역 굴착암석의 물리적 특성 (Physical Properties of Excavated Rocks in Taegu Area)

  • 이상호;차완용;김영수;이재호
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 1999년도 Proceedings of the 1999 Annual Conference The Korean Society of Agricutural Engineers
    • /
    • pp.265-270
    • /
    • 1999
  • At this study, we investigated the chemical component and the mineral granular composition of sedimentary rock and others where were distributed in Taegu area and compared correlations with each data through the various physicla and mechanical characteristic test. As the result, d and E, they are kinds of granite, which contain much albite than others were proved to be strong by mechanical tests and the correlation moduli were proved to be more than 0.8 except P wave velocity-Poisson's ration relation when examined Elastic moduluous -Poisson's ration, P, wave velocity-Uniaxial compression strength, Elastic modulous -Uniaxial compression strength and Uniaxial compression strength-Poisson's ration correlation function graph.

  • PDF

소결분말금속의 항복함수 (A Yield Function for Sintered Porous Metals)

  • 박종진
    • 대한기계학회논문집
    • /
    • 제17권5호
    • /
    • pp.1115-1122
    • /
    • 1993
  • Several yield criteria for porous materials are compared with each other, defining the apparent yield stress as the yield stress of the porous material in simple compression. It was found that the plastic Poisson's ratio is the parameter needed to define the yield criterion, rather than the relative density. The plastic Poisson's ratio is regarded as a material characteristic that is obtained from a simple compression test. A new form of yield criterion was suggested, and it was applied to hydrostatic compression as well as uniaxial strain compression of sintered Al-2024 powder. The crossover point in the mean stress vs volume change curves of the processes was predicted. It is presented that the flow stress of the fully densed material can be obtained from that of the porous material using relations obtained from the yield criterion.

동결 온도와 재하속도에 따른 동결토의 일축압축 및 쪼갬인장 강도특성 (Experimental Study on Unconfined Compression Strength and Split Tensile Strength Properties in relation to Freezing Temperature and Loading Rate of Frozen Soil)

  • 서영교;최헌우
    • 한국해양공학회지
    • /
    • 제26권6호
    • /
    • pp.19-26
    • /
    • 2012
  • Recently the world has been suffering from difficulties related to the demand and supply of energy due to the democratic movements sweeping across the Middle East. Consequently, many have turned their attention to never-developed extreme regions such as the polar lands or deep sea, which contain many underground resources. This research investigated the strength and initial elastic modulus values of eternally frozen ground through a uniaxial compression test and indirect tensile test using frozen artificial soil specimens. To ensure accurate test results, a sandymud mixture of standard Jumunjin sand and kaolinite (20% in weight) was used for the specimens in these laboratory tests. Specimen were prepared by varying the water content ratio (7%, 15%, and 20%). Then, the variation in the strength value, depending on the water content, was observed. This research also established three kinds of environments under freezing temperatures of $-5^{\circ}C$, $-10^{\circ}C$, and $-15^{\circ}C$. Then, the variation in the strength value was observed, depending on the freezing environment. In addition, the tests divided the loading rate into 6 phases and observed the variation in the stress-strain ratio, depending on the loading rate. The test data showed that a lower freezing temperature resulted in a larger strength value. An increase in the ice content in the specimen with the increase in the water content ratio influenced the strength value of the specimen. A faster load rate had a greater influence on the uniaxial compression and indirect tensile strengths of a frozen specimen and produced a different strength engineering property through the initial tangential modulus of elasticity. Finally, the long-term strength under a constant water content ratio and freezing temperature was checked by producing stress-strain ratio curves depending on the loading rate.

Ti-Al금속간화합물의고온변형거동및라멜라조직의결정방위분포 (High Temperature Deformation Behavior of Ti-Al Intermetallic Compound and Orientation Distribution of Lamellae Structure)

  • 박규섭;강창용;이근진;정한식;정영관;복부양지
    • 한국정밀공학회지
    • /
    • 제21권10호
    • /
    • pp.162-169
    • /
    • 2004
  • High temperature uniaxial compression tests in the alpha single phase region were carried out on the Ti -43mo1%Al intermetallic compound, in order to obtain oriented lamellar microstructure. The compression deformation temperatures and strain rates are from 1573k to 1623k and 1.0x10$^{-4}$ s to 5.0x10$^{-3}$ s, respectively. Fully lamellar microstructure was observed after the uniaxial compression deformation in a single phase region followed by cooling to room temperature. Lamellar colony diameter depended on strain rates and test temperatures. The diameter varied between 8601m and 300fm. Stress-strain curve showed a work softening and the size of lamellar colony diameter varied depending on peak stresses. This shows the occurrence of dynamic recrystallization. Texture measurements after the uniaxial compression deformation, showed the development of fiber during dynamic recrystallization. It is seen that the area for the maximum pole density existed in 35 degrees away from the compression plane. The texture sharpens with a decrease in strain rate

배수성 아스팔트 표층용 혼합물의 강도특성 (The Strength Properties of Permeable Hot Mix Asphalt for Surface Course)

  • 이관호;함상민
    • 한국산학기술학회논문지
    • /
    • 제12권7호
    • /
    • pp.3296-3301
    • /
    • 2011
  • 배수성포장은 다양한 장점을 가지고 있어 점차 보편화되고 있는데, 주요 효과로는 수막현상 최소화, 빗물에 의한 미끄럼저항값을 일정하게 유지하고, 차량과 포장체 사이에서 발생하는 소음을 저감시켜준다. 도로소음 및 수막현상 감소효과에 대한 많은 연구가 수행되었다. 본 연구의 목적은 배수성 포장 표층의 역학적 특성(강도 및 탄성계수)을 평가하는 것이다. 시험에 사용된 시편은 선회다짐기를 이용하여 제작하였다. 배수성포장의 상부표층 및 하부표층용 시편을 실험에 이용하였다. 마샬안정도시험(KS F 2377), 자유단공진주시험(KS F 2730), 일축압축시험(KS F 2314), 슈미트햄머시험 등을 수행하였다. 일축압축강도 및 슈미트햄머를 이용한 강도값을 비교 분석하였다.

풍화에 따른 퇴적암의 강도 변화 (The Variation of Sedimentary Rock Strength due to Weathering)

  • 배우석;이봉직;오세욱;이종규
    • 한국안전학회지
    • /
    • 제18권1호
    • /
    • pp.89-93
    • /
    • 2003
  • The failure of rock slopes were influenced by weathering, which causes change in the shear strength. The weathering is also directly related to slaking and swelling characteristics. In the paper, the core of diameter loom was obtained by digging on rock slope of Kong-ju in Korea and then EDX(Energy Dispersive X-ray spectrometer) analysis was carried out to verified element of chief rock-forming minerals. Uniaxial compression tests, slaking tests, and point load test are performed to study engineering characteristics of conglomerate and red shale. As a results of slaking test, slaking index of conglomerate indicate range of 85.11-99.58 and shale indicate 58.37-99.23. Therefore, it is recognized that the resistance of shale to weathering decreases in shallow depth and it greatly influences the strength of rock. The result of uniaxial compression test and Point load test show that the strength of sedimentary such as conglomerate and red shale has an influence on both weathering and saturation.

연직 매트로 보강된 연약지반의 지지력 특성 (Characteristics of Bearing Capacity of Soft Ground Reinforced by Vertical Mat)

  • 신은철;이길호
    • 한국지반환경공학회 논문집
    • /
    • 제13권6호
    • /
    • pp.83-90
    • /
    • 2012
  • 일반적으로 심층혼합공법에 의한 점토지반의 개량효과는 물리적 개량효과에 비해서 훨씬 크며 조기에 큰 개량 강도를 얻을 수 있으나, 국내 시공실적이 부족하고 시멘트-점토의 혼합방법에 따른 품질관리에 문제점이 있는 것으로 알려져 있다. 본 연구에서는 시멘트, 모래, 점토의 배합비에 따른 강도특성과 연직MAT의 형태에 따른 연약지반의 개량특성을 파악하기 위해 해성점토를 이용하여 일축압축 강도시험과 모형토조시험을 수행하였다. 일축압축강도 시험을 위한 공시체는 시멘트와 물의 중량비를 기준으로하여 모래를 일정 비율로 혼합하였고, 시멘트는 점토중량대비 각각 10%, 20%, 30%, 40%를 혼합하였고 대상지반토의 함수비는 40%, 60%, 80%로 조정하여 제작하였다. 공시체는 습윤방법을 이용하여 7일, 14일, 28일간 양생하여 양생기간에 따른 일축압축강도시험을 수행하였다. 지지력시험은 모형토조를 제작하고 Mat식으로 개량한 지반을 형성한 다음 개량률에 따른 지지력을 비교하고 연직MAT 장벽 상호간의 간섭효과를 분석하였다.

고로슬래그미분말 및 하수슬러지를 혼입한 시멘트계 저강도 재료의 기초적 물성 (Fundamental Properties of Controlled Low Strength Materials Mixed Blast Furnace Slag and Sewage Sludge)

  • 김동훈;박신;임남기
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.53-54
    • /
    • 2015
  • As the result of uniaxial compression strength test on the CLMS mixing BFS and SS with BFS 4000, it required to determine the desired strength through increasing unit quantity of cement in mixing process because of dramatic strength deterioration of strength according to increasing replacing rate. In this study's result, regardless of differences in fine aggregates used, in order to get uniaxial compression strength in the scope exceeding criteria of minimum strength for applying to the field, the most reasonable combination was to mix replacing BFS with fineness of 6000 in 30%. For the CLMS mixing BFS and SS, in order to improve flow ability by securing quantity of minimum unit and to repress bleeding rate with securing uniaxial compress strength considering the field applicability, regardless of differences in fine aggregates used, to mix BFS over 6000 in 30% was most effective.