• 제목/요약/키워드: Tungsten Alloy

검색결과 186건 처리시간 0.028초

알루미늄 합금 용접부의 피로균열성장거동에 관한 파괴력학적 연구 (A Fracture Mechanics Study on the Fatigue Crack Growth Behaviors in Aluminum Alloy Weldments)

  • 차용훈
    • 한국생산제조학회지
    • /
    • 제5권3호
    • /
    • pp.31-39
    • /
    • 1996
  • The objective of this study is to investigate the influence of welding residual stresses on the fatigue crack growth behavior of cracks located transverse to the weld bead. For this purpose, G. T. A (Gas Tungsten Arc) welding was performed on hte Al alloy 1100-O plate and the same initial crack is made on HAZ(Heat Affected Zone), weld metal and base meta respectively. Specimens were used CT(Compact Tension) specimens. Initial welding residual stresses were measured by using strai gage sectioning method. All specimens were tested under constant amplitude load with stress ratio R=0.1, It is possible to predict fatigue crack growth behaviors and the fatigue life, using numerical analysis together with distribution of initial residual stress and the values of C and m obtained from $da/dN-{\Delta}K$

  • PDF

동-텅스텐 소결합금(Cu-W)과 동(Cu)의 마찰용접 특성에 미치는 업셋압력의 영향에 관한 연구 (Effects of Upset Pressure on Weldability in the Friction Welding of Cu to Cu-W Sintered Alloy)

  • 강성보;민택기
    • Journal of Welding and Joining
    • /
    • 제17권5호
    • /
    • pp.69-76
    • /
    • 1999
  • A copper-tungsten sintered alloy(Cu-W) has been friction welded to a tough pitch copper in order to investigate the effect of upset pressure on friction weldability. Under the condition of friction time 0.8sec, upset pressure 150MPa, the tensile strength and Charpy impact value of the friction welded joint were 336MPa, $400KJ/m^2$ respectively. And highest temperature of the weld measured was below $800^{circ}K$ which is very lower than melting point of Cu($1356^{circ}K$). Under the same conditions, W grains picked up in Cu matrix from Cu-W profitably affected on these mechanical fracture, and were dispersed in Cu by plastic flow during brake time.

  • PDF

삼원소 전극촉매 이용에 따른 에탄올 산화반응에 관한 연구 (The study of ethanol electro-oxidation using ternary electrocatalysts)

  • 노창수;손정민
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 추계학술대회 논문집
    • /
    • pp.191-194
    • /
    • 2009
  • PtRu based and PtSn based ternary catalysts were prepared by a conventional impregnation method using NaBH4 as reducing agent. The alloy formation, crystalline size and chemical composition of the in-house catalysts were determined by XRD, TEM and EDX, respectively. The chemical compositions of in-house catalysts were quite similar to the nominal value and good alloy formations were also observed. Further, crystalline sizes of ternary catalysts were comparatively smaller than binary catalysts and were approximately 3.5 ~ 5.5 nm. The electrochemical measurements were carried out in the solution 1 M $H_2SO_4$ with 1 M $C_2H_5OH$ at room temperature. LSV results obtained that ternary catalysts were higher current densities and specific activities. Especially, in case of tungsten addition system, Pt5Sn4W/C have the highest specific activities values and was approximately 21.2 and 3.1 times higher than that of PtRu/C and PtSn/C electrocatalyst.

  • PDF

Microstructures of W-Mo-Ni-Fe Heavy Alloys

  • Lin, Kuan-Hong;Hsu, Chen-Siang;Lin, Shun-Tian
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.937-938
    • /
    • 2006
  • Tungsten heavy alloys with different ratios of Mo and Ni-Fe matrix were liquid-phase-sintered to investigate their microstructural evolution. Results indicated that increased Mo in the alloy promoted the formation of a (W,Mo)(Ni,Fe) type intermetallic compound in the furnace-cooled condition. It was a monoeutectic reaction when the added Mo content was higher than 49at.%, or a eutectic reaction when this value was between 37at,% to 49at.%. When Mo was added between 25at.% to 37at.%, the precipitation of the intermetallic compound took place by either a eutectoid or peritectoid reaction.

  • PDF

AI 합금 용접부의 잔류응력 및 피로강도 해석 (Analysis of the Residual Stresses and Fatigue Strenth in Aluminum Alloy Weldments)

  • 차용훈
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1996년도 춘계학술대회 논문집
    • /
    • pp.177-182
    • /
    • 1996
  • The objective of this thesis is to investigate the influence of welding residual stresses on the fatigue growth behavior of welding residual stresses on the fatigue growth behavior of cracks located transverse to the weld bead. For this purpose, G.T.A. (Gas Tungsten Arc) welding was performed on the Al. Alloy 1100-0 plate and the same initial crack is made on HAZ(Heat Affected Zone), weld metal and base metal respectively. C.T.(Compact Tension) specimens were used as experimental material. Initial welding residual stresses were measured by using strain gage sectioning method. All specimens were tested under constant amplitude load with stress ratio R=0.1

  • PDF

Electrochemical Behavior and Biocompatibility of Co-Cr Dental Alloys

  • Kang, Jung-In;Yoon, Jun-Bin;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2015년도 춘계학술대회 논문집
    • /
    • pp.107-107
    • /
    • 2015
  • In order to investigate electrochemical behavior and biocompatibility of Co-Cr dental alloy by electrochemical corrosion test and MTT assay, the xCo-25Cr-yW-zNi alloys were used in this study. Samples of Co-Cr-W-Ni alloys were manufactured using arc melting furnace. The microstructure of the alloys was examined by optical microscopy (OM), Field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD), MTT assay, and corrosion test. Corrosion resistance increased slightly as cobalt (Co) content increased. And bioactivity was concerned with nickel (Ni) and tungsten (W). Biocompatibility of Co-Cr alloy depended on Ni and W contents.

  • PDF

Impact 구동 방식 압전 엑츄에이터의 마찰재 특성 (Properties of friction material for impact driven piezoelectric actuator)

  • 이동균;강병우;문재호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.285-285
    • /
    • 2007
  • Friction material in a piezoelectric system is a important part to affect to moving performance. In this paper, alumina ceramics $(AlO_2)$, silicon carbide (SiC), high speed steel and super-hard alloy (WC, Tungsten Carbide) having a hardness knoop of 1000 to 2000 $kg/mm^2$ were tested as a friction material of AF module. Even though $AlO_2$, SiC and high speed steel were a high-hardness material, $AlO_2$ and SiC were worn by a rough surface, and SiC is rusted in humidity condition. AF module using super-hard alloy has showed a stable moving performance in life time test.

  • PDF

B와 W의 함량이 무전해 Co 합금 박막의 경도에 미치는 영향 연구 (Effect of B and W Contents on Hardness of Electroless Co Alloy Thin Films)

  • 임태호;김재정
    • Korean Chemical Engineering Research
    • /
    • 제56권6호
    • /
    • pp.895-900
    • /
    • 2018
  • 본 연구에서는 Co-B, Co-W-B 합금 박막 형성을 위한 무전해 전착법을 고안하고, 이를 통해 형성한 합금 박막의 B과 W의 함량이 박막의 경도에 미치는 영향을 살펴보았다. 무전해 전착을 통해 무정형 상태의 Co 합금 박막을 성공적으로 형성할 수 있었으며, 환원제인 dimethylamine borane과 W의 원료인 sodium tungstate dihydrate의 농도를 조절함으로써 Co 합금 박막 내 혼합되는 B과 W의 함량을 조절하였다. 이를 통해 Co 합금 박막 내 전위(dislocation)의 전파(propagation)를 억제하는 B과 W의 함량이 증가할수록 박막의 경도가 증가함을 확인할 수 있었다. 뿐만 아니라, 무전해 전착 시 포기(aeration)를 수행하지 않을 경우에 포기를 수행한 경우보다 Co 합금 박막 내 B과 W의 함량을 대폭 증가시킬 수 있었고 최종적으로 Co-W-B 합금 박막의 경도를 8.9 (${\pm}0.3$) GPa까지 향상시켰다.

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

극저온 환경에 적용되는 INCONEL 718합금의 GTAW 기계적 특성 평가 (Mechanical Properties Evaluation of GTAW for INCONEL 718 alloy apply to Cryogenic Condition)

  • 김기홍;문인상;이병호;이수용
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2009년도 제33회 추계학술대회논문집
    • /
    • pp.619-622
    • /
    • 2009
  • INCONEL 718합금은 상온, 고온 및 저온환경에서 기계적 특성이 아주 우수하다. 상온에서의 모재 강도는 약 900MPa이며, 열처리 후 시효경화처리에 의해 강도가 약 1300MPa까지 증가한다. 이러한 INCONEL 718합금의 기계적 특성은 시험결과에서도 유사한 값을 나타내었고, GTAW 용접부의 상온 기계적 특성도 모재보다 우수한 강도를 나타내었다. 또한 저온에서의 기계적 특성은 모든 시험조건에서 상온보다 높은 강도를 나타내었으며, 열처리 모재시편과 용접시편은 1400MPa에 달하는 고강도를 나타내었다. 이러한 결과를 바탕으로 INCONEL 718합금의 저온 기계적 특성이 우수한 것을 증명하였고, 용접성 또한 모재의 특성과 같이 상온 및 저온 특성이 우수한 것을 알 수 있었다. INCONEL 718 합금과 STS 316L의 이종접합의 경우에도 $-100^{\circ}C$환경의 인장강도가 상온보다 300MPa 이상 증가하는 것을 알 수 있었다. 따라서, INCONEL 718합금은 $100^{\circ}C$이하부터 일정온도까지는 기계적 특성이 계속 증가 할 것으로 사료되며, 극저온 고압 상태로 공급되는 산화제 배관 제작에 적합한 소재로 판단된다.

  • PDF