PURPOSES: This study is to investigate the Hot In-Place recycling asphalt mixture in Korea using field produced materials. METHODS: Hot In-Place reclaimed asphalt mixture was investigated to evaluate the mixture properties based on various test results such as Marshall Test, Indirect Tensile Test, TSR, and Wheel Tracking Test. These test values were compared with domestic standard specification. RESULTS: The result of the laboratory experiment indicates that the Hot In-Place Reclaimed(HIR) asphalt mixture produced at the field constrution site was satisfied all of the test criteria such as Indirect tensile test, Marshall and TSR test, and wheel tracking test. During the test, the research team found that current HIR system is required an extention of mixing time to improve quality and to reduce variation of sample to sample. Although the current HIR mixture was passed the test criteria, there is a potential capability to enhance the mixture properties as extend mixting time. CONCLUSIONS: Based on these laboratory test results, It would be concluded that domestic HIR mixture's properties were satisfied all standard specification related with evaluation of recycling asphalt mixtures. Based on this case study result, there is a chance to save construction cost and increase the usage of reclaimed asphalt concrete in the future.
Field or laboratory wheel tracking tests have been employed for the evaluation of the rutting potential of asphalt paving mixtures. Compared to field tests, laboratory wheel tracking tests are much less expensive and more manageable for most road projects. However, most test laboratories are not equipped to perform such tests because there does not exist any standard test procedure, and the required equipment is rather expensive. Futhermore, the size of test specimens and the relatively large quantity of test mixture required present difficulties for laboratory specimen mixing and compaction. This paper describes a project conducted to study the feasibility of replacing wheel tracking testsby a repeated-load creep test for rutting potential evaluation. Comparisons were made between the results of the two tests for different test temperatures, loading speeds and applied pressures. Three types of asphalt mixtures were studied in the test program. Favorable conclusions concerning the use of the repeated-load test for rutting potential evaluation were drawn based on the findings of the experimental test results. The correlation between the two types of tests was found to be good for all threeasphalt mixtures. Adopting the repeated-load creep test would lead to cost savings since it employs standard test equipment already available in most laboratories. It would also result in substantial time savings due to the much smaller quantity of mix needed, and the ease in specimen preparation.
PURPOSES : The main distress of asphalt pavements in monsoon climate regions are caused by water damage and plastic deformation due to repeated rain season and increased heavy vehicle traffic volume. In this study, the mechanical properties of polymer-modified warm mix asphalt (PWMA) materials are evaluated to use in monsoon climate regions such as Indonesia. METHODS : Comprehensive laboratory tests are conducted to evaluate moisture resistance and permanent deformation resistance for three different asphalt mixtures such as the Indonesian conventional hot-mix asphalt (HMA) mixture, the polymer-modified asphalt mixture, and the polymer-modified warm mix asphalt (PWMA) mixture. Dynamic immersion test and indirect tensile strength ratio test are performed to evaluate moisture resistance. The wheel tracking test is performed to evaluate rutting resistance. Additionally, the Hamburg wheel tracking test is performed to evaluate rutting and moisture resistances simultaneously. RESULTS :The dynamic immersion test results indicate that the PWMA mixture shows the highest resistance to moisture. The indirect tensile strength ratio test indicates that TSR values of PWMA mixture, Indonesian PMA mixture, and Indonesian HMA mixture show 87.2%, 84.1%, and 67.9%, respectively. The wheel tracking test results indicate that the PWMA mixture is found to be more resistant to plastic deformation than the Indonesian PMA. The dynamic stability values are 2,739 times/mm and 3,150 times/mm, respectively. Moreover, the Hamburg wheel tracking test results indicate that PWMA mixture is more resistant to plastic deformation than Indonesian PMA and HMA mixtures. CONCLUSIONS :Based on limited laboratory test results, it is concluded that rutting resistance and moisture susceptibility of the PWMA mixture is superior to Indonesian HMA and Indonesian PMA mixtures. It is postulated that PWMA mixture would be suitable for climate and traffic conditions in Indonesia.
Park, Jeong-Jun;Kim, Ju-Ho;Kim, Ki-Sung;Kim, Dongwook;Hong, Gigwon
Journal of the Korean Geosynthetics Society
/
v.17
no.1
/
pp.75-83
/
2018
This paper described a results of dynamic stability by using wheel tracking test and unconfined compression test, in order to evaluate behavior characteristics on the developed pocketable expansion material for emergency restoration of ground cavity. The wheel tracking test result showed that the settlement increment ratio of the recovered ground by the expansion material was decreased compared to the sandy ground in high load condition. That is, it was confirmed that the expansion material was able to restrain the settlement due to the material stiffness, and the same results were obtained for the dynamic stability evaluation results. From the results of unconfined compression test, the pocketable expansion material was found to be able to fully support load on the restored cavity.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2004.07b
/
pp.1121-1124
/
2004
Aging test to estimate life property of polymer insulator is executed through several international standard such as IEC 61109 and CEA tracking wheel test, but is not getting clear conclusion yet. There are two methods in the diagnosis method of polymer insulator such as off-line and on-line. The diagnosis methods in off-line are external condition analysis by the eye, contaminant analysis on surface, surface analysis, pollution withstand voltage test, power frequency flashover voltage test, lightning impulse flashover test, tensile fracture load test and flexural load test. The diagnosis methods in off-line most are the method for virgin and last aged sample. However, the diagnosis method in on-line is method that can be evaluate sample state as progressing continuously aging test in beginning, The diagnosis method in on-line is arranged as following: leakage current measurement, electric field, surface state investigation, thermal image, emitting light measurement and then so. In this paper, the tracking performance of polymer insulator with salt solution which is added surface active agent. The diagnosis of insulator sample has been analyzed by leakage current and visual examination.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2004.07a
/
pp.469-472
/
2004
There have been numerous accelerated aging laboratory tests for evaluating suitability of polymeric materials and devices. Aging test for materials and its full scale device has been conducted, but poor correlation of aging test such as service experience were observed. Service experience plays a key role in the utility section of composite insulators. A meaningful and reliable accelerated aging test is needed for evaluating composite insulator. During the service these insulators are subjected to aging stress such as humidity, pollution, and electrical field, and erosion and tracking of the weathershed occurs. This paper presents the criteria of reliability evaluation and evaluation facilities for 22.9 kV suspension composite insulator. We adopt the criteria of reliability evaluation consist of two test methods. One is CEA tracking wheel test for examining the tracking and erosion performance of composite insulator. The other is multi-stress aging test for examining effects of environmental factors such as UV, temperature, humidity, etc on composite insulator.
This study is on the performance analysis of modified asphalts which were prepared by mixing the asphalt with polymer modifiers of varying compositions which were synthesized by the emulsion polymerization method. Thermal properties of mired asphalt were investigated by DSC (differential scanning calorimetry), and dispersion of modifiers in asphalt was investigated by the fluorescence microscope. Dynamic stability and permanent deformation velocities of mixed asphalt were investigated by wheel tracking measurements. Modifier 6 showed the best results in both penetration test and wheel tracking measurement among investigated modifiers, which supports MMA(methyl methacrylate) moiety in modifiers plays better contribution for the enhancement of asphalt performance than styrene moiety does.
Kim, Seung-Hyun;Noh, Yo-Han;Cheong, Jong-Hun;Cho, Han-Goo
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.33
no.2
/
pp.135-140
/
2020
An experimental study was conducted using the tracking wheel test (IEC 62217) method for evaluating the performance of insulator materials, in particular ethylene propylene diene monomer (EPDM) and silicone rubber. In addition, we studied the tracking characteristics resulting from applying the same method for the shape of the insulator housing, that is, the performance of regular and alternating sheds. The evaluation parameters were leakage current, surface characteristics, SEM, EDX, hydrophobicity, and temperature distribution; likewise, we applied the commercial frequency dry (and wet) flashover voltage test. We found that the regular shed had a greater leakage current than the alternating shed and that the recovery of the hydrophobicity in terms of rest time was greater than that of the EPDM in terms of leakage current. All of the regular-shed insulators of silicone rubber had tracking traces and choking on the sheath parting line, while the alternating shed showed only choking at the interface but no tracking traces. Therefore, it can be concluded that the commercial frequency wet flashover voltage of the silicone rubber with regular shed before and after the tracking wheel test is higher than that of the alternating shed.
Transactions of the Korean Society of Automotive Engineers
/
v.11
no.4
/
pp.189-195
/
2003
The steel wheels are widely used in the passenger cars because of their low cost of production although the aluminum wheels have many advantages in their performance and appearance. It is known that the steering wheel vibration with steel wheels is generated more often than one with aluminum wheels. Both the constant velocity driving test and the m up test are carried out in this study to analyze the causes and path of the steering wheel vibration generated from the steel wheels. And this study shows that the steering wheel vibration is affected by the fastening torque of the wheel mounting bolts between the steel wheel and the suspension disk.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.