• 제목/요약/키워드: Ti-based alloys

검색결과 148건 처리시간 0.032초

Study of TiCN Aditions to an 2xxx Series Aluminium Alloy

  • Ruiz-Navas, E.M.;Delgado, Tienda M.L.;Benito, Gonzalez S.;Gordo, E.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1037-1038
    • /
    • 2006
  • The increasing demand of PM parts for automobile and aerospace applications has caused a strong development of the aluminium based metal matrix composites (MMCs).Aluminium alloys are one of most widely used materials as matrix in MMCs, both in research and development as well as in industrial applications. In the present work, the influence of the ceramic reinforcement addition to a 2xxx series aluminium alloy is studied. Several percentages of TiCN have been added to the Al-Cu alloy using PM techniques, in order to analyze its influence on the liquid phase sintering process and on the final properties of the material.

  • PDF

치과보철용 자석재료의 전기화학적 안정성 개선효과 (IMPROVEMENT EFFECTS OF ELECTROCHEMICAL STABILITY OF MAGNETIC MATERIALS FOR PROSTHETIC DENTISTRY)

  • 곽종하;오상호;최한철;정재헌
    • 대한치과보철학회지
    • /
    • 제44권5호
    • /
    • pp.628-641
    • /
    • 2006
  • Statement of problem: Dental magnetic materials have been applied to removable prosthetic appliances, maxillofacial prostheses, obturator and dental implant but they still have some problems such as low corrosion resistance in oral environments. Purpose: To increase the corrosion resistance of dental magnetic materials, surfaces of Sm-Co and Nd-Fe-B based magnetic materials were plated with TiN and sealed with stainless steels. Materials and methods : Surfaces of Sm-Co and Nd-Fe-B based magnetic materials were plated with TiN and sealed with stainless steels, and then three kinds of electrochemical corrosion test were performed in 0.9% NaCl solution; potentiodynamic, potentiostatic, and electrochemical impedance test. From this study, corrosion behavior, amount of elements released, mean average surface roughness values, the changing of retention force, and magnetic force values were measured comparing with control group of non-coated magnetic materials. Results: The values of surface roughness of TiN coated Sm-Co and TiN coated Nd-Fe-B based magnetic materials were lower than those of non coated Sm-Co and Nd-Fe-B alloy. From results of potentiodynamic test, the passive current density of TiN coated Sm-Co alloy were smaller than those of TiN coated Nd-Fe-B alloy and non coated alloys in 0.9% NaCl solution. From results of potentiostatic and electrochemical impedance test, the surface stability of the TiN coated Sm-Co alloy was more drastically increased than that of the TiN coated Nd-Fe-B alloy and non-coated alloy. The retention and magnetic force after and before corrosion test did not change in the case of TiN coated magnetic alloy sealed with stainless steel. Conclusion: It is considered that the corrosion problem and improvement for surface stability of dental magnetic materials could be solved by ion plating with TiN on the surface of dental magnetic materials and by sealing with stainless steels.

Effect of metal conditioner on bonding of porcelain to cobalt-chromium alloy

  • Minesaki, Yoshito;Murahara, Sadaaki;Kajihara, Yutaro;Takenouchi, Yoshihisa;Tanaka, Takuo;Suzuki, Shiro;Minami, Hiroyuki
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권1호
    • /
    • pp.1-8
    • /
    • 2016
  • PURPOSE. The purpose of this study was to evaluate the efficacy of two different metal conditioners for non-precious metal alloys for the bonding of porcelain to a cobalt-chromium (Co-Cr) alloy. MATERIALS AND METHODS. Disk-shaped specimens ($2.5{\times}10.0mm$) were cast with Co-Cr alloy and used as adherend materials. The bonding surfaces were polished with a 600-grid silicon carbide paper and airborne-particle abraded using $110{\mu}m$ alumina particles. Bonding specimens were fabricated by applying and firing either of the metal conditioners on the airborne-particle abraded surface, followed by firing porcelain into 5 mm in diameter and 3 mm in height. Specimens without metal conditioner were also fabricated. Shear bond strength for each group (n=8) were measured and compared (${\alpha}=.05$). Sectional view of bonding interface was observed by SEM. EDS analysis was performed to determine the chemical elements of metal conditioners and to determine the failure modes after shear test. RESULTS. There were significant differences among three groups, and two metal conditioner-applied groups showed significantly higher values compared to the non-metal conditioner group. The SEM observation of the sectional view at bonding interface revealed loose contact at porcelain-alloy surface for non-metal conditioner group, however, close contact at both alloy-metal conditioner and metal conditioner-porcelain interfaces for both metal conditioner-applied groups. All the specimens showed mixed failures. EDS analysis showed that one metal conditioner was Si-based material, and another was Ti-based material. Si-based metal conditioner showed higher bond strengths compared to the Ti-based metal conditioner, but exhibited more porous failure surface failure. CONCLUSION. Based on the results of this study, it can be stated that the application of metal conditioner is recommended for the bonding of porcelain to cobalt-chromium alloys.

Nanodispersion-Strengthened Metallic Materials

  • Weissgaerber, Thomas;Sauer, Christa;Kieback, Bernd
    • 한국분말재료학회지
    • /
    • 제9권6호
    • /
    • pp.441-448
    • /
    • 2002
  • Dispersions of non-soluble ceramic particles in a metallic matrix can enhance the strength and heat resistance of materials. With the advent of mechanical alloying it became possible to put the theoretical concept into practice by incorporating very fine particles in a flirty uniform distribution into often oxidation- and corrosion- resistant metal matrices. e.g. superalloys. The present paper will give an overview about the mechanical alloying technique as a dry, high energy ball milling process for producing composite metal powders with a fine controlled microstructure. The common way is milling of a mixture of metallic and nonmetallic powders (e.g. oxides. carbides, nitrides, borides) in a high energy ball mill. The heavy mechanical deformation during milling causes also fracture of the ceramic particles to be distributed homogeneously by further milling. The mechanisms of the process are described. To obtain a homogeneous distribution of nano-sized dispersoids in a more ductile matrix (e.g. aluminium-or copper based alloys) a reaction milling is suitable. Dispersoid can be formed in a solid state reaction by introducing materials that react with the matrix either during milling or during a subsequent heat treatment. The pre-conditions for obtaining high quality materials, which require a homogeneous distribution of small dis-persoids, are: milling behaviour of the ductile phase (Al, Cu) will be improved by the additives (e.g. graphite), homogeneous introduction of the additives into the granules is possible and the additive reacts with the matrix or an alloying element to form hard particles that are inert with respect to the matrix also at elevated temperatures. The mechanism of the in-situ formation of dispersoids is described using copper-based alloys as an example. A comparison between the in-situ formation of dispersoids (TiC) in the copper matrix and the milling of Cu-TiC mixtures is given with respect to the microstructure and properties, obtained.

높은 자장하에서 자기공명 영상 왜곡이 완화된 생체용 Ti 복합재료 (Bio-applicable Ti-based Composites with Reduced Image Distortion Under High Magnetic Field)

  • 김성철;김유찬;석현광;양석조;손인진;이강식;이재철
    • 대한금속재료학회지
    • /
    • 제50권5호
    • /
    • pp.401-406
    • /
    • 2012
  • When viewed using a magnetic resonance imaging (MRI) system, invasive materials inside the human body, in many cases, severely distort the MR image of human tissues. The degree of the MR image distortion increases in proportion not only to the difference in the susceptibility between the invasive material and the human tissue, but also to the intensity of the magnetic field induced by the MRI system. In this study, by blending paramagnetic Ti particles with diamagnetic graphite, we synthesized $Ti_{100-x}C_x$ composites that can reduce the artifact in the MR image under the high-strength magnetic field. Of the developed composites, $Ti_{70}C_{30}$ showed the magnetic susceptibility of ${\chi}=67.6{\times}10^{-6}$, which corresponds to 30% of those of commercially available Ti alloys, the lowest reported in the literature. The level of the MR image distortion in the vicinity of the $Ti_{70}C_{30}$ composite insert was nearly negligible even under the high magnetic field of 4.7 T. In this paper, we reported on a methodology of designing new structural materials for bio-applications, their synthesis, experimental confirmation and measurement of MR images.

Fe-Cr-Al 기 산화물 분산강화 합금의 미세조직에 미치는 분말제조 공정 영향 (Effect of Powder Synthesis Method on the Microstructure of Oxide Dispersion Strengthened Fe-Cr-Al Based Alloys)

  • 박성현;오승탁
    • 한국재료학회지
    • /
    • 제27권9호
    • /
    • pp.507-511
    • /
    • 2017
  • An optimum route to fabricate oxide dispersion strengthened ferritic superalloy with desired microstructure was investigated. Two methods of high energy ball milling or polymeric additive solution route for developing a uniform dispersion of $Y_2O_3$ particles in Fe-Cr-Al-Ti alloy powders were compared on the basis of the resulting microstructures. Microstructural observation revealed that the crystalline size of Fe decreased with increases in milling time, to values of about 15-20 nm, and that an FeCr alloy phase was formed. SEM and TEM analyses of the alloy powders fabricated by solution route using yttrium nitrate and polyvinyl alcohol showed that the nano-sized Y-oxide particles were well distributed in the Fe based alloy powders. The prepared powders were sintered at 1000 and $1100^{\circ}C$ for 30 min in vacuum. The sintered specimen with heat treatment before spark plasma sintering at $1100^{\circ}C$ showed a more homogeneous microstructure. In the case of sintering at $1100^{\circ}C$, the alloys exhibited densified microstructure and the formation of large reaction phases due to oxidation of Al.

Electrochemical Performance of Ti-Si Alloy Anode using Nodule Type Current Collector

  • Shin, Min-Seon;Park, Jung-Bae;Lee, Sung-Man
    • 전기화학회지
    • /
    • 제20권4호
    • /
    • pp.61-66
    • /
    • 2017
  • The cycle performance of Ti-Si alloy anode material for Li-ion batteries has been investigated as a function of loading level of electrode using a nodule type of substrate, in which the current collector of flat foil is also used for comparison. The Ti-Si alloy powders are prepared by mechanical alloying method. The electrodes with the nodule type of current collector exhibit enhanced cycling performance compared to those using the flat foil because the alloy particles are more strongly adhered to substrate and the stress caused by lithiation and delithiation reaction can be effectively relaxed by nodule-type morphology. It appears, however, that the cycle performance is critically dependent on the loading level of electrode, even when the nodule type of current collector is applied. With high loading level, cracks are initiated at surface of electrode due to a steep stress gradient through the electrode thickness during cycling, leading to capacity fading.

ECAP가공에 의한 초미세립 소재의 기계적 물성 (Mechanical Properties of Ultrafine Grained Materials via Equal-Channel Angular Pressing)

  • 고영건;김우겸;안정용;박경태;이종수;신동혁
    • 소성∙가공
    • /
    • 제15권2호
    • /
    • pp.105-111
    • /
    • 2006
  • A study was made to investigate the microstructure and the mechanical properties of low-carbon steel, Al-Mg alloy and Ti-6Al-4V alloy each representing bcc, fcc and hcp crystal structures, respectively fabricated by equal-channel angular(ECA) pressing. After a series of ECA pressings was performed, most grains were significantly refined below ${\mu}m$ in diameter with high mis-orientation of grain boundaries irrespective of different crystal structure used. Regarding the strain hardening capability, tensile tests of ultrafine grain (UFG) dual-phase (ferrite/martensite) steel which was different from UFG ferrite-pearlite steel were carried out at ambient temperature, and corresponding mechanical properties were discussed in relation to modified C-J analysis. Low-temperature and/or high strain-rate superplasticity of the UFG Al-Mg alloy and UFG Ti-6Al-4V alloy were also studied. Based on the analysis used in this study, it was concluded that UFG alloys exhibited the enhanced mechanical properties as compared to coarse-grained (CG) counterparts.

cBN 지립과 Ag계 필러합금에서의 브레이징 특성 (The Brazing Characters of cBN Grit with Ag-based Filler Alloys)

  • 송민석;안상재;정기정
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.215-217
    • /
    • 2007
  • 철계 피삭재 가공 시 적용되는 cBN(cubic Boron-Nitride)의 경우 열적/구조적 안정성으로 인해 융착 시 계면에서 화학적 결합이 어려워, 지립이 단일층으로 형성되어야 하는 융착 공구의 경우 적용되질 못하고 있다. 이러한 문제를 해결하기 위해 세라믹과의 젖음성이 우수한 Ti 성분이 포함된 67Ag+28Cu+5Ti(wt.%) 조성의 합금분말을 이용하여 cBN을 접합을 하였으며, 이때 융착조건은 진공 분위기($6{\times}10^{-6}$Torr), $900^{\circ}C$ 온도에서 5분간 유지하여 융착을 실시하였다. 본 연구의 주목적은 Ti 합금화 된 Ag계 합금분말 및 cBN의 융착 계면에서의 융착 계면거동해석을 통한 건전한 접합공정을 찾는데 있다. 이에 온도 $900^{\circ}C$, 유지시간 5분에서 건전한 융착층을 형성함을 알 수 있었다. 또한 결합력 측정기를 이용하여 결합력을 측정한 결과 diamond와 융착하였을 때가 123N, cBN을 융착하였을 때 107N으로써, cBN 융착이 diamond 융착의 87%정도의 결합력을 보임을 알 수 있었다. 한편 cBN과 Ag-Cu-Ti계 브레이징 필러의 계면에서의 미세조직 및 화학반응의 메커니즘은 SEM, EDS를 이용하여 분석하였다.

  • PDF

Effect of Boron Additions on Glass Formation and Magnetic Properties of Fe-Co-Ti-Zr-B Amorphous Ribbons

  • Kim, Sumin;Han, Bo Kyeong;Choi-Yim, Haein
    • Journal of Magnetics
    • /
    • 제21권2호
    • /
    • pp.164-167
    • /
    • 2016
  • The effect of the B additions on glass formation and magnetic properties is reported for the $Fe_{(87-x-y)}Co_yTi_7Zr_6B_x$ (x = 2, 4, 6 and y = 35, 40) alloy system. The ribbon samples with the width of 2 mm for each composition were prepared by the melt spinning technique; furthermore, their phase information was obtained from X-ray diffraction. Glass formation and magnetic properties were measured using differential scanning calorimetry and vibrating sample magnetometer respectively. The $Fe_{45}Co_{40}Ti_7Zr_6B_2$ (x = 2 and y = 40) system has the nanocrystalline phase identified as ${\alpha}-Fe$, as well as the amorphous phase, whereas all other alloys are fully amorphous. It is associated with the role of B on the glass formation. The widest supercooled liquid region is obtained as 71 K at x = 4 (both y = 35 and 40). The saturation magnetization decreases with the increase of the amount of the B addition, and the highest value is 1.59 T as x = 2 and y = 35 for this alloy system.