• Title/Summary/Keyword: Ti scrap

Search Result 20, Processing Time 0.025 seconds

Effect of (Ti-B) and Sr Additives on Impact and Fatigue Properties of Recycled AC4A Aluminum Casting Alloy (재활용 AC4A 알루미늄 합금의 충격 및 피로 특성에 미치는 (Ti-B), Sr 첨가제의 영향)

  • Oh, Seung-Hwan;Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.39 no.4
    • /
    • pp.61-74
    • /
    • 2019
  • The effects of Sr and (Ti-B) additives on the impact and fatigue properties of recycled (35% scrap content) AC4A aluminum alloy are investigated here. The acicular morphology of the eutectic Si phase of as-cast specimens was converted to the fibrous one with Sr additives. The grain size of the α-solid solution decreased by the addition of (Ti-B) additives. The crack initiation energy (Ei) of the impact absorption energy decreased due to the incorporation of an oxide film and inclusions depending on the scrap used. The modification of the eutectic Si morphology by Sr additives is considered as the main factor of the increase of the average impact absorption energy (Et). The addition of (Ti-B) additives contributed to an increase in the occurrence of crack deflections due to the refining of α-Al grains, resulting in improved fatigue properties.

[ $K_2Ti_6O_{13}$ ]-filled Rubber Composite (육티탄산칼륨이 함유된 고무복합체)

  • Park, Jong-Il;Kang, Dong-Heon;Kang, Suck-Choon;Chung, Kyung-Ho;Hong, Young-Keun
    • Elastomers and Composites
    • /
    • v.35 no.3
    • /
    • pp.180-187
    • /
    • 2000
  • For the purpose of developing a new type of frictional material using scrap rubber in which rubber makes continuous phase, potassium titanate($K_2Ti_6O_{13}$) was synthesized and added to rubber matrix. Needle-typed $K_2Ti_6O_{13}$ powders were obtained through the flux method using KCI salt and excess $K_2CO_3$. It was also found that the powders should be surface-treated to enhance adhesion and 10 phr of epoxy be added for the physical properties of the rubber composite.

  • PDF

A Study of Process factors on the Recycling of Reactive Metal Scraps in Plasma Arc Remelting (Plasma Arc Remelting에서 활성 금속 Scrap 재활용에 미치는 공정인자의 연구)

  • Jung, Jae-Young;Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.26 no.6
    • /
    • pp.3-9
    • /
    • 2017
  • In this study, plasma arc remelting behaviors according to arc current, arc voltage, and types of plasma gas were investigated using Kroll processed Ti sponges as anode. In the discharge pressure range of vacuum pump ($200{\sim}300kgf/cm^2$), the arc voltage did not vary greatly with the increase of discharge pressure at a given arc length. This means that the pressure in the vacuum chamber during operation hardly changes and the atmospheric pressure maintains. Under various conditions of arc currents (700~900A), the arc voltage slightly increased with arc current. The effects of anode materials and operational variables on the arc length-arc voltage relationship were compared with the results in previous studies. When the atmospheric gas changed from argon to helium, double effect of improvement on the output of the steady state was observed. The increase of output in the plasma arc device was accompanied by an increase in the melting rate of the Ti sponge and the quality of the ingot surface was also improved. The plasma arc remelting of the new scrap titanium and the old scrap zirconium alloy could result in the fabrication of an ingot with high surface quality.

Effects of Ti on Mechanical Property and Damping Capacity in Hot-rolled Fe-17%Mn Alloy (열간압연한 Fe-17wt%Mn 합금의 기계적 성질과 진동감쇠능에 미치는 티타늄 첨가의 영향)

  • Kim, Tai-Hoon;Kim, Jung-Chul
    • Journal of Korea Foundry Society
    • /
    • v.29 no.2
    • /
    • pp.59-63
    • /
    • 2009
  • Effects of Ti on damping capacity and mechanical properties are investigated in hot rolled Fe-17%Mn alloy. The existing damping alloy with Fe-Mn binary system was limited the use by high production cost, however in case of using scrap iron instead of pure iron although the content of carbon is higher it is possible to be applied wider field especially construction items because the production cost is lower. However, the excellent specific damping capacity is dropped due to the high content of carbon, we developed advanced type of damping alloy included Ti. TiC is formed with added Ti and it holds the specific damping capacity similar to existing damping alloy. The effect of Ti on damping capacity is found to be beneficial in carbon-containing alloy, which is attributed to the depletion of carbon solute due to the formation of TiC.

Recycling of Ti Turning Scraps for Production of Consumable Arc Electrode (아크용(用) 소모성(消耗性) 전극(電極) 제조(製造)를 위한 타이타늄 선삭(旋削) 스크랩의 재활용(再活用))

  • Oh, Jung-Min;Lim, Jae-Won
    • Resources Recycling
    • /
    • v.21 no.5
    • /
    • pp.58-64
    • /
    • 2012
  • Ti button type ingots were prepared by recycling of Ti turning scraps using vacuum arc melting process for production of consumable arc electrode. The behavior of impurities such as Fe, W, O, and N in the Ti button ingots was investigated and the properties of the Ti button ingots were also evaluated. In the case of oxygen gaseous impurity, the oxygen layers on the surface of the Ti turning scraps were easily removed by the first vacuum arc melting. On the other hand, the solute oxygen in the Ti turning scraps was not removed by the next melting. In the case of Fe, major impurity in the Ti turning scraps, the removal degree in the final Ti button ingot refined by vacuum arc melting for 20 minutes was approximately 43 %, which is due to the vapor pressure difference between Ti and Fe. As a result, the Ti button ingots with ASTM grade 3 could be obtained by multiple vacuum arc melting from the Ti turning scraps. Therefore, it was confirmed that the preparation of consumable electrode for vacuum arc remelting could be possible by recycling of Ti turning scraps.

Preparation and oxygen control of Ti-6Al-4V alloys by recycling dental pure Ti scraps (치과용(齒科用) 순(純) 타이타늄 스크랩을 재활용(再活用)한 Ti-6Al-4V 합금(合金)의 제조(製造) 및 산소(酸素) 제어(制御))

  • Oh, Jung-Min;Lee, Back-Kyu;Choi, Good-Sun;Lim, Jae-Won
    • Resources Recycling
    • /
    • v.21 no.1
    • /
    • pp.60-65
    • /
    • 2012
  • The Ti-6Al-4V alloys were prepared by recycling of dental Ti pure scraps using vacuum arc melting process, and their physical properties were evaluated the Ti-6Al-4V alloys with different oxygen concentrations. For the preparation of Ti-6Al-4V alloys, Ti pure scraps used for dental implant were utilized as a raw material, and their different oxygen concentrations were ranged from G1 to G4 grade in ASTM standards. It was confirmed that the weight loss of Al in the composition of Ti-6Al-4V alloy could be controlled under the Ar pressure of 875 torr during the melting of alloy. The oxygen concentrations of the Ti-6Al-4V alloys were ranged from 1170 to 3340 ppm. The vickers hardness change of the Ti-6Al-4V alloys showed a similar behavior with that of pure Ti. As a result, we confirmed a possibility of preparation of Ti-6Al-4V alloy by recycling of dental Ti scraps using vacuum arc melting process in this study.

Recycling and Applications of Titanium Alloy Scraps (티타늄 합금 스크랩의 재활용 및 응용 기술 현황)

  • Oh, Jung-Min;Kwon, Hanjung;Lim, Jae-Won
    • Clean Technology
    • /
    • v.19 no.2
    • /
    • pp.75-83
    • /
    • 2013
  • In the present paper, we review recycling and applications of titanium binary alloy scraps. The recycling techniques are to successfully prepare low oxygen content ingots using hydrogen plasma arc melting (HPAM) and to produce low oxygen content titanium alloy powders by Hydrogenation-dehydrogenation (HDH) and Deoxidation in solid state (DOSS) process. In addition, as applications of the titanium binary alloy scraps, Ti based solid-solution carbide powders, which would be used for producing Ti based solid-solution cermets with high toughness, were prepared using the titanium binary alloy scraps. These results confirmed that the titanium alloy scraps could be recycled and refined using the HPAM. The resulting oxygen content of the titanium alloy powders were below 1,000 ppm after powderizing. Finally, we had confirmed that the refined titanium alloy powders were able to be utilized as raw materials for preparing the toughened cermets.

Electrochemical Corrosion Characteristics of the Iron-based Damping Alloy (철기제진합금의 전기화학적 부식특성)

  • Shim, Hyun Yee;Jee, Choong Soo;Lee, Jin Hyung;Lee, Kyu Hwan;Shin, Myung Chul
    • Analytical Science and Technology
    • /
    • v.8 no.1
    • /
    • pp.85-90
    • /
    • 1995
  • Corrosion characteristics of 4 kinds of the Fe-Al damping alloys has been studied in the 3.5% NaCl solution and compared with a cold rolled mild steel and pure Ti, No passivation, besides Ti, was observed in the Fe-Al damping alloys and a cold rolled mild steel. Corrosion rate was decreased with lower carbon concentration. In the case of Mn addition for improving damping capacity, corrosion rate was decreased in scrap iron but was not decreased in electrolytic iron. It has been shown that corrosion rate of Fe-Al damping alloys lays between that of the pure Ti and that of a cold rolled mild steel.

  • PDF

Preparation of Metal Injection Molded Dental Components using Spheroidized Ti Powders by Plasma Process (플라즈마 공정으로 구상화된 티타늄 분말과 금속사출성형 공정을 이용한 치과용 부품 제조)

  • Gwak, Ji-Na;Yang, Sangsun;Yun, Jung-Yeul;Kim, Ju-Yong;Park, Seongjin;Kim, Hyun-Seung;Kim, Yong-Jin;Park, Yong-Ho
    • Journal of Powder Materials
    • /
    • v.20 no.6
    • /
    • pp.467-473
    • /
    • 2013
  • This research presents a preparation method of dental components by metal injection molding process (MIM process) using titanium scrap. About $20{\mu}m$ sized spherical titanium powders for MIM process were successfully prepared by a novel dehydrogenation and spheroidization method using in-situ radio frequency thermal plasma treatment. The effects of MIM process parameters on the mechanical and biological properties of dental components were investigated and the optimum condition was obtained. After sintering at $1250^{\circ}C$ for 1 hour in vacuum, the hardness and the tensile strength of MIMed titanium components were 289 Hv and 584 MPa, respectively. Prepared titanium dental components were not cytotoxic and they showed a good cell proliferation property.

A Study on the Properties of Transition Metal Nitride Coating Materials for the Recovery of Tungsten and Rare Metals (텅스텐 및 희유금속 회수를 위한 초경합금 전이금속질화물 코팅소재 특성연구)

  • Kim, Jiwoo;Kim, Myungjae;Kim, Hyokyeong;Park, Sohyun;Seo, Minkyeong;Kim, Jiwoong
    • Resources Recycling
    • /
    • v.31 no.1
    • /
    • pp.46-55
    • /
    • 2022
  • The recycling of coated cemented carbide scraps is becoming increasingly significant for the recovery of rare metals. However, coatings consisting of Group IV and V transition metal nitrides are one of the challenging factors in obtaining high-purity materials. We investigated the structural, elastic, and mechanical properties of Group IV and V transition-metal nitrides (TiN, VN, ZrN, NbN, HfN, and TaN) using first-principle calculations. Convergence tests were performed to obtain reliable calculated results. The equilibrium structures of the nitrides were in good agreement with those of a previous study, indicating the reliability of the data. Group IV transition metal nitrides show a higher covalent bonding nature. Thus, they exhibit a higher degree of brittleness than that of Group V transition metal nitrides. In contrast, Group V transition metal nitrides show weaker resistance to shear loading and more ductile behavior than Group IV transition metal nitrides because of the metallic bonds characterized by valence electron concentration. The results of the crystal orbital Hamilton population analysis showed good agreement with the shear resistance tendencies of all transition metal nitrides.