본 논문은 바탕면의 함수조건에 따른 보수재료로서 MKPC의 인발 부착강도, 전단 부착강도, 계면 부착강도를 폴리머 시멘트 모르타르, 에폭시 모르타르와 비교 분석하였다. 그 결과 MKPC는 PC 및 MKPC와 비교하여 바탕면 함수조건에 따른 부착성능의 변화가 상대적으로 작은 것으로 나타났다. 또한 MKPC의 경우 절건 바탕면에서의 부착성능은 무기계 보수재료인 폴리머 시멘트 모르타르와 비교하여 우수한 특성을 지니고 있으며, 습윤 바탕면에서의 부착성능은 폴리머 시멘트 모르타르와 유사한 수준을 보이고 있으나 에폭시 모르타르와 비교하여 우수한 특성을 지니는 것으로 나타났다.
Flowable resin composite is a relatively new restorative material. It has been reported that a low viscosity, low modulus intermediate resin applied between the bonding agent and restorative resin act as an "elastic buffer" that can relieve contraction stress. This in-vitro study aimed to evaluate the effect of flowable composite resin as a restorative material on regional tensile bond stredgth to cervical wedge shaped cavity walls. (omitted)
This study evaluated the influence of a desensitizer(MS coat) on microtensile bond strength of different adhesives:a three-step adhesive(All-Bond 2), a two-step adhesive(Single Bond), a one-step adhesive(One-up Bond F). Non-caries extracted human molars were used. Dentin surface was obtained by horizontal section on mid-portion of crown using a water-cooled low speed diamond saw. Teeth were randomly divided into 6 group. AMO(MS coat + All Bond), SMO(MS coat + Single Bond)- and OMO(MS coat + One-up Bond F)-dentin surface were treated with 17% EDTA before bonded adhesive. AMX-, SMX- and OMX-dentin surface were bonded with All-Bond 2, Single Bond and One-up Bond F, respectively. with no previous treatment with MS coat and 17% EDTA. About 1cm high resin composite($Z-250^{TM}$) were incrementally build-up on the treated surface. The specimens for the microtensile test were serially sectioned perpendicular to the adhesive layer to obtain $0.7{\times}0.7mm$ sticks. 30 sticks were prepared from each group. After that. tensile bond strength for each stick was measured with Microtensile Tester at a 1mm/min crosshead speed. Fractured dentin surfaces were observed under the SEM. The results were statistically analysed by using a One-way ANOVA and Tukey's test(p<0.05). Value in MPa were: $AMO-44.35{\pm}13.21;{\;}SMO-39.35{\pm}13.32;{\;}OMO-31.07{\pm}10.25;{\;}AMX-49.22{\pm}16.38;{\;}SMX-56.02{\pm}13.35;{\;}OMX-72.93{\pm}16.19$. Application of MS coat reduced microtensile bond strengths of both Single Bond and One-up Bond F, whereas microtensile bond strengths of All-Bond 2 were not affected significantly.
Turker, Nurullah;Buyukkaplan, Ulviye Sebnem;Basar, Ebru Kaya;Ozarslan, Mehmet Mustafa
The Journal of Advanced Prosthodontics
/
제12권4호
/
pp.189-196
/
2020
PURPOSE. The aim of the present study was to investigate the effects of surface treatments on the bond strengths between polymer-containing restorative materials and two dual-cure resin cements. MATERIALS AND METHODS. In the present study, rectangular samples prepared from Lava Ultimate (LU) and Vita Enamic (VE) blocks were used. The specimen surfaces were treated using CoJet sandblasting, 50 ㎛ Al2O3 sandblasting, % 9 HF (hydrofluoric) acid, ER,Cr:YSGG laser treatment, and Z-Prime. Dual-cure resin cements (TheraCem and 3M RelyX U 200) were applied on each specimen's treated surface. A micro-tensile device was used to evaluate shear bond strength. Statistical analysis was performed using the SAS 9.4v3. RESULTS. While the bond strength using TheraCem with LU or VE was not statistically significant (P=.164), the bond strength using U200 with VE was statistically significant (P=.006). In the TheraCem applied VE groups, Z-Prime and HF acid were statistically different from CoJet, Laser, and Sandblast groups. In comparison of TheraCem used LU group, there was a statistically significant difference between HF acid and other surface treatments. CONCLUSION. The bonding performance between the restorative materials and cements were material type-dependent and surface treatment had a large effect on the bond strength. Within the limitations of the study, the use of both U200 and TheraCem may be suggested if Z-prime was applied to intaglio surfaces of VE. The cementation of LU using TheraCem is suitable after HF acid conditioning of the restoration surfaces.
Park, Cheolwoo;Park, Younghwan;Kim, Seungwon;Ju, Minkwan
Smart Structures and Systems
/
제17권4호
/
pp.593-610
/
2016
In this study, an innovative and smart glass fiber-reinforced polymer (GFRP) hybrid bar was developed for stronger durability of concrete structures. As comparing with the conventional GFRP bar, the smart GFRP Hybrid bar can promise to enhance the modulus of elasticity so that it makes the cracking reduced than the case when the conventional GFRP bar is used. Besides, the GFRP Hybrid bar can effectively resist the corrosion of conventional steel bar by the GFRP outer surface on the steel bar. In order to verify the bond performance of the GFRP hybrid bar for structural reinforcement, uniaxial pull-out test was conducted. The variables were the bar diameter and the number of strands and pitch of the fiber ribs. Tensile tests showed a excellent increase in the modulus of elasticity, 152.1 GPa, as compared to that of the pure GFRP bar (50 GPa). The stress-strain curve was bi-linear, so that the ductile performance could be obtained. For the bond test, the entire GFRP hybrid bar test specimens failed in concrete splitting due to higher shear strength resulting in concrete crushing as a function of bar deformation. Investigation revealed that an increase in the number of strands of fiber ribs enhanced the bond strength, and the pitch guaranteed the bond strength of 19.1 mm diameter hybrid bar with 15.9 mm diameter of core section of deformed steel the ACI 440 1R-15 equation is regarded as more suitable for predicting the bond strength of GFRP hybrid bars, whereas the CSA S806-12 prediction is considered too conservative and is largely influenced by the bar diameter. For further study, various geometrical and material properties such as concrete cover, cross-sectional ratio, and surface treatment should be considered.
In this study, six specimens were prepared for two type FRP sheets(carbon and polyacetal) to evaluate the behavior of FRP-concrete interfacial bond. A direct tensile test was conducted and the test results show that fiber type influences both bond strength and the shape of strain distribution. The failure mode for carbon type specimens seems to bond failure between concrete and FRP, but for polyacetal type indicates interface failure between FRP and expoxy. The local bond stress-slip relations were obtained from test results, and it was shown good shape for the polyacetal type. But for the carbon type it was scattered.
본 연구에서는 고로슬래그 미분말을 이용한 SBR혼입 폴리머 시멘트 콘크리트의 강도 성상에 미치는 고로슬래그 치환율 및 폴리머 결합재비의 영향에 대하여 구명하였다. 그 결과, 고로슬래그 미분말을 이용한 SBR혼입 폴리머 시멘트 콘크리트의 압축, 인장 및 휨강도는 폴리머-결합재비 및 고로슬래그 치환율의 증가에 따라 증가하였으며, 고로슬래그 치환율 40%에서 가장 높은 강도를 나타내었다. 특히 고로슬래그 치환율 40%의 SBR혼입 폴리머 시멘트 콘크리트의 인장 및 휨강도는 폴리머 미혼입의 강도보다 약 2배 이상의 높은 강도를 보였다. 이와 같이 높은 강도의 발현은 SBR 폴리머의 높은 인장강도와 SBR라텍스의 혼입에 의한 시멘트 수화물과 골재간의 접착성이 개선되었기 때문이라 판단된다.
This paper is concerned with a study on fracture strength of composites in an adhesive single lap joint. The tests were carried out on joint specimens made with hybrid stacked composites consisting of the polyester and bamboo natural fiber layer. The main objective of this work was to evaluate the fracture properties adjacent to adhesive bonded joint of natural fiber reinforced composite specimens. From the results, natural fiber reinforced composites have lower tensile strength than the original polyester. But tensile-shear strength of natural fiber reinforced composites with bamboo layer far from adhesive bond is as high as that of the original polyester adhesive bonded joints. Spew filet at the end of the overlap reduced the stress concentration at the bonded area. Spew fillet and position of bamboo natural fiber layer have a peat effect on the tensile-shear strength of natural fiber reinforced composites including adhesive bonded joints.
International Journal of Concrete Structures and Materials
/
제18권1E호
/
pp.29-34
/
2006
Elastic modulus, tensile and bond capacities are important factors for developing an effective reinforcing action of a flexural member as a reinforcing material for concrete structures. Reinforcement must have enough bond capacity to prevent the relative slip between concrete and reinforcement. This paper presents an experimental study to clarify the bond capacity of prestressed carbon fiber reinforced polymer(CFRP) rod manufactured by an automatic assembly robot. The bond characteristics of CFRP rods with different pitch of helical wrapping were analyzed experimentally. As the result, all types of CFRP rods show a high initial stiffness and good ductility. The mechanical properties of helical wrapping of the CFRP rods have an important effect on the bond of these rods to concrete after the bond stress reached the yield point. The stress-slip relationship analyzed from the pull-out test of embedded cables within concrete was linear up to maximum bond capacity. The deformation within the range of maximum force seems very low and was reached after approximately 1 mm. The average bond capacity of CF20, CF30 and CF40 was about 12.06 MPa, 12.68 MPa and 12.30 MPa, respectively. It was found that helical wrapping was sufficient to yield bond strengths comparable to that of steel bars.
연구목적: 많은 의치 환자들은 의치의 유지력, 안정성 그리고 저작기능을 향상시키기 위해 의치접착제를 사용하고 있다. 이상적인 의치접착제는 독성이나 자극이 없고, 구강점막에 편안함을 제공하고, 나쁜 냄새나 맛이 없어야 한다. 의치접착 크림의 세포독성 여부를 확인하고, 의치접착제의 효과와 시간에 따른 유지력의 변화를 알아보고자 하였다. 연구재료 및 방법: 의치접착크림의 세포독성 여부를 알아보기 위해 mouse 섬유아세포를 이용한 MTT 시험을 통해 의치접착크림의 농도와 1일에서 4일까지의 시간에 따른 세포독성 여부를 평가하였다. 의치 접착제가 유지력 향상에 미치는 효과와 시간에 따른 유지력의 변화를 알아보기 위해 무치악 덴티폼과 이에 맞는 의치상을 제작하여 의치 접착제 적용 후 3일까지의 인장결합강도를 측정하였다. 결과: 1. 의치접착크림은 농도와 시간에 따라 세포독성이 관찰되는 것은 없었다. 2. 의치접착크림과 인공타액을 동시에 사용한 경우 통계학적으로 가장 높은 인장 결합강도를 나타내었고, 의치접착크림을 단독으로 사용한 경우보다 인장 결합강도가 통계학적으로 유의성 있게 높았다. 이는 인공타액과 의치접착크림의 인장 결합강도의 단순 합계보다 높았다. 3. 의치접착크림과 인공타액을 동시에 사용한 군에서 도포 후부터 1시간 후까지 인장 결합강도는 최대치를 기록하였고 3시간부터 인장 결합강도는 점차 감소하기 시작하여 12시간 후는 최대 인장 결합강도의 70%, 1일후에50%까지 감소하였다. 이상의 결과를 토대로 의치접착크림은 1일에서 4일까지 세포독성이 없었고 의치의 유지력을 향상시키는데 효과적이며, 타액과 같이 작용하여 효과를 더 발휘할 수 있었다. 향후 장기적인 사용에 따른 다양한 세포독성 실험과 접착력의 감소에 대한 연구가 필요하리라 사료된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.