EFFECT OF A DESENSITIZER ON MICROTENSILE BOND STRENGTH OF DIFFERENT ADHESIVES  

Hwang, Sung-Yeon (Department of Conservative Dentistry & Institute for Oral Bioscience College of Dentistry, Chonbuk National University)
Lee, Kyung-Ha (Department of Conservative Dentistry & Institute for Oral Bioscience College of Dentistry, Chonbuk National University)
Yu, Mi-Kyung (Department of Conservative Dentistry & Institute for Oral Bioscience College of Dentistry, Chonbuk National University)
Lee, Kwang-Won (Department of Conservative Dentistry & Institute for Oral Bioscience College of Dentistry, Chonbuk National University)
Publication Information
Restorative Dentistry and Endodontics / v.28, no.5, 2003 , pp. 378-384 More about this Journal
Abstract
This study evaluated the influence of a desensitizer(MS coat) on microtensile bond strength of different adhesives:a three-step adhesive(All-Bond 2), a two-step adhesive(Single Bond), a one-step adhesive(One-up Bond F). Non-caries extracted human molars were used. Dentin surface was obtained by horizontal section on mid-portion of crown using a water-cooled low speed diamond saw. Teeth were randomly divided into 6 group. AMO(MS coat + All Bond), SMO(MS coat + Single Bond)- and OMO(MS coat + One-up Bond F)-dentin surface were treated with 17% EDTA before bonded adhesive. AMX-, SMX- and OMX-dentin surface were bonded with All-Bond 2, Single Bond and One-up Bond F, respectively. with no previous treatment with MS coat and 17% EDTA. About 1cm high resin composite($Z-250^{TM}$) were incrementally build-up on the treated surface. The specimens for the microtensile test were serially sectioned perpendicular to the adhesive layer to obtain $0.7{\times}0.7mm$ sticks. 30 sticks were prepared from each group. After that. tensile bond strength for each stick was measured with Microtensile Tester at a 1mm/min crosshead speed. Fractured dentin surfaces were observed under the SEM. The results were statistically analysed by using a One-way ANOVA and Tukey's test(p<0.05). Value in MPa were: $AMO-44.35{\pm}13.21;{\;}SMO-39.35{\pm}13.32;{\;}OMO-31.07{\pm}10.25;{\;}AMX-49.22{\pm}16.38;{\;}SMX-56.02{\pm}13.35;{\;}OMX-72.93{\pm}16.19$. Application of MS coat reduced microtensile bond strengths of both Single Bond and One-up Bond F, whereas microtensile bond strengths of All-Bond 2 were not affected significantly.
Keywords
Microtensile; Desensitizer; Three-step adhesive; Two-step adhesive; One-step adhesive; Bond strength;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Yoshiyama M, Noire Y, Azoic K et al : Transmission electron microscopic characterization of hypersensitive hyman radicular dentin J Dent Res. 69:1293-1297, 1990   DOI   PUBMED   ScienceOn
2 Jain P, Vargas MA, Denehv GE and BoyerDB : Dentin desensitizing agents: SEM and X ray microanalysis assessment. Am J Dent 10(1):21-26, 1997   PUBMED
3 Zhang Y, Agee K, Pashley DH and Pashley EL : The effects of pain free desensitizer on dentine permeability and tobule occlusion over time, in vitro. J Clin Perlodontol 25:884-891, 1998   DOI
4 Pashley EL, Tao Land Pashely D : Effest of oxalate on dentin bonding. Am J Dent 6(2) :61-64, 1993   PUBMED
5 Tagami J, Tao L and Pashley DH : Correlation among dentin depth, permeability and bond strength of adhesive resins. Dental Material 6(1):45-60, 1990   DOI   ScienceOn
6 Henry O Trowbridge and David R, Silver : A review of current approaches to in office management of tooth hypersensitivity a Review Dental Clinics of North America 34(3):561-578, 1990   PUBMED
7 Snuggs AK Cox LK et al : colloidal MSE for differential diagnosis and treatment of dentin permeability. In: Shimona M, Maeda T, Suda H, etal. dentin/pulp complex Quintessence 245-247, 1996
8 Seam SF, Erthral BS, Ribeiro M, Kroll L and Pereira GDS : The influence of a dentin desensitizer on the microtensile bond strength of two bonding systems. Operative Dentistry 27: 154-160, 2002   PUBMED
9 Pashley DH : Dentin permeability. dentin sensitivity, and treatment through tubule occlusion. J Endodont 12:465-474, 1986   DOI   ScienceOn
10 Kern DG, Scheidt and Pashley DH : Dentinal tubule occlusion and root hypersensitivity. J. Periodont. 62(7):421-428, 1991
11 Jean Camps, Stephana Piazant. Jacoues Dejou. and Jean Claude Franquin : Effect of desensitizing agents on human dentin permeability. Am J Dent. 11(6):286-290, 1998   PUBMED
12 Steven R Armstrong and Daniel B Boyer : Microtensile bond strength testing and failure analysis of two dentin adhesives. Dent Mater 14:44-50, 1998   DOI   ScienceOn
13 Mausner IK, Goldstein GR and Georgescu M : Effect of two dentinal desensitizing agents on retention of complete cast coping using four cements. J Prosthetic Dent 75(2):129-134, 1996   DOI   ScienceOn
14 David H Pashley, Ricardo M Carvalho, Hideheko Sane and Masatoshi Nakajima : The microtensile bond test : a review. J adhesive Dent 1:299-309, 1999   PUBMED
15 Nantiya H Yim, Frederick A, Rueggeberg W, Frank Caughman, Michael Oeroer F and David H Pashley : Effect of dentin desensitizers and cementing agents on etention of fuul crowns using standardized crown preparations. J Prosthet Dent 83:459-465, 2000   DOI   ScienceOn
16 Braem M, Lambrecchts P and Vanherle G. : Stress induced cervical lesion. J Prosthet Dent 67:718-722, 1992   DOI   ScienceOn
17 Gillam DG, Mordan NJ, Sinodiou AD, Tang JY, Knowles JC and Otbsson R : the effect of oxalate containing products on the exposed dentine surface: an SEM investigation. J Oral Rehabilitation 28:1037-1044, 2001   DOI   ScienceOn
18 Levitch LC, Barder JD, Shugars DA and Heymann HO : Non carious cervical lesionl(review). J Dent 22:195-207, 1994   DOI   ScienceOn
19 Lucinda C Hogan and Michael F Burrow : The microtensile strength of bonding resins. Austrian Dental J 46(3):194-197, 2001   DOI   ScienceOn
20 Scene K, Taira Y, Matsumura H and Atsura : Effect of desensitizers on bond strength of 접착제 luting agents to dentin. J Oral Rehabilitation 28: 1122-1128, 2001   DOI   ScienceOn
21 Edward J Swift JR, Ashley H. Lloyd and David A Felton : The effect of resin desensitizing agents on crown retention. JADA 128:195-200, 1997   DOI