PURPOSES: The purpose of this paper is to evaluate interface performance while using various tack coat materials for asphalt overlay. METHODS : The evaluation was conducted with tracking test, permeability, and interface bond strength. Tracking test was conducted using an image processing technique, to investigate the susceptibility of the tack coat materials. BBS and pull-off test were conducted to evaluate bond strength. The permeability test was conducted to evaluate the effect of tack coat materials. RESULTS : Results reveal that the trackless tack coat material demonstrates less tracking compared to other materials. Moreover, both BBS and pull-off tests can effectively evaluate the bond strength at the interface. RSC-4 was measured less bond strength. Moreover, tack coat prevents water penetration through the surface and aids the extension of the surface life of asphalt pavement. CONCLUSIONS : Trackless tack coat demonstrated a high and consistent bond strength performance. The tack coat types demonstrate marginally different performance as function of curing times. Field applicability was tested based on visual observation. Therefore, these should be considered when trackless tack coat is slightly enhanced the pavement performance based on limited this study results. Finally, it is necessary to allow reasonable time for the tack coat to completely cure.
Bond shear strengths of recycled asphalt concrete were evaluated under different tack coat applications. Regardless of the new and old mixtures, the bond shear strengths at $30^{\circ}C$ were increased by 10-20% than those at 1$0^{\circ}C$. The bond shear strengths of recycled asphalt concrete without tack coat showed very low ones. These are the main reasons for the frequent longitudinal interface crack in the field. The effect of tack coat curing time on bond shear strengths was inferior to the tack coat construction temperature.
International conference on construction engineering and project management
/
2022.06a
/
pp.784-791
/
2022
Tack coat is a thin layer of asphalt between the existing pavement and asphalt overlay. During construction, insufficient tack coat layering can later cause surface defects such as slippage, shoving, and rutting. This paper proposed a method for tack coat inspection improvement using an unmanned aerial vehicle (UAV) and deep learning neural network for automatic non-uniform assessment of the applied tack coat area. In this method, the drone-captured images are exploited for assessment using a combination of Mask R-CNN and Grey Level Co-occurrence Matrix (GLCM). Mask R-CNN is utilized to detect the tack coat region and segment the region of interest from the surroundings. GLCM is used to analyze the texture of the segmented region and measure the uniformity and non-uniformity of the tack coat on the existing pavements. The results of the field experiment showed both the intersection over union of Mask R-CNN and the non-uniformity measured by GLCM were promising with respect to their accuracy. The proposed method is automatic and cost-efficient, which would be of value to state Departments of Transportation for better management of their work in pavement construction and rehabilitation.
Kim, Dong kyu;Hwang, Hyun sik;Christopher, Jabonero;Ryu, Sung woo;Cho, Yoon ho
International Journal of Highway Engineering
/
v.18
no.5
/
pp.1-9
/
2016
PURPOSES : This study focuses on the evaluation of interface performance with varying surface texture and tack coat application in an asphalt overlay. METHODS : The evaluation is carried out in two phases: tracking test and interface bond strength test. Using an image processing tool, tracking test is conducted to evaluate the susceptibility of the tack coat material to produce excessive tracking during application. Using the pull-off test method, the bond strength test is performed to determine the ability of the interface layer to resist failure. RESULTS : Results show that the underseal application yields less tracking compared to other applications. However, the bond strength is barely within the minimum acceptable value. On the other hand, RSC-4 produces higher bond strength for all surface types, but the drying time is long, which produces excessive tracking. CONCLUSIONS : While underseal application may be suitable for a trackless condition, the bond strength is less appealing compared to the rest of the tack applications available. RSC-4 demonstrated a high and consistent bond strength performance, but more time is required for drying to avoid excessive tracking. Tack coat application and surface type combination produce varying results. Therefore, these should be considered when selecting suitable future tack coat application options.
PURPOSES : The objective of this study is to evaluate the tack-coating material's properties using the bitumen bond strength(BBS) test and damping test as function of changed curing times. In this study, bonding strength tests were performed according to the curing time of tack coating materials. METHODS : In order to investigate bonding characteristic of tack coating materials, the Pneumatic Adhesion tensile Testing Instrument(PATTI) device is used to measure the bond strength between the tack coating materials and aggregate substrate based on the AASHTO TP-91. Also, damping test as in situ test was used to determine an appropriate traffic openting time for construction vehicle. Four different tack-coating materials were used in this study. The BBS tests were performed a one hour curing and testing temperatures of $5^{\circ}C$, $15^{\circ}C$, and $25^{\circ}C$. Damping test was conducted at 30min, 60min, 90min, and 120 min of curing times with temperatures of $20^{\circ}C$ and $30^{\circ}C$. RESULTS and CONCLUSIONS : The BBS test results show various bond strength as function of tack coat materials. At the same testing condition, A tack coat material shows almost two times higher than D tack coat materials although both materials are satisfied the criteria of material's physical properties. Also, Dampting test results shows similar trend with BBS test result. The damping test result was significantly changed as function of tack coat materials. Based on this study, the tack coating material's curing time is very important. Therefore, both curing time and the bond strength's characteristic has to be considered in standard specification.
OBJECTIVES : Bituminous materials, such as tack coat, are utilized between pavement layers for improving the bond strength in pavement construction sites. The standards regarding the application of bituminous material are not clearly presented in the Korean construction guideline without RS(C)-4. Hence, the objective of this study is to determine the optimum content of bituminous materials by analyzing interlayer shear strength (ISS) from the direct shear tester, which was developed in this research. The shear strength of tack coat was defined with the sort of bituminous materials. METHODS : The mixtures for the shear test were made using marshall mix design. The specimens were vertically and horizontally separated for the direct shear test. The separated specimens were bonded using bituminous material. The objectives of the experiment are to determine the performance of bond and shear properties resulting from slippage, rutting, shovel, and corrugation of asphalt pavements. A machine based on the Louisiana interlayer shear strength tester (LISST) of NCHRP Report-712 was developed to determine the ISS. The applied types of tack coat were RS(C)-4, AP-3, QRS-4, and BD-coat with contents of $0.3{\ell}/m^2$, $0.45{\ell}/m^2$, $0.6{\ell}/m^2$, and $0.8{\ell}/m^2$, respectively. RESULTS : Table 2 gives the results of the direct shear test using the developed shear machine. The BD-coat type indicated the highest average ISS value compared to the others. Between the surface and binder course, optimum tack coat application rates for AP-3, RS(C)-4, QRS-4, and BD-Coat were $0.6{\ell}/m^2$, $0.3{\ell}/m^2$, $0.6{\ell}/m^2$, and $0.45{\ell}/m^2$, respectively. These optimum contents were determined using the ISS value. CONCLUSIONS : The ISS values of AP-3, RS(C)-4, and QRS-4 showed similar tendencies when ISS increased in the range $0.3{\sim}0.6{\ell}/m^2$, while ISS decreased when the applied rate exceeded $0.6{\ell}/m^2$. Similarly, the highest ISS value of the BD-coat was observed when the applied rate was $0.45{\ell}/m^2$. However, shear strength was similar to the maximum value of ISS when the tack-coat application rate of BD-Coat exceeded $0.45{\ell}/m^2$.
PURPOSES: The objectives of this study were to develop a new polymer-modified emulsion for application to tack coats and to evaluate its properties by comparing it with other types of asphalt emulsions, with the goal of providing an enhanced tack coat material for use in construction. METHODS: Modified asphalt binders were developed from using SBS and SBR latex in the laboratory, and their fundamental properties, such as their penetration index and PG grade, were evaluated. Based on the properties, a new tack coat material was developed. To evaluate the newly developed asphalt emulsion, the bonding strength between the two layers of HMA was measured by applying a uniaxial tensile test and shear test. For the tests, a total of four different conditions were applied to the specimens, including the developed asphalt emulsion, latex modified asphalt emulsion, conventional asphalt emulsion, and non-tack coating. RESULTS AND CONCLUSIONS: Overall, the developed asphalt emulsion exhibits the best bonding strength behavior among all of the three types. Also, the two types of polymer-modified emulsions were found to be better for application for use as a tack coat than a conventional emulsion. Especially, at a high temperature ($50^{\circ}C$), the conventional asphalt emulsion no longer acts as a tack coating material. Therefore, the polymer-modified emulsion should be considered for application to tack coat construction during the summer.
Jo, Shinheang;Kim, Kyungnam;Cui, Wenhui;Kim, Nakseok
KSCE Journal of Civil and Environmental Engineering Research
/
v.41
no.6
/
pp.737-744
/
2021
Spray paving minimizes material lost during the construction or repair of a road surface, and it can be done in conjunction with tack coating. This approach involves applying the asphalt mixture at the same time as spraying the tack coat by attaching a spraying device to the asphalt paver. When applying an asphalt overlay to an aged concrete surface, it is important to ensure the adhesion performance between different material properties. Accordingly, there is a need for a tack coat that can be applied by spray paving and that exhibits good adhesive performance on different materials. In this study, bonding strength tests under various conditions were performed to evaluate the basic performance of a tack coat developed for use with a spray paver. The bonding performance of the tack coat was observed to be affected by curing conditions and material lost during construction. The test results also showed that the tensile and shear bonding strengths of the developed tack coat were 1.21 and 1.99 times higher than those of a conventional one, respectively. As a result, the developed tack coat is considered suitable for application to spray paving.
Hong, Ki;Kim, Young Kyu;Bae, Abraham;Lee, Seung Woo
International Journal of Highway Engineering
/
v.19
no.6
/
pp.37-46
/
2017
PURPOSES : A composite pavement utilizes both an asphalt surface and a concrete base. Typically, a concrete base layer provides structural capacity, while an asphalt surface layer provides smoothness and riding quality. This pavement type can be used in conjunction with rollercompacted concrete (RCC) pavement as a base layer due to its fast construction, economic efficiency, and structural performance. However, the service life and functionality of composite pavement may be reduced due to interfacial bond failure. Therefore, adequate interfacial bonding between the asphalt surface and the concrete base is essential to achieving monolithic behavior. The purpose of this study is to investigate the bond characteristics at the interface between asphalt (HMA; hot-mixed asphalt) and the RCC base. METHODS : This study was performed to determine the optimal type and application rate of tack coat material for RCC-base composite pavement. In addition, the core size effect, temperature condition, and bonding failure shape were analyzed to investigate the bonding characteristics at the interface between the RCC base and HMA surface. To evaluate the bond strength, a pull-off test was performed using different diameters of specimens such as 50 mm and 100 mm. Tack coat materials such as RSC-4 and BD-Coat were applied in amounts of 0.3, 0.5, 0.7, 0.9, and $1.1l/m^2$ to determine the optimal application rate. In order to evaluate the bond strength characteristics with temperature changes, a pull-off test was carried out at -15, 0, 20, and $40^{\circ}C$. In addition, the bond failure shapes were analyzed using an image analysis program after the pull-off tests were completed. RESULTS : The test results indicated that the optimal application rate of RSC-4 and BD-Coat were $0.8l/m^2$, $0.9l/m^2$, respectively. The core size effect was determined to be negligible because the bond strengths were similar in specimens with diameters of 50 mm and 100 mm. The bond strengths of RSC-4 and BD-Coat were found to decrease significantly when the temperature increased. As a result of the bonding failure shape in low-temperature conditions such as -15, 0, and $20^{\circ}C$, it was found that most of the debonding occurred at the interface between the tack coat and RCC surface. On the other hand, the interface between the HMA and tack coat was weaker than that between the tack coat and RCC at a high temperature of $40^{\circ}C$. CONCLUSIONS : This study suggested an optimal application rate of tack coat materials to apply to RCC-base composite pavement. The bond strengths at high temperatures were significantly lower than the required bond (tensile) strength of 0.4 MPa. It was known that the temperature was a critical factor affecting the bond strength at the interface of the RCC-base composite pavement.
PURPOSES : A tack coat has been utilized to increase the bond performance between the surface layer and base course (intermediate course) at various road pavement sites. This is similarly true in other nations. Based on this connection, the objective of the present study is to evaluate the properties of hot mix asphalt (HMA) mixtures with an RSC-4 or BD-Coat and determine the application rate of the tack coat. METHODS : The HMA specimens were manufactured using superpave gyratory compaction. The HMA mixtures were composed of a 5-cm thick surface layer and a 10-cm thick base course. An impact hammer resonance test (IHRT) and a static load shear test were conducted to evaluate the performance of the HMA mixtures with a tack coat. From these tests, the dynamic moduli related to the high-frequency resistance and interlayer shear strength (ISS) of HMA could be obtained. RESULTS : The results of the dynamic moduli of HMA are discussed based on the resonance frequency (RF). To check the accuracy of the IHRT, we conducted a coherence analysis. A direct shear test using the application of a static load test was carried out to evaluate the interlayer shear strength (ISS) of HMA. CONCLUSIONS : The maximum ISS was demonstrated at an RSC-4 application rate of 462 gsm, and the maximum dynamic modulus was demonstrated at an RSC-4 application rate of 306 gsm. By averaging the results of the ISS, the maximum ISS values were obtained when a BD-Coat application rate of 602 gsm was applied.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.