In this paper, we introduce silicon dioxide films deposited by Laser CVD, and evaluate the breakdown characteristics of these films by TZDB(Time Zero Dieiectric Breakdown) and TDDB(Time Dependent Dielectric Breakdown) test, failure times against eletric field are examined and accelation factors ${\beta}$ are obtained, and also, long term reliability is described by examining TDDB under positive voltage bias, all the above results are compared with PECVD(Plasma Enhanced CVD) $SiO_2$ breakdown, data, as a result, it is shown that the breakdown characteristics of Laser CVD $SiO_2$ films is improved.
서로 다른 두께를 가진 다층구조 $BaTiO_3$ 박막의 절연신뢰성을 time-zero dielectric breakdown (TZDB) 기법과 time-dependent dielectric breakdown (TDDB) 기법을 사용하여 평가하였으며 통계적 방법을 이용하여 그 결과를 분석하였다. 다층구조 $BaTiO_3$ 박막은 rf-magnetron sputtering 방법으로 ITO가 코팅된 유리기판 위에 형성되었다 TZDB 측정 결과, 박막의 두께가 증가 할수록 최고 빈도수를 보이는 항복전기장의 세기는 낮아지는 것으로 확인되었으며, 두께에 따라 다른 항전기장의 분포를 보였다. TDDB 결과로부터 박막의 두께 증가에 파라 안정적인 시간거동 특성이 확인되었으며 이것은 항전기장의 분포 특성과 관계가 있는 것으로 보인다.
Proceedings of the Korean Institute of Information and Commucation Sciences Conference
/
1998.11a
/
pp.165-168
/
1998
Re-oxidized nitrided oxides which have been investigated as alternative gate oxide for Metal- Oxide -Semiconductor field effect devices were grown by conventional furnace process using pure NH$_3$ and dry $O_2$ gas, and were characterized via a Fowler-Nordheim Tunneling electron injection technique. We studied Ig-Vg characteristics, leakage current, $\Delta$Vg under constant current stress from electrical characteristics point of view and TDDB from reliability point of view of MOS capacitors with SiO$_2$, NO, ONO dielectrics. Also, we studied the effect of stress temperature (25, 50, 75, 100, and 1$25^{\circ}C$). Overall, our results indicate that optimized re-oxidized nitrided oxide shows improved Ig-Vg characteristics, leakage current over the nitrided oxide and SiO$_2$. It has also been shown that re-oxidized nitrided oxide have better TDDB performance than SiO$_2$ while maintaining a similar temperature and electric field dependence. Especially, the Qbd is increased by about 1.5 times.
Kim, Jae-Ho;Yi, Seung-Hwan;Kim, Chun-Sub;Sung, Yung-Kwon
Proceedings of the KIEE Conference
/
1989.07a
/
pp.359-363
/
1989
Recently, it is reported that the behavior of thermal $SiO_2$ under high electric field and current condition has a major effect on MOS device degration. Furthermore, when thin oxide films are applied in practical device, the presence of oxide defects will be a serious problem. In this paper, because TDDB is the useful method to measure the effective density of defects, we stressed MOS structure that is 150 A of thermally grown $SiO_2$as a function of electric field (9-19 MV/cm), temperature ($22^{\circ}C$ - $150^{\circ}C$) and current. By examing TDDB under positive voltage, long-term oxide breakdown reliabiliy is described. From these data, breakdown wearout limitation for the oxide films can be characterized.
Journal of the Korean Institute of Telematics and Electronics D
/
v.34D
no.6
/
pp.43-49
/
1997
Tungsten poycide has studied gate oxide reliability and dielectric strength charactristics as the composition of gate electrode which applied submicron on CMOS and MOS device for optimizing gate electrode resistivity. The gate oxide reliability has been tested using the TDDB(time dependent dielectric breakdwon) and SCTDDB (stepped current TDDB) and corelation between polysilicon and WSi$_{2}$ layer. iN the case of high intrinsic reliability and good breakdown chracteristics on polysilicon, confirmed that tungsten polycide layer is a better reliabilify properities than polysilicon layer. Also, hole trap is detected on the polysilicon structure meanwhile electron trap is detected on polycide structure. In the case of electron trap, the WSi$_{2}$ layer is larger interface trap genration than polysilicon on large POCL$_{3}$ doping time and high POCL$_{3}$ doping temperature condition. WSi$_{2}$ layer's leakage current is less than 1 order and dielectric strength is a larger than 2MV/cm.
본 논문에서는 SiH$_{4}$-N$^{2}$ 혼합가스에 의한 PECVD 방법으로 퇴적시킨 실리콘 질화막의 신뢰성을 평가하기 위해 절연파괴 분포와 TDDB(Time Dependent Dielectric Breakdown)특성을 고찰하였다. MNS 캐패시터의 절연파괴 분포는 7-8NV/cm의 전계세기에서 그 파괴전계가 집중되었으며 전계와 온도 stress에 의해 파괴시간이 지수함수적으로 감소함을 알 수 있었다. 아울러 이러한 TDDB 특성과 계면준위 밀도 및 SiN 막내의 공간전하형성과의 관련성을 고찰하였다.
THE ELECTRICAL CHARACTERISTICS Of RAPID THERMAL OXIDES AND NITRIDED OXIDES HAVE BEEN INVESTIGATED. R.T.OXIDE FILMS HAVE BEEN PREPARED BY ONLY R.T. OXIDATION OR R.T.OXIDATION AND SUBSEQUENT R.T.ANNEAL. NITRIDED OXIDE FILMS HAVE BEEN PREPARED BY R.T.OXIDATION AND SUBSEQUENT R.T.NITRIDATION.AND CONVENTIONAL OXIDES ALSO HAVE BEEN PREPARED TO COMPARE WITH R.T.P OXIDES. R.T.ANNEALED OXIDES SHOW EXCELLENT BREAKDOWN FIELD. LEAKAGE CURRENT AND TDDB CHARACTERISTICS. ALSO, CAPACITANCE Of R.T NITRIDED OXIDES ARE SUPERIOR BY 10% TO CONVENTIONAL OXIDES, BUT TDDB CHARACTERISTIC ARE POORER THAN OXIDE FILMS.
Since the integration level of VLSI circuits progresses very quickly, a highly reliable thin $SiO_2$ film is required to fabricate a small-geometry MOS device. In the present study we have attempted to eliminate the failure-causing defects that develop in thin oxide films during the oxidation step by performing a long-time preoxidation and postoxidation annealing. The TDDB test and the copper decoration method were used to calculate the oxide defects density of MOS device. The dielectric reliability of high-quality thin oxides have been studied by using the time-zero-dielectric-breakdown (ramp-voltage-stressed I-V) and time-dependent-dielectric -breakdown (Constant-stressed I-V) tests. Failure times against temperature and electric field are examined and acceleration factors are abtained for each parameter. Based on the data obtained, breakdown wearout limitation for thin oxide films is estimated.
The dielectric reliability of a polycrystalline and a multilayered $BaTiO_3$ thin films was evaluated using a time-zero dielectric breakdown (TZDB) and a time-dependent dielectric breakdown (TDDB) techniques. The $BaTiO_3$ thin films were prepared by rf-magnetron sputtering technique on ITO-coated glass substrates. In case of the multilayered $BaTiO_3$ thin film, the dielectric breakdown histogram, which was obtained from the TZDB measurements, showed a typical Weibull distribution. While in case of polycrystalIine $BaTiO_3$ thin film, a randomly distributed dielectric breakdown histogram was observed. The TDDB results of the multilayered $BaTiO_3$ thin film guaranteed about $10^5$ hours-operation under the stress field of 1 MV/cm.
Seo, Seung-Ho;Jin, Gwang-Seon;Lee, Han-Gyeol;Lee, Won-Jun
Proceedings of the Korean Vacuum Society Conference
/
2011.02a
/
pp.179-179
/
2011
관통전극(TSV, Trough Silicon Via) 기술은 전자부품의 소형화, 고성능화, 생산성 향상을 이룰 수 있는 기술이다. Cu는 현재 배선 기술에 적용되고 있고 전기적 저항이 낮아서 TSV filling 재료로 사용된다. 하지만 확산 방지막에 의해 완벽히 감싸지지 않는다면, Cu+은 빠르게 절연막을 통과하여 Si 웨이퍼로 확산된다. 이런 현상은 절연막의 누설과 소자의 오동작 등의 신뢰성 문제를 일으킬 수 있다. 현재 TSV의 제조와 열 및 기계적 응력에 관한 연구는 활발히 진행되고 있으나 Biased-Thermal Stress(BTS) 조건하의 Cu 확산에 관한 연구는 활발하지 않는 것이 실정이다. 이를 위해 본 연구에서는 TSV용 Cu 확산 방지막 Ti에 대해 Cu+의 drift 억제 특성을 조사하였다. 실험을 위해 Cu/확산 방지막/Thermal oxide/n-type Si의 평판 구조를 제작하였고 확산 방지막의 두께에 따른 영향을 조사하기 위해 Ti의 두께를 10 nm에서 100 nm까지 변화하였으며 기존 Cu 배선 공정에서 사용되는 확산 방지막 Ta와 비교하였다. 그리고 Cu+의 drift 측정을 위해 Biased-Thermal Stress 조건(Thermal stress: $275^{\circ}C$, Bias stress: +2MV/cm)에서 Capacitance 및 Timedependent dielectric breakdown(TDDB)를 측정하였다. 그 결과 Time-To Failure(TTF)를 이용하여 Cu+의 drift를 측정할 수 있었으며, 확산 방지막의 두께가 증가할수록 TTF가 증가하였고 물질에 따라 TTF가 변화하였다. 따라서 평판 구조를 이용한 본 실험의 Cu+의 drift 측정 방법은 향후 TSV 구조에서도 적용 가능한 방법으로 생각된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.