• Title/Summary/Keyword: Subtrate

Search Result 13, Processing Time 0.027 seconds

Preferred Orientation, Microstructure, Surface Morphology and Mechanical Properties of Electrodeposited Copper Foils (電解銅薄의 優先方位, 斷面組織, 表面形態 및 機械的 性質)

  • Kim, Yoon-Keun;Lee, Dong-Nyung
    • Journal of Surface Science and Engineering
    • /
    • v.18 no.3
    • /
    • pp.95-104
    • /
    • 1985
  • A study has been made of preferred orientation, crose sectional microstructure, surface morphology and mechanical properties of copper foils fabricated by electrodeposition on 304 stainless steel plate from copper sulfate baths for high speed plating. The preferred orientation of the copper foils changed from the [110] to the [111] to ture with decreasing bath temperature and increasing cathode current density. The foils with the [110] texture had the field oriented texture type structure and the surface of many asperities grooved approximately perpendicular to the subtrate. A specimen with the [111]+[311] texture had the lower strength than one with the [10] texture, if they were obtained under similar electrolysis conditions.

  • PDF

Characteristics of Defects in SiOx Thin films on Ethylene Terephthalate by High-temperature E-beam Deposition (고온 전자빔 증착에 의한 Ethylene Terephthalate상의 SiOx 박막의 특성 평가)

  • Han Jin-Woo;Kim Young-Hwan;Kim Jong-Hwan;Seo Dae-Shlk;Moon Dae-Gyu
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.1
    • /
    • pp.71-74
    • /
    • 2006
  • In this paper, we investigated the characterization of silicon oxide(SiOx) thin film on Ethylene Terephthalate(PET) substrates by e-beam deposition for transparent barrier application. The temperature of chamber increases from $30^{\circ}C$ to $110^{\circ}C$, the roughness increase while the Water vapor transmission rate (WVTR) decreases. Under these conditions, the WVTR for PET can be reduced from a level of $0.57 g/m^2/day$ (bare subtrate) to $0.05 g/m^2/day$ after application of a 200-nm-thick $SiO_2$ coating at 110 C. A more efficient way to improve permeation of PET was carried out by using a double side coating of a 5-${\mu}m$-thick parylene film. It was found that the WVTR can be reduced to a level of $-0.2 g/m^2/day$. The double side parylene coating on PET could contribute to the lower stress of oxide film, which greatly improves the WVTR data. These results indicates that the $SiO_2$ /Parylene/PET barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

Improvement of Permeation of Applied Multi-layer Encapsulation of Thin Films on Ethylene Terephthalate(PET) (고분자 기판위에 다층 구조의 박막형 보호층을 적용한 투습률 향상)

  • Kim Jong-Hwan;Han Jin-Woo;Kim Young-Hwan;Seo Dae-Shik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.3
    • /
    • pp.255-259
    • /
    • 2006
  • In this paper, the inorganic-organic thin film encapsulation layer was newly adopted to protect the organic layer from moisture and oxygen. Using the electron beam, Sputter and Spin-Coater system, the various kinds of inorganic and organic thin-films were deposited onto the Ethylene Terephthalate(PET) and their interface properties between organic and inorganic layer were investigated. In this investigation, the SiON and Polyimide(PI) layer showed the most suitable properties. Under these conditions, the WVTR(water vapour transition rate) for PET can be reduced from level of $0.57\;g/m^2{\cdot}day$ (bare subtrate) to $1{\times}10^{-5}\;g/m^2{\cdot}day$ after application of a SiON and Polyimide layer. These results indicates that the SiON/PI/SiON/PI/PET barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

Development of OLED Passivation Method for High efficency and life time (고효율 및 장수명의 OLED Passivation 기술 개발)

  • Han, Jin-Woo;Kim, Jong-Hwan;Kim, Young-Hwan;Seo, Dae-Shik;Kim, Yong-Hoon;Moon, Dae-Gyu;Han, Jeong-In
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.11a
    • /
    • pp.267-268
    • /
    • 2005
  • In this paper, the inorganic-organic thin film encapsulation layer was newly adopted to protect the organic layer from moisture and oxygen. Using the electron beam, Sputter and Spin-Coater system, the various kinds of inorganic and organic thin-films were deposited onto the Ethylene Terephthalate(PET) and their interface properties between organic and inorganic layer were investigated. In this investigation, the SiON and Polyimide(PI) layer showed the most suitable properties. Under these conditions, the WVTR(water vapour transition rate) for PET can be reduced from level of 0.57 g/$m^2$/day (bare subtrate) to $1{\times}10^{-5}$ /$m^2$/day after application of a SiON and Polyimide layer. These results indicates that the SiON/PI/SiON/PI/PET barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

  • PDF

Improvement of Permeation of Solvent-free Multi-layer Encapsulation of Thin Films on Polyethylene Terephthalate (PET) (고분자 기판위에 유기 용매를 사용하지 않은 다층 박막 Encapsulation 기술 개발)

  • Han Jin-Woo;Kang Hee-Jin;Kim Jong-Yeon;Seo Dae-Shik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.8
    • /
    • pp.754-757
    • /
    • 2006
  • The inorganic multi-layer thin film encapsulation was newly adopted to protect the organic layer from moisture and oxygen. Using the electron beam, sputter, inorganic multi-layer thin-film encapsulation was deposited onto the Polyethylene Terephthalate (PET) and their interface properties between inorganic and organic layer were investigated. In this investigation, the SiON, $SiO_2$ and parylene layer showed the most suitable properties. Under these conditions, the WVTR for PET can be reduced from level of $0.57g/m^2/day$ (bare subtrate) to $1*10^{-5}g/m^2/day$ after application of a SiON and $SiO_2$ layer. These results indicates that the $PET/SiO_2/SiON/Parylene$ barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

EO Performances of Flexible TN-LCD using in-situ Ultraviolet Exposure during Imidization of Polyimide on the Polymer Film

  • Moon, Hyun-Chan;Hwang, Jeoung-Yeon;Lee, Whee-Won;Seo, Dae-Shik
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.3
    • /
    • pp.106-109
    • /
    • 2005
  • We have investigated the generation of pretilt angle for a nematic liquid crystal (NLC) alignment with in-situ photoalignment method on polyimide (PI) surfaces using polymer films. Especially, we studied in-situ photoalignment changing heating temperature from $50^{\circ}C\;to\;120^{\circ}C$ on the polymer film. The LC aligning capabilities and pretilt angle on the polymer substrates were better than those on the glass substrate using in-situ photoalignment method. It is considered that this increase in pretilt angle may be attributed to the roughness of the micro-groove substrate induced by the in-situ photoalignment. As temperature of heated subtrate and UV exposure time increase, pretilt angle of the cell used polymer film increased. It is considered that the heating temperature of substrate is attributed to generate pretilt angle. Also, electro-optical performances of the in-situ photoaligned TN cell using the polymer substrate are almost the same as that of the TN cell using the glass substrate.

Phenoloxidases and Photomorphogenesis in Coprinus congregatus (Coprinus congregatus의 분화와 Phenoloxidase와의 관계)

  • 최형태
    • Proceedings of the Botanical Society of Korea Conference
    • /
    • 1987.07a
    • /
    • pp.157-167
    • /
    • 1987
  • The have been many reports that phenoloxidase are correlated with development in many fungi. C. congregatus, one of nushroom-forming basidiomycetes, which requires light for its development also has phenoloxidases. In C. congragatus, there are two sets of membrane-associated phenoloxidase (PHO I and PHO II) which are differentiated by their isozyme patterns, and each enzyme set consists of two different subtrate specific enzyme protein; o-tolidine reacting enzyme, and DOPA reacting enzyme. PHO I which is localized by a protoplast-concanavalin A technique by using a new solidifying agent, Pluronic Polyol F 127, instead of agar appears in the vegetative hyphae, and PHO II appears at the early primordial stage on agar and at the sclerotial stage of liquid shake cultures. Inhibition of PHO I with the enzyme inhibitors inhibits mushroom formation as well as melanization of the vegetative hyphae at concentrations which do not inhibit the vegetative growth. PHO I deficient mutants do not form mushrooms or melanins, and the mutants show abnormal nuclear migration patterns. PHO II has roles; possibly cementing the adjacent hyphae during the actual three dimensonal structure formation, and melanizing mushrooms and sclerotia. The possible roles of PHO I in the light reception complex and in melanin formation, the function of malanin, and possible roles of postulated post translational modifying enzymes which regulate the phenoloxidases, nuclear migration pattern, and self-nonself recognition mechanism are discussed.

  • PDF

Direct Alcohol Fermentation of Starch by Schwanniomyces castellii (Schwanniomyces castellii에 의한 전분의 직접 알콜발효)

  • 성정헌;고성환유연우
    • KSBB Journal
    • /
    • v.7 no.3
    • /
    • pp.229-234
    • /
    • 1992
  • Alcohol fermentations were carried out to confirm the capacity of ethanol production from glucose, starch and soluble starch(dextrin) by Schwanniomyces castellii NRRL Y-2477. Schw. castellii NRRL Y-2477 was able to produce the 63.9g/l ethanol using 94% subtrate from 150g/l-glucose medium. The direct alcohol fermentation of starch having the maximum solubility of 20g/1 at $30^{\circ}C$ yielded 9.1g/l ethanol upon complete depletion of starch, whereas 34.5g/1 ethanol was produced by utilizing 82% of 100g/1 soluble starch medium. The fermentation of 150g/1 soluble starch produced 52.1g/l ethanol using about 79% of substrate. Thus, it was found that the limiting step of direct alcohol fermentation of starch by Schwanniomyces castellii NRRL Y-2477 was a hydrolysis of starch.

  • PDF

Simultaneous Saccharification and Fermentation of Ground Corn Stover for the Production of Fuel Ethanol Using Phanerochaete chrysosporium, Gloeophyllum trabeum, Saccharomyces cerevisiae, and Escherichia coli K011

  • Vincent, Micky;Pometto III, Anthony L.;Leeuwen, J. (Hans) Van
    • Journal of Microbiology and Biotechnology
    • /
    • v.21 no.7
    • /
    • pp.703-710
    • /
    • 2011
  • Enzymatic saccharification of corn stover using Phanerochaete chrysosporium and Gloeophyllum trabeum and subsequent fermentation of the saccharification products to ethanol by Saccharomyces cerevisiae and Escherichia coli K011 were achieved. Prior to simultaneous saccharification and fermentation (SSF) for ethanol production, solid-state fermentation was performed for four days on ground corn stover using either P. chrysosporium or G. trabeum to induce in situ cellulase production. During SSF with S. cerevisiae or E. coli, ethanol production was the highest on day 4 for all samples. For corn stover treated with P. chrysosporium, the conversion to ethanol was 2.29 g/100 g corn stover with S. cerevisiae as the fermenting organism, whereas for the sample inoculated with E. coli K011, the ethanol production was 4.14 g/100 g corn stover. Corn stover treated with G. trabeum showed a conversion 1.90 and 4.79 g/100 g corn stover with S. cerevisiae and E. coli K011 as the fermenting organisms, respectively. Other fermentation co-products, such as acetic acid and lactic acid, were also monitored. Acetic acid production ranged between 0.45 and 0.78 g/100 g corn stover, while no lactic acid production was detected throughout the 5 days of SSF. The results of our experiment suggest that it is possible to perform SSF of corn stover using P. chrysosporium, G. trabeum, S. cerevisiae and E. coli K011 for the production of fuel ethanol.

Improvement of Permeation of Solvent-free Multi-Layer Encapsulation of thin films on Ethylene Terephthalate(PET) (고분자 기판위에 유기 용매를 사용하지 않은 다층 박막 Encapsulation 기술 개발)

  • Kang, Hee-Jin;Han, Jin-Woo;Kim, Jong-Yeon;Moon, Hyun-Chan;Choi, Sung-Ho;Park, Kwang-Bum;Kim, Tae-Ha;Kim, Hwi-Woon;Seo, Dae-Shik
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.04a
    • /
    • pp.56-57
    • /
    • 2006
  • In this paper, the inorganic multi-layer thin film encapsulation was newly adopted to protect the organic layer from moisture and oxygen. Using the electron beam, Sputter, inorganic multi-layer thin-film encapsulation was deposited onto the Ethylene Terephthalate(PET) and their interface properties between inorganic and organic layer were investigated. In this investigation, the SiON SiO2 and parylene layer showed the most suitable properties. Under these conditions, the WVTR for PET can be reduced from a level of $0.57\;g/m^2/day$ (bare subtrate) to 1*10-5 g/$m^2$/day after application of a SiON and SiO2 layer. These results indicates that the PET/SiO2/SiON/Parylene barrier coatings have high potential for flexible organic light-emitting diode(OLED) applications.

  • PDF