Development of Estimation of Model for Mechanical Properties of Steel Fiber Reinforced Concrete according to Aspect Ratio and Volume Fraction of Steel Fiber (강섬유의 형상비와 혼입률에 따른 강섬유 보강 콘크리트 보의 역학적 특성 추정 모형 개발)

  • Kwak, Kae-Hwan;Hwang, Hae-Sung;Sung, Bai-Kyung;Jang, Hwa-Sup
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.48 no.3
    • /
    • pp.85-94
    • /
    • 2006
  • Practially useful method of steel fiber for construction work is presented in this study. The most important purpose of this study is to develop a model which can predict mechanical behavior of the structure according to aspect ratio and volume fraction of steel fiber. Experiments on compressive strength, elastic modulus, and splitting strength were performed with self-made cylindrical specimens of variable aspect ratios and volume fractions. The experiment showed that compressive strength was not in direct proportion to volume fraction which doesn't seem to have great influence over compressive strength. However, splitting strength showed almost direct proportion to aspect ratio and volume fraction. Improvement of optimal efficiency was confirmed when the aspect ratio was 70. Experiments on flexural strength, fracture energy, and characteristic length were carried out with self-manufactured beams with notch. As a result, increases of flexural strength, fracture energy, and characteristic length according to increase of volume fraction tend to be prominent when aspect ratio is 70. The steel fiber improves concrete to be more ductile and tough. Moreover, regression analysis was the performed and predictable model was developed after determining variables. With comparison and analysis of suggested estimated values and measured data, reliance of the model was verified.

Mechanical Properties of Steam Cured High-Strength Steel Fiber-Reinforced Concrete with High-Volume Blast Furnace Slag

  • Yang, Jun-Mo;Yoo, Doo-Yeol;Kim, You-Chan;Yoon, Young-Soo
    • International Journal of Concrete Structures and Materials
    • /
    • v.11 no.2
    • /
    • pp.391-401
    • /
    • 2017
  • In this study, the effects of water-to-binder (W/B) ratio and replacement ratio of blast furnace slag (BFS) on the compressive strength of concrete were first investigated to determine an optimized mixture. Then, using the optimized high-strength concrete (HSC) mixture, hooked steel fibers with various aspect ratios and volume fractions were used as additives and the resulting mechanical properties under compression and flexure were evaluated. Test results indicated that replacement ratios of BFS from 50 to 60% were optimal in maximizing the compressive strength of steam-cured HSCs with various W/B ratios. The use of hooked steel fibers with the aspect ratio of 80 led to better mechanical performance under both compression and flexure than those with the aspect ratio of 65. By increasing the fiber aspect ratio from 65 to 80, the hooked steel fiber volume content could be reduced by 0.25% without any significant deterioration of energy absorption capacity. Lastly, complete material models of steel-fiber-reinforced HSCs were proposed for structural design from Lee's model and the RILEM TC 162-TDF recommendations.

Mechanical Properties of Steel-Fiber Reinforced Concrete (강섬유보강콘크리트의 역학적 거동 특성)

  • 홍성구;권숙국
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.31 no.3
    • /
    • pp.81-91
    • /
    • 1989
  • The aims of this study were to determine mechanical properties of steel-fiber reinforced concrete under splitting tensile, flexural and compressive loading, and thus to improve the possible applications of concrete. The major factors experimentally investigated in this study were the fiber content and the length and the diameter of fibers. The major results obtained are summarized as follows : 1.The strength, strain, elastic modulus and energy obsorption capability of steel-fiber reinforced concrete under splitting tensile loading were significantly improved by increasing the fiber content or the aspect ratio. 2.The flexural strength, central deflection, and flexural toughness of steel4iber reinforced beams were significantly improved by increasing the fiber content or the aspect ratio. And flexural behavior characteristic was good at the aspect ratio of about 60 to 75. 3.The strength, strain, and energy absorption capability in compression were increased with the increase of the fiber content. These effects were not so sensitive to the aspect ratio. The energy absorption capability was improved only slightly with the increase of the fiber length. 4.The elastic modulus, transverse strains, and poisson's ratios in compression were not influenced by the fiber content. 5.The steel-fibers were considered to be appropriated as the materials covering the weakness of concrete because the mechanical properties of concrete in tension and flexure were significantly improved by steel-fiber reinforcement.

  • PDF

Study on the Strength Characteristics and Flexural Toughness of Steel Fiber Reinforced Polymer Concrete (강섬유 보강 폴리머 콘크리트의 강도특성 및 휨인성에 관한 연구)

  • 김기락;연규석;이윤수
    • Journal of the Korea Concrete Institute
    • /
    • v.11 no.4
    • /
    • pp.137-145
    • /
    • 1999
  • The use of steel fiber reinforced to improve the strength and flexural toughness of concrete is well known, but reinforcement of polymer concrete with steel fibers has been hardly reported till now. Polymer concrete has high strength, durability and freeze-thaw resistance than that of cement concrete, but it has disadvantage such as low flexural toughness. In this paper, the strength characteristics and flexural toughness of steel fiber reinforced polymer concrete are investigated experimentally with various steel fiber aspect ratios($\ell$/d), and contents(vol.%). As the result, the flexural and splitting tensile strengths and flexural toughness were increased aspect ratio, and reach the maximums at a aspect ratio of 50. The relationship between the compressive, flexural and splitting tensile strength were high. And the relationship between flexural strength and strain energy was approximately linear.

Compressive and Flexural Behavior of High-Strength Concrete Incorporating Different Types of Hooked-End Steel Fibers (강섬유 특성에 따른 고강도 콘크리트의 압축 및 휨 거동)

  • Jeong, Woo-Jin;Jin, Ai-Hua;Yun, Hyun-Do
    • Journal of Korean Association for Spatial Structures
    • /
    • v.23 no.2
    • /
    • pp.69-78
    • /
    • 2023
  • This paper investigates the effects of aspect ratio and volume fraction of hooked-end normal-strength steel fibers on the compressive and flexural properties of high-strength concrete with specified compressive strength of 60 MPa. Three types of hooked-end steel fibers with aspect ratios of 64, 67 and 80 were considered and three volume fractions of 0.25%, 0.50% and 0.75% for each steel fiber were respectively added into each high-strength concrete mixture. The test results indicated that the addition of normal-strength steel fibers is effective to improve compressive and flexural properties of high-strength concrete but fiber aspect ratio had little effect on the modulus of elasticity and compressive strength. As steel fiber content and aspect ratio increased, flexural beahvior of notched high-strength concrete beams was effectively improved.

A Stydy on Steel Wire Fiber Reinforced Refractory Castable (철근 캐스터블 내화물의 고온특성에 관한 연구)

  • 박금철;최영섭;한문희;장영재;박근원
    • Journal of the Korean Ceramic Society
    • /
    • v.17 no.2
    • /
    • pp.69-74
    • /
    • 1980
  • This study deals with the wire content, wire diameter, aspect ratio , it's arrangement of steel, wire fiber and the sorts of castable which affected the character of steel wire fiber reinformced refractory castable. Two kinds of alumina based refractory castables, one is for 1650℃ and the other is for 1800℃, and stainless steel which is SUS 304 type 0.25, 0.34 , 0.37 and 0.50m/min diameter were used respectively. Aspect ratio was adjusted to 50, 75, 100 and steel fiber content was also adjusted to 1-4wt% each. The results of the experiment were as follows : 1. At firing temperature around 1,000℃, MOR is increased with increasing wire content and aspect ratio with decreasing firing temperature, which depends on the Romualdi's Fiber Spacing Theory. But for calculation of the fiber spacing, Swamy equation is more a aplicable to the extensive fiber mixing conditions. However, the condition differs from the above at firing temperature around 1,350℃ ,because of the degradation of wire and the progress of sintering of castable. 2. Linear change is getting larger corresponding to the increase of wire content, and the spaling resistivity is increasing corresponding to the increase of wire content and to aspect ratio, and with decreasing wire diameter. 3. Firing shrinkage under load is getting greater as higher wire content, and the shrinkage of the test pieces which fiber is vertically oriented is getting greater than the test pieces which fiber is randomly oriented.

  • PDF

Tensile Strain of Steel Fiber Reinforced Concrete under Fatigue Load (피로하중을 받는 강섬유보강콘크리트의 인장변형에 관한 연구)

  • 장동일;채원규;박철우;민인기
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1992.10a
    • /
    • pp.82-87
    • /
    • 1992
  • In this thesis, the fatigue tests were performed on a series of SFRC (steel fiber reinforced concrete)to investigate the flexural tensile behavior of SFRC varying with the steel fiber contents and the steel fiber aspect ratios. Beam specimens of 10$\times$10$\times$60cm are used. the specimen series are classified according to the steel fiber contents varying 0.5. 1.0, 1.5%, and to the steel fiber aspect ratios varying 60, 80, 100. The three point loading system was used in the fatigue tests. The minimum value of repeated loading was fixed at 10.0kgf and maximum value was 75% to static ultimate strength for periodically using concrete strain gages located at the lower end of the mid-span, and the stress-strain curves were drawn for each specimens, respectively. From the tests result, it was found that the larger steel fiber content and the smaller the steel fiber aspect ratio is , the tensile strain of SFRC under fatigue load proportionally increases. By the regression analysis on these results, the empirical formulae to predict the tensile strain of SFRC were suggested. In comparison of the tensile elastic modulus under fatigue load, it was also found that the larger steel fiber content and the smaller steel fiber aspect ratio is , the smaller decreasing rate of the stiffness of SFRC under fatigue load decreased.

  • PDF

Effect of steel fiber volume fraction and aspect ratio type on the mechanical properties of SIFCON-based HPFRCC

  • Kim, Seugnwon;Jung, Haekook;Kim, Yongjae;Park, Cheolwoo
    • Structural Engineering and Mechanics
    • /
    • v.65 no.2
    • /
    • pp.163-171
    • /
    • 2018
  • Plain concrete is a brittle material with a very low tensile strength compared to compressive strength and critical tensile strain. This study analyzed the dynamic characteristics of high-performance fiber-reinforced cementitious composites based on slurry-infiltrated fiber concrete (SIFCON-based HPFRCC), which maximizes the steel-fiber volume fraction and uses high-strength mortar to increase resistance to loads, such as explosion and impact, with a very short acting time. For major experimental variables, three levels of fiber aspect ratio and five levels of fiber volume fraction between 6.0% and 8.0% were considered, and the flexural strength and toughness characteristics were analyzed according to these variables. Furthermore, three levels of the aspect ratio of used steel fibers were considered. The highest flexural strength of 65.0 MPa was shown at the fiber aspect ratio of 80 and the fiber volume fraction of 7.0%, and the flexural strength and toughness increased proportionally to the fiber volume fraction. The test results according to fiber aspect ratio and fiber volume fraction revealed that after the initial crack, the load of the SIFCON-based HPFRCC continuously increased because of the high fiber volume fraction. In addition, sufficient residual strength was achieved after the maximum strength; this achievement will bring about positive effects on the brittle fracture of structures when an unexpected load, such as explosion or impact, is applied.

A Study on the flexural Behavior of Ultra-Strength Steel Fiber Reinforced Concrete (초고강도 강섬유 보강 콘크리트의 휨특성에 관한 연구)

  • Ryu, Gum-Sung;Park, Jung-Jun;Kang, Su-Tea;Koh, Kyung-Taeg;Kim, Sung-Wook
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.333-336
    • /
    • 2005
  • This paper presents a comparative evaluation of eight different types of steel fibers used as reinforcing material in concrete beams. The fibers which used ultra-strength steel fiber reinforced concrete were fiber length of 30 to 60mm, aspect ratio of 43 to 86, W/B ratio 0.16 to 0.30, fiber types of both ends hooked and straight shape and fiber volume fraction of 1 to 5$\%$. As for the test results, it estimated the influence of fiber volume, length and aspect ratio on the mechanical properties of high toughness concrete, the mechanical properties improved according to increase fiber volume, to increase aspect ratio and to long fiber length. And the resonable fiber volume in high toughness concrete was analyzed 2$\%$ based on the results of mechanical properties.

  • PDF

An Experimental Study on Shear Strength of Steel Fiber Reinforced Concrete (강섬유보강 콘크리트의 전단강도에 관한 실험적 연구)

  • 박홍용;곽규영
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.737-742
    • /
    • 2002
  • This experimental study were carried out in order to investigate the shear strength of steel fiber reinforced Concrete(SFRC). 96 specimens have been tested for shear strength and 32 specimens for flexural. The test parameters were the volume fraction of steel fiber and aspect ratio. The test results show that shear strength are increased as fiber content, aspect ratio increases.

  • PDF