• Title/Summary/Keyword: Specimen

Search Result 10,863, Processing Time 0.04 seconds

Effect of Shot-peening on Fatigue Crack Growth (균열진전에 대한 쇼트피닝 효과)

  • SHIM DONG-SUK;LEE SEUNG-HO;LEE MYUNG-HO
    • Journal of Ocean Engineering and Technology
    • /
    • v.18 no.6 s.61
    • /
    • pp.91-95
    • /
    • 2004
  • In this study, to investigate the effects of shot peening on crack growth behavior, crack growth tests are conducted on spring steels and shot peened cracks. The probabilistic crack growth equation, which can represemt the sigmoidal crack growth behavior as recently reported by Kim and Shim, is used to evaluate the experimental results. The results show that fatigue cracks grows slower in the shot peened specimen than in the unpeened and, due to the compressive residual stress occurring on the specimen surface. In the case of the shot peened specimen, the initial stress intensity factor range and the fracture toughness is higher than the non-peened specimen because the compressive residual stress affects crack growth and fracture of the specimen.

Experimental Study on the Effect of Specimen Size on Electrical Resistivity Measurement (전기비저항 측정에서 실험체 크기의 영향에 대한 실험적 연구)

  • Lim, Young-Chul
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.6
    • /
    • pp.164-169
    • /
    • 2018
  • In this study, the effect of the size of the specimen on the apparent resistivity was investigated at the laboratory level for electrical resistivity. The specimens were measured for apparent resistivity by fabricating specimens with different sides and heights. Experimental results show that the apparent resistivity increases as the side and height of the specimen become smaller. Also, it was confirmed that the influence of the size of the specimen on the electrical resistivity measurement was not linear.

Transmission Electron Microscopy Specimen Preparation for Layer-area Graphene by a Direct Transfer Method

  • Cho, Youngji;Yang, Jun-Mo;Lam, Do Van;Lee, Seung-Mo;Kim, Jae-Hyun;Han, Kwan-Young;Chang, Jiho
    • Applied Microscopy
    • /
    • v.44 no.4
    • /
    • pp.133-137
    • /
    • 2014
  • We suggest a facile transmission electron microscopy (TEM) specimen preparation method for the direct (polymer-free) transfer of layer-area graphene from Cu substrates to a TEM grid. The standard (polymer-based) method and direct transfer method were by TEM, high-resolution TEM, and energy dispersive X-ray spectroscopy (EDS). The folds and crystalline particles were formed in a graphene specimen by the standard method, while the graphene specimen by the direct method with a new etchant solution exhibited clean and full coverage of the graphene surface, which reduced several wet chemical steps and accompanying mechanical stresses and avoided formation of the oxide metal.

The Dielectric Characteristics of Low Density Polyethylene Film due to Thermal Treatment Effect (열처리효과에 따른 저밀도 폴리에틸렌 박막의 유전특성)

  • 김왕곤;가출현;이용우;홍진웅
    • Journal of the Korean Society of Safety
    • /
    • v.11 no.1
    • /
    • pp.67-74
    • /
    • 1996
  • In order to investigate the effect and reliability coming up to properties of the matter due to the change of solid structure in dielectrics, the effect of dielectric characteristics for thermal treated LDPE film was made researches. Specimens of LDPE with thickness 100 [$\mu\textrm{m}$] were investigated into the change of solid structure by ageing. Thermal treated specimen were made, that were after applying heat at 100 [$^{\circ}C$] for 1 [hour] \circled1 air-cooled specimen slowly, \circled2 water-cooled specimen under the ,com temperature, \circled3 liquid nitrogen gas-cooled specimen rapidly. With specimen of thermal treated three types turn out and original, it was for dielectric characteristics to be experimented in the temperature range of 20~120 [$^{\circ}C$], frequency range of 30~1.5${\times}10^5/$[Hz], appling voltage from 300 to 1500[㎷]. Consequently, the degree of crystallinity was changed with 49~57 [%] according to the thermal treatment. In case of frequency, 100 [Hz], on the thermal dependance in dielectric characteristics, tan decreases due to cooling method.

  • PDF

Brittle fracture analysis of the offset-crack DCDC specimen

  • Ayatollahi, M.R.;Bagherifard, S.
    • Structural Engineering and Mechanics
    • /
    • v.29 no.3
    • /
    • pp.301-310
    • /
    • 2008
  • Applications of fracture mechanics in the strength analysis of ceramic materials have been lately studied by many researchers. Various test specimens have been proposed in order to investigate the fracture resistance of cracked bodies under mixed mode conditions. Double Cleavage Drilled Compression (DCDC) specimen, with a hole offset from the centerline is a configuration that is frequently used in subcritical crack growth studies of ceramics and glasses. This specimen exhibits a strong crack path stability that is due to the strongly negative T-stress term. In this paper the maximum tensile stress (MTS) criterion is employed for investigating theoretically the initiation of brittle fracture in the DCDC specimen under mixed mode conditions. It is shown that the T-stress has a significant influence on the predicted fracture load and the crack initiation angle. The theoretical results suggest that brittle fracture in the DCDC specimen is controlled by a combination of the singular stresses (characterized by KI and KII) and the non-singular stress term, T-stress.

The Roles of Reinforcing Fibers on the Performance of Automotive Brake Pads (자동차용 마찰재의 성능에 미치는 강화섬유의 역할)

  • Lim, Hyun-Woo;Yoon, Ho-Gyu;Jang, Ho
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2000.06a
    • /
    • pp.173-179
    • /
    • 2000
  • The friction and wear characteristics of brake friction materials reinforced with aramid fiber, carbon fiber, glass fiber, and potassium titanate whiskers were investigated using a pad-on-disk type friction tester. In particular, the morphology of rubbing surfaces was carefully investigated to correlate the friction performance and properties of transfer films. The aramid fiber reinforced specimen showed severe oscillation of friction coefficient at low speed and low applied pressure. The carbon fiber reinforced specimen showing better friction stability exhibited uniform and stable transfer film than any other specimens. The glass fiber reinforced specimen showed unstable friction changes at high speed and high-applied pressure and the non-uniform transfer film was observed in both friction material and rotor surface. The potassium titanate whiskers reinforced specimen showed stable coherent transfer film. The wear test exhibited the potassium titanate whiskers reinforced specimen was lowest in wear amount and glass fiber reinforced specimen showed the severe wear.

  • PDF

Development of Thermal Sensor Devices in the $BaTiO_3$ Systems ($BaTiO_3$계 박막형 열전센서소자 개발)

  • Song, Min-Jong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05d
    • /
    • pp.100-104
    • /
    • 2003
  • $BaTiO_3$ ceramic thin films were manufactured by rf/dc magnetron sputter technique. We have investigated crystal structure, surface morphology and PTCR(positive-temperature coefficient of resistance) characteristics of the specimen depending on second heat-treatment temperatures. Second heat treatments of the specimen were performed in the temperature range of 400 to $1350^{\circ}C$. X-ray diffraction patterns of $BaTiO_3$ thin films show that the specimen heat treated below $600^{\circ}C$ is an amorphous phase and the one heat treated above $1100^{\circ}C$ forms a poly-crystallization. In the specimen heat-treated at $1300^{\circ}C$, a lattice constant ratio (c/a) was 1.188. Scanning electron microscope(SEM) image of $BaTiO_3$ thin films of the specimen heat treated in between 900 and $1100^{\circ}C$ shows a grain growth. At $1100^{\circ}C$, the specimen stops grain-growing and becomes a poly-crystallization.

  • PDF

Effect of the boundary shape of weld specimen on the stress distribution (용접시편의 테두리 모양이 응력 분포에 미치는 영향)

  • Yang, Seung-Yong;Goo, Byeong-Choon
    • Proceedings of the KSME Conference
    • /
    • 2004.11a
    • /
    • pp.348-352
    • /
    • 2004
  • In finite element analysis of mechanical behavior of weld, typical process is first to obtain a finite element model containing residual stress by conducting welding analysis and then to examine the computational specimen for various external loading. The numerical specimen with residual stress has irregular boundary lines since one usually begins the welding analysis from a body having regular straight boundary lines and large thermal contraction takes place during cooling of weld metal. We notice that these numerical weld specimens are different from the real weld specimens as the real specimens are usually cut from a bigger weld part and consequently have straight boundaries neglecting elastic relaxation associated with the cutting. In this paper, an iterative finite element method is described to obtain a weld specimen which is bounded by straight lines. The stress distributions of two types of weld specimen, one with regular and the other with irregular boundaries, are compared to check the effect of the boundary shape. Results show that the stress distribution can be different when large plastic deformation is induced by the application of external loading. In case of elastic small deformation, the difference turns out almost negligible.

  • PDF

Effect of Grain Size on the Damping Capacity of Fe-26Mn-4Co-2Al Damping Alloy (Fe-26Mn-4Co-2Al 제진합금의 감쇠능에 미치는 결정립 크기의 영향)

  • Jeong, Kyu-Seong;Kim, Doe-Hoon;Kwon, Soon-Doo;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.28 no.3
    • /
    • pp.129-134
    • /
    • 2018
  • This study was carried out to investigate the effect of grain size on the damping capacity of the Fe-26Mn-4Co-2Al damping alloy. ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ were formed by cold working, and these martensites were formed with a specific direction and surface relief. With an increase in grain size, the volume fraction of ${\alpha}^{\prime}$ and ${\varepsilon}-martensite$ increased by decrement the austenite phase stability. This volume fraction more rapidly increased in cold-rolled specimen than in the specimen that was not cold-rolled. The damping capacity also increased more with the augmentation an increased grain size and more rapidly increased in cold-rolled specimen than in the specimen that was not cold rolled. The effect of grain size on the damping capacity was larger in the cold-rolled specimen than the specimen that was not cold-rolled. Damping capacity linearly increased with an increase in volume fraction of ${\varepsilon}-martensite$. Thus, the damping capacity was affected by the ${\varepsilon}-martensite$.

Effect of SiC Particles Size on the Densification of $Al_2O_3-SiC$ Composite During Pressureless Sintering ($Al_2O_3-SiC$ 복합재료의 상압소결시 치밀화에 미치는 SiC 원료분말의 크기영향)

  • 채기웅
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.11
    • /
    • pp.1261-1265
    • /
    • 1999
  • Effect of SiC particle size of the densification of Al2O3-SiC composite during pressureless sintering was investigated. Two types of SiC powders having average particle size of 0.15${\mu}{\textrm}{m}$ and 3${\mu}{\textrm}{m}$ were used. Densification rate of the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles was slower than that of the specimen containg 3${\mu}{\textrm}{m}$ SiC particles. Although the relative density of the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles was below 90% of theoretical density after sintering at 155$0^{\circ}C$ the complete closure of open pores occurred. Therefore full densification could be obtained by subsequent HIP. On the other hand in the specimen containing 3${\mu}{\textrm}{m}$ SiC particles the complete closed pore was observed at 95% of theoretical density. Such a fast pore closure in the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles is likely to occur as a result of dense reaction layer formation on the specimen surface which is attributed to the high reactivity of small size particles with sintering atmosphere.

  • PDF