• Title/Summary/Keyword: Sintering Temperature

Search Result 2,552, Processing Time 0.031 seconds

Effect of Sintering Temperature on Electrical Properties and Stability of Zn-Pr-Co-Cr-Tb-Based Varistors (Zn-Pr-Co-Cr-Tb계 바리스터의 전기적 특성 및 안정성에 소결온도가 미치는 영향)

  • Nahm, Choon-Woo
    • Korean Journal of Materials Research
    • /
    • v.17 no.6
    • /
    • pp.298-302
    • /
    • 2007
  • The electrical properties and its stability of Zn-Pr-Co-Cr-Tb-based varistors were investigated for different sintering temperatures. As the sintering temperatures increased, the varistor voltage decreased in the range of $705.2{\sim}299.1$ V/mm, the nonlinear coefficient decreased in the range of $42.4{\sim}31.7$, and the leakage current was in the range of $1.0{\sim}1.7\;{\mu}A$. The stability of electrical characteristics increased with the increase of sintering temperature. The varistors sintered at $1350^{\circ}C$ marked the high electrical stability, with $%\Delta$ $V_{1mA}=+0.1%,\;%\Delta{\alpha}=+3.2%$, and $%{\Delta}I_L=+117.6%$ for DC accelerated aging stress state of $0.95V_{1mA}/150^{\circ}C/24\;h$.

Microwave Dielectric Properties of Low-temperature Sintered $Mg_4Nb_2O_9$ Ceramics (저온소결 $Mg_4Nb_2O_9$ 세라믹스의 마이크로파 유전특성)

  • Lee, Ji-Hun;Bang, Jae-Cheol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.11a
    • /
    • pp.439-442
    • /
    • 2004
  • The effects of sintering additives on the low-temperature sintering and microwave dielectric properties of $Mg_4Nb_2O_9$ dielectric ceramics were studied. When $3{\sim}20wt%$ of $0.242Bi_2O_3-0.758V_2O_5$ was added, the sintering temperature decreased from $1100{\sim}1300^{\circ}C$ to $950^{\circ}C$ and high density was obtained. When $Mg_4Nb_2O_9$ was sintered at $950^{\circ}C$ with 10wt% of sintering additive, the microwave dielectric properties of $Q{\times}f_0\;=\;80.035GHz,\;\epsilon_r\;=\;13.3\;and\;\tau_f\;=\;-12.9\;ppm/^{\circ}C$ were obtained.

  • PDF

Effect of Sintering Conditions on the Electromagnetic Properties of Mn-Zn Ferrites (소결조건이 Mn-Zn Ferrites의 전자기적 물성에 미치는 효과)

  • 최윤호;신명승;한승기;한영호
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.6
    • /
    • pp.561-568
    • /
    • 1997
  • The effects of sintering temperature and oxygen partial pressure on the electromagnetic properties of Mn-Zn ferrites were investigated. The grain increased with increasing temperature. The power loss at 100 kHz was decreased, while the power loss at 500 kHz was increased as the grain size increased with sintering temperature. Sintering with low oxygen partial pressure at 115$0^{\circ}C$ resulted in high density and initial permeability, and decreased the power loss at 100 kHz and 500 kHz. The oxygen partial pressure lower than 10-2 atm. during heating, significantly suppressed the hysteresis loss. However, the oxygen activity did not affect the grain size of sintered cores.

  • PDF

Sintering Temperature Effect on Electrical and Dielectric Stability of ZPCCL-Based Varistors (소결온도가 ZPCCL계 바리스터의 전기적, 유전적 안정성에 미치는 영향)

  • Nahm, Choon-Woo
    • Korean Journal of Materials Research
    • /
    • v.16 no.8
    • /
    • pp.466-472
    • /
    • 2006
  • The electrical, dielectric properties, and its stability of ZPCCL-based varistors were investigated for different sintering temperatures in the range of $1230{\sim}1300^{\circ}C$. As the sintering temperatures increased, the varistor voltage decreased in the range of $777.9{\sim}108$ V/mm, the nonlinear coefficient decreased in the range of $77.9{\sim}7.1$, and the leakage current increased in the range of $0.3{\sim}50.6\;{\mu}A$. The stability of electrical and dielectric characteristics was obtained from sintering temperature of $1260^{\circ}C$. the varistors sintered at $1260^{\circ}C$ marked the high electrical and dielectric stability, with $%{\Delta}{V_{1mA}=+1.9%,\;%{\Delta}{\alpha}=-10.6%,\;%{\Delta}I_L=+20%\;and\;%{\Delta}tan\;{\delta}=+9.9%$ for DC accelerated aging stress state of $0.95V_{1mA}/150^{\circ}C$/24 h.

Effects of Sintering Condition and composition on the Magnetic Properties of Sintered Fe-Si-P (소결조건 및 조성이 Fe-Si-P 소결제의 자기특성에 미치는 영향)

  • 송재성;김기욱
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.40 no.7
    • /
    • pp.684-689
    • /
    • 1991
  • Magnetic properties of sintered Fe-Si-P alloys have been investigated as a function of sintering condition and composition. Sintering was carried in the temperature range from 1100ø C to 1400ø C in vacuum. As the sintering temperature increases, the magnetic properties of specimens were improved mainly due to the easy movement of domain wall because large pores and large grains were formed during the sintering process at high temperature. When sintered at 1400ø C, Fe-2w/o Si-0.5w/o P compact had the best mgnetic properties, but more phosphorus addition degraded magnetic properties. It appears that the degradation was caused by the formation of non-magnetic compounds such as Si P, Fe3P in the compacts with high phosphorus contents.

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT ceramics with the amount of $WO_3$ addition (저온소결 PMN-PNN-PZT세라믹스의 $WO_3$첨가에 따른 압전 및 유전특성)

  • Kim, Kook-Jin;Yoo, Joo-Hyun;Chung, Young-Ho
    • Proceedings of the KIEE Conference
    • /
    • 2006.10a
    • /
    • pp.61-62
    • /
    • 2006
  • In this study, in order to develop the low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics using ${Fe_2}{O_3}$ and $WO_3$ as sintering aids were manufactured with the amount of $WO_3$ addition, and the specimens were sintered at 900, 930, $960^{\circ}C$, respectively. Thereafter, their dielectric and piezoelectric properties were investigated. The sintering aids were proved to lower the sintering temperature of piezoelectric ceramics due to the effects of ${Fe_2}{O_3}$ and $WO_3$ liquid phase. At 0.3wt% $WO_3$ added specimen sintered at $930^{\circ}C$, kp, Qm, dielectric constant and $d_{33}$ showed the optimum values of 0.60, 1402, 1440 and 360[pC/N], respectively, for multilayer piezoelectric actuator application.

  • PDF

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMgN-PMnN-PZT Ceramics (저온소결 PMgN-PMnN-PZT 세라믹스의 압전 및 유전 특성)

  • Lee, Sang-Ho;Yoo, Ju-Hyun;Hong, Jae-Il;Chung, Kwang-Hyun;Jeong, Young-Ho
    • Proceedings of the KIEE Conference
    • /
    • 2006.07c
    • /
    • pp.1400-1401
    • /
    • 2006
  • In this study, in order to develop low temperature sintering piezoelectric ceramics for multilayer piezoelectric actuator, $PbSr(Mn_{1/3}Nb_{2/3})O_3-(Mg_{1/3}Nb_{2/3})O_3-(ZrTi)O_3$ ceramics were fabricated using $Na_{2}CO_{3}-Li_{2}CO_{3}$ as sintering aids and their piezoelectric and dielectric characteristics were investigated according to the sintering tempo rature. At the sintering temperature of $900^{\circ}C$, the density, electrom echanical coupling factor(kp), mechanical quality factor(Qm) and dielectric constant(${\varepsilon}r$) of specimen showed the optimum value of $7.730[g/cm^2]$, 0.552, 1134, 1492 and 330[pC/N], respectively.

  • PDF

Piezoelectric Properties and Sintering of PCW-PNN-PZT+0.5 wt%MnO2 Ceramics (PCW-PNN-PZT+0.5 wt%MnO2 세라믹스의 소결 및 압전특성)

  • Shin, Hyea-Kyoung;Chung, Bo-Ram;Ju, Jin-Soo;Bae, Seon-Gi
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.5
    • /
    • pp.453-457
    • /
    • 2008
  • In this thesis, piezoelectric properties and sintering properties of PCW-PNN-PZT+0.5 wt%$MnO_2$ ceramics adding $B_2O_3$ after creating the specimens with a general method. The lattice constant from the analysis of crystal structure showed that the crystal structure of ceramic features both rhombohdral and tetragonal structures and that the pychlore structure was decreased with the increase of the sintering temperature. The electromechanical coupling coefficient showed its maximum of 31 % in the sintered specimens at $1050^{\circ}C$, and its minimum of 20 % in the sintered specimens at $1150^{\circ}C$. The mechanical quality coefficient marked the maximum of 139 at the sintering temperature of $1150^{\circ}C$.

Influence of Sintering Atmosphere on Abnormal Grain Growth Behaviour in Potassium Sodium Niobate Ceramics Sintered at Low Temperature

  • Fisher, John G.;Choi, Si-Young;Kang, Suk-Joong L.
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.6
    • /
    • pp.641-647
    • /
    • 2011
  • The present study aims to identify the effect of sintering atmosphere [$O_2$, 75$N_2$-25 $H_2$ (mol%) and $H_2$] on microstructural evolution at the relatively low sintering temperature of 1040$^{\circ}C$. Samples sintered in $O_2$ showed a bimodal microstructure consisting of fine matrix grains and large abnormal grains. Sintering in 75 $N_2$ - 25 $H_2$ (mol %) and $H_2$ caused the extent of abnormal grain growth to increase. These changes in grain growth behaviour are explained by the effect of the change in step free energy with sintering atmosphere on the critical driving force necessary for rapid grain growth. The results show the possibility of fabricating $(K_{0.5}Na_{0.5})NbO_3$ at low temperature with various microstructures via proper control of sintering atmosphere.

Piezoelectric Characteristics of Low temperature sintering PMW-PMN-PZT Ceramics for Piezoelecric Transformer (저온소결 압전변압기용 PMW-PMN-PZT 의 압전특성)

  • Lee, Hyun-Seok;Chung, Kwang-Hyun;Yoo, Ju-Hyun;Park, Chang-Yub;Ryu, Sung-Lim;Jeong, Yeong-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.11a
    • /
    • pp.214-215
    • /
    • 2005
  • In this paper, in order to develop low temperature sintering piezoelectric ceramics for piezoelectric transformer, PMW-PMN-PZT ceramics using 0.25wt%$CaCO_3$ and 0.2wt%$Li_2CO_3$ as sintering aids were fabricated according to the variation of amount of PMW and Zr/Ti ratio. Specimens could be sintered at 900$^{\circ}C$ by adding sintering aids. As Zr/Ti ratio was increased, kp was increased and Qm was decreased by approaching MPB region, and kp showed the largest value of 0.58 at Zr/Ti:50/50. The variation of amount of PMN substitution affected the liquid phase sintering of the ceramics using sintering aids, and decreased piezoelectric properties.

  • PDF