콘크리트 바닥 시험체의 크기가 SL재의 균열에 미치는 영향 - SL재의 하자 발생에 영향을 미치는 콘크리트 표층부의 품질 평가방법(I) - (Evaluation on Crack in Self-leveling Material and Investigation about Influence of Specimen Size - Evaluation Method about Surface Layer Quality of Concrete Floor Groundwork Corresponding to Defect in Self-leveling Material (Part I) -)

  • 김두호;최수경
    • 한국건축시공학회지
    • /
    • 제7권2호통권24호
    • /
    • pp.99-106
    • /
    • 2007
  • The purpose of this study presents in Relations between cracks in self-leveling material and quality of floor groundwork surface are experimentally examined. As the first stage, the experiment to observe cracks in self-leveling material constructed on floor groundwork made from various kinds of concrete was carried. As a result, following basic findings were obtained. First, observation of cracks should be continued until an increase in width of cracks stop, without constructing any finishing material. Second, degree of cracks may be indicated quantitatively by the product of length and width. Finally, Cracks and separation is not be influenced by specimen size. Based on these findings, the method of predicting cracks by evaluating surface layer quality of floor groundwork will be established.

고강도 Self-Leveling재의 최적 결합재비 (The Optimum Binder Ratio for High-Strength Self-Leveling Material)

  • 김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2002년도 학술.기술논문발표회
    • /
    • pp.67-76
    • /
    • 2002
  • Self-leveling material(SLM) is one of the floor finishing materials which make flat surface like as water level by itself in a short time. So it is possible to increase construction speed and enhance economical efficiency. In this study, author intended to develop SLM for the industrial warehouse and factory loading heavy weight machinery and vehicles. The demanded properties for this type of SLM are above 20mm of flow value and above 300kgf/cm2 of 28-days compressive strength. To possess demended strength and fluidity, SLM have to be composed of many types of binders and chemical additives. So it is difficult to decide suitable mixing proportion of composition materials. In this study, author investigated the weight percentage effect of main composition materials for high-strength self-leveling material, by experimental design such as tables of orthogonal arrays and simplex design, and by statistical analysis such as analysis of variance and analysis of response surface. Variables of experiments were ordinary portland cement(OPC), alumina cement(AC), anhydrous gypsum(AG), lime stone(LS) and sand, and properties of tests were fluidity of fresh state and strength of hardened state. Results of this study are showed that suitable mix proportions of binders for the high strength self-leveling materials are two groups. One is 78~85.5% OPC, 7.5~9.5% AC, 9~12.5% AG and the other is 72.5~78% OPC, 9~12.5% AC, 13~l5% AG.

  • PDF

콘크리트 표층부 품질이 SL재의 하자에 미치는 영향 - SL재의 하자 발생에 영향을 미치는 콘크리트 표층부의 품질 평가방법(II) - (The Relationship Between the Quality of Surface Layer of Concrete Floor and the Defect of Self-Leveling Material - Evaluation Method about Surface Layer Quality of Concrete Floor Groundwork Corresponding to Defect in Self-leveling Material (Part II) -)

  • 김두호;최수경
    • 한국건축시공학회지
    • /
    • 제7권4호
    • /
    • pp.125-132
    • /
    • 2007
  • The use of Self-Leveling material is increasing recently. This paper assesses the quality of surface layer of concrete floor when Self-Leveling material is defective. The paper shows how to predict the defect of SL material before construction begins. The relationship between the quality of surface layer of concrete floor and the defect of SL material was determined and the quality of surface layer of concrete floor was then estimated. The relations between the quality of surface layer and the defect of SL material were determine considering surface strength, moisture, and consistency of surface layer. Absorbing amount was used as the indicator of consistency and the absorbing amount of test material was measured. Then the relations between the test material and surface strength were determined. Generally concrete floor with greater consistency has greater surface strength, however in this study, we hound that high impact concrete floor could have lower surface strength as the consistency gets bigger. The relations between the level of defect occurred in SL material and the quality of surface layer were examined and we clarified that the surface layer with lower consistency gets higher possibility to occur exfoliation in early stage, one or two weeks after constructing SL material. When the consistency is sufficient, the occurring situation of defect depends upon the moisture of surface layer. Little amount of moisture gets higher possibility not to occur the defect. As the amount increases, fissure generates and early exfoliation may occur. In addition, the level of fissure is highly related with the surface strength.

고강도 Self-Leveling재의 최적 결합재비 (The Optimum Binder Ratio for High-Strength Self-Leveling Material)

  • 김진만
    • 한국건축시공학회지
    • /
    • 제2권4호
    • /
    • pp.89-98
    • /
    • 2002
  • Self-leveling material(SLM) is one of the floor finishing materials which make flat surface like as water level by itself in a short time. So it is possible to increase construction speed and enhance economical efficiency In this study, author intended to develop SLM for the industrial warehouse and factory loading heavy weight machinery and vehicles. The demanded properties for this type of SLM are above 200mm of flow value and above 300kgf/$cm^2$ of 28-days compressive strength. To possess demended strength and fluidity, SLM have to be composed of many types of binders and chemical additives. So it is difficult to decide suitable mixing proportion of composition materials. In this study, author investigated the weight percentage effect of main composition materials for high-strength self-leveling material, by experimental design such as tables of orthogonal arrays and simplex design, and by statistical analysis such as analysis of variance and analysis of response surface. Variables of experiments were ordinary Portland cement(OPC), alumina cement(AC), anhydrous gypsum(AG), lime stone(LS) and sand, and properties of tests were fluidity of fresh state and strength of hardened state. Results of this study are showed that suitable mix proportions of binders for the high strength self-leveling materials are two groups. One is 78~85.5% OPC, 7.5~9.5% AC, 9~12.5% AG and the other is 72.5~78% OPC, 9~12.5% AC, 13~15% AG.

셀프레벨링 모르타르용 Primer 성상에 따른 특성평가에 관한 실험적 연구 (An Experimental Study on the Characteristics of Evaluation with Feature of Self Levelling Primer)

  • 강동균;김경덕;김정환
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.505-508
    • /
    • 2006
  • Self-leveling mortar is walkable bottom mortar which can maintain the horizontality of self fluid and have the the quick-setting quality, the low-human-effort practicable material of high-quality bottom in construction. In accordance with more adhesive strength with bottom side and absorption control, Primer is used for purpose to prevent pin-hole occurrence by self leveling mortar application prior to construction. This study is composed measurement of absorption, adhesive strength. Used material is NP-40 as nonionic emulsifying agent, uses SA-210L as negative ion emulsifying agent, uses APS, SBS as ridical initiator. A result of test, in accordance with image of Primer, as low temperature and application frequency, indicates low absorption rate and adhesive strength, as solid powder and dryness time is increse, absorption rate and adhesive strength lowly shows figure.

  • PDF

유한요소해석을 통한 되메움재 종류에 따른 지하매설관의 변형 특성 연구 (A Study on the Deformation Characteristics on Underground Pipe to Backfill Material Types Using Finite Element Method)

  • 변요셉;안병제;강병주;천병식
    • 한국지반환경공학회 논문집
    • /
    • 제10권5호
    • /
    • pp.11-18
    • /
    • 2009
  • 지하매설관 설치시 매설관 아래의 베딩면 상부 되메움재는 적절한 다짐이 필요하다. 그러나 원형매설관 설치시 기존 시공법의 경우는 관 하부의 다짐이 어렵고, 또한 다짐효율이 떨어져서 지하매설관의 안정성을 저감시키며, 이로 인하여 매설관의 파손이 발생한다. 이러한 지하매설관 되메움시 발생하는 문제점을 해결할 수 있는 방법 중의 하나가 유동성 채움재(CLSM)를 이용하는 것이다. 유동성 채움재는 저강도 콘크리트 개념을 지반공학에 적용하여 만들어진 것이다. 이의 대표적인 특성은 자기수평화(self-leveling), 자기다짐(self-compacting), 유동성(flowablility), 인위적인 강도조절, 시공단계를 줄여 시공비 절감이 가능하다는 것이다. 따라서, 본 논문에서는 유한요소해석을 수행하여 동일한 조건에서 현장발생토, 일반모래, 유동성채움재를 되메움재로 사용하였을 경우의 거동을 비교 분석하였다. 그 결과 되메움재로 유동성채움재를 사용하는 경우가 현장발생토사나 일반모래를 사용한 경우보다 지표침하 및 매설관의 변위를 감소시키는 것으로 나타났다.

  • PDF

CHARACTERISTICS OF SELF-LEVELING BEHAVIOR OF DEBRIS BEDS IN A SERIES OF EXPERIMENTS

  • Cheng, Songbai;Yamano, Hidemasa;Suzuki, TYohru;Tobita, Yoshiharu;Nakamura, Yuya;Zhang, Bin;Matsumoto, Tatsuya;Morita, Koji
    • Nuclear Engineering and Technology
    • /
    • 제45권3호
    • /
    • pp.323-334
    • /
    • 2013
  • During a hypothetical core-disruptive accident (CDA) in a sodium-cooled fast reactor (SFR), degraded core materials can form roughly conically-shaped debris beds over the core-support structure and/or in the lower inlet plenum of the reactor vessel from rapid quenching and fragmentation of the core material pool. However, coolant boiling may ultimately lead to leveling of the debris bed, which is crucial to the relocation of the molten core and heat-removal capability of the debris bed. To clarify the mechanisms underlying this self-leveling behavior, a large number of experiments were performed within a variety of conditions in recent years, under the constructive collaboration between the Japan Atomic Energy Agency (JAEA) and Kyushu University (Japan). The present contribution synthesizes and gives detailed comparative analyses of those experiments. Effects of various experimental parameters that may have potential influence on the leveling process, such as boiling mode, particle size, particle density, particle shape, bubbling rate, water depth and column geometry, were investigated, thus giving a large palette of favorable data for the better understanding of CDAs, and improved verifications of computer models developed in advanced fast reactor safety analysis codes.

고성능 다기능 특수 그라우트 신재료 개발 및 기초지반보강재로의 사례 연구 (Research & Development of High Performance & Multi-Functional New Grouting Materials for Ground Improvement & Reinforcement)

  • 박봉근;조국환;나경;윤태국;이용준
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2010년도 춘계 학술발표회
    • /
    • pp.338-350
    • /
    • 2010
  • As existing materials for ground reinforcement, chemical grout material using cementitous materials and waterglass was used. But many problems in terms of ground reinforcement effects were implicated. In this study, for development and applicability verification of new materials, viscosity, fluidity, permeability, Self-Leveling, keeping of drilled hole, antiwashout underwater, resistance of water (groundwater dilution and minimize material eluting) and the early strength and long-term strength characteristics of developed materials was confirmed, and material standards, and establishing construction standards for the various model tests were conducted. As a result, high viscosity, flowability, permeability and keeping of drilled hole characteristics are excellent, in addition to the early strength properties, dilution does nat occur to groundwater, including groundwater is available for dealing with environmental issues. Application of basic and reinforcement method by Filler function in addition to structure can also or development of a new concept can be expected. In addition, middle and large-diameter drilled shaft, micropile, ground anchors, soil-nailing, steel pipes multi-grouting reinforcement for cement injection process could be used enough to even be considered.

  • PDF

SL 무기질 바닥재의 경제성 분석에 관한 연구 (A study on the economic analysis of the SL(Self Leveling) Inorganic Floor covering)

  • 박호근;홍성욱;양재영;김상원;신찬호;최민권
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 춘계 학술논문 발표대회 2부
    • /
    • pp.105-109
    • /
    • 2011
  • This study is concerned with the development of the SL inorganic floor covering. First, volatile organic compounds, inorganic test profile on the SL through the flooring is environment-friendly inorganic noncombustible floor finishes the event of fire toxic gases (such as volatile organic compounds) emissions have been identified as not at all. Second, SL-breathable material, the concrete floor to prevent aging, long life, which are three levels of noise, shock-absorbing function was decreased. Third, SL economic analysis of mineral flooring terrazzo tile floors compared with the normal material. On a terrazzo tile cost 13,500 won ~ 24,500 won, but It have found that, in terms of labor SL 36,899 won ~ 38,899 won flooring mineral balance. Occurs in the total amount when compared with terrazzo tile floors and 25,399 won 3T, 5T and economical analysis concludes that the original 12,399 won.

  • PDF

유동성 및 조기강도 확보가 가능한 자기수평 모르타르 배합선정에 관한 연구 (A Study on the Formulation Selection of Self Leveling Floor Mortar with Fluidity and Early Strength Improvements)

  • 류화성;김득모;권성준;박원준;신상헌
    • 한국건축시공학회지
    • /
    • 제18권1호
    • /
    • pp.41-49
    • /
    • 2018
  • 본 연구는 고강도, 고유동의 성질을 갖고, 시공 후 수축현상이 저감되어 균열발생을 저감시킬 수 있는 바닥모르타르 배합선정에 관한 연구로서, 최적배합을 선정하기 위한 배합시험과 선정된 배합의 압축강도, 휨강도, 플로, 길이변화성능 및 염화물침투 저항성, 내화학성 등의 성능시험을 실시하였다. 시험결과, 유동성과 조기강도 발현이 가능하며, 수축저감을 통하여 균열발생 위험성을 개선시킬 수 있을 것이라 판단되는 배합을 선정하였으며, 선정된 배합은 자기수평모르타르 규격에 만족하는 성능을 확보하는 것으로 확인되었다. 본 연구의 결과를 통하여 우수한 재료성능과 경제성, 시공성을 갖는 고성능, 고유동의 바닥모르타르 시공기술을 확보할 예정이다.