  • Protection in HVDC(High Voltage Direct Current) have the very fast velocity of fault detection. Because Fault in HVDC has the fast propagation, large currents, high interruption cost. The focus to velocity caused possibility of errors like a detection error like a high impedance fault. In this paper, Proposed complex composition for get the reliability and velocity. That used SFCL(Super Conducting Fault Current Limiter), Protection Zone and DTS(Distributed Temperature Sensing). The SFCL was detect the fault by quench and DTS&Protection Zone were perceive the detect by variation too. To examine the proposed method, PSCAD/EMTDC simulated. The results of simulation, proposed methods could the detect of fault to whole HVDC line. And that improved the reliability of fault clearing.

소형 초전도 코일의 펜치특성에 관한 기초 연구 (A Study on the Quench Characteristics in the Small Superconducting Coils)

  • 김성래;오상수;오봉환;권영길;한일용;하동우;조전욱;류강식
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 A
    • /
    • pp.150-152
    • /
    • 1995
  • In order to study the basic I-V behavior and quench characteristics, we fabricated two kinds of small superconducting coils which were wound with different superconductors. In this study, it was made clear that the propagation. velocity of normal zone preferentially depends on the operation current rather than heat pulse energy and also increases exponentially with respect to operation current.

  • PDF

Effect of Epoxy Cracking on Initial Quench Behavior about High Field Superconducting Magnet

  • Lee, B.S.;Kim, D.L.;Choi, Y.S.;Yang, H.S.;Yoo, J.S.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제8권4호
    • /
    • pp.26-29
    • /
    • 2006
  • The study to be presented related on initial behavior of quench concerned with many considerations, such as epoxy impregnated coil, critical current density related on strain and temperature, winding effect and behavior of internal superconducting wire. Especially, the deformation behavior of coils under magnetic field and thermal contractions at cryogenic temperatures to be dealt with the analytical method related on Fracture Mechanics. From the results, we know that the strain by self weight contribute to epoxy cracking at the edge of deformed coils and the deformation behavior relate on epoxy cracking must be dealt with biaxial loading problem. Then, the epoxy crack on $r\theta-plane$ under biaxial loading have been propagated with inclined crack angle and joined superconducting wire. Also, we can explain transfer of epoxy crack propagation energy from epoxy resin to superconducting wire.

은비가 다른 Bi-2223 팬케이크 코일의 ?치 특성 (Quench Properties of Bi-2223 Pancake Coils with Different Ag/SC Ratio)

  • 장현만;오상수;하홍수;하동우;장국렬;류강식;김상현
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 1999년도 제1회 학술대회논문집(KIASC 1st conference 99)
    • /
    • pp.109-112
    • /
    • 1999
  • The normal zone propagation (NZP) velocity and V-I characteristics of two Bi-2223 pancake coils with different Ag/SC ratio were investigated by experiment. Non-uniformity of Ic and broad restive transition was oberserbed in two coils. The NZP velocity of azimuth direction is faster than radius direction, and the NZP velocity of coil with higher Ag/SC ratio is faster than another coil with lower Ag/SC ratio.

  • PDF

산화물 초전도선재의 상전도전파특성 (Normal-zone Propagation Properties in Oxide Superconductors)

  • 김석범;석산돈사;한경희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 하계학술대회 논문집 A
    • /
    • pp.41-43
    • /
    • 1996
  • This paper describes on concerning electromagnetical and thermal behaviors during normal transition in Bi-2223/Ag superconducting multifilamentary tapes by conduction cooling. Some experiments were carried with operating temperature, 10-40K, and transport current as parameters in zero magnetic field. Sample tapes are transited normally with heater to intiate a quench. The voltage and temperature properties which accord to normal transition are measured by voltage taps and thermocouples attached to sample tapes, we also calculated longitudinal and transverse directions normal-zone propagation velocities from the voltage traces.

  • PDF

무유도성 초전도전류제한기의 특성 해석 및 컴퓨터 시뮬레이션 (The Computer Simulation on the Characteristics of the Non-Inductive Superconducting Fault Current Limiter)

  • 주민석;이상진;오윤상;고태국
    • 대한전기학회논문지
    • /
    • 제43권7호
    • /
    • pp.1050-1060
    • /
    • 1994
  • This paper is a study on the computer simulation of the characteristics of the superconducting fault current limiter. Input variable parameters are apparent power, load resistance value, line resistance value and so on. Initial fault current 2 times larger than the trigger current is required to reduce the switching time of SFCL. The propagation velocity increases abruptly, the transport current is several times larger than the ciritical current. In this paper, the switching time is calculated to be 323$\mu$ sec, and the initial fault current is 19 times larger than the critical current. Because the trigger coils are bifilar winding, they have little impedance in superconducting state. After fault occurred, the limiting coil acts as a superconducting reactor and the trigger coils quench at a critical current. Without the SFCL in the circuit, fault current after the load impedence is shorted might be increased to 1100A. The fault current is, therefore, successfully limited by the superconducting limiting coil to 100A determined by the coil inductance.

  • PDF

Stability of superconductor by integration formula

  • Seol, S.Y.
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제21권3호
    • /
    • pp.1-5
    • /
    • 2019
  • The superconductor stability theories are consistently described by the integral formula. If the defined stability function is a simple decreasing function, it becomes a cryogenic stability condition. If the stability function has a maximum value and a minimum value, and the maximum value is less than 0, then it is a cold-end recovery condition. If the maximum value is more than 0, it can be shown that the unstable equilibrium temperature, that is, the MPZ (minimum propagation zone) temperature distribution can exist. The MPZ region is divided into two regions according to the current ratio. At the low current ratio, the maximum dimensionless temperature is greater than 1, and at the relatively high current ratio, the maximum dimensionless temperature is less than 1. In order to predict the minimum quench energy, the dimensionless energy was obtained for the MPZ temperature distribution. In particular, it was shown that the dimensionless energy can be obtained even when the MPZ maximum temperature is 1 or more.

A Study of Characteristic of Electrical-magnetic and Neutron Diffraction of Long-wire High-superconductor for Reducing Energy Losses

  • Jang, Mi-Hye
    • Transactions on Electrical and Electronic Materials
    • /
    • 제9권6호
    • /
    • pp.265-272
    • /
    • 2008
  • In this paper, AC losses of long wire Bi-2223 tapes with different twist pitch of superconducting core were fabricated, measured and analyzed. These samples produced by a powder-in-tube method are multi-filamentary tape with Ag matrix. Also, it's produced by non-twist. The critical current measurement was carried out under the environment in Liquid nitrogen and in zero field by 4-prob method. And the Magnetic measurement was carried out under the environment of applied time-varying transport current by transport method. From experiment, the susceptibility measurements were conducted while cooling in a magnetic field. Flux loss measurements were conducted as a function of ramping rate, frequency and field direction. The AC flux loss increases as the twist-pitch of the tapes decreased, in agreement with the Norris Equation. Neutron-diffraction measurements have been carried out investigate the crystal structure, magnetic structures, and magnetic phase transitions in Bi-2223([Bi, Pb]:Sr:Ca:Cu:O).

은 피복 Bi-2223 고온초전도 선재의 안정성 (Stability of Ag Sheathed Bi-2223 HTS Tape)

  • 장현만;오상수;하홍수;하동우;정종만;류강식;김상현
    • 한국초전도학회:학술대회논문집
    • /
    • 한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
    • /
    • pp.369-372
    • /
    • 1999
  • Using Ag sheathed multi filamentary Bi-2223 tape, stability against heat pulse has been investigated. The measured normal zone propagation(NZP) velocity of the tape was found to be faster due to increase of operating current and magnetic field, and agree well with calculated data from one dimensional heat balance equation. Minimum quench energy(MQE) was found to be larger than 17 J at 30 K zero magnetic filed at operating current of 96.5 with respect to I$_c$.

  • PDF

고온 초전도 한류퓨즈의 전압별 동작특성 (Operating characteristics of high Tc superconducting current limiting fuse at various voltages)

  • 최효상;현옥배;김혜림;황시돌;박권배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 연구회
    • /
    • pp.161-163
    • /
    • 2001
  • We present the basic properties of a superconducting current limiting fuse (SCLF) based on YBCO/Au films. The SCLFs consists of YBCO stripes covered with Au layers for current shunt. Under the source voltage of 100 $V_{rms}$, the longer the duration time of fault current was, the shorter its discharge time was. The duration time of fault current and its discharge time were reduced by increased voltages in the range of 200 - 300 $V_{rms}$. We thought that this was because the quench propagation was limited by local melting generated with higher voltage.