• Title/Summary/Keyword: Porous silica

Search Result 222, Processing Time 0.03 seconds

Preparation and Gas Permeation Properties of Silica Membranes on Porous Stainless Steel-Tube Supports (다공성 금속 지지체에 제조된 실리카 분리막의 기체 투과 특성)

  • Lee, Hye Ryeon;Seo, Bongkuk
    • Membrane Journal
    • /
    • v.24 no.3
    • /
    • pp.177-184
    • /
    • 2014
  • Silica membranes with high permeability were prepared using colloidal and polymeric silica sols on a porous stainless steel-tube support by a DRFF and SRFF method. Silica sols were derived with tetraethylorthosilicate (TEOS) by sol-gel method and analyzed with DLS, FE-SEM, and $N_2$ adsorption. The coating of the intermediate layer with colloidal silica sol on the stainless steel-tube support led to a denser surface morphology of the membrane along with a considerable reduction in the number of surface defect. As the polymeric silica sol enclosed the colloidal silica sol with spherical particles during the SRFF method, the separation-layer-coated silica membrane showed a denser surface than the intermediate layer. Moreover, the silica membranes showed high hydrogen gas permeability of $(6.63-9.21){\times}10^{-5}mol{\cdot}m^{-2}{\cdot}s^{-1}{\cdot}Pa^{-1}$ with low $H_2/N_2$ perm-selectivity (2.9-3.1) at room temperatures.

Preparation of $ZrO_2/Al_2O_3-Mullite$ Composites Using the Silica Sol Infiltration Method (실리카 졸 침투법을 이용한 $ZrO_2/Al_2O_3-Mullite$ 복합체의 제조)

  • 현상훈;최지영
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.9
    • /
    • pp.719-728
    • /
    • 1992
  • ZrO2/Al2O3-Mullite composites were prepared by infiltration of the silica sol to the porous ZrO2/Al2O3 bodies. The porous ZrO2/Al2O3 bodies for infiltration were fabricated using ZrO2 (20wt%)/Al2O3 composite powders synthesized by the emulsion-hot kerosene drying method. The preparation of silica sols was conducted by the hydrolysis-peptization of an alcoholic TEOS solution. When ZrO2/Al2O3-Mullite and ZrO2/Al2O3 composites were sintered at 1$650^{\circ}C$ for 4 hrs, both of them showed an excellent sinterability. As the amount of mullite added in the composites increased, the ratio of the tetragonal phase of zirconia to the monoclinic phase at the room temperature became higher. It was known that values of the fracture toughness of the ZrO2/Al2O3-Mullite composites were about 5.48 MPa.m1/2 much larger than that of the ZrO2/Al2O3 system.

  • PDF

A Study on the Properties of Fiber Reinforced Porous Concrete for Pavement using Industrial By-product (산업부산물을 이용한 섬유보강 포장용 포러스콘크리트의 특성에 관한 연구)

  • Park Seong Bum;Lee Yoon Sun;Lee Jun;Jang Young Il;Kim Bong Kyun;Kim Jeong Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.699-702
    • /
    • 2005
  • This study evaluates the properties of porous concrete for pavement according to content of silica fume and steel fiber. The results of the test indicate that in every condition, the void ratio and the coefficient of water permeability of porous concrete for pavement satisfy both the domestic standards and proposition values. Among the properties of strength, the compressive strength satisfies the standards in the specification of KNHC as for every factor of mixture but in the case of the flexural strength, more than $0.6vol.\%$ of steel fiber satisfied the JCI proposition values. The case when silica fume and steel fiber are used simultaneously presents the strongest durability and Noise Reduction Coefficient is 0.48 to prove that it possesses almost $50\%$ sound absorption.

  • PDF

Influence of solvent on the nano porous silica aerogels prepared by ambient drying process (상압건조 나노다공성 실리카 에어로젤에 대한 용매의 영향)

  • Ryu, Sung-Wuk;Kim, Sang-Sig;Oh, Young-Jei
    • Journal of Sensor Science and Technology
    • /
    • v.15 no.5
    • /
    • pp.371-377
    • /
    • 2006
  • Nano porous, transparent silica aerogels monoliths were prepared under ambient drying (1 atm, $270^{\circ}C$) condition by the combination of sol-gel process and surface modification with subsequent heat treatment. Three kinds of solvent, n-hexane, n-heptane and xylene, were selected in the point view of low surface tension and vapor pressure in order to restrain a formation of cracks during drying. Crack-free silica aerogels with over 93 % of porosity and below $0.14g/cm^3$ of density were obtained by solvent exchange and surface modification under atmosphere condition. Optimum solvent was confirmed n-heptane among these solvents through estimation of FT-IR, TGA, BET and SEM. Modified silica aerogel exhibited a higher porosity and pore size compare to unmodified aerogels. Hydrophobicity was also controled by C-H and H-OH bonding state in the gel structure and heat treatment over $400^{\circ}C$ effects to the hydrophobicity due to oxidation of C-H radicals.

Enzymatic Synthesis of Meth.yl Fructoside by Immobilized Invertase (고정화 전화당 효소에 의한 메틸 프룩토시드의 합성)

  • 허주형;김해성
    • KSBB Journal
    • /
    • v.8 no.4
    • /
    • pp.313-319
    • /
    • 1993
  • Methyl fructoside was synthesized from sucrose and methanol using an immobilized invertase. The enzyme was covalently bound by glutaraldehyde on porous silica coated with polyethyleneimine to give loading capacity of 120mg of invertase per one gram of dry porous silica and effective activity of 100U per one milligram of bound invertase. Polyethyleneimine coating imparted a hydrophillic character, good activity retention and high loading capacity to the surface of porous silica as well as hydrophillic microenviroment in the vicinity of bound invertase. The immobilized enzyme was formed into an alginate-enclosed silica bead to have enough activity for methyl fructoside synthesis from aqueous methanol-sucrose solution. Using the alginate-enclosed biocatalyst the yield of methyl fructoside was obtained as high as 55.9% from aqueous 30% (v/v) methanol and 0.291mo1/l sucrose with 2U/ml activity at $25^{\circ}C$, pH 4.8.

  • PDF

Strength and Reliability of Porous Ceramics Measured by Sphere Indentation on Bilayer Structure

  • Ha, Jang-Hoon;Kim, Jong-Ho;Kim, Do-Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.7
    • /
    • pp.503-507
    • /
    • 2004
  • The importance of porous ceramics has been increasingly recognized and adequate strength of porous ceramics is now required for structural applications. Porosities of porous ceramics act as flaws in inner volume and outer surface which result in severe strength degradation. The effect of pore structure, however, on strength and reliability of porous ceramics has not been clearly understood. We investigate the relationship between pore structure and mechanical properties using a sphere indentation on bilayer structure, porous ceramic top layer with soft polymer substrate. Porous alumina and silica were prepared to characterize the isolated pore structure and interconnected pore structure, respectively. The porous ceramic with 1mm thickness were bonded to soft polycarbonate substrate and then fracture strengths were estimated from critical loads for radial cracking of porous ceramics during sphere indentation from top surface. This simple and reproducible technique provides Weibull modulus of strength of porous ceramics with different pore structure. It shows that the porous ceramics with isolated pore structure have higher strength and higher Weibull modulus as well, than those with interconnected pore structure even with the same porosity.

Adsorption of Colloidal Silica Particles on a Glass Substrate

  • Sim, Soo-Man
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.11
    • /
    • pp.1011-1016
    • /
    • 2002
  • Colloidal particles of silica (100 nm in size) were electrostatically dispersed and adsorbed on a glass substrate coated with silica sol or alumina sol. Stability of the suspensions and microstructure of the adsorbed particle layers were discussed in terms of total potential energies between the particles and the substrate. Well-dispersed suspension resulted in a layer with densely packed and regularly arranged particles, whereas less stable suspension resulted in a porous layer with loosely packed and irregularly arranged particles. Despite repulsive interactions between the particles and the substrate coated with silica sol, the observed adsorption can be attributed to chemical bonds formed at the interface between the particle and silica sol. In contrast, the adsorption of the particles on the substrate coated with alumina sol formed a layer with strongly adhered and densely packed particles, due to large attractive interactions between the particles and alumina sol.

A Study on the ZnO Supported Silica Gel (ZnO가 담지된 실리카 겔 연구)

  • Kim, S.Y.;Kim, M.Y.;Ju, C.S.
    • Journal of Power System Engineering
    • /
    • v.15 no.4
    • /
    • pp.75-78
    • /
    • 2011
  • There are various types of materials used in electronic industry, such as electrode material, conductor, insulator, anode, cathode and semiconductor. Electrode material type is Cu, Ti, ZnO and so on. Especially if we use mixed ZnO in soil cement or silica gel, we can have advantages in ice road to prevent freezing. We have great impact if we use supported in inorganic substances like silica gel. In this paper we have studied that ZnO supported silica gel and its properties. Zinc acetate dissolved in distilled water were loaded on the silica gel by the reaction with ammonia at $80^{\circ}C$. And we investigated particle structures of ZnO by scanning electron microscopy(SEM) and X-ray diffraction(XRD).