In bone tissue engineering, polycaprolactone (PCL) is one of the most widely used biomaterials to manufacture scaffolds as a synthetic polymer with biodegradability and biocompatibility. The polymer deposition system (PDS) with four axis heads, which can dispense bio-polymers, has been used in scaffold fabrication for tissue engineering applications. A dual-head deposition technology of PDS is an effective technique to fabricate 3D scaffolds. The electrospinning technology has been widely used to fabricate porous and highly interconnected polymer fibers. Thus, PDS can fabricate nanofiber-combined hybrid scaffolds using fused deposition modeling (FDM) and electrospinning methods. This study aims to fabricate nanofiber-combined scaffolds with uniform nanofibers using PDS. The PCL nanofibers were fabricated and evaluated according to the fabrication process parameters. PCL nanofibers were successfully fabricated when the applied voltage, tip-to-collector distance, flow rate, and solution concentration were 5 kV, 1 cm, 0.1 ml/h, and 8 wt%, respectively. The cell proliferation was evaluated according to the electrospinning time. Scanning electron microscopy was used to acquire images of the cross-sectioned hybrid scaffolds. The cell proliferation test of the PCL and nanofiber-combined hybrid scaffolds was performed using a CCK-8 assay according to the electrospinning time. The result of in-vitro cell proliferation using osteosarcoma MG-63 cells shows that the hybrid scaffold has good potential for bone regeneration.
조직 공학에 있어 인공지지체는 손상된 조직 및 기관의 기능을 재생하기 위한 거푸집으로 제공되며 3 차원 구조물이다. 인공지지체의 재료 중에서 폴리카프로락톤(Polycaprolactone, PCL)과 삼인산칼슘(${\beta}$-tricalcium phosphate, ${\beta}$-TCP)은 생분해성과 생체적합성을 가지고 있다. 본 연구에서는 다축 인공지지체 제작 시스템을 이용하여 3 차원 PCL, blended PCL(60 wt %)/${\beta}$-TCP(40 wt %), 그리고 ${\beta}$-TCP 인공지지체를 제작하였다. 제작된 인공지지체는 주사전자현미경 분석을 통해 $600{\pm}20{\mu}m$의 공극 크기로 잘 제작되었다. 기계적 특성 평가를 통해 3 차원 PCL, blended PCL(60 wt %)/${\beta}$-TCP(40 wt %), 그리고 ${\beta}$-TCP 인공지지체의 효과는 분석되었다. 게다가 Saos-2 세포를 이용한 in vitro 연구를 수행하여 세포 증착 및 증식과 같은 세포 거동에 의한 3 차원 인공지지체의 효과를 확인하였다. 요컨대 3D blended PCL(60 wt %)/${\beta}$-TCP(40 wt %) 인공지지체가 압축 강도와 생체적합성 그리고 골전도성에 있어서 인체의 해면골에 더욱 적합하였다. 따라서 3D 인공지지체의 제작에 있어 PCL과 ${\beta}$-TCP를 혼합하는 것은 효과적인 골 재생을 위해 촉망되는 전략이 될 것이다.
조직공학의 중요한 요소로 작용하는 scaffold는 여러 가지 필수적인 조건들을 만족시켜야 한다. 대표적인 특징들로는 (1)생분해성 및 비독성, (2)넓은 표면적을 갖는 상호 연결된 내부 다공성 구조, (3)구조적 안정성, (4)세포부착 기질의 제공, (5)낮은 면역 반응성, (6)혈전 형성 억제, (7)친수성, (8)생체 기능성 등을 들 수 있다. 이러한 scaffold가 갖추어야 할 특성 중에서 세포 부착 기질 제공을 위하여 scaffold에 표면 개질을 통한 기능기를 도입하였다. 본 연구에서는 BCP scaffold의 구조적 안정성 부여를 위하여 PCL(polycaprolactone)을 infiltration 하였다. PCL은 소수성의 특징을 갖고 있어 세포와 상호작용 할 수 있는 생물학적 반응기가 없기 때문에 세포와의 친화성이 떨어진다. 세포의 친화성을 높여주기 위해 실리콘의 전구체인 TEOS(tetraethly orthosilicate)를 코팅하고, 그 위에 카복실기(carboxylic acid group)를 도입하였다. 또한 세포의 고정화를 높여주기 위해 fibronectin을 코팅하여 BCP/PCL scaffold의 세포 친화성을 높여주었다. 이와 같이 제조된 고기능성 BCP/PCL scaffold의 내부 구조와 특성을 Micro-CT로 확인하였고, 또한 실리콘 코팅 여부를 확인하기 위하여 SEM-EDS를 통해 관찰하였으며, FT-IR 관찰을 통해 카복실기 도입 여부를 확인 하였다. 또한 생체적합성 평가를 위해 MTT assay, 조골세포의 부착에 미치는 영향을 관찰하기 위해 SEM, 조골세포의 유전자 발현에 미치는 영향을 관찰하기 위해 RT-PCR을 통해 확인 하였다.
골 조직 공학에서 폴리카프로락톤(Polycaprolactone, PCL)은 생분해성 및 생체적합성의 합성고분자로서 인공지지체의 제작에 널리 이용되고 있는 생체재료 중 하나이다. 인공지지체의 제작에서 지지대폭은 생체 내/외 실험에서 공극 크기뿐만 아니라 공극률에도 영향을 미치기 때문에 지지대 폭을 일정하게 유지하는 것이 조직 재생에 중요하게 고려되는 부분이다. 본 연구에서는 온도, 공압, 이송 속도, 그리고 노즐 팁 높이를 이용하여 체계적이고 효율적인 인공지지체 제조 공정이 될 수 있도록 실험 계획법을 통해 최적 공정 조건을 탐색하였다. $150{\mu}m$ 지지대 폭을 가지는 PCL 인공지지체를 제작하는 것이 목표였으며, 한 가지의 공극 패턴이 아니라 다양한 공극 패턴에 따른 PCL 인공지지체를 제작하는 연구를 수행함으로써 모든 실험 그룹에서 지지대 폭이 일정함을 증명하였다.
In this study, we used a polymer deposition system, based on fused deposition modeling, to fabricate the 3D scaffold and then fabricated micro-pores on a 3D scaffold using a salt leaching method. Materials included polycaprolactone (PCL) and sodium chloride (NaCl). The 3D porous scaffolds were fabricated according to blending ratio such as PCL (70 wt%)/NaCl (30 wt%) and PCL (50 wt%)/NaCl (50 wt%). The 3D porous scaffolds were observed by scanning electron microscopy. The results showed that 3D porous scaffolds had a deposition width of $500{\mu}m$, contained a pore size of $500{\mu}m$ and below $100{\mu}m$. To evaluate the 3D porous scaffolds for bone tissue engineering, we carried out the cell proliferation experiment using a CCK-8 and a mechanical strength test using a universal testing machine. In summary, the 3D porous scaffold was found to be suitable for cancellous bone of human in accordance with the result of in-vitro cell proliferation and mechanical strength. Thus, a 3D porous scaffold could be a promising approach for effective bone regeneration.
본 연구는 조직공학용 지지체로 사용될 막을 개발하기 위한 초도 연구 수행으로, 염화나트륨(NaCl)을 기공형성체로 혼합한 폴리카프로락톤(PCL)용액을 유리 캐스팅판에 분주한 후 필름 어플리케이터를 이용하여 다공성 PCL필름을 성형하였다. 성형된 필름은 건조 후 증류수에 침지시켜 NaCl을 추출하여 최종 멤브레인형 다공성 지지체를 제조하였다. 3차원 다공망을 형성시키기 위하여 NaCl을 기공형성체로 이용하였으며 $4^{\circ}C$, 실온, $40^{\circ}C$의 세 가지 건조조건에 따른 다공망의 형성과 형태를 주사전자현미경(SEM)을 이용하여 관찰 하였으며 기초적인 안전성 확보를 위한 세포독성평가를 시행하였다. 세 가지의 건조조건별 결과에서는 실온 건조조건에서 거대기공과 미세기공이 혼재된 3차원 다공망이 우수하게 형성된 것이 관찰되었으며 세포독성 시험결과 ISO10993-5 규격의 세포독성 판단기준에 따라 grade 2(mildly cytotoxic)로 나타난바 생체용으로 적합하다고 볼 수 있다. 본 연구를 통하여 멤브레인형 다공성 지지체 제조에 건조조건이 3차원 다공망의 형성 및 거대기공과 미세기공이 함께 형성되는 것에도 영향을 미치는 것으로 나타났으며 이 결과는 다공성 멤브레인 지지체의 분해성 조절 및 약물 담지 효과를 개선하기 위한 연구에서 다공도의 조절에 대한 기초적인 공정이 될 수 있다.
The electrospinning process was established as a promising method to fabricate nano and micro-textured scaffolds for tissue engineering applications. A BCP-loaded PCL micro-textured scaffold thus can be a viable option. The biocompatibility as well as the mechanical properties of such scaffold materials should be optimized for this purpose. In this study, a composite scaffold of poly ($\varepsilon$-caprolactone) (PCL)-biphase calcium phosphate (BCP) was successfully fabricated by electrospinning. EDS and XRD data show successful loading of BCP nano particles in the PCL fibers. Morphological characterization of fibers shows that with a higher loaded BCP content the fiber surface was rougher and the diameter was approximately 1 to 7 ${\mu}m$. Tensile modulus and ultimate tensile stress reached their highest values in the PCL- 10 wt% BCP composite. When content of nano ceramic particles was low, they were dispersed in the fibers as reinforcements for the polymer matrix. However, at a high content of ceramic particles, the particles tend to agglomerate and lead to decreasing tensile modulus and ultimate stress of the PCL-BCP composite mats. Therefore, the use of nano BCP content for distribution in fiber polymer using BCP for reinforcement is limited. Tensile strain decreased with increasing content of BCP loading. From in vitro study using MG-63 osteoblast cells and L-929 fibroblast like cells, it was confirmed that electrospun PCL-BCP composite mats were biocompatible and that spreading behavior was good. As BCP content increased, the area of cell spreading on the surface of the mats also increased. Cells showed the best adherence on the surface of composite mats at 50 wt% BCP for both L-929 fibroblast-like cells and MG-63 osteoblast cell. PCL- BCP composites are a promising material for application in bone scaffolds.
Nam, Jeoung Hyun;Lee, So Yun;Khan, Galina;Park, Eun Soo
Archives of Plastic Surgery
/
제47권4호
/
pp.310-316
/
2020
Background To produce patient-specific nasal implants, it is necessary to harvest and grow autologous cartilage. It is crucial to the proliferation and growth of these cells for scaffolds similar to the extracellular matrix to be prepared. The pore size of the scaffold is critical to cell growth and interaction. Thus, the goal of this study was to determine the optimal pore size for the growth of chondrocytes and fibroblasts. Methods Porous disc-shaped scaffolds with 100-, 200-, 300-, and 400-㎛ pores were produced using polycaprolactone (PCL). Chondrocytes and fibroblasts were cultured after seeding the scaffolds with these cells, and morphologic evaluation was performed on days 2, 14, 28, and 56 after cell seeding. On each of those days, the number of viable cells was evaluated quantitatively using an MTT assay. Results The number of cells had moderately increased by day 28. This increase was noteworthy for the 300- and 400-㎛ pore sizes for fibroblasts; otherwise, no remarkable difference was observed at any size except the 100-㎛ pore size for chondrocytes. By day 56, the number of cells was observed to increase with pore size, and the number of chondrocytes had markedly increased at the 400-㎛ pore size. The findings of the morphologic evaluation were consistent with those of the quantitative evaluation. Conclusions Experiments using disc-type PCL scaffolds showed (via both morphologic and quantitative analysis) that chondrocytes and fibroblasts proliferated most extensively at the 400-㎛ pore size in 56 days of culture.
줄기세포를 기반으로 한 세포치료제는 생체 이식시 생착률이 낮아서 치료효과를 기대하기 어렵다. 이를 극복하기 위하여 줄기세포를 탑재할 수 있는 다양한 세포담체들이 개발되어 활용되고 있다. 이렇게 개발된 세포담체를 3-dimentional (3D) 프린팅하여 스캐폴드를 만들 경우, 환자의 손상부위 맞춤형 이식재를 제작할 수 있을 뿐만 아니라, 줄기세포를 탑재하여 손상부위를 기계적으로 보완하는 동시에 세포치료제로서의 효과도 얻을 수 있다. Polycaprolactone (PCL)은 저렴할 뿐 아니라 현재 가장 널리 쓰이고 있는 3D 프린팅 소재이기 때문에, PCL을 프린팅하여 세포담체로 활용할 경우 빠르고 경제적인 기술발전을 도모할 수 있다. 하지만 PCL 소재는 세포담체로서의 성능이 우수하지 못하여, 극히 일부의 세포만이 PCL 표면에서 생존한다. 본 연구에서는 이를 극복하기 위해서 PCL 소재에 세포의 탑재능력을 극대화되는 조건을 찾고자 하였다. PCL의 표면에 플라즈마를 처리하는 조건, PCL 표면을 콜라겐 코팅처리, PCL의 3D 프린팅 형상, 세포배양방법 변경 등 다양한 조건을 바탕으로 하여 PCL 소재에 인간 중간엽줄기세포의 세포탑재능력을 확인하였다. 세포탑재능력을 향상시킨다고 알려진 콜라겐 코팅과 플라즈마 처리를 적용하여, 플라즈마 처리 후 3% 콜라겐 코팅을 하였을 때 세포탑재능력이 가장 우수함을 확인하였고, 세포탑재능력에 영향을 줄 수 있는 세포배양방법과 스캐폴드의 구조변화를 적용하여, spheroid 세포배양시 기존의 단일세포배양법보다 탑재능력이 우수함을 확인하였으며, 스캐폴드의 구조는 세포탑재능력에 영향을 주지 못함을 확인하였다. 이를 바탕으로 PCL 소재를 세포 담체로 활용한 다양한 연구를 시도하고자 한다.
The aim of this study was to develop a multi-nozzle based bioprinting system for fabrication of three-dimensional (3D) biological structure. In this study, a thermoplastic biomaterial that has relatively high mechanical stability, polycaprolactone (PCL) was used to make the 3D structure. A multi-nozzle bioprinting system was designed to dispense thermoplastic biomaterial and hydrogel simultaneously. The system that consists of 3-axes of x-y-z motion control stage and a compartment for injection syringe control mounted on the stage has been developed. Also, it has 1-axis actuator for position change of nozzle. The controllability of the printed line width with PCL was tested as a representative performance index.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.