Effect of the Electrode Type on the Dielectric and Piezoelectric Properties of Piezoelectric PMN-PZT Single Crystals (압전 PMN-PZT 단결정의 유전 및 압전 특성에 미치는 전극 종류의 영향)

  • Lee, Jong-Yeb;Oh, Hyun-Taek;Choi, Kyoon;Lee, Ho-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.1
    • /
    • pp.77-82
    • /
    • 2015
  • The effect of the electrode type on the dielectric and piezoelectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbZrO_3-PbTiO_3$ (PMN-PZT) single crystals was investigated in an effort to improve their properties for various piezoelectric applications. First, three different types of PMN-PZT single crystals [PMN-PZT-A (piezoelectrically soft type; dielectric constant ~ 10,000), PMN-PZT-B (piezoelectrically soft type; phase-transition temperature between the rhombohedral and tetragonal phases ($T_{RT}$) ~ $145^{\circ}C$), PMN-PZT-C (piezoelectrically hard type; high mechanical quality factor ($Q_m$) ~ 1,000)] were fabricated using the solid-state single crystal growth (SSCG) method. Then, four different types of electrodes [sputtered Au, sputtered Cr/Au, sputtered Ti/Au, and fired Ag] were formed on the single crystals, and their dielectric and piezoelectric properties were measured. The single crystals with a sputtered Ti/Au electrode showed the highest dielectric and piezoelectric constants but the lowest coercive electric field ($E_C$). The single crystals with a fired Ag electrode showed the lowest dielectric and piezoelectric constants but the highest coercive electric field ($E_C$). This dependence on the type of electrode was most significant in the piezoelectrically hard PMN-PZT-C single crystals. However, the effects of the electrode type on the phase transition temperatures ($T_C$, $T_{RT}$) and dielectric loss were negligible. These results clearly demonstrate that it is important to select an appropriate electrode so as to maximize the dielectric and piezoelectric properties of single crystals in each type of piezoelectric application.

Aging Effect of Bio-inspired Artificial Basilar Membrane with Piezoelectric PVDF Thin Film

  • Kim, Wan Doo;Park, Su A;Kim, Sang Won;Kwak, Jun-Hyuk;Jung, Young Do;Hur, Shin
    • Elastomers and Composites
    • /
    • v.50 no.4
    • /
    • pp.292-296
    • /
    • 2015
  • Biomimetic artificial basilar membrane being a core part of artificial cochlear requires performance evaluation through aging test. To evaluate the aging properties of PVDF piezoelectric membrane used for artificial basilar membrane, its mechanical properties such as tensile strength and elastic modulus and piezoelectric property such as piezoelectric constant were measured. The aging test conditions and acceleration constants were calculated based on Arrhenius model. The changes in tensile strengths and elastic moduli measured were less than 10~20% after aging test equivalent for 10 years. The piezoelectric constants were decreased drastically to 80% of its initial value in the early stage of the aging test and expected to decrease slowly down to 65% over 10 years. The experimental results show the reliability of totally implantable novel artificial cochlear and will contribute its commercialization.

Piezoelectric and Dielectric Properties of (Na,Li)$NbO_3$ Ceramics According to the $BaTiO_3$ substitution ($BaTiO_3$ 치환에 따른 (Na,Li)$NbO_3$ 세라믹스의 압전 및 유전특성)

  • Lee, Sang-Ho;Lee, Kab-Soo;Ryu, Ju-Hyun;Ryu, Sung-Lim;Song, Hyun-Seon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.272-273
    • /
    • 2007
  • In this study, in order to develop the composition ceramics of lead-free ultrasonic motor, (Na,Li)$NbO_3-BaTiO_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $BaTiO_3$, substitution. $BaTiO_3$ substitution enhanced density, dielectric constants$({\varepsilon}_r)$ and electromechanical coupling factor$(k_p)$. However, mechanical quality factor was deteriorated. At the $BaTiO_3$ substitution of 4mol%, density, electromechanical coupling factor$(k_p)$, dielectric constants$({\varepsilon}_r)$ and piezoelectric constant$(d_{33})$ of specimen showed the optimum value of $4.493g/cm^3$, 0.236, 175, 70pC/N, respectively.

  • PDF

Fabrication and Characterization of a Flexible PVDF Fiber-based Polymer Composite for High-performance Energy Harvesting Devices

  • Nguyen, Duc-Nam;Moon, Wonkyu
    • Journal of Sensor Science and Technology
    • /
    • v.28 no.4
    • /
    • pp.205-215
    • /
    • 2019
  • A flexible polyvinylidene fluoride (PVDF)/polydimethylsiloxane (PDMS) composite prototype with high piezoelectricity and force sensitivity was constructed, and its huge potential for applications such as biomechanical energy harvesting, self-powered health monitoring system, and pressure sensors was proved. The crystallization, piezoelectric, and electrical properties of the composites were characterized using an X-ray diffraction (XRD) experiment and customized experimental setups. The composite can sustain up to 100% strain, which is a huge improvement over monolithic PVDF fibers and other PVDF-based composites in the literature. The Young's modulus is 1.64 MPa, which is closely matched with the flexibility of the human skin, and shows the possibility for integrating PVDF/PDMS composites into wearable devices and implantable medical devices. The $300{\mu}m$ thick composite has a 14% volume fraction of PVDF fibers and produces high piezoelectricity with piezoelectric charge constants $d_{31}=19pC/N$ and $d_{33}=34pC/N$, and piezoelectric voltage constants $g_{31}=33.9mV/N$ and $g_{33}=61.2mV/N$. Under a 10 Hz actuation, the output voltage was measured at 190 mVpp, which is the largest output signal generated from a PVDF fiber-based prototype.

Effects of Interface Porosity on Dielectric and Piezoelectric Properties of BaTiO3-Polymer Composites of O-3 Type Connectivity (O-3형 BaTiO3-폴리머 복합체의 계면기공율 변화에 따른 유전 및 압전특성)

  • 이형규;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.5
    • /
    • pp.617-624
    • /
    • 1989
  • Piezoelectric composites of O-3 connectivity were prepared by thermosetting barium titanate-phenolic resin composite under various cruing pressure. Among three kinds of pore in O-3 type ceramic-polymer composite, such as matrix pores, particle pores, and ceramic-polymer interface pores, the effect of interface porosity on the dielectric and piezoelectric constant was investigated. In pure barium titanate ceramics, the porosity factor of dielectric and piezoelectric constants were 5.7 and 5.0, respectively. However, in BaTiO3-polymer composite, the interface porosity factor of the piezoelectric constant was greater than that of the dielectric constant, interface porosity factor b in d33 was 9.8 and in r 4.6. On the other, piezoelectric voltage constant g33 was independent of the porosity of barium titanate ceramics. But in composite system, the piezoelectric voltage constant g33 was decreased with interface porosity.

  • PDF

Selection of Piezoelectric Materials for Ultrasonic Transudcers (초음파 센서를 위한 압전 세라믹 선택)

  • 노용래
    • Proceedings of the Acoustical Society of Korea Conference
    • /
    • 1992.06a
    • /
    • pp.107-110
    • /
    • 1992
  • We investigate the influence of individual properties of piezoceramics such as elastic, dielectric, piezoelectric constants, and the coupling factor on the performance of the transducer operating in thickness mode oscillation. The investigation employs equivalent circuit analysis techniques. Appropriate transfer functions are obtained and discussed which suggest optimum selection guides of piezoelectric ceramics for each purpose, i.e. a transmitter, a receiver, and a pulse-echo transducer. The guides can help ceramic scientists find the direction to proceed in new material development.

  • PDF

An In-silico Simulation Study on Size-dependent Electroelastic Properties of Hexagonal Boron Nitride Nanotubes (인실리코 해석을 통한 단일벽 질화붕소 나노튜브의 크기 변화에 따른 압전탄성 거동 예측연구)

  • Jaewon Lee;Seunghwa Yang
    • Composites Research
    • /
    • v.37 no.2
    • /
    • pp.132-138
    • /
    • 2024
  • In this study, a molecular dynamics simulation study was performed to investigate the size-dependent electroelastic properties of single-walled boron nitride nanotubes(BNNT). To describe the elasticity and polarization of BNNT under mechanical loading, the Tersoff potential model and rigid ion approximation were adopted. For the prediction of piezoelectric constants and Young's modulus of BNNTs, piezoelectric constitutive equations based on the Maxwell's equation were used to calculate the strain-electric displacement and strain-stress relationships. It was found that the piezoelectric constants of BNNTs gradually decreases as the radius of the tubes increases showing a nonnegligible size effect. On the other hand, the elastic constants of the BNNTs showed opposites trends according to the equivalent geometrical assumption of the tubular structures. To establish the structure-property relationships, localized configurational change of the primarily bonded B-N bonded topology was investigated in detail to elucidate the BNNT curvature dependent elasticity.

A Study on the Piezoelectric Sounder Using the PMN-PT-PZ with Sr Sustitutions (Sr이 치환된 PMN-PT-PZ 계 세라믹스를 이용한 압전 발음체에 관한 연구)

  • You, H.S.;Paek, D.S.;Kang, J.K.;Park, C.Y.
    • Proceedings of the KIEE Conference
    • /
    • 1991.11a
    • /
    • pp.293-295
    • /
    • 1991
  • In this study, we investigated the possibilty that $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3-PbZrO_3$ ceramics with strontium substitutions could be used for piezoelectric sounders. Piezoelectric buzzer is one of them. By partially substituting Sr for Ph, dielectric constants had values greater than 2000, the value proper piezoelectric buzzer, piezoelectric constant($d_{31}$) had a maximum value, 298 $[10^{-12}C/N]$, at the Sr 5 mol % substitution. Sound level of piezoelectric buzzer had the highest value of 91 dB at the Sr 5 mol % substitution.

  • PDF

The Characteristics of Piezoelectric Strian Constants on PNN-PZ-PT Ceramics (PNN-PZ-PT계 세라믹스의 압전변위특성)

  • 정수태;남효덕;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.6
    • /
    • pp.802-810
    • /
    • 1989
  • The temperature dependence of piezoelectric strain constant and the electric field induced strain are investigated as a function of PT in 0.5[xPT-(1-x)PZ]-0.5PNN ceramics. The piezoelectric strain constant d31 has the highest value(360$\times$10-12m/V) at PT=0.68. The temperature dependence of d31 is improved as Curie temperature of sample is increased, and the electric field dependence of induced strain is decreased with the coercive field increased. This ceramic system shows both piezoelectric effect and electrostrictive effect under the applied electric field. The piezoelectric of tetragonal phase is higher than that of rhombohedral phase, and the magnitude of electrostrictive constant is appeared in the order of morphotropic, rhombohedral and tetragonal phase. The piezoelectric strain constant with applied field must be considered theelectrostrictive effect due to 90$^{\circ}$domain wall displacements, and the displacement of bimorph type actuator agrees with the calulated value well.

  • PDF

Characterization of the Material Properties of 0.68Pb ($Mg_{1}$3/$Nb_{2}$3/)$O_3$-0.32PbT$iO_3$ Single Crystals Grown by the Solid-State-Crystal-Growth Method (고상단결정법으로 성장시킨 0.68Pb ($Mg_{1}$3/$Nb_{2}$3/)$O_3$-0.32PbT$iO_3$ 압전단결정의 물성평가)

  • 이상한;노용래
    • The Journal of the Acoustical Society of Korea
    • /
    • v.23 no.2
    • /
    • pp.103-108
    • /
    • 2004
  • In this paper, all the materials constants of the PMN-32%PT single crystals grown by the solid state crystal growth method were measured by the resonance method. PMN-PT crystals of tetragonal symmetry have six elastic constants, three piezoelectric constants and two dielectric constants for their independent material constants. These materials constants were extracted from six sets of crystal samples of each different geometry to have different vibration modes respectively. Measured results showed that the crystal has larger electromechanical coupling factor k/sub 33/ (∼86%) and piezoelectric constant d/sub 33/ (∼1200pC/N) than conventional piezoceramics. Validity of the measurement was confirmed through comparison of the results with the impedance spectrum from finite element analysis of the samples and the results measured with a commercial do meter.