• 제목/요약/키워드: Perovskite-type Oxide

검색결과 49건 처리시간 0.035초

고체산화물 연료전지 연결재용 세라믹 소재 (Ceramic Materials for Interconnects in Solid Oxide Fuel Cells - A Review)

  • 박범경;송락현;이승복;임탁형;박석주;박종욱;이종원
    • 한국세라믹학회지
    • /
    • 제51권4호
    • /
    • pp.231-242
    • /
    • 2014
  • An interconnect in solid oxide fuel cells (SOFCs) electrically connects unit cells and separates fuel from oxidant in the adjoining cells. The interconnects can be divided broadly into two categories - ceramic and metallic interconnects. A thin and gastight ceramic layer is deposited onto a porous support, and metallic interconnects are coated with conductive ceramics to improve their surface stability. This paper provides a short review on ceramic materials for SOFC interconnects. After a brief discussion of the key requirements for interconnects, the article describes basic aspects of chromites and titanates with a perovskite structure for ceramic interconnects, followed by the introduction of dual-layer interconnects. Then, the paper presents protective coatings based on spinel-or perovskite-type oxides on metallic interconnects, which are capable of mitigating oxide scale growth and inhibiting Cr evaporation.

Stoichiometry, Thermal Stability and Reducibility of Perovskite-Type Mixed Oxide LaBO$_3$ (B = Fe, Co, Ni)

  • Park, Il-Hyun;Lee, Hyung-Pyo
    • Bulletin of the Korean Chemical Society
    • /
    • 제9권5호
    • /
    • pp.283-288
    • /
    • 1988
  • The titled properties on reduction of the perovskite $LaBO_3$ (B = Fe, Co, Ni) have been investigated by means of temperature-programmed reduction, isothermal reduction and X-ray diffraction methods. Nominal composition of $LaFeO_{3.18},\;LaCoO_{3.00}\;and\;LaNiO_{2.92}$ are determined. Reduction reaction of these mixed oxides differed according to B-site transition metal and thermal stability on reduction decreased as following order: $LaFeO_{3.18}$ > $LaCoO_{3.00}$ > $LaNiO_{2.92}$. From the results of isothermal reaction, kinetics on reduction of the perovskite has been discussed in detail.

메탄-산소 혼합가스 조건에서의 페롭스카이트계 산화물의 촉매특성 평가 (Catalytic Characteristics of Perovskite-type Oxides under Mixed Methane and Oxygen Gases)

  • 안기용;김형철;정용재;손지원;이해원;이종호
    • 한국세라믹학회지
    • /
    • 제45권4호
    • /
    • pp.232-237
    • /
    • 2008
  • As the single chamber SOFC(SC-SOFC) showed higher prospect on reducing the operation temperature as well as offering higher design flexibility of SOFCs, lots of concerns have been given to investigate the catalytic activity of perovskite-type oxide in mixed fuel and oxidant conditions. Hence we thoroughly investigated the catalytic property of various perovskite-type oxides such as $La_{0.8}Sr_{0.2}MnO_3(LSM),\;La_{0.6}Sr_{0.4}CoO_3(LSC),\;La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_3(LSCF),\;Sm_{0.5}Sr_{0.5}CoO_3(SSC),\;and\;Ba_{0.5}Sr_{0.5}Co_{0.8}Fe_{0.2}(BSCF)$ under the partial oxidation condition of methane which used to be given for SC-SOFC operation. In this study, powder form of each perovskite oxides whose surface areas were controlled to be equal, were investigated as functions of methane to oxygen ratios and reactor temperature. XRD, BET and SEM were employed to characterize the crystalline phase, surface area and microstructure of prepared powders before and after the catalytic oxidation. According to the gas phase analysis with flow-through type reactor and gas chromatography system, LSC, SSC, and LSCF showed higher catalytic activity at fairly lower temperature around $400^{\circ}C{\sim}450^{\circ}C$ whereas LSM and BSCF could be activated at much higher temperature above $600^{\circ}C$.

Perovskite-Like Strontium Titanium Zirconium Oxide Solid Solutions Prepared at Atmospheric Pressure

  • Choy, Jin-Ho;Kim, Ha-Suck;Kwon, Young-Uk;Kim Chong Hee
    • Bulletin of the Korean Chemical Society
    • /
    • 제6권6호
    • /
    • pp.344-347
    • /
    • 1985
  • Perovskite type oxides of $SrTiO_3,SrZrO_3,and\;SrTi_{1-x}Zr_xO_3$ have been systematically synthesized at $1250^{\circ}C$and $1550^{\circ}C$ with specimens containing additions of up to x=0.9 of zirconium by solid state reactions and characterized by X-ray diffraction. X-ray diffraction studies showed that the compound $SrTi_{1-x}Zr_xO_3$ has cubic structure. The lattice paramters of $SrTi_{1-x}Zr_xO_3$ solid solutions obey the Vegard's law and fairly large increase in volume can acompany the formation of this solution with increasing Zr content(X). Assuming the lattice constants of perovskite type compounds $A(B_{1-x}B'_x)O_3$where $B_{1-x}B'_x$ is $Ti_{1-x}Zr_x$, to be a linear function of the ionic radii of B and B' ions, the disordered ion pair of $Ti^{4+}$and $Zr^{4+}$ was verified from the lattice constants of a series compounds varying x=0,0.05, 0.25, 0.5, 0.75, 0.9, and 1.0 with known isovalent pairs.

페로프스카이트 $La_{0.98}Sr_{0.02}MnO_3$의 고온전기특성 (High Temperature Electrical Conductivity of Perovskite La0.98Sr0.02MnO3)

  • 김명철;박순자
    • 한국세라믹학회지
    • /
    • 제29권11호
    • /
    • pp.900-904
    • /
    • 1992
  • High temperature electrical conductivity was measured for perovskite La0.98Sr0.02MnO3 at 200~130$0^{\circ}C$ as a function of Po2 and 1/T. Perovskite La1-xSrxMnO3 system is the typical oxygen electrode in solid oxide fuel cell (SOFC). Acetate precursors were used for the preparation of mixed water solution and the calcined powders were reacted with Na2CO3 flux in order to obtain highly reactive powders of perovskite La0.98Sr0.02MnO3. The relative density was greatly increased above 90% because of the homogeneous sintering. From the conductivity ($\sigma$)-temperature and conductivity-Po2 at constant temperature, the defect structure of La0.98Sr0.02MnO3 was discussed. From the slope of 1n($\sigma$) vs 1/T, the activation energy of 0.069 and 0.108eV were evaluated for above 40$0^{\circ}C$, respectively. From the relationship between $\sigma$ and Po2, it was found that the decomposition of La0.98Sr0.02MnO3 was occurred at 10-15.5 atm(97$0^{\circ}C$) and 10-11 atm(125$0^{\circ}C$). It is supposed that the improvement of p-type conductivity may be leaded by the increase of Mn4+ concentration through the substitution of divalent/monovalent cations for La site in LaMnO3.

  • PDF

고체산화물 연료전지용 Strontium Titanate 세라믹 접속자 소재의 소결 거동 및 전기적 특성 (Sintering Behavior and Electrical Properties of Strontium Titanate-Based Ceramic Interconnect Materials for Solid Oxide Fuel Cells)

  • 박범경;이종원;이승복;임탁형;박석주;송락현;신동열
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2010년도 추계학술대회 초록집
    • /
    • pp.80.1-80.1
    • /
    • 2010
  • A strontium titanate ($SrTiO_3$)-based material with a perovskite structure is considered to be one of the promising alternatives to $LaCrO_3$-based materials since $SrTiO_3$ perovskite shows a high chemical stability under both oxidizing and reducing atmospheres at high temperatures. $SrTiO_3$ materials exhibit an n-type semiconducting behavior when it is donor-doped and/or exposed to a reducing atmosphere. In this work, $Sr_{1-x}La_xTi_{1-y}M_yO_3$ materials doped with $La^{3+}$ in A-sites and aliovalent transition metal ions ($M^{n+}$) in B-sites were synthesized by the modified Pechini method. The X-ray diffraction analysis indicated that the materials synthesized by the Pechini process exhibited a single curbic perovskite-type structure without any impurity phases, and are tolerant, to some extent, to cation doping. The sintering behaviors of $Sr_{1-x}La_xTi_{1-y}M_yO_3$ in $H_2/N_2$ and air were characterized by dilatometry and microstructural observations. The electrical conduction mechanism and the dopant effect are discussed based on the defect structures and the electrical conductivities measured at various oxygen partial pressures and temperatures.

  • PDF

기상 반응용 스마트 용출 촉매 연구 동향 (A review of smart exsolution catalysts for the application of gas phase reactions)

  • 황루이;김형준;한정우
    • 세라미스트
    • /
    • 제23권2호
    • /
    • pp.211-230
    • /
    • 2020
  • Perovskite-type oxides with the nominal composition of ABO3 can exsolve the B-site transition metal upon the controlled reduction. In this exsolution process, the transition metal emerges from the oxide lattice and migrates to the surface at which it forms catalytically active nanoparticles. The exsolved nanoparticles can recover back to the bulk lattice under oxidation treatment. This unique regeneration character by the redox treatment provides uniformly dispersed noble metal nanoparticles. Therefore, the conventional problem of traditional impregnated metal/support, i.e., sintering during reaction, can be effectively avoided by using the exsolution phenomenon. In this regard, the catalysts using the exsolution strategy have been well studied for a wide range of applications in energy conversion and storage devices such as solid oxide fuel cells and electrolysis cells (SOFCs and SOECs) because of its high thermal and chemical stability. On the other hand, although this exsolution strategy can also be applied to gas phase reaction catalysts, it has seldomly been reviewed. Here, we thus review recent applications of the exsolution catalysts to the gas phase reactions from the aspects of experimental measurements, where various functions of the exsolved particles were utilized. We also review non-perovskite type metal oxides that might have exolution phenomenon to provide more possibilities to develop higher efficient catalysts.

페롭스카이트형 산화물에서 일산화탄소에 의한 질소산화물의 환원반응 (Catalytic Reduction of Nitric Oxide by Carbon Monoxide over Perovskite-Type Oxide)

  • 문행철;선창봉;이근대;안병현;임권택;홍성수
    • 공업화학
    • /
    • 제10권3호
    • /
    • pp.407-414
    • /
    • 1999
  • 능금산법으로 제조된 페롭스카이트형 산화물에서 CO에 의한 NO의 환원반응에 대한 연구를 행하였다. 촉매는 주로 Lanthanoid계 페롭스카이트를 사용하였고, 활성을 증가시키기 위해 A, B site에 Sr, Ba 및 Fe, Mn 등을 치환시켰다. $LaCoO_3$ 촉매에서 A site에 Sr을 일부 치환시키면 NO전환율이 증가하였다. 한편 B site에 Fe나 Mn을 일부 치환시키면 NO의 전환율이 증가하였으나 Fe의 치환량이 커지면 오히려 전환율이 감소하였다. 한편 $La_{0.6}Sr_{0.4}Co_{0.8}Fe_{0.2}O_3 $ 촉매에 $SnO_2$$MnO_2$를 혼합하면 촉매활성이 증가하는 상승효과를 보였다. 반응물에 첨가된 물은 촉매활성을 감소시켰으나 촉매에 대한 물의 작용은 어느 정도 가역적이었다. 또한 반응물에 첨가된 이산화황은 NO의 전환율을 감소시켰다.

  • PDF

폐롭스카이트형 촉매에서 입자상물질의 촉매연소반응 (Catalytic Combustion of Soot Particulate over Perovskite-Type Oxides)

  • 양진섭;홍성수;정덕영;오광중;조경목;류봉기;박대원
    • 공업화학
    • /
    • 제9권6호
    • /
    • pp.803-810
    • /
    • 1998
  • 능금산법으로 제조된 페롭스카이트 촉매에서 입자상물질의 연소반응에 대하여 연구하였다. 페롭스카이트 산화물의 A 및 B site에 금속이온을 치환시켜 연소반응의 활성을 증가시켰다. 또한 반응온도, 산소의 농도, 공간속도, $SO_2$ 및 물의 영향에 대하여 조사하였다. $LaCoO_3$형 촉매의 A site에 알칼리족 금속을 치환시키면 연소개시 온도가 낮아졌고, 알카리족 금속은 Cs>K>Na의 순서로 연소활성을 증가시켰다. 그러나 $La_{0.6}Cs_{0.4}CoO_3 $촉매에서 B site에 Fe나 Mn을 치환시키더라도 연소개시 온도의 변화가 거의 없었다. 산소의 농도가 증가함에 따라 연소개시 온도는 낮아졌고 이산화탄소의 생성속도는 산소분압의 영향을 별로 받지 않았다. 한편 공간속도의 증가에 따라 연소개시온도가 낮아졌고, 이산화황에 대한 촉매의 비활성화는 일어나지 않았으며, 반응물 중에 첨가된 물에 의해 연소반응이 촉진되었다.