SHAPE EFFECT ON PERFORMANCE OF MULTILAYER CERAMIC ACTUATOR

  • Wee, S. B.;Jeong, S. J.;Song, J. S.
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2003.12a
    • /
    • pp.163-168
    • /
    • 2003
  • In the present study, the piezoelectricity and polarization of multilayer ceramic actuator, being designed to stack PMN-PZ-PT ceramic layers and Ag-Pd electrode layers alternatively, were investigated under a consideration of geometric factor, the volume ratio of the ceramic to the electrode layers. The actuators were fabricated by tape casting of $0.2Pb(Mg_{1/3}Nb_{2/3)O_3-0.38PbZrO_3-0,42PbTiO_3$ followed by lamination and burnout & co-firing processes. The actuators of $10\times10\times0.6~2\textrm{mm}^3$ in size were formed in a way that $60 ~ 200\mu\textrm{m}$ thick were stacked alternatively with $5\mu\textrm{m}$ thick electrode layer. Increases in polarization and electric field-induced displacement with thickness of the ceramic layer were attributed to change of $90^{\circ}$/$180^{\circ}$ domain ratio, which was affected by interlayer internal stress. The piezoelectricity and actuation behaviors were found to depend upon the volume ratio (or thickness ratio) of ceramic to electrode layers.

  • PDF

Field-induced Strain and Polarization Switching Mechanisms in Ba-modified PMN-PT Ceramics (Ba 변성 PMN-PT계 강유전체의 전계유기변위와 분극특성)

  • 장명철
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.1
    • /
    • pp.12-20
    • /
    • 2000
  • Dielectric property of Ba-modified 0.65Pb(Mg1/3Nb2/3)O3-0.35PbTiO3 ceramics having compositions near the morphotropic phase boundary was investigated. For the specimens having Ba contents between 0 and 20 at%, the average transition temperature was decreased linearly with increasing Ba contents and the degree of hysteresis was also decreased with increasing Ba contents. The maximum dielectric constants (K), electric field induced polarization(P) and electrically-induced strain(S) were found to exihibit a maximum value at∼3 at% of Ba. The increase of S and the decrease of hysteresis by minor additions of Ba impurities indicated the development of new higher perfomance actuator materials. The composition of Ba-PMN-PT (10/65/35) may be appropriate for capacitor materials because of low hysteresis and high polarization.

  • PDF

The compact size piezoelectric transformer to lower an operating voltage of plasma display devices

  • Choi, Chung-Sock;Ahn, Sung-Il;Choi, Kyung-Cheol
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.719-720
    • /
    • 2009
  • We suggest a new approach to lower the operating voltage of plasma display devices using a piezoelectric transformer (PT). $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$ (PMNT) was used as a piezoelectric material. The Rosen-type PT, with a compact size of 10 mm ${\times}$ 20 mm ${\times}$ 0.3 mm, was fabricated on a glass substrate. The fabricated PT was operated as a half-wave vibration mode at around 80~90 kHz. The maximum voltage step-up ratio was 3 at 87.8 kHz when the input voltage was 10.32 V (peak-to-peak).

  • PDF

Hysteresis Reduction in piezoelectric actuator by a charge control method (전하 제어법을 이용한 압전 액추에이터의 이력저감)

  • Jeong Soonjong;Lee Daesu;Song Jaesung;Hong Younpyo;Kang Eungu;Choi Wonjong
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2005.05a
    • /
    • pp.35-39
    • /
    • 2005
  • This paper presents a method to reduce hysteresis in multilayer ceramic actuator by connecting the actuator with a capacitor in a series circuit. The change in hysteresis with respect to the capacitor was examined. $0.2Pb(Mg_{1/3}Nb_{2/3})O_3-0.8Pb(Zr_{0.475}Ti_{0.525})O_3$ ceramic material was used as a piezoelectric material for the actuator. Displacement of the actuator was measured in a capacitive gap sensor measuring system. In case of inserting a capacitor in a total circuit, hysteresis became dramatically decreased, and then finally the hysteresis value can be reduced below $0.2\%$. It was found in this present study that reducing the hysteresis in the actuator is dependent upon the characteristics of the capacitor in total circuit and also operating frequency.

  • PDF

Preparation of PMN-PT-BT Powder by Modified Mixed Oxide Method and Effect of Ag on Dielectric Properties (Modified Mixed Oxide 방법에 의한 PMN-PT-BT 분말 합성 및 그의 물성에 미치는 Ag의 영향)

  • Lim, Kyoung-Ran;Jeong, Soon-Yong;Kim, Chang-Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.2
    • /
    • pp.159-163
    • /
    • 2002
  • A single phase perovskite relaxor ferroelectric PMN-PT-BT was prepared by a single calcination and the modified mixed oxide process. It was accomplished by ball-milling PbO, $Nb_2O_5,\;Ti(OC_3H_7)_4,\;BaCO_3,\;and\;Mg(NO_3)_2$ instead of MgO, removing the solvent, and then followed by calcination at 900$^{\circ}C$ for 2h. The specimen sintered at 1100$^{\circ}C$/2h showed the sintered density of 7.83 g/$cm^3$, room temperature dielectric constant of 22000, and dielectric loss of 2.5%. Addition of 1.0 mole% (0.3 wt%) of Ag as $AgNO_3$ and followed by calcination at 550$^{\circ}C$/2h lowered the sintering temperature to 900$^{\circ}C$. It still showed the sintered density of 7.88 g/$cm^3$, room temperature dielectric constant of 20000 and dielectric loss of 2.4%.

A Research for Piezoelectric Energy Harvesters Based on Flammable Material (가연성 소재 기반의 에너지 하베스터 연구)

  • Kang, Woo-Seok;Koh, Jung-Hyuk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.12
    • /
    • pp.863-865
    • /
    • 2014
  • Energy problem has been issued in worldwide because fossil fuel has being almost exhausted. A lot of renewable energy have been received attention to replace the energy from fossil fuel. Among them, piezoelectric energy harvester is one of excellent candidates. In general, micro scaled small sized energy harvesters were usually based on the lithography process. However, these lithography process require complicated process and high cost. In this paper, a new process has been proposed for micro-scaled piezoelectric energy harvester. $0.2Pb(Mg_{1/3}Nb_{2/3})O_3-0.8Pb(Zr_{0.52}Ti_{0.48})O_3$ composition was used as piezoelectric material due to excellent piezoelectric properties and also can be easily prepared by mixed oxide method.

Geochemical Composition of Volcanic Ash from Historical Eruptions of Mt. Baekdu, Korea (역사시대에 분화한 백두산 화산재의 화학 성분)

  • Yun, Sung-Hyo;Koh, Jeon Seon;Chang, Cheolwoo
    • The Journal of the Petrological Society of Korea
    • /
    • v.27 no.1
    • /
    • pp.37-47
    • /
    • 2018
  • Volcanic ash samples of historical eruptions from Mt. Baekdu were analyzed for major oxides, trace and rare earth elements by a variety of analytical techniques. The results indicate that the ashes consist of approximately 58.8~71.1 wt.% $SiO_2$, 9.6~16.8 wt.% $Al_2O_3$, 4.5~6.9 wt.% $Fe_2O_{3t}$, 0.1~1.7 wt.% MgO, 0.3~1.6 wt.% CaO, 5.2~6.3 wt.% $Na_2O$, 4.3~5.9 wt.% $K_2O$ and less than 1.2 wt.% $TiO_2$. Thirty two trace metals including Ba, Cu, Cr. Co, Ni, Sr, V, Zn, and Zr were analyzed. The ashes can be divided two groups: group A(1 ka Millennium pumice, 1668 and $190{\underline{3}}$ pumice) and group B(1702 pumice) according to the relative enrichment of HREEs. The abundances of heavy metals such as Cu, Co, Mn, and Zn were relatively low. As compared to the Sakurajima volcanic ash, Baekdusan volcanic ash has low concentrations of Y, Nb, Pb, U, Sc, V, Ni and Cu and high concentrations of Zr, Ba, Hf, Cr, Co, Zn and rare-earth (except Eu).

Preparation of PMN-PT-BT/Ag Composite and its Mechanical and Dielectric Properties (PMN-PT-BT/Ag 복합체 제조 및 기계적, 유전적 특성)

  • Lim, Kyoung-Ran;Jeong, Soon-Yong;Kim, Chang-Sam;Nahm, Sahn
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.9
    • /
    • pp.846-850
    • /
    • 2002
  • A PMN-PT-BT/Ag composite was prepared by surface modification with MgO sol with hoping to suppress silver's migration during sintering. The mixture of PbO, $N_2O_5,\;TiO_2\;with\;Mg(NO_3)_2$ instead of MgO was ball milled, the solvent was removed and then the dried powders were calcined at 950$^{\circ}C$/1h. The calcined powder were treated with 3.0 mol% $Ag_2O$ and 1.0 wt% MgO sol and calcined at 550$^{\circ}C$/1h. The dielectrics sintered at 1000$^{\circ}C$/4h under a flowing oxygen showed the density of 7.84g/$cm^3$, the room temperature dielectric constant of 18400, the dielectric loss of 2.4%, the specific resistivity of $0.24{\times}10^{12}{\Omega}{\cdot}cm$. It also showed the bending strength of $120.7{\pm}11.26$ MPa and the fracture toughness of $0.87{\pm}0.002\;MPam^{1/2}$ which were comparable to commercial PZT. The microstructure sonsisted of grains of ∼4${\mu}m$. SEM and SIMS analysis showed that Ag grew as ∼1${\mu}m$ and excess MgO as ∼0.5${\mu}m$.

Processing Study for the Piezoelectric Energy Harvest of Composit Structure (복합구조의 압전 에너지 하베스터를 위한 공정연구)

  • Lee, Kyoung-Soo;Shin, Dong-Jin;Koh, Jung-Hyuk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.25 no.4
    • /
    • pp.286-289
    • /
    • 2012
  • In this paper, we have proposed piezoelectric energy harvester employing the pillar structure with the diameter size of 500 um. So we have selected the Su-8 photo-resist and modified lithography process to manufacture the pillar structure with height above the $500{\mu}m$. Simultaneously, we tried to make a comparative study to use ceramic bulk - polymer structure In this paper, we will report the process and properties of micro pillar structure based on the PMN-PZT ($Pb(Mg_{1/3}Nb_{2/3})O_3-PbZrTiO_3$) materials. Finally, We will propose a method for generating electrical energy with a piezoelectric element using vibration, an energy source can be obtained from the "clean" energy.

Properties of Piezoelectric thick film with detailed structure following particle size (입자 크기에 따른 미세구조를 가지는 압전 후막 특성)

  • Moon, Hi-Gyu;Song, Hyun-Cheol;Kim, Sang-Jong;Choi, Ji-Won;Kang, Jong-Yoon;Kim, Hyun-Jai;Jo, Bong-Hee;Yoon, Seok-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.325-325
    • /
    • 2008
  • 스크린 프린팅에 의한 압전 후막은 MEMS 공정을 이용하여 마이크로 펌프, 마이크로 벨브, 마이크로 센서, 마이크로 로봇 등 여러 초소형 기계부품에 응용되고 있으며, Sol-Gel, PLD를 이용해 증착된 막 등에 비해 수십${\mu}m$의 비교적 두꺼운 막을 형성시킬 수 있는 장점을 가지고 있다. 그러나 실리콘 기판을 사용하여 스크린 프린팅으로 형성된 압전 후막의 경우, 공정상 바인더를 연소시키는 과정을 거치게 되므로, 밀집된(Dense) 구조를 가지는 막을 만들기가 어렵다. 이로 인해 스크린 프린팅에 의한 후막은 전기적 특성 및 기계적 특성이 떨어지는 경향이 있다. 본 연구에서는 스크린 프린팅에 의한 압전 후막의 밀집된 구조 및 특성을 향상시키기 위해 0.01Pb$(Mg_{1/2}W_{1/2})$O3-0.41Pb$(Ni_{1/3}Nb_{2/3})O_3-0.35PbTiO_3-0.23PbZrO_3$의 powder와 Attrition 밀링 처리된 powder를 비율별로 혼합하여 입자의 크기를 변화시켜 막의 충진 밀도를 향상시켰으며, 열처리 효과를 극대화시키기 위해 RTA(Rapidly Thermal Annealing)를 통해 열처리 하였다. Attrition 밀링에 의한 파우더를 각각 비율별로 100%, 50%, 25%로 혼합하여 만든 압전 세라믹 페이스트는 P-type(100)Si Wafer sample 위에 $1{\mu}m$의 하부전극용($1100^{\circ}C$) Ag 전극을 screen print하여 소결했다. 그리고 다시 전극이 형성된 Si wafer 위에 스크린 프린팅하고, 건조 한 후 RTA로 300초 동안 열처리 한 결과 밀집된 구조를 가지는 압전 후막을 제작 수 있었다.