Open-Cell Rigid Polyurethane Foam Using Reactive Cell Opening Agents (반응성 기포개방제를 이용한 개방기포형 경질우레탄폼)

  • Ahn, WonSool
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.5
    • /
    • pp.2524-2528
    • /
    • 2013
  • Cell opening characteristics dependent on the cell openers for the conventional formulation of a closed-cell polyurethane foam (PUF) was studied using 1-butanol and lithium salt of 12-hydroxystearic acid (Li-12HSA) as the reactive cell opening agents. While cell openining content of only 10.5 % was obtained for the sample with 4 phr of 1-butanol as the single reactive cell opener, that of 98.0% could be obtained for the sample with 2 phr of Li-12HSA as the reactive co-cell opener. As the results, it showed that a fully open-cell rigid PUF could be obtained by introducing a novel reactive cell opener, having a functional group able to form a bulky side-chain on the urethane networks, without severe loss of mechanical properties of the closed-cell PUF like cell size, bulk density, and thermal conductivity.

A study on the Damping Properties of NR Vulcanizates. (천연(天然)고무의 Damping Property에 관(關)한 연구(硏究))

  • Choi, Jae-Woon;Paik, Nam-Chul
    • Elastomers and Composites
    • /
    • v.20 no.3
    • /
    • pp.189-204
    • /
    • 1985
  • The purpose of this study is to examine the dynamic properties, especially the damping and fatigue properites, of NR vulcanizates and to find out the vulcanizate which can be used as damping materials in industry. The results of this study can be summarized as follows: 1. In the ODR test, the S-2 vulcanizate was the fastest one in terms of having reached to optimum cure times($t_{90}$) and, with the same formula, when 50phr of HAF carbon black loaded, the shortest optimum cure times has shown. 2. The S - 2 vulcanizate was the best than the others in the physical properties. In aging properties, however, the E - 1 vulcanizate appeared to be better than the other vulcanizates. 3. The results of the RDS test for the NR vulcanization system under the condition of 0.1% strain amplitude and 1 Hz frequency showed no connection between Tg and the the nature of the crosslinking system, but 50phr loading of HAF carbon black increased Tg. The damping values of vulcanizates in the elastic region showed a strong relations the damping values and the crosslinking system. The S - 2 vulcanizate with higher crosslink density had lower damping values than other vulcanizates, and furthermore, the SH - 2 vulcanizates with 50phr loading of HAF carbon black increased the damping values. 4. The Goodrich Flexometer test showed that the heat buildup for the gum NR vulcanizates was less than for those which contained 50phr of HAF carbon black. In particular, the fatigue life of the vulcanizate with lower damping values appeared to be longer than that of the vulcanizates with higher damping values. In the fatigue test, the increasment of the loading or the temperature, applied to the vulcanizates, appeared to be shorten their fatigue life.

  • PDF

Detection of Magnetic Bacteria Using PHR Sensors with Trilayer Structure (삼층박막 구조의 PHR 센서를 이용한 자기 박테리아 감지)

  • Yoo, Sang Yeob;Lim, Byeong Hwa;Song, In Cheol;Kim, Cheol Gi;Oh, Sun Jong
    • Journal of the Korean Magnetics Society
    • /
    • v.23 no.6
    • /
    • pp.200-204
    • /
    • 2013
  • In this study, we have fabricated magnetoresistive sensors of $50{\mu}m{\times}50{\mu}m$ cross type by trilayer structure of antiferromagnetic/nonmagnetic/ferromagnetic. The magnetic signal and magnetic domain of this sensor is measured. The sensor hysteresis loop is not in symmetrical at 0 Oe. This is may be due to the exchange coupling between ferromagnetic layer and anti ferromagnetic layer. This exchange bias value is 20 Oe. The sensor signal is measured at between the applied magnetic field and current. The sensor signal is measured between the applied magnetic field and current at $20^{\circ}$ and $90^{\circ}$ angles. The sensitivity of sensor signals is $20{\mu}V/Oe$ and $7{\mu}V/Oe$ at $20^{\circ}$ and $90^{\circ}$ angles, respectively. In addition, this sensor is also applied for the detection of magnetic bacteria at $20^{\circ}$ angle. From these results, we calculate the stray field of single bacteria is to be $5{\times}10^{-5}$Oe.

The Effect of Cure System for the Viscoelastic Properties of Vulcanized Rubber (가황시스템 변화가 가황고무의 점탄성적 특성에 미치는 효과)

  • Park, Nam-Cook;Lee, Seog
    • Elastomers and Composites
    • /
    • v.34 no.1
    • /
    • pp.11-19
    • /
    • 1999
  • Rebound, storage and loss modulus, and tan ${\delta}$ were investigated on cured rubbers with various ratios of sulfur to accelerator and the volume fraction of carbon black in the cured rubbers. The rebound was increased as the sulfur to accelerator ratio and the volume fraction of carbon black decreased. The storage modulus decreased as the loading of carbon black and the strain increased regardless of the cure systems. The network structure formed by filler-filler interaction was destroyed above 6% strain regardless of the loading of carbon black, because constant storage modulus was shown at the higher strain than 3% for $40{\sim}50phr$ loading of carbon black and at the higher strain than 6% for 60 phr and above loading of carbon black. Little effect on loss modulus was found at the low loading of carbon black, but the peak of loss modulus was shown at 1% strain as the loading of carbon black was increased. Tan ${\delta}$ increased as the loading of carbon black and the strain were increased regardless of the cure system, and maximum tan ${\delta}$ was shown at 2% strain regardless of the loading of carbon black.

  • PDF

Reactions and Properties of a RT-Castable PU Elastomer Modified with Oligomeric Diol (올리고머형 디올로 개질된 상온주형용 PU 엘라스토머의 반응과 물성)

  • Ahn, Won-Sool;Kim, Hoon-Seop
    • Elastomers and Composites
    • /
    • v.43 no.1
    • /
    • pp.18-24
    • /
    • 2008
  • An oligomeric diol was utilized as a modifier for the reaction rate and mechanical properties of a RT-castable polyurethane elastomer. Both the reaction rate and the tensile strength of the blend samples, in which the modifier and the base resins were mixed with one-shot method, showed an exponential decrease as the increase of modifier concentration. Thermal analysis method of Kissinger was also effectively applied in the present study, showing good linearity in the plot of ln $(q/T^2_p)$ vs. $(1/T_p)$ and activation energy $E_a$ of 44.80 kJ/mol, which is similar to the general castable polyurethane. In the mechanical properties, remarkable decrease of strength was found by the addition of modifier concentration range up to about 20 phr, while characteristic elongation property of the elastomer, high elongation at lower strength, was observed over 20 phr of the modifier. Exponential decrease of the break strength of the blend sample exhibited that the mechanical properties of the blend might be considerably sensitive to the modifier concentration.

Cure Characteristics and Mechanical Properties of Ternary Accelerator System in NR/BR Compounds (NR/BR Compounds의 가황촉진제 병용에 의한 가황 특성 및 기계적 물성 연구)

  • Kim, Il-Jin;Kim, Wook-Soo;Lee, Dong-Hyun;Bae, Jong-Woo;Byon, Young-Hoo;Kim, Wonho
    • Korean Chemical Engineering Research
    • /
    • v.47 no.4
    • /
    • pp.403-409
    • /
    • 2009
  • In the 1840s, Goodyear found out sulfur cure system, but cure time was too slow. So producing of rubber product takes a long time. In 1904, Oenslager et al. found that aniline is accelerated sulfur cure system. Recently, many rubber industries needed high yield and good quality. So, many researchers have studied a rubber system with fast vulcanization time and good mechanical properties. In this study, cure characteristics and mechanical properties of NR/BR compounds by accelerator with MBTS(2,2' Dithiobisbenzothiazole), TMTM(Tetramethylthiuram Monosulfide), ZDMC (Zinc dimethyldithiocarbamate), CBS(N-Cyclohexyl benzothiazolyl-2-sulfenamide), DPG(Diphenylguanidine) were evaluated. The results of the study indicate that cure charateristics($t_{90}$: 235 sec, $T_{max}$: 5.77 Nm) and mechanical properties (100, 300% modulus : 2,180, 5.656 Mpa and tear strength: 59.58 kgf/cm) of NR/BR compounds shows efficient acceleration with MBTS 1.5 phr, TMTM 0.5 phr, DPG 0.15phr. This is due to the synergistic activity of ternary accelerator system in rubber vulcanization.

Antibacterial Effect of the Surface-Modified Biomedical Polyurethane against Staphylococcus aureus and Staphylococcus epidermidis

  • Jeon, Sung-Min;Kim, Hyun-Jung;Lee, Kyu-Back;Kim, Jong-Won;Kim, Mal-Nam
    • Journal of Microbiology and Biotechnology
    • /
    • v.11 no.2
    • /
    • pp.259-265
    • /
    • 2001
  • Staphylococal infection still remains to be one of the most serious infections, having various complications in the clinical use of indwelling polymeric medical devices. However, there are a few promising systems showing a high antibacterial effect without causing any demage of polymer backbone under biological environments such as blood or body fluid. In order to resolve this problem, we have designed a new antibiotic releasing system via a hydrolysis mechanism. The surface of biomedical polyurethane (PU) was modified by using 1,6-diisocyanatohexane (HMDI) to immobilize the rifampicon. Also, the immobilized rifampicin was designed to be released by a selective cleavage of the unstable carbamate linkage that exists on the rifampicin-immobilized polyurethane (PHR). The immobilization of rifampicin on the surface of polyurethane was confirmed by the disappearance of the characteristics IR absorbance peak of the isocyanate (-NCO) group at $2,267\;cm^{-1}$. The PHR showed a continuous rifampicin release profile under an aqueous environment of 10 mM of PBS (phosphate-buffered saline) for ove 6 days. The rifampicin molecules, which are released from PHR under an optimal bacterial infection environment, had a higher antibacterial activity against both S. aureus and S. epidermidis than rifampicin-incorporated polyurethane (RIP). In addition, the PHR maintained a stable antibacterial effect under a blood-mimic aqueous environment such as bovine calf serum.

  • PDF

A Study on Thermal Conductivity and Fracture Toughness of Alumina Nanofibers and Powders-filled Epoxy Matrix Composites (알루미나 나노섬유와 분말이 첨가된 에폭시 복합재료의 열전도도 특성 및 파괴인성에 대한 연구)

  • Choi, Jeong-Ran;Park, Soo-Jin
    • Polymer(Korea)
    • /
    • v.37 no.1
    • /
    • pp.47-51
    • /
    • 2013
  • In this work, the effect of alumina nanofibers on thermal conductivity and fracture toughness of alumina nanofibers and powder filled epoxy (EP) composites were investigated with varying alumina nanofiber content from 20 to 100 phr. Thermal conductivity was tested using a laser flash analysis (LFA). The fracture toughness of the composites were studied through the critical stress intensity factor ($K_{IC}$) measurement. The mophologies were observed by scanning electron microscopy (SEM). From the results, it was found that the thermal conductivity was enhanced with increasing alumina nanofiber content, which played a key factor to determine the thermal conductivity. The $K_{IC}$ value was increased with increasing alumina nanofiber content, whereas the value decreased above 40 phr alumina nanofiber content. This was probably considered that the alumina nanofiber entangled each other in EP due to an excess of alumina nanofibers.

EMI shielding effectiveness and mechanical properties of MWCNTs-reinforced biodegradable epoxy matrix composites

  • Yim, Yoon-Ji;Chung, Dong Chul;Park, Soo-Jin
    • Carbon letters
    • /
    • v.22
    • /
    • pp.36-41
    • /
    • 2017
  • Biodegradable epoxy (B-epoxy) was prepared from diglycidyl ether of bisphenol A and epoxidized linseed oil. The mechanical properties of B-epoxy composites reinforced with multi-walled carbon nanotubes (MWCNTs/B-epoxy) were examined by employing dynamic mechanical analysis, critical stress intensity factor ($K_{IC}$) tests, and impact strength tests. The electromagnetic interference shielding effectiveness (EMI-SE) of the composites was evaluated using reflection and absorption methods. Mechanical properties of MWCNTs/B-epoxy were enhanced with an increase in the MWCNT content, whereas they deteriorated when the MWCNT content was >5 parts per hundred resin (phr). This can likely be attributed to the entanglement of MWCNTs with each other in the B-epoxy due to the presence of an excess amount of MWCNTs. The highest EMI-SE obtained was ~16 dB for the MWCNTs/B-epoxy composites with a MWCNT content of 13 phr at 1.4 GHz. The composites (13 phr) exhibited the minimum EMI-SE (90%) when used as shielding materials at 1.4 GHz. The EMI-SE of the MWCNTs/B-epoxy also increased with an increase in the MWCNT content, which is a key factor affecting the EMI-SE.

A Study on Frequency Dependence on Dielectric Properties of Silicone Rubber Sheets (실리콘 고무 시트의 유전특성에 미치는 주파수 의존성에 관한 연구)

  • Lee, Sung Ill
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.33 no.5
    • /
    • pp.405-410
    • /
    • 2020
  • In this study, the following results were obtained by analysis of electric properties with FT-IR, DSC, XRD, and SEM, in the range of temperature 30~160℃ and frequency 0.1~200 kHz, when filling agent (0~100 phr) and silicone oil (0~12 phr) were added to raw silicone rubber. In the case of 100 phr mixed samples, the relative dielectric constant εr gradually decreased from 4.3 to 3.96 as frequency increased, and the dielectric loss tan δ decreased to 0.01 at 300 Hz, then increased to 0.022 at 30 kHz, then decreased to 200 kHz. The FT-IR analysis identified the same binding structure according to the chemical composition of added silica (SiO2). Through DSC analysis, we could determine the change of heat quantity and the glass transition temperature of each specimen. In the XRD analysis, it was found that the images SiO2, TiO2, and Fe2O3 appeared for specimens with 0%, 50% and 100% filling agent. Finally, the SEM analysis confirmed that particles of 0.5 to 1.5 ㎛ size with silica (SiO2) mixing were dispersed evenly.