• Title/Summary/Keyword: Oxide Semiconductor

Search Result 1,419, Processing Time 0.03 seconds

Material and Electrical Characteristics of Oxynitride Gate Dielectrics prepared in $N_2$O ambient by Rapid Thermal Process (RTP로 $N_2$O 분위기에서 제조한 Oxynitride Gate 절연체의 물질적 전기적 특성)

  • Park, Jin-Seong;Lee, Woo-Sung;Shim, Tea-Earn;Lee, Jong-Gil
    • Korean Journal of Materials Research
    • /
    • v.2 no.4
    • /
    • pp.285-292
    • /
    • 1992
  • Ultrathin(8nm) oxynitride (SiOxNy) film have been formed on Si(100) by rapid thermal processing(RTP) in $O_2$and $N_2$O as reactants. Compared with conventional furnace $O_2$ oxide, the oxynitride dielectrics shows better characteristics of I-V and TDDB, and less flat-band voltage shift. The oxynitride has a behavior of Fowler-Nordheim tunneling in the region of V 〉${\varphi}_0$ simialr to pure Si$O_2$oxide. The relative dielectric constant of oxynitride is higher than that of conventional pure oxide. Excellent diffusion harrier property to dopant(B$F_2$) is also observed. Nitrogen depth profiles by SIMS, AES, and XPS show nitrogen pile - up at Si$O_2$/Si interface, which can explain the improved properties of oxynitride dielectrics.

  • PDF

Effect of Annealing Temperature on the Electrical Performance of SiZnSnO Thin Film Transistors Fabricated by Radio Frequency Magnetron Sputtering

  • Kim, Byoungkeun;Lee, Sang Yeol
    • Transactions on Electrical and Electronic Materials
    • /
    • v.18 no.1
    • /
    • pp.55-57
    • /
    • 2017
  • Amorphous oxide thin film transistors (TFTs) were fabricated with 0.5 wt% silicon doped zinc tin oxide (a-0.5SZTO) thin film deposited by radio frequency (RF) magnetron sputtering. In order to investigate the effect of annealing treatment on the electrical properties of TFTs, a-0.5SZTO thin films were annealed at three different temperatures ($300^{\circ}C$, $500^{\circ}C$, and $700^{\circ}C$ for 2 hours in a air atmosphere. The structural and electrical properties of a-0.5SZTO TFTs were measured using X-ray diffraction and a semiconductor analyzer. As annealing temperature increased from $300^{\circ}C$ to $500^{\circ}C$, no peak was observed. This provided crystalline properties indicating that the amorphous phase was observed up to $500^{\circ}C$. The electrical properties of a-0.5SZTO TFTs, such as the field effect mobility (${\mu}_{FE}$) of $24.31cm^2/Vs$, on current ($I_{ON}$) of $2.38{\times}10^{-4}A$, and subthreshold swing (S.S) of 0.59 V/decade improved with the thermal annealing treatment. This improvement was mainly due to the increased carrier concentration and decreased structural defects by rearranged atoms. However, when a-0.5SZTO TFTs were annealed at $700^{\circ}C$, a crystalline peak was observed. As a result, electrical properties degraded. ${\mu}_{FE}$ was $0.06cm^2/Vs$, $I_{ON}$ was $5.27{\times}10^{-7}A$, and S.S was 2.09 V/decade. This degradation of electrical properties was mainly due to increased interfacial and bulk trap densities of forming grain boundaries caused by the annealing treatment.

Flexibility Improvement of InGaZnO Thin Film Transistors Using Organic/inorganic Hybrid Gate Dielectrics

  • Hwang, B.U.;Kim, D.I.;Jeon, H.S.;Lee, H.J.;Lee, N.E.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.341-341
    • /
    • 2012
  • Recently, oxide semi-conductor materials have been investigated as promising candidates replacing a-Si:H and poly-Si semiconductor because they have some advantages of a room-temperature process, low-cost, high performance and various applications in flexible and transparent electronics. Particularly, amorphous indium-gallium-zinc-oxide (a-IGZO) is an interesting semiconductor material for use in flexible thin film transistor (TFT) fabrication due to the high carrier mobility and low deposition temperatures. In this work, we demonstrated improvement of flexibility in IGZO TFTs, which were fabricated on polyimide (PI) substrate. At first, a thin poly-4vinyl phenol (PVP) layer was spin coated on PI substrate for making a smooth surface up to 0.3 nm, which was required to form high quality active layer. Then, Ni gate electrode of 100 nm was deposited on the bare PVP layer by e-beam evaporator using a shadow mask. The PVP and $Al_2O_3$ layers with different thicknesses were used for organic/inorganic multi gate dielectric, which were formed by spin coater and atomic layer deposition (ALD), respectively, at $200^{\circ}C$. 70 nm IGZO semiconductor layer and 70 nm Al source/drain electrodes were respectively deposited by RF magnetron sputter and thermal evaporator using shadow masks. Then, IGZO layer was annealed on a hotplate at $200^{\circ}C$ for 1 hour. Standard electrical characteristics of transistors were measured by a semiconductor parameter analyzer at room temperature in the dark and performance of devices then was also evaluated under static and dynamic mechanical deformation. The IGZO TFTs incorporating hybrid gate dielectrics showed a high flexibility compared to the device with single structural gate dielectrics. The effects of mechanical deformation on the TFT characteristics will be discussed in detail.

  • PDF

Metal-Semiconductor Contact Behavior of Solution-Processed ZnSnO Thin Film Transistors (용액법으로 제작된 ZnSnO 박막트랜지스터의 전극 물질에 따른 계면 접촉특성 연구)

  • Jeong, Young-Min;Song, Keun-Kyu;Woo, Kyoo-Hee;Jun, Tae-Hwan;Jung, Yang-Ho;Moon, Joo-Ho
    • Korean Journal of Materials Research
    • /
    • v.20 no.8
    • /
    • pp.401-407
    • /
    • 2010
  • We studied the influence of different types of metal electrodes on the performance of solution-processed zinc tin oxide (ZTO) thin-film transistors. The ZTO thin-film was obtained by spin-coating the sol-gel solution made from zinc acetate and tin acetate dissolved in 2-methoxyethanol. Various metals, Al, Au, Ag and Cu, were used to make contacts with the solution-deposited ZTO layers by selective deposition through a metal shadow mask. Contact resistance between the metal electrode and the semiconductor was obtained by a transmission line method (TLM). The device based on an Al electrode exhibited superior performance as compared to those based on other metals. Kelvin probe force microscopy (KPFM) allowed us to measure the work function of the oxide semiconductor to understand the variation of the device performance as a function of the types metal electrode. The solution-processed ZTO contained nanopores that resulted from the burnout of the organic species during the annealing. This different surface structure associated with the solution-processed ZTO gave a rise to a different work function value as compared to the vacuum-deposited counterpart. More oxygen could be adsorbed on the nanoporous solution-processed ZTO with large accessible surface areas, which increased its work function. This observation explained why the solution-processed ZTO makes an ohmic contact with the Al electrode.

Optically transparent and electrically conductive indium-tin-oxide nanowires for transparent photodetectors

  • Kim, Hyunki;Park, Wanghee;Ban, Dongkyun;Kim, Hong-Sik;Patel, Malkeshkumar;Yadav, Pankaj;Kim, Joondong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.390.2-390.2
    • /
    • 2016
  • Single crystalline indium-tin-oxide (ITO) nanowires (NWs) were grown by sputtering method. A thin Ni film of 5 nm was coated before ITO sputtering. Thermal treatment forms Ni nanoparticles, which act as templates to diffuse Ni into the sputtered ITO layer to grow single crystalline ITO NWs. Highly optical transparent photoelectric devices were realized by using a transparent metal-oxide semiconductor heterojunction by combining of p-type NiO and n-type ZnO. A functional template of ITO nanowires was applied to this transparent heterojunction device to enlarge the light-reactive surface. The ITO NWs/n-ZnO/p-NiO heterojunction device provided a significant high rectification ratio of 275 with a considerably low reverse saturation current of 0.2 nA. The optical transparency was about 80% for visible wavelengths, however showed an excellent blocking UV light. The nanostructured transparent heterojunction devices were applied for UV photodetectors to show ultra fast photoresponses with a rise time of 8.3 mS and a fall time of 20 ms, respectively. We suggest this transparent and super-performing UV responser can practically applied in transparent electronics and smart window applications.

  • PDF

Oxide Semiconductor Thin Film Transistor based Solution Charged Cellulose Paper Gate Dielectric using Microwave Irradiation

  • Lee, Seong-Yeong;Jo, Gwang-Won;Jo, Won-Ju
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2015.08a
    • /
    • pp.207.1-207.1
    • /
    • 2015
  • 차세대 디스플레이 소자로서 TAOS TFT (transparent amorphous oxide semiconductor Thin Film Transistor)가 주목 받고 있다. 또한, 최근에는 값 비싼 전자 제품을 저렴하고 간단히 처분 할 수 있는 시스템으로 대신 하는 연구가 진행되고 있다. 그중, cellulose-fiber에 전기적 시스템을 포함시키는 e-paper에 대한 관심이 활발하다. cellulose fiber는 가볍고 깨지지 않으며 휘는 성질을 가지고 있다. 가격도 저렴하고 가공이 용이하여 차세대 기판의 재료로서 주목받고 있다. 하지만, cellulose-fiber 위에는 고온의 열처리공정과 고품질 박막 성장이 어려워서 TFT 제작에 어려움을 겪고 있다. 이러한 문제를 해결하기 위해서 산화물 반도체를 이용하여 TFT를 제작한 사례가 보고되고 있다. 또한, 채널 물질 뿐만 아니라 cellulose fiber에도 다른 물질을 첨가하거나 증착하여 전기적 화학적 특성을 개선시킨 사례도 많이 보고되고 있다. 본 연구에서는 가장 저품질의 용지로 알려진 신문지와 A4용지를 gate dielectric을 이용하여서 a-IGZO TFT를 제작하였다. 하지만, cellulose fiber로 만들어진 TFT의 경우에는 고온의 열처리가 불가능 하다. 따라서 저온에서 높을 효율은 보이는 microwave energy를 이용하여 열처리를 진행하였다. 추가적으로 저품질의 종이의 특성을 개선시키기 위해서 high-k metal-oxide solution precursor를 첨가 하여 TFT의 특성을 개선시켰다. 결과적으로 cellulose fiber에 metal-oxide solution precursor을 첨가하는 공정과 micro wave를 조사하는 방법을 사용하여 100도 이하에서 cellulose fiber를 저렴하고 우수한 성능의 TFT를 제작에 성공하였다.

  • PDF

Electrical Properties of Transparent Indium-Tin-Zinc Oxide Semiconductor for Thin-Film Transistors

  • Lee, Gi-Chang;Choe, Jun-Hyeok;Han, Eon-Bin;Kim, Don-Hyeong;Lee, Jun-Hyeong;Kim, Jeong-Ju;Heo, Yeong-U
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.159-159
    • /
    • 2008
  • 투명전도체 (transparent conducting oxides: TCOs) 는 일반적으로 $10^3\Omega^{-1}Cm^{-1}$의 전도도, 가시광 영역에서 80%이상의 투명성을 가지는 재료로서, 액정 박막 표시 장치(TFT-LCD), 광기전성 소자, 유기 발광 소자, 에너지 절약 창문, 태양전지(sollar cell) 등 전극으로 사용되고 있다. 최근에는 TCO의 전도도특성을 조절하여 반도성특성을 가진 투명 산화물 반도체(transparent oxide semiconductor: TOS) 을 이용한 박막 트랜지스터 연구가 활발히 진행 중이다. 기존의 실리콘을 기반으로 하는 박막 트랜지스터의 낮은 이동도, 불투명성의 특성을 가지고 있지만, 산화물 박막트랜지스터는 높은 이동도를 발현 할 수 있을 뿐만 아니라, 넓은 밴드갭 에너지를 갖는 산화물을 이용하므로 투명한 특성도 발현 할 수 있어 차세대 디스플레이의 구동소자로서 응용연구가 되고 있다. 이에 본 연구에서는 박막트랜지스터 channel layer로서의 Indium-Tin-Zinc oxide 적용특성을 조사하였다. Indium, Tin, Zinc 의 혼합비율을 다양하게 조절하여 타겟을 제작하였다. 이를 RF magnetron sputtering 를 이용하여 박막으로 성장시켰으며, 기판으로는 glass 기판을 사용하였다. 박막 성장시 아르곤과 산소의 비율을 다양하게 조절하였다. 성장시킨 박막은 Hall effect, Transmittance, Work function, XRD등을 이용하여 전기적, 광학적, 구조특성을 평가하였다. Indium-Tin-Zinc Oxide(ITZO) 을 channel layer로 사용하여 Thin-film transistor 을 제작하여, TFT의 I-V 및 stability특성을 평가하였다.

  • PDF

Determination of Memory Trap Distribution in Charge Trap Type SONOSFET NVSM Cells Using Single Junction Charge Pumping Method (Single Junction Charge Pumping 방법을 이용한 전하 트랩형 SONOSFET NVSM 셀의 기억 트랩분포 결정)

  • 양전우;홍순혁;서광열
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.10
    • /
    • pp.822-827
    • /
    • 2000
  • The Si-SiO$_2$interface trap and nitride bulk trap distribution of SONOSFET(polysilicon-oxide-nitride-oxide-semiconductor field effect transistor) NVSM (nonvolatile semiconductor memory) cell is investigated by single junction charge pumping method. The device was fabricated by 0.35㎛ standard logic fabrication process including the ONO stack dielectrics. The thickness of ONO dielectricis are 24$\AA$ for tunnel oxide, 74 $\AA$ for nitride and 25 $\AA$ for blocking oxide, respectively. By the use of single junction charge pumping method, the lateral profiles of both interface and memory traps can be calculated directly from experimental charge pumping results without complex numerical simulation. The interface traps were almost uniformly distributed over the whole channel region and its maximum value was 7.97$\times$10$\^$10/㎠. The memory traps were uniformly distributed in the nitride layer and its maximum value was 1.04$\times$10$\^$19/㎤. The degradation characteristics of SONOSFET with write/erase cycling also were investigated.

  • PDF

Characteristics of Nickel Oxide Thin Film Manufactured by Reactive Magnetron Sputtering Method (반응성 마그네트론 스퍼터링법에 의한 Nickel Oxide 박막 제작 특성에 관한 연구)

  • Kim, Gi-Bum;Hwang, Yun-Sik;Kim, Yeung-Shik;Park, Jang-Sick
    • Journal of the Semiconductor & Display Technology
    • /
    • v.7 no.1
    • /
    • pp.29-34
    • /
    • 2008
  • In this paper, the DE(double erosion) cathode for the reactive magnetron sputtering system is developed for high deposition rate and high target utilization efficiency. The utilization efficiency of the developed DE cathode is 22% higher than that of normal SE(single erosion) cathode. Sputtering process for the nickel oxide thin films with the DE cathode is performed under the following conditions; power with $1kW{\sim}3kW$, pressure with 4mtorr and 8mtorr, oxygen flow ratio with $0%{\sim}80%$. As a result, the hysteresis phenomenon of discharge voltage in 4mtorr is lower than that in 8mtorr and the hysteresis phenomenon of discharge voltage is getting lower as the applied power is getting higher. The structure of cross section and surface roughness of the thin films are observed by FE-SEM and AFM. The structure of cross section of the thin films is columnar and the average surface roughness under oxygen flow ratio of 0%, 52.5% and 65.0% are $2.08{\AA}$, $2.20{\AA}$ and $0.854{\AA}$, respectively.

  • PDF

Development of Transfer Method for Transparent Thin Film Transistor of Heat-treated Zinc Oxide Thin Film by Solution Process (용액공정을 이용한 열처리된 산화아연 박막의 투명한 박막 트랜지스터 구현을 위한 전사방법 개발)

  • Kwon, Soon Yeol;Jung, Dong Geon;Choi, Young Chan;Lee, Jae Yong;Kong, Seong Ho
    • Journal of the Semiconductor & Display Technology
    • /
    • v.17 no.2
    • /
    • pp.57-60
    • /
    • 2018
  • Recently, Thin-film transistors (TFTs) are fundamental building blocks for state-of-the-art microelectronics, such as flat-panel displays and system-on-glass. Zinc oxide thin films have the advantage that they can grow at low temperature and can obtain high charge movility. Also the zinc oxide thin film can be used to control the resistance according to the oxygen content, so it is very easy to obtain the desired physical properties. In this paper, we fabricated a zinc oxide thin film on a polished copper substrate through a solution process, then improved the crystallinity through a geat treatment porcess, and studied to transfer it on a flexible substrate after the heat treatment was completed.