순환회분식 광촉매시스템의 영향인자 연구: 광촉매 주입량, 용존산소, 체류시간,전자포획 첨가금속 (Factors influencing a Photocatalytic System in Circulating Batch Mode: Photocatalyst Dosage, DO, Retention Time and Metal Impurities)

  • 김일규
    • 상하수도학회지
    • /
    • 제27권1호
    • /
    • pp.49-58
    • /
    • 2013
  • A selected halogenated organic contaminant, monochlorophenol was successfully degraded by photocatalytic reaction in a circulating batch system. The photocatalytic degradation in most cases follows first-order kinetics. The photocatalytic reaction rate increased in the $TiO_2$ dosage range of 0.1 g/L to 0.4 g/L, then decreased with further increase of the dosage. Also the degradation rate increased over the range of the retention time from 0.49 min. to 0.94 min., then decreased with further increase of the retention time in the circulating batch reactor. The photocatalytic activity was enhanced by addition of metal impurities, platinum(Pt) and palladium(Pd) onto the photocatalysts. The photocatalytic degradation rate increased with the increase of Pt and Pd in the content range of 0 to 2wt %, then decreased with further increase of the metal contents. Therefore the metal loading to $TiO_2$ influence the degradation rate of a halogenated organic compound by acting as electron traps, consequently reducing the electron/positive hole pair recombination rate.

Photocatalytic degradation of textile dye CI Basic Yellow 28 wastewater by Degussa P25 based TiO2

  • Konecoglu, Gulhan;Safak, Toygun;Kalpakli, Yasemen;Akgun, Mesut
    • Advances in environmental research
    • /
    • 제4권1호
    • /
    • pp.25-38
    • /
    • 2015
  • Wastewaters of textile industry cause high volume colour and harmful substance pollutions. Photocatalytic degradation is a method which gives opportunity of reduction of organic pollutants such as dye containing wastewaters. In this study, photocatalytic degradation of C.I. Basic Yellow 28 (BY28) as a model dye contaminant was carried out using Degussa P25 in a photocatalytic reactor. The experiments were followed out at three different azo dye concentrations in a reactor equipped UV-A lamp (365 nm) as a light source. Azo dye removal efficiencies were examined with total organic carbon and UV-vis measurements. As a result of experiments, maximum degradation efficiency was obtained as 100% at BY28 concentration of $50mgL^{-1}$ for the reaction time of 2.5 h. The photodegradation of BY28 was described by a pseudo-first-order kinetic model modified with the langmuir-Hinshelwood mechanism. The adsorption equilibrium constant and the rate constant of the surface reaction were calculated as $K_{dye}=6.689{\cdot}10^{-2}L\;mg^{-1}$ and $k_c=0.599mg\;L^{-1}min^{-1}$, respectively.

Photodegradation of Butachlor and Pyrazosulfuron-ethyl in Rice Paddy Water under Natural Sunlight

  • Ok, Junghun;Watanabe, Hirozumi;Cho, Junglai;An, Nanhee;Lee, Byungmo
    • 한국환경농학회지
    • /
    • 제33권2호
    • /
    • pp.134-137
    • /
    • 2014
  • BACKGROUND: Dissipation of herbicides in paddy water varies significantly, being dependent on environmental conditions such as sunlight. The photodegradation under natural sunlight may be one of natural degradation routes of herbicides dissipation. Therefore, the aim of this study was to monitor the degradation of butachlor and pyrazosulfuron-ethyl in paddy water under natural sunlight. METHODS AND RESULTS: The 12 water sample bottles of treatment were covered by quart glass plates, which allow about 90% of UV radiation (280-2000 nm) to pass through, to minimize the UV attenuation. The other 12 water sample bottles of the control were covered by glass lids and wrapped with aluminum foils to prevent the sunlight. The concentration of butachlor and pyrazosulfuron-ethyl in paddy water samples bottles was monitored under ambient conditions with and without natural sunlight. The concentration of butachlor and pyrazosulfuron-ethyl for treatment decreased from $355.3{\mu}g/L$ to $37.8{\mu}g/L$ and from $10.5{\mu}g/L$ to $3.9{\mu}g/L$, respectively, during consecutive 21 days after herbicide application under natural sunlight. CONCLUSION: The concentration of butachlor in paddy water decreased quickly under ambient conditions with natural sunlight. The degradation of butachlor in paddy water was enhanced by the natural sunlight. However, the degradation of pyrazosulfuron-ethyl was insignificant under natural sunlight.

토양중(土壤中)에 있어서 제초제(除草劑) Pretilachlor의 분해성(分解性)에 미치는 몇가지 토양특성(土壤特性)의 영향(影響) (Effect of Some Soil Properties on Degradation of Herbicide Pretilachlor in Soils)

  • 문영희;마상용;장익선;양환승
    • Applied Biological Chemistry
    • /
    • 제31권2호
    • /
    • pp.200-204
    • /
    • 1988
  • 토양중(土壤中)에 있어서 제초제(除草劑) pretilachlor의 분해성(分解性)에 미치는 토성(土性), 유기물함량(有機物含量), 온도(溫度), 수분상태(水分狀態)의 영향(影響)에 대하여 연구(硏究)하였다. 토양중(土壤中) pretilachlor의 잔효기간(殘?期間)은 60g a.i./10a 처리수준(處理水準)에서 약(約) 50일(日)였으며, 피에 대하여 GR 50치(値)까지 달하는 기간(期間)은 약(約) $25{\sim}27$일(日)이었다. pretilachlor의 분해속도(分解速度)는 사양토(砂壤土)에서 보다 유기물(有機物)과 점토(粘土)의 함량(含量)이 높았든 사질식양토(砂質植壤土)에서 빨랐다. 토양중(土壤中) pretilachlor의 분해(分解)는 유기물첨가(有機物添加)에 의하여 촉진(促進)되였으며, $20^{\circ}C$에서 보다 $30^{\circ}C$에서, 습윤조건하(濕潤條件下)에서보다 담수조건하(湛水條件下)에서 빨랐다.

  • PDF

Preparation of Nanosized Palladium-Graphene Composites and Photocatalytic Degradation of Various Organic Dyes

  • Kim, Jae Jin;Ko, Weon Bae
    • Elastomers and Composites
    • /
    • 제51권1호
    • /
    • pp.10-16
    • /
    • 2016
  • Nanosized palladium particles were synthesized using palladium(II) chloride, trisodium citrate dihydrate, and sodium borohydride under stirring condition. Nanosized palladium-graphene composites were prepared from palladium nanoparticles, and graphene was enclosed with polyallylamine under stirring condition for 1 h followed by ultrasonication for 3 h. Nanosized palladium-graphene composites were heated in an electric furnace at $700^{\circ}C$ for 2 h and characterized by X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. UV-vis spectrophotometry was used to evaluate the nanosized palladium-graphene composites as a catalyst in the photocatalytic degradation of various organic dyes such as methylene blue, methyl orange, rhodamine B, and brilliant green under ultraviolet light at 254 nm.

Synthesis of SnO2-Mn-C60 Nanocomposites and Their Photocatalytic Activity for Degradation of Organic Dyes

  • Li, Jiulong;Ko, Jeong Won;Ko, Weon Bae
    • Elastomers and Composites
    • /
    • 제52권4호
    • /
    • pp.287-294
    • /
    • 2017
  • Nanocomposites based on $SnO_2-Mn$ were synthesized by the reaction of tin (II) chloride dihydrate and manganese (II) chloride tetrahydrate at a molar ratio of 10:1 in the presence of ammonium hydroxide at $80^{\circ}C$. The $SnO_2-Mn$ nanocomposites were stirred with fullerene [$C_{60}$] in a mass ratio of 2:1 in tetrahydrofuran to prepare $SnO_2-Mn-C_{60}$ nanocomposites; these nanocomposites were obtained upon heating the mixture of $SnO_2-Mn$ nanocomposites and fullerene [$C_{60}$] in an electric furnace at $700^{\circ}C$ for 2 h. The synthesized $SnO_2-Mn-C_{60}$ nanocomposites were confirmed through various characterization methods such as X-ray diffraction and scanning electron microscopy. The photocatalytic activities of the $SnO_2-Mn-C_{60}$ nanocomposites were demonstrated by the degradation of the organic dyes BG, MB, MO, and RhB under 254 nm irradiation and evaluated using UV-Vis spectrophotometry.

Sonochemical Synthesis of $PbMoO_4$ Nanoparticles and Evaluation of its Photocatalytic Activity

  • Uresti, Diana B. Hernandez;De la Cruz, Azael Martinez;Martinez, Leticia M. Torres;Lee, Soo-Wohn
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 춘계학술발표대회
    • /
    • pp.49.2-49.2
    • /
    • 2011
  • $PbMoO_4$ nanoparticles were successfully obtained in the presence of ethylene glycol (EG) with the assistance of a prolonged sonication process. The nanoparticles were characterized by X-ray powder diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), diffuse reflectance spectroscopy (DRS) and adsorption-desorption $N_2$ isotherms (BET). The catalyst prepared sonochemically showed higher photocatalytic activity than $PbMoO_4$ prepared by solid-state reaction in the degradation reactions of rhodamine B (rhB), indigo carmine (IC), orange G (OG), and methyl orange (MO) under UV-Vis light radiation. In order to elucidate aspects of the degradation mechanism of the organic dyes, some experimental variables were modified such as pH, $O_2$ level in solution, and radiation source. In general, the photocatalytic activity for the degradation of organic dyes followed the sequence IC>OG>rhB>MO.

  • PDF

Effects of hypochlorite exposure on morphology and trace organic contaminant rejection by NF/RO membranes

  • Simon, Alexander;Nghiem, Long D.
    • Membrane and Water Treatment
    • /
    • 제5권4호
    • /
    • pp.235-250
    • /
    • 2014
  • The impacts of membrane degradation due to chlorine attack on the rejection of inorganic salts and trace organic contaminants by nanofiltration (NF) and reverse osmosis (RO) membranes were investigated in this study. The rejection of trace contaminants was examined at environmentally relevant concentrations. Changes in the membrane surface morphology were observed as a result of chlorine exposure. A small increase in rejection was consistently observed with all four membranes selected in this study after being exposed to a low concentration of hypochlorite (100 ppm). In contrast, a higher concentration of hypochlorite (i.e., 2000 ppm) could be detrimental to the membrane separation capacity. Membranes with severe chlorine impact showed a considerable decrease in rejection over filtration time, possibly due to rearrangement of the polyamide chains under the influence of chlorine degradation and filtration pressure. The reported results indicate that loose NF membranes are more sensitive to chlorine exposure than RO membranes. The impact of hypochlorite exposure (both positive and negative) on rejection is dependent on the strength of the hypochlorite solution and is more significant for the neutral carbamazepine compound than the negatively charged sulfamethoxazole.

생물학적 유류오염토양 복원제의 현장 적용성 평가 (Field Test Assessment of Biological Recovering Agent for treating Oil Contaminated Soil)

  • 김수홍;송승구;서정호
    • KSBB Journal
    • /
    • 제25권1호
    • /
    • pp.73-78
    • /
    • 2010
  • In this study, recovering agent was produced with organic sludge and modified peat moss (MPM) in pilot plant mixer to recover oil contaminated soil, and field test of it was estimated using landfarming method. Oil contaminated soil recovering agent was thought to contain more microorganisms than raw waste sludge and was no problem to come onto the market because there were not any items of specified wastes. According to the results of TPH variation with time, it was observed the initial degradation velocity of oil with produced recovering agent was rapid up to 50% after 4 days, remarkably. Because the microorganisms in the organic sludge discharged from chemical plant already acclimated with oil, therefore, it could be estimated initial degradation velocity of recovering agent might be rapid. It was concluded that the oil contaminated soil recovering agent produced in this study have high marketability because of its two aspects on recycling of wastes and initial rapid degradation capacity.

Preparation of C60 Nanowhiskers/WO3 Nanocomposites and Photocatalytic Degradation of Organic Dyes

  • Kim, Keun Hyung;Ko, Jeong Won;Ko, Weon Bae
    • Elastomers and Composites
    • /
    • 제50권2호
    • /
    • pp.126-131
    • /
    • 2015
  • $C_{60}$ nanowhiskers were synthesized from $C_{60}$ by liquid-liquid interfacial precipitation (LLIP) using $C_{60}$-saturated toluene and isopropyl alcohol. The $WO_3$ nanoparticles were synthesized by adding $3.8{\times}10^{-4}$ mole amount of ammonium metatungstate hydrate ($H_{26}N_6O_{40}W_{12}{\cdot}H_2O$) to 500 ml of distilled water, and the resulting solution was heated on a hot plate for 4 h. The $C_{60}$ nanowhiskers/$WO_3$ nanocomposites were prepared with $C_{60}$ nanowhiskers and $WO_3$ nanoparticles in an electric furnace at $700^{\circ}C$ in an argon gas atmosphere for 2 h. The $C_{60}$ nanowhiskers/$WO_3$ nanocomposites were characterized by X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. UV-vis spectroscopy was used to evaluate the performance of the $C_{60}$ nanowhiskers/$WO_3$ nanocomposites as a photocatalyst in the degradation of organic dyes, such as methylene blue (MB) and brilliant green (BG) under ultraviolet light (254 nm).