• Title/Summary/Keyword: Optical microscope

Search Result 1,392, Processing Time 0.037 seconds

Characteristics of film-type crystal growth mechanism of CO2 hydrate (CO2 하이드레이트의 film형 결정성장 거동에 관한 연구)

  • Lee, Hyunju;Kim, Soomin;Lee, Ju-Dong;Kim, Yangdo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.2
    • /
    • pp.93-100
    • /
    • 2013
  • Many researches have been carried out to reduce and/or to capture the major global warming gases. Especially, the hydrate formation mechanisms were intensively investigated for carbon dioxide sequestration and storage process applications. In this study, the characteristics of film-type crystal growth mechanism of carbon dioxide hydrate were comprehensively examined. Carbon dioxide hydrate crystal was formed in semi-batch type stir reactor at various pressure conditions while the temperature was fixed to be constant to reduce and minimize the guest gas solubility effects. A supply gas composition was 99.999 % of Carbon dioxide, the observation data was collected by optical microscope adopted CCD camera (Nikon DS-5M/Fi1/2M-U2). This study revealed that the guest gas pressure changes significantly altered the crystal growth mechanism and film growth rate of carbon dioxide hydrate crystal. The critical pressure of the carbon dioxide hydrate of crystal growth mechanism change was found to be 2.0 MPa. The capillary force and gas concentration gradient also significantly changed the film-type crystal growth mechanism of carbon dioxide hydrate crystal.

Fabrication and characterization of Sn-3.0Ag-0.5Cu, Sn-0.7Cu and Sn-0.3Ag-0.5Cu alloys (Sn-3.0Ag-0.5Cu, Sn-0.7Cu 및 Sn-0.3Ag-0.5Cu 합금의 제조 및 특성평가)

  • Lee, Jung-Il;Paeng, Jong Min;Cho, Hyun Su;Yang, Su Min;Ryu, Jeong Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.3
    • /
    • pp.130-134
    • /
    • 2018
  • In the past few years, various solder compositions have been a representative material to electronic packages and surface mount technology industries as a replacement of Pb-base solder alloy. Therefore, extensive studies on process and/or reliability related with the low Ag composition have been reported because of recent rapid rise in Ag price. In this study, Sn-3.0Ag-0.5Cu, Sn-0.7Cu and Sn-0.3Ag-0.5Cu solder bar samples were fabricated by melting of Sn, Ag and Cu metal powders. Crystal structure and element concentration were analyzed by XRD, XRF, optical microscope, FE-SEM and EDS. The fabricated solder samples were composed of ${\beta}-Sn$, ${\varepsilon}-Ag_3Sn$ and ${\eta}-Cu_6Sn_5$ phases.

Role of the periosteum on bone regeneration in rabbit calvarial defects (가토의 두개골 결손부에서 골재생에 끼치는 골막의 역할)

  • Jang, Hyun-Seon;Kim, Sang-Mok;Park, Joo-Cheol;Kim, Byung-Ock
    • Journal of Periodontal and Implant Science
    • /
    • v.35 no.4
    • /
    • pp.939-948
    • /
    • 2005
  • The role of the periosteum on osteointegration of $Bio-Oss^{(R)}$(Geistlich, Wolhusen/Switzerland) was studied in rabbit calvarial defect. 12 New Zealand white male rabbits between 2.8 and 4 kg were included in this randomized, blinded, prospective study. Each rabbit was anesthetized with Ketamine HCl(5 mg/kg) and Xylazine HCl(1.5 ml/kg). An incision was made to the bony cranium and the periosteum was reflected. Using a 6-mm trephine bur(3i. USA), four 8-mm defects were created with copious irrigation. The defects were classified into barrier membrane($Tefgen^{(R)}$, Lifecore Biomedical. Inc, U.S.A.) only group as a control, $Bio-Oss^{(R)}$ with barrier membrane group, $Bio-Oss^{(R)}$ with periosteum covering group, and $Bio-Oss^{(R)}$ without periosteum covering group. There were 2 rabbits in each group. The wound was closed with resorbable suture materials. Rabbits were sacrificed using phentobarbital(100 mg/kg) intravenously at 1, 2, and 4 weeks after surgery. The samples were fixed in 4% paraformaldehyde, and decalcified in hydrochloric acid decalcifying solution(Fisher Scientific, Tustin, CA) at $4^{\circ}C$ for 2-4 weeks. It was embedded in paraffin and cut into 6 ${\mu}m$ thickness. The sections were stained with H & E and observed by optical microscope. The results were as follows; 1. The periosteum played an important role in osteointegration of $Bio-Oss^{(R)}$ in bone defects. 2. When the periosteum remained intact and $Bio-Oss^{(R)}$ was placed on the defect, $Bio-Oss^{(R)}$ with periosteum covering has been incorporated into the newly formed bone from 2-week postoperatively. 3. When the periosteum was removed at the surgical procedure, invasion of connective tissue took place among the granules, and new bone formation was delayed compared to periosteum covering group. Therefore, when the bone grafting was performed with periosteal incision procedure to achieve tension-free suture, the integrity of the overlying periosteum should be maintained to avoid fibrous tissue ingrowth.

HISTOMORPHOMETRIC STUDY OF DENTAL IMPLANTS WITH DOUBLE ACID-ETCHED AND ANODIC OXIDIZED SURFACE IN THE RABBIT TIBIA (토끼 경골에서 치과용 임프란트의 이중 산부식 및 양극 산화 표면처리에 따른 조직계측학적 연구)

  • Han, Ye-Sook;Kim, Il-Kyu;Chang, Keum-Soo;Park, Tae-Hwan;Jeon, Won
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • v.28 no.5
    • /
    • pp.434-444
    • /
    • 2006
  • This study was performed to evaluate the effects of three different implant surface treatments to the bone formation during osseous healing period under unloading conditions. Machined, double-acid etched and anodic oxidized implants were inserted into tibia of 3.0 - 3.5 kg NZ white male rabbits and 2 animals of each group were sacrificed at 2, 4 and 8 weeks. The specimens containing implant was dehydrated and embedded into hard methylmethacrylate plastic. After grinding to $50{\mu}m$, the specimens were stained with Villanueva bone stain. From each specimen, histomorphometric evaluation and the bone implant contact rate were analysed with optical microscope. The results were as follows; 1. In the scanning electronic microscopic examination, machined surface implant had several shallow and paralleled scratches on plain surface, double acid-etched implant had lots of minute wrinkles, rough valley and also irregularly located craters that looked like waves, anodic oxidized surface implant had porosity that minute holes were wholly distributed on the surface. 2. After 2 weeks of implantation, the percentages of bone-to-implant contact in the machined implant, double acid-etched implant and anodic oxidized implant were 26.85%, 62.64% and 59.82%, after 4 weeks of implantation they were 64.29%, 77.85% and 75.23%, and after 8 weeks they were 82.66%, 85.34% and 86.39%. 3. After 2 weeks of implantation, the percentages of bone area between threads in the machined implant, double acid-etched implant and anodic oxidized implant were 21.55%, 42.81%, and 40.33%, after 4 weeks of implantation they were 49.32%, 62.60% and 75.56%, and after 8 weeks they were 71.62%, 87.73% and 83.94%. In summary, percentages of implant surface contacted to bone trabeculae and bone formation area inside threads in double acid-etched implants and anodic oxidized implants were greater than machined implants in early healing stage. These results suggest that double acid-etched and anodic oxidized surface implants could reduce the healing period for osseointegration and may enable to do early function.

Ferroelectric domain inversion in $LiNbO_3$ crystal plate during heat treatment for Ti in-diffusion ($Ti:LiNbO_3$ 도파로 제작을 위한 열처리 과정 동안 강유전 도메인 특성에 미치는 영향)

  • Yang, W.S.;Lee, H.Y.;Kwon, S.W.;Kim, W.K.;Lee, H.Y.;Yoon, D.H.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.3
    • /
    • pp.124-127
    • /
    • 2005
  • It is demonstrated that the annealing process for Ti in-diffusion to z-cut $LiNbO_3$ at temperature lower than the curie temperature in a platinum (Pt) box can cause a ferroelectric micro-domain inversion at the +z surface and Li out-diffusion, therefore which should be avoided or suppressed for waveguide type periodically poled lithium niobate (PPLN) devices. The depth of the inversion layer depends on the Ti-diffusion conditions such as temperature, atmosphere, the sealing method of $LiNbO_3$ in the Pt box and crystal orientation is experimentally examined. The result shows that the polarization-inverted domain boundary appears at the only +z surface and its thickness is about $1.6{\mu}m$. Also, for the etched $LiNbO_3$, surface the domain shape was observed by the optical microscope and atomic force microscopy (AEM), and distribution of the cation concentrations in the $LiNbO_3$ crystal by the secondary ion mass spectrometry (SIMS).

Surface reaction of $HfO_2$ etched in inductively coupled $BCl_3$ plasma ($BCl_3$ 유도결합 플라즈마를 이용하여 식각된 $HfO_2$ 박막의 표면 반응 연구)

  • Kim, Dong-Pyo;Um, Doo-Seunng;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.477-477
    • /
    • 2008
  • For more than three decades, the gate dielectrics in CMOS devices are $SiO_2$ because of its blocking properties of current in insulated gate FET channels. As the dimensions of feature size have been scaled down (width and the thickness is reduced down to 50 urn and 2 urn or less), gate leakage current is increased and reliability of $SiO_2$ is reduced. Many metal oxides such as $TiO_2$, $Ta_2O_4$, $SrTiO_3$, $Al_2O_3$, $HfO_2$ and $ZrO_2$ have been challenged for memory devices. These materials posses relatively high dielectric constant, but $HfO_2$ and $Al_2O_3$ did not provide sufficient advantages over $SiO_2$ or $Si_3N_4$ because of reaction with Si substrate. Recently, $HfO_2$ have been attracted attention because Hf forms the most stable oxide with the highest heat of formation. In addition, Hf can reduce the native oxide layer by creating $HfO_2$. However, new gate oxide candidates must satisfy a standard CMOS process. In order to fabricate high density memories with small feature size, the plasma etch process should be developed by well understanding and optimizing plasma behaviors. Therefore, it is necessary that the etch behavior of $HfO_2$ and plasma parameters are systematically investigated as functions of process parameters including gas mixing ratio, rf power, pressure and temperature to determine the mechanism of plasma induced damage. However, there is few studies on the the etch mechanism and the surface reactions in $BCl_3$ based plasma to etch $HfO_2$ thin films. In this work, the samples of $HfO_2$ were prepared on Si wafer with using atomic layer deposition. In our previous work, the maximum etch rate of $BCl_3$/Ar were obtained 20% $BCl_3$/ 80% Ar. Over 20% $BCl_3$ addition, the etch rate of $HfO_2$ decreased. The etching rate of $HfO_2$ and selectivity of $HfO_2$ to Si were investigated with using in inductively coupled plasma etching system (ICP) and $BCl_3/Cl_2$/Ar plasma. The change of volume densities of radical and atoms were monitored with using optical emission spectroscopy analysis (OES). The variations of components of etched surfaces for $HfO_2$ was investigated with using x-ray photo electron spectroscopy (XPS). In order to investigate the accumulation of etch by products during etch process, the exposed surface of $HfO_2$ in $BCl_3/Cl_2$/Ar plasma was compared with surface of as-doped $HfO_2$ and all the surfaces of samples were examined with field emission scanning electron microscopy and atomic force microscope (AFM).

  • PDF

Study on the Non-isothermal Crystallization Kinetics of Branched Polypropylene (분지형 폴리프로필렌의 비등온결정화 거동 연구)

  • Yoon, Kyung-Hwa;Shin, Dong-Yup;Kim, Youn-Cheol
    • Polymer(Korea)
    • /
    • v.36 no.2
    • /
    • pp.245-250
    • /
    • 2012
  • Branched polypropylenes (PP) with long chain branch were prepared by solid state reaction with three different branching agent of 0.3 wt% content. The chemical structures, non-isothermal crystallization behavior and complex viscosity of the branched PP were investigated by FTIR, DSC, optical microscope, and dynamic rheological measurement. The chemical structure of the branched PP was confirmed by the existence of =C-H stretching peak of the branching agent at 3100 $cm^{-1}$. There was no distinct change in melting temperature in case of PP-D-0-3 and PP-F-0-3, but PP-H-0-3 indicated a decrease in melting temperature. The decrease in melting temperature was interpreted by the fact that the degradation reaction of PP was more dominant than branched reaction, and confirmed by a decrease in complex viscosity. The non-isothermal crystallization behavior of the branched PP was analyzed using by Avrami equation. The Avrami exponent of PP was 3, and the values of the branched PP with DVB and FS were below 3. The activation energy of PP calculated by Kissinger method was 25 kJ/mol, and there were no big difference in activation energies of the branched PPs compared to PP.

Manufacturing of Metal Micro-wire Interconnection on Submillimeter Diameter Catheter (서브-밀리미터 직경의 카테터 표면 위 금속 마이크로 와이어 접착 공정)

  • Jo, Woosung;Seo, Jeongmin;Kim, Taek-Soo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.24 no.2
    • /
    • pp.29-35
    • /
    • 2017
  • In this paper, we investigated a manufacturing process of metal micro-wire interconnection on submillimeter diameter catheter. Over the years, flexible electronic researches have focused on flexible plane polymer substrate and micro electrode manufacturing on its surface. However, a curved polymer substrate, such as catheter, is very important for medical application. Among many catheters, importance of submillimeter diameter steerable catheter is increasing to resolve the several limitations of neurosurgery. Steering actuators have been researched for realizing the steerable catheter, but there is no research about practical wiring for driving these actuators. Therefore we developed a new manufacturing process for metal micro-wire interconnection on submillimeter diameter catheter. We designed custom jigs for alignment of the metal micro-wires on the submillimeter diameter catheter. An UV curing system and commercial products were used to reduce the manufacturing time and cost; Au micro-wire, UV curable epoxy, UV lamp, and submillimeter diameter catheter. The assembled catheter was characterized by using an optical microscope, a resistance meter, and a universal testing machine.

A Study on the Effectiveness of Remanufacturing Technology for the Catalyzed Diesel Particulate Filter-trap(DPF) Deactivated by Diesel Exhaust Gas (촉매가 담지된 사용후 경유차 매연저감장치 DPF의 재제조 효과에 관한연구)

  • Choi, Kang-Yong;Park, Hea-Kyung
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.32 no.10
    • /
    • pp.957-964
    • /
    • 2010
  • The deactivated catalyzed diesel particulate filter-trap (DPF) was remanufactured by ultrasonic wave treatment with various prepared solutions, followed by active component re-impregnation, and the emission control performance and surface properties of remanufactured DPF were studied at various remanufacturing conditions. The proper ultrasonic wave cleaning time at various prepared solutions and optimal re-impregnation amounts of active component for the best emission control performance of DPF were investigated and its performance tests were also carried out with various temperatures for the conversions of CO, THC (total hydrocarbon) and PM (particulate matter) by catalytic reaction test unit using bypass gas from the diesel engine dynamo system. It was found that the emission control performance of DPF remanufactured with the high-temperature air washing, ultrasonic wave cleaning at acid/base solutions and active component re-impregnation method was recovered to 95% level of its activity compared to that of the fresh DPF, which was caused by removing the deactivating materials from the surface of the DPF, through the analyses of performance test and their surface characterization by Optical microscope, EDX, ICP, TGA, and porosimeter.

Delphinidin Chloride Effects on the Expression of TNF-$\alpha$ Induced Cell Adhesion Molecules (TNF-$\alpha$에 의해 유도된 세포부착분자의 발현에 대한 Delphinidin chloride의 억제 효과)

  • Koh, Eun-Gyeong;Chae, Soo-Chul;Seo, Eun-Sun;Na, Myung-Suk;Lee, Jong-Bin
    • Korean Journal of Environmental Biology
    • /
    • v.27 no.1
    • /
    • pp.88-94
    • /
    • 2009
  • The process of atherosclerosis begins through secretion of inflammatory cytokine or adhesion of leukocyte from damage in blood vessels and transmigration. This study was conducted to investigate the effects of delphinidin chloride (DC) in the initial process of atherosclerosis on the expression of ICAM-1 (Intracellular Adhesion Molecule-1) and VCAM-1 (Vascular Adhesion Molecule-1) related to adhesion of leukocyte at the HUVEC (human umbilical vein endothelial cell line. As a result, cell growth inhibition rate at 50 ${\mu}M$ was respectively 4, 3 and 5% without cell toxicity. As a result of morphological observation monocyte-endothelial cell adhesion assay and optical microscope carried out to measure attachment of mononuclear cells to endothelial cells induced by Tumor necrosis factor-alpha (TNF-$\alpha$) at concentrations without cell toxicity, DC concentration-dependently suppressed attachment. When effects on the expression of VCAM-1 and ICAM-1, cell adhesion molecules induced from endothelial cells by TNF-$\alpha$, were comparatively analyzed using western blot analysis and RT-PCR methods, protein of VCAM-1 and ICAM-1 and expression at the level of mRNA were concentration-dependently reduced. Taken together, the results of this studies provide evidence that DC possess an anti-metastatic activity.