• Title/Summary/Keyword: One side friction test

Search Result 12, Processing Time 0.022 seconds

Effect of Different Annealing Temperatures on Friction Characteristic and Formation of Coatings in Galvannealed sheet steels (GA 강판의 합금화 온도가 도금층 형성 및 마찰 특성에 미치는 영향)

  • Lee Jung-Min;Jun Sung-Jin;Kim Dong-Hwan;Kim Byung-Min
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.1012-1015
    • /
    • 2005
  • This paper is designed to estimate friction and powdering characteristic of coating layer on galvannealed sheet steel with different annealing temperature, which is 465, 505, 515 and $540^{\circ}C$. Estimations of powdering and friction were done using a $60^{\circ}$ bending test and one side friction test, respectively. In order to obviously understand the effect of coatings on friction cross-section of coatings before and after friction test was also observed by SEM. The results show that powdering of coatings is increased with increasing of annealing temperature and that friction characteristic greatly depends on powdering which leads to increase of real contact area between tools and coatings.

  • PDF

Evaluation of Frictional Characteristic of Galvannealed sheet steel with different annealing temperatures at Lower Normal Loads (저면압 영역에서 합금화 온도에 따른 합금화용융아연도금 강판의 마찰특성 평가)

  • Lee Jung-Min;Jeon Seong-Jin;Kim Dong-Hwan;Kim Dong-Jin;Park Sung-Ho;Kim Byung-Min
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.23 no.4 s.181
    • /
    • pp.109-115
    • /
    • 2006
  • This paper is designed to estimate friction and powdering characteristic of coating layer on galvannealed sheet steel with different annealing temperature, which is 465, 505, 515 and $540^{\circ}C$, Estimations of powdering and friction were done using a $60^{\circ}$ bending test and one side friction test, respectively. In order to obviously understand the effect of coatings on friction cross-section of coatings before and after friction test was also observed by SEM. The results show that powdering of coatings is increased with increasing of annealing temperature and that friction characteristic greatly depends on powdering which leads to increase of real contact area between tools and coatings.

Bearing Capacity and Control Method of Driven Piles (기성말뚝의 지지력 거동해석과 시공관리방안)

  • 박영호;김경석
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1999.03a
    • /
    • pp.249-258
    • /
    • 1999
  • Dynamic load and static load tests are performed on steel pipe piles and concrete piles at five construction sites in highway to compare the difference of load bearing mechanisms. At each site, one steel pile is instrumented with electric strain gages and dynamic tests are performed on the pile during installation. Damages of strain gages due to the installation are checked and static test is performed upon the same pile after two or seven days as well. It shows that load transfer from side friction to base resistance behaves somewhat differently according to the results of load-settlement analysis obtained from PDA and static load test. Initial elastic stage of load settlement curves of two load tests is almost similar. But after the yielding point, dynamic resistance of pile behaves more stiffer than static resistance, thus, dynamic load test result might overestimate the real pile capacity compared with static result. Analysis of gage readings shows that unit skin friction increases exponentially with depth. The skin friction is mobilized at the 1∼2m above the pile tip and contributes to the considerable side resistance. Comparison of side and base resistances between the measured value and the calculated value by Meyerhof's bearing capacity equation using SPT N value shows that the calculated base resistance is higher than the measured. Therefore, contribution of side resistance to total capacity shouldn't be ignored or underestimated. Finally, based upon the overall test results, a construction control procedure is suggested.

  • PDF

Development of Side Impact Crash Simulation Methodology and Its Applications (측면충돌모의시험 방법 개발과 응용)

  • 하영호
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.8 no.1
    • /
    • pp.101-109
    • /
    • 2000
  • Occupant protection in the side impact of a car became one of the most important issues of car crashworthiness due to high injury level in a side impact crash. An accurate simulation of the side impact crash is an essential tool for the reduction of development time and cost for side impact safety system. This paper describes a new test methodology that can accurately generate the crash pulses of a vehicle and a door in a very cost-effective manner, and then evaluates the injury values of the dummy for the various sled pulses. This test methodology is simple and easy to approach because the door velocity is controlled by the hydraulic actuator and brake and the seat velocity is only adjusted by the friction force of the hydraulic brake. The superiority of the proposed test methodology is proven by the evaluation of dummy's injury values according to the change of the pressure of the hydraulic brake and by the application as a tool for the development of side airbag.

  • PDF

Comparison between US NCAP and IIHS Side Impact Tests and a Study of Noise Factors of Side Impact Tests (US NCAP 및 IIHS 측면 충돌 시험법간 특성 비교 및 시험 시 오차 인자에 의한 영향 검토)

  • Junsuk Bae;Ho Kim;Young Myoung So
    • Journal of Auto-vehicle Safety Association
    • /
    • v.16 no.1
    • /
    • pp.12-20
    • /
    • 2024
  • Side impact with MDB (moving deformable barrier) is common in side crash test protocols around the globe, most of which are quite similar to that of US NCAP side impact protocol but IIHS side impact protocol is considered to be the most harsh one due to the MDB's weight and impact speed. In this study US NCAP side impact and IIHS side impact test conditions are compared with respect to delta-V (impulse of the test vehicle), roll speed, and yaw speed as well as survival space (the smallest distance between the front driver seat cushion center to B pillar after the test). Error factors (friction between tire and ground, tolerance of vertical and longitudinal position of the MDB with respect to the test vehicle), which are resident in the test protocol is studied with respect to the global vehicle behavior (delta-V, roll, yaw) as well as survival space.

Side Friction of Deep Foundation for Transmission Tower in Rock (암반에 설치된 송전철탑 심형기초의 주면마찰력 평가)

  • Kim, Dae-Hong;Lee, Dae-Soo;Chun, Byung-Sik;Kim, Byung-Hong
    • Journal of the Korean Geotechnical Society
    • /
    • v.23 no.4
    • /
    • pp.149-160
    • /
    • 2007
  • Six prototype field tests (five 1/8 and one 1/2 scale tests) have been conducted in order to determine the uplift resistance of deep foundation for transmission line structures. Test sites, located in the city of Eumseng in Choongbuk province, are classified as gneiss. These test results reveal failures not along the foundation-rock interface but either along the damaged surrounding rock mass caused by excavation or along the pre-existing rock joint. Test results also show the uplift resistance which is 20 $\sim$ 30% higher than the current design strength of side friction. In addition to fold tests, four concrete core samples between the liner plate and the surrounding rock mass have been obtained from the existing transmission foundations to study the effect of the liner plate which is installed prior to placing concrete. The compressive strength of these concrete core samples shows 63 $\sim$ 72% of the strength at the time of foundation construction. Side frictional resistance based on such less compacted concrete reaches satisfying uplift design strength.

An Experimental Study for Drainage Capacity Increment at Surcharged Manholes with a 90° Bend (과부하 90° 접합맨홀의 배수능력 증대에 관한 실험 연구)

  • Kim, Jung Soo;Song, Ju Il;Yoon, Sei Eui
    • Journal of Korean Society of Water and Wastewater
    • /
    • v.23 no.4
    • /
    • pp.447-458
    • /
    • 2009
  • Energy loss at manholes, often exceeding friction loss of pipes under surcharged flow, is considered as one of the major causes of inundation in urban areas. Therefore, it is necessary to analyze head loss at manholes, especially in case of surcharged flow. Hydraulic experiments were conducted with three cases. Case A is to test whether the shapes of the manholes influence head loss coefficients. Case B and C were proposed to further reduce head losses by improving the manhole hydraulic efficiency. In case B, the joining part of the pipe at both shapes of manholes is shifted from central part to side part. The test in case C is to check the average head loss coefficient by installing the side benching in square manhole, based on shifted joining part model. The average head loss coefficient for circular and square manhole on case A was 1.6. This did not show much difference of the head loss coefficients in spite of the discharge variation in this case. However, case B and C show large difference between head loss coefficients due to the strong oscillation of water surface and the horizontal swirl motion. The circular and square manholes in case B reduced the head loss by 30% and 6% than ones in case A, respectively. The average head loss coefficient for circular manhole in case B was 1.1. Case C reduced average loss coefficients of the square manhole in case A from 1.6 to 1.1. Accordingly, the circular manhole in case B and the square manhole in case C showed the effective way to reduce the head loss. These head loss coefficients could be available to apply to the urban sewer system with surcharged flow.

Skin Friction Mobilized on Pack Micropiles Subjected to Uplift Force (인발력을 받는 팩마이크로파일의 주면마찰력)

  • Hong, Won-Pyo;Cho, Sam-Deok;Choi, Chang-Ho;Lee, Choong-Min
    • Journal of the Korean Geotechnical Society
    • /
    • v.28 no.6
    • /
    • pp.19-29
    • /
    • 2012
  • Pack micropiles were recently developed to improve pile capacity of general micropiles. Pack micropiles were made by warping thread bar or steel pipe of general micropile by geotexlile pack and grouting inside the pack with pressure. According to the pressure, the boring hole could be enlarged. A series of pile uplift tests were performed on three micropiles. Two out of the three piles were the pack micropiles and the other was the general micropile, in which a thread bar was used in the boring hole. According to the pressure applied to the pack micropiles, the diameter of boring hole was enlarged from 152 mm to 220 mm. Unit skin friction mobilized on side surfaces of micropiles increased with displacement of pile head and reached on a constant value, which represents that the relative displacement between piles (or thread bar) and soils was reached on critical state. And the uplift resistance of pack micropile was higher than that of general micropile. Two reasons can be considered: One is that the frictional surface increases due to enlarging diameter of boring holes and the other is that the unit skin friction could increase due to compressing effect of surrounding soils by soil displacement as much as the enlarging volume of boring hole. The compression effect appeared at deeper layer rather than surface layer. The unit skin friction mobilized on micropiles with small diameter was higher than the ones on large bored piles.

Comparison of Performance between Regular Drilled Shaft and Isolation Tube Drilled Shafts (일반 현장 타설 말뚝과 분리형 현장 타설 말뚝의 거동 비교)

  • Kim, Myung-Hak;O'Neill, Michael W.
    • Journal of the Korean Geotechnical Society
    • /
    • v.16 no.1
    • /
    • pp.211-220
    • /
    • 2000
  • An experimental study that included detailed observation of four 305-mm-diameter drilled shafts, one reference shaft of standard design and three test shafts with isolation tubes to mitigate skin friction in the vadose zone of a clay soil profile, is described. The shafts were loaded only by naturally expanding and contraction soil over a period of 17 months. The soil at the test site was instrumented to track suction and elevation changes. Maximum ground surface movements exceeding 40 mm were observed. Heave movements of less than 1.5 mm were observed in the test shafts with isolation tubes, while movements of 5 mm were observed in the reference shaft. Unit side shear loads in the shafts protected by the isolation tubes were minimal compared to those measured in the reference shaft. This indicates that the isolation tubes were very effective.

  • PDF

Effect of Rib Arrangement on Heat Transfer in the Divergent Channel (확대 채널에서 리브 배열이 열전달에 미치는 효과)

  • Lee, Myung-Sung;Lee, Gyeong-Ju;Kim, Sang-Moon;Min, Se-Chan;Bae, Jae-Moon;Hwang, Jun-Su;Park, Cheol-O;Kim, Dong-Chan;Jung, Jung-Hyeon;Ahn, Soo-Whan
    • Journal of Power System Engineering
    • /
    • v.21 no.5
    • /
    • pp.35-40
    • /
    • 2017
  • The effects of the different rib geometries such as V-shaped continuous (case A), parallel broken (case B), and V-shaped broken (case C) ribs on the heat transfer and pressure drops in a divergent channel with $45^{\circ}$ inclined ribs on one wall or two walls are checked out. The top and bottom walls are adiabatic; two side walls are uniformly heated in the divergent rectangular channel. The tested Reynolds numbers are ranged from 22,000 to 75,000. The channel with two opposite walls inclined only has the length of test section of 1 m and the channel divergence ratio of $D_{ho}/D_{hi}=1.49$, corresponding to $1.43^{\circ}$ inclined walls. The results show in the identical pumping power that the V-shaped continuous rib (case A) with two ribbed walls is the greatest, but the parallel broken rib (case B) with one ribbed wall is the worst in the thermal performance.