Hot Corrosion Behavior of Al-Y Coated Haynes 263 in Lithium Molten Salt under Oxidation Atmosphere (리튬용융염계 산화성분위기에서 Al-Y 코팅한 Haynes 263의 고온 부식거동)

  • Cho Soo-Hang;Lim Jong-Ho;Chung Jun-Ho;Seo Chung-Seok;Park Seoung-Won
    • Korean Journal of Materials Research
    • /
    • v.15 no.3
    • /
    • pp.155-160
    • /
    • 2005
  • The electrolytic reduction of spent oxide fuel involves the liberation of oxygen in a molten LiCl electrolyte, which results in a chemically aggressive environment that is very corrosive fir typical structural materials. So, it is essential to choose the optimum material f3r the process equipment handling molten salt. In this study, the corrosion behavior of Al-Y coated Haynes 263 in a molten salt of $LiCl-Li_2O$ under oxidation atmosphere was investigated at $650^{\circ}C$ for $72\~168$ hours. The corrosion rate of Al-Y coated Haynes 263 was low while that of bare Haynes 263 was high in a molten salt of $LiCl-Li_2O$. Al-Y coated Haynes 263 improved the corrosion resistance better than bare Haynes 263 alloy. An Al oxide layer acts as a protective film which Prohibits Penetration of oxygen. Corrosion Products were formed $Li(Ni,Co)O_2$ and $LiTiO_2$ on bare Haynes 263, but $LiAlO_2,\;Li_5Fe_5O_8\;and\;LiTiO_2$ on Al-Y coated Haynes 263.

In vitro evaluation of resistance to sliding in self-ligating and conventional bracket systems during dental alignment

  • Cordasco, Giancarlo;Giudice, Antonino Lo;Militi, Angela;Nucera, Riccardo;Triolo, Giuseppe;Matarese, Giovanni
    • The korean journal of orthodontics
    • /
    • v.42 no.4
    • /
    • pp.218-224
    • /
    • 2012
  • Objective: To investigate the resistance to sliding (RS) in self-ligating and conventional ligation bracket systems at 5 different second-order bracket angulations by using low-stiffness alignment wires in a 3-bracket experimental model and to verify the performance of the main RS components in both systems when these wires are used. Methods: Interactive self-ligating brackets with closed and open slides were used for the self-ligating (SL) and conventional ligation (CL) groups, respectively; elastomeric ligatures (1 mm inner diameter) were used in the latter system. The alignment wire used was 0.014 inch heat-activated NiTi (austenitic finish temperature set at $36^{\circ}C$ by the manufacturer). A custom-made testing machine was used to measure frictional resistance. Tests were repeated 5 times at every angulation simulated. All data were analyzed statistically. Results: The RS increased significantly with increasing angulation in both SL and CL groups (p < 0.0001). However, the RS values were significantly higher at every angulation (p < 0.0001) in the CL group. Conclusions: Despite the relevance of the binding phenomenon, ligation forces predominantly affect the RS when lowstiffness alignment wires are used.

Synthesis of Pentadentate Nitrogen-Oxygen(N3-O2) Ligands with Substituents and the Determination of Stability Constants of Their Heavy(II) Metal Complexes (치환기를 가진 질소-산소(N3-O2)계 리간드 합성과 중금속(II)이온 착물의 안정도상수 결정)

  • Kim, Sun-Deuk;Seol, Jong-Min
    • Journal of Environmental Science International
    • /
    • v.20 no.6
    • /
    • pp.687-700
    • /
    • 2011
  • A new $N_3-O_2$ pentadentate ligand, H-BHPT, was synthesized. Hydrochloric acid salts of Br-BHPT, Cl-BHPT, $CH_3O$-BHPT and $CH_3$-BHPT, having Br-, Cl-, $CH_{3-}$ and $CH_3O-$ substituents at the para position of the phenol hydroxyl group of H-BHPT were synthesized. Hydrochloric acid salts of 3OH-BHPT and 4OH-BHPT, having different position of the phenol hydroxyl group of H-BHPT were also synthesized. The synthesis of each ligand was confirmed by C. H. N. atomic analysis and $^1H$ NMR, $^{13}C$ NMR, UV-visible, and mass spectra. The calculated proton dissociation constants ($log{K_n}^H$) of the phenol hydroxyl group and secondary amine group of the synthesized $N_3-O_2$ ligands showed five steps of the proton dissociations. The order of the overall proton dissociation constants ($log{\beta}_p$) of the ligands was Br-BHPT < Cl-BHPT < H-BHPT < $CH_3O$-BHPT < $CH_3$-BHPT. The order agreed with that of Hammett substituent constants (${\delta}_p$). However, dissociation steps of 3OH-BHPT were four and that of 4OH-BHPT was three. The calculated stability constants ($logK_{ML}$) between the ligands and transition metal ions agreed with the order of $log{\beta}_p$ values of the ligands. The order of the stability constants between the transition metal ions with the synthesized ligands was Co(II) < Ni(II) < Cu(II) > Zn(II) > Cd(II) > Pb(II). The order agreed well with that of the Iriving-Williams.

Characteristics of Urease from Vibrio parahaemolyticus Possessing tah and the Genes Isolated in Korea

  • Kim, Young-Hee;Kim, Jong-Sook
    • Journal of Microbiology
    • /
    • v.39 no.4
    • /
    • pp.279-285
    • /
    • 2001
  • Vibrio parahaemolyticus is a halophilic bacterium associated with seafood gastroenteritis. An unusual strain of Kanagawa-positive urease producing Vibrio parahaemolyticus O1:K1 was isolated from the environment and identified . A polymerase chain reaction assay revealed that this strain harbored both the tdh and the genes. The urease from this strain was studied. Maximum urease production was induced in LB medium containing 0.2% urea, 0.5% glucose, 2% NaCl and pH 5.5 with 6h of culti-vation at 37$\^{C}$ under aeration. Purification of urease was achieved by the process of whole cell lysate, 65% ammonium sulphate precipitation, DEAE-cellulose ion exchange column chromatography, Sepharose CL-6B gel filtration and oxirane activated Sepharose 6B-urea affinity chromatography with 203 fold purification and 2.2% yield. Analysis of the purified enzyme by SDS-PAGE demonstrated the presence of the subunits with a molecular weight of 85kDa, 59kDa, 41kDa and the molecular weight for the native enzyme by nondenaturing PAGE and gel filtration chromatography was 255kDa. The purified urease was stable at pH 7.5 and the opeimal pH in HEPES buffer was 8.0 The enzyme was stable at 60$\^{C}$ for 2 h with a residual activity of 32% . The addition of 10$\mu$M if NiCl$_2$maintained stability for 30 min. The Km value of the purified enzyme was 35.6 mM in urea substrate. The TD$\_$50/(median toxic dose) of the purified urease was 2.5$\mu\textrm{g}$/ml on human leukemia cells.

  • PDF

Chemical Compositions and Spatial Distribution Analysis of Fall-Out Particles in Suwon Area (수원지역 강하분진의 화학조성및 공간분포 분석)

  • 김현섭;이태정;김동술
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.15 no.1
    • /
    • pp.23-32
    • /
    • 1999
  • Deposition is one of the important removal mechanisms for the ambient aerosol, and it also leads to adverse environmental and economic impacts. The purpose of this study was to investigate chemical compositions and spatial distributions of fall-out aerosols. A total number of 340 samples were collected at 35 sampling sites in Suwon area from January to November, 1996. Twelve inorganic elements (Al, Ba, Cd, Cr, K, Pb, Sb, Zn, Cu, Fe, Ni, and V) and eight ionic components ($F^-$, Cl, $NO_3^-$, $SO_4^{2-}$, $Na^+$, $NH_4^+$, $Mg^{2+}$, and $Ca^{2+}$) were analyzed by AAS and IC, respectively. The monthly variation showed that the flux of fall-out particles was increased in the spring season(March, April, and May) and decreased from August to October. Arithmetic mean flux of fall-out particles was 176.8 kg/$ extrm{km}^2$/day during the study period. The fluxes of each chemical species were $SO_4^{2-}$ 12.414, $Ca^{2+}$ 7.369, $NO_3^-$ 5.812, $Cl^-$ 3.566, $NH_4^+$ 3.176, Fe 3.107 kg/$\textrm{km}^2$/day, and so on. By using a kriging analysis, spatial distribution pattern of those fluxes was intensively studied. Total fluxes estimated in Suwon city were 8424.72t/y of fall-out particles, 519.27t/y of $SO_4^{2-}$, 336.79t/y of $Ca^{2+}$,267.34 t/y of $NO_3^+$, 155.36t/y of $Cl^-$, 147.79t/y of Fe.

  • PDF

Synthesis and Properties of Tetraaza Macrocycles Containing Two 3-Pyridylmethyl, 4-Pyridylmethyl, or Phenylmethyl Pendant Arms and Their Nickel(Ⅱ) and Copper(Ⅱ) Complexes: Effects of the Pendant Arms on the Complex Formation Reaction

  • Kang, Shin-Geol;Kim, Seong-Jin
    • Bulletin of the Korean Chemical Society
    • /
    • v.24 no.3
    • /
    • pp.269-273
    • /
    • 2003
  • The synthesis and properties of 2,13-bis(3'-pyridylmethyl) $(L^3)$, 2,13-bis(4'-pyridylmethyl) $(L^4)$, and 2,13-bis(phenylmethyl) $(L^5)$ derivatives of 5,16-dimethyl-2,6,13,17-tetraazatrcyclo$[16.4.0.^{1.18}0^{7.12}]$docosane are reported. The 3- or 4-pyridylmethyl groups of $[ML^3](ClO_4)_2\;or\;[ML^4](ClO_4)_2$ (M = Ni(Ⅱ) or Cu(Ⅱ)) are not involved in coordination, and the coordination geometry (square-planar) and ligand field strength of the complexes are quite similar to those of $[ML^5](ClO_4)_2$, bearing two phenylmethyl pendant arms. However, the complex formation reactions of $L^3\;and\;L^4$ are strongly influenced by the pyridyl groups, which can interact with a proton or metal ion outside the macrocyclic ring. The macrocycle $L^5$ exhibits a high copper(Ⅱ) ion selectivity against nickel(Ⅱ) ion; the ligand readily reacts with copper(Ⅱ) ion to form $[CuL^5]^{2+}$ but does not react with hydrated nickel(Ⅱ) ion in methanol solutions. On the other hand, $L^3\;and\;L^4$ form their copper(Ⅱ) and nickel(Ⅱ) complexes under a similar condition, without showing any considerable metal ion selectivity. The ligands $L^3\;and\;L^4$ react with copper(Ⅱ) ion more rapidly than does $L^5$ at pH 6.4. At pH 5.0, however, the reaction rate of the former macrocycles is slower than that of the latter. The effects of the 3- or 4-pyridylmethyl pendant arms on the complex formation reaction of $L^3\;and\;L^4$ are discussed.

The Influence of Chemical Compositions of Weld Metal and Welding Conditions on Hot Cracking by Hot Cracking Test (Inconel 690 오버레이용접부의 고온균열 발생에 미치는 용접금속의 화학조성 및 용접조건의 영향)

  • 양병일;지병하;김정태;박광식;최해수;박화순
    • Journal of Welding and Joining
    • /
    • v.20 no.3
    • /
    • pp.74-83
    • /
    • 2002
  • In order to investigate the hot cracking phenomena of the Inconel 690 overlay welds, the hot cracking test(modified Varestraint test) was performed by varying augmented strain and welding speed in GTAW. A total of five kinds of specimens was used in the hot cracking test. The specimens used were two kinds of one layer specimens that were composed of just Inconel 690 deposited metal and three kinds of double layer specimens that were composed with as upper part of Inconel 690 weld metal and lower part of SA508 cl.3 or STS 309L. The main results are as fo11ows: In the welds composed of just Inconel 690, as the augmented strain was more increased and the welding speed was more decreased, the extent of cracking was more increased. And these cracks were mainly solidification cracks, and liquation cracks were also observed partially in HAZ. And hot cracking susceptibily of Inconel 690 welds by using filler metals containing Nb were higher than that of the welds with Nb free. The hot cracking susceptibility of Inconel 690 weld metal was increased with dilution of SA 508 cl.3 and STS 309L, and the influence of SA 508 cl.3 was higher than that of 575 309L. The results of calculation of $TSC\Delta$ and $TLC\Delta$ in Inconel 690 weld metal changed by dilution with base metal or neighboring welds were agreed well with the results of hot cracking test in this study. Therefore, it was expected that the hot cracking was considerably decreased or prevented by using proper welding conditions such as lower heat input, filler metals, base metal and neighboring welds.

Composition of Chemical Components and Amount of Natural Supplies by Precipitation in Chinan Area of Chonbuk Province (전북 진안지역 강우의 화학성분 조성 및 천연공급량)

  • Han, Kang-Wan;Cho, Jae-Young;Son, Jae-Gwon
    • Korean Journal of Environmental Agriculture
    • /
    • v.17 no.4
    • /
    • pp.291-295
    • /
    • 1998
  • Changes of chemical components and natural supplies by precipitation at agricultural zone in Chinan area of Chonbuk province from May 1, 1997 to April 30, 1998 were investigated. pH of precipitation ranged $6.44{\sim}7.24$ and EC showed $14.23{\sim}30.67{\mu}S/cm$. The $total{\sim}N$, NH4-N and NO3-N were $1.43{\sim}10.14$, $0.57{\sim}4.39$, and $0.18{\sim}1.69㎎/L$ respectively. The content of total-P showed $0.015{\sim}0.087㎎/L$ but ortho-P was not detected. The content of suspended solid, $Ca^{++}$, $Mg^{++}$, $Na^+$ and $K^+$ showed $3.6{\sim}15.3$, $0.37{\sim}1.66$, $0.17{\sim}0.52$, $0.22{\sim}0.87$, and $0.17{\sim}0.58㎎/L$. The content of SO42- and Cl- showed $3.37{\sim}014.47㎎/L$ and $1.02{\sim}7.24㎎/L$ respectively. Only Cu and Zn of heavy metals were detected $0{\sim}0.019㎎/L$ and $0.009{\sim}0.098㎎/L$ but Cd, Cu, Ni and Cr were not detected. Natural supplies of chemical components were 39.48㎏/ha/yr of total-N, 21.82㎏/ha/yr of $NH_4-N$, 6.90㎏/ha/yr of $NO_3-N$ and 0.68㎏/ha/yr of total-P. Also $Ca^{++}$, $Mg^{++}$, $Na^+$, $K^+$, $SO_4^{2-}$ and $Cl^-$ were supplied 14.46, 5.00, 7.26, 5.46, 98.76 and 31.16㎏/ha/yr respectively. Only of heavy metals were supplied 0.024㎏/ha/yr of Cu and 0.044㎏/㏊/yr of Zn.

  • PDF

Regiospecific Orientation of Single-chain Antibody and Atomic Force Microscope (AFM) Images

  • Kyusik Yun;Park, Seonhee;Hyeonbong Pyo;Kim, Seunghwan;Lee, Sooyeul
    • Biotechnology and Bioprocess Engineering:BBE
    • /
    • v.4 no.1
    • /
    • pp.72-77
    • /
    • 1999
  • An antibody containing a genetically engineered lipid group at the N-termunus and a hexahistidinyl tag at the C-terminus (Lpp-scF-His6) was immobilized in an oriented manner on the surface of liposome. Liposomes, consisting of antibody and phosphatidyl-choline, have been prepared and imaged by AFM. For AFM visualization, the resulting liposomes were bound on the surface of mica by two different mechanisms. The histidine tags present in the antibody molecules of the immonuliposome were anchored to the NiCl2 treated mica surface. Alternatively, the immunoliposomes were immunochemically bound on antigen-coated mica surface. Both approaches yielded liposomes which were clearly imaged without damage by AFM in ambient condition.

  • PDF

Mechanical Characteristics and Fatigue Strength of Ceramic-Sprayed S45C Steel (세라믹 용사된 S45C강재의 기계적 특성 및 피로강도)

  • 오맹종;오창배;김귀식
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.1
    • /
    • pp.32-38
    • /
    • 1998
  • This paper is to investigate of microhardness, adhesive strength, tensile strength, and fatigue strength of ceramic sprayed steel. Rotary bending fatigue tests have been conducted at room temperature in air and 3% NaCl solution using specimens of carbon steel(S45C) with sprayed coating layers of Ni-4.5% Al(under coating) and $TiO_2$ (top coating). The microhardness has been improved at $800^{\circ}C$ heat treatment and 150mm spraying distance. Tensile strength of the sprayed steel is dependent on the substrate strength. The fatigue strength of the sprayed steel is larger than that of substrate due to blasting and constraint surface of plastic deformation effect. In low stress level, the corrosion fatigue strength of the sprayed steel were lower than that of fatigue strength in air by corrosion.