철계 소결합금의 오스테나이트 안정성 (Austenite Stability of Sintered Fe-based Alloy)

  • 최승규;서남혁;전준협;손승배;이석재
    • 한국분말재료학회지
    • /
    • 제27권5호
    • /
    • pp.414-419
    • /
    • 2020
  • In the present study, we investigated the austenite stability of a sintered Fe-based nanocrystalline alloy. The volume fraction of austenite was measured based on the X-ray diffraction data of sintered Fe-based nanocrystalline alloys, which were prepared by high-energy ball milling and spark plasma sintering. The sintered alloy samples showed a higher volume fraction of austenite at room temperature as compared to the equilibrium volume fraction of austenite obtained using thermodynamic calculations, which resulted from the nanosized crystalline structure of the sintered alloy. It was proved that the austenite stability of the sintered Fe-based alloy increased with a rise in the amount of austenite stabilizing elements such as Mn, Ni, and C; however, it increased more effectively with a decrease in the actual grain size. Furthermore, we proposed a new equation to predict the martensite starting temperature for sintered Fe-based alloys.

방전 플라즈마 소결로 제조된 나노결정 Fe-7wt.%Mn 합금의 오스테나이트 안정성에 미치는 Mo 첨가 효과 (Effect of Mo Addition on the Austenite Stability of Nanocrystalline Fe-7wt.%Mn Alloy Fabricated by Spark Plasma Sintering)

  • 신우철;손승배;정재길;이석재
    • 한국분말재료학회지
    • /
    • 제29권6호
    • /
    • pp.517-522
    • /
    • 2022
  • We investigate the austenite stability in nanocrystalline Fe-7%Mn-X%Mo (X = 0, 1, and 2) alloys fabricated by spark plasma sintering. Mo is known as a ferrite stabilizing element, whereas Mn is an austenite stabilizing element, and many studies have focused on the effect of Mn addition on austenite stability. Herein, the volume fraction of austenite in nanocrystalline Fe-7%Mn alloys with different Mo contents is measured using X-ray diffraction. Using a disk compressive test, austenite in Fe-Mn-Mo alloys is confirmed to transform into strain-induced martensite during plastic deformation by a disk d. The variation in austenite stability in response to the addition of Mo is quantitatively evaluated by comparing the k-parameters of the kinetic equation for the strain-induced martensite transformation.

Ga 첨가가 $\alpha$-Fe기 Nd-Fe-B 합금의 자기특성에 미치는 영향 (Influence of Ga-Addition on the Manetic Properties of $\alpha-Fe$ Based Nd-Fe-B Alloy)

  • 조덕호;이병엽;조용수
    • 한국자기학회지
    • /
    • 제7권1호
    • /
    • pp.44-48
    • /
    • 1997
  • 약 30 nm의 미세결정립으로 구성된 ( .alpha. -Fe)-(Nd$_{2}$Fe$_{14}$B$_{1}$)형 저 Nd함유 Nd-Fe-B계 합금이 급속응고법으로 제조된 비정질상으로 부터 결정화하여 제조되었다. Nd$_{4}$Fe$_{82}$B$_{10}$Mo$_{3}$Cu$_{1}$ 조성에 Ga의 첨가는 각형성 개선효과와 함께 잔류자화를 1.29 T까지 증가시킨다. Nd의 함유량을 증가시킨 초미세결정립 Nd$_{5}$Fe$_{81}$B$_{9}$Mo$_{3}$Cu$_{1}$Ga$_{1}$ 합금의 Nd$_{2}$Fe$_{81}$B$_{9}$Mo$_{3}$Cu$_{1}$Ga$_{1}$ 합금의 잔류자화, 보자력 및 최대자기에너지적은 각각 1.24 T, 257.4 kA/m(3.23 kOe), and 100.3 kJ/m$^{3}$(12.6 MGOe)이다.다.

  • PDF

MAGNETIC PROPERTIES OF Fe-Al-B-Zr-Cu ALLOYS WITH FINE NANOCRYSTALLINE STRUCTURE

  • Kim, K.J.;Park, J.Y.;Kim, K.Y.;Noh, T.H.;Kang, I.K.
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.491-495
    • /
    • 1995
  • The crystallization behaviors and magnetic properties for $Fe_{81-x}Al_{4}B_{10}Zr_{5}Cu_{x}$ (x=0, 1, 2 at%) alloys is investigated. By the addition of 1~2 Cu, the temperature range, where a single bcc phase exists, expands largely over 200 K and the grain size of bcc phase represents to less than 10 nm. For the optimally annealed Cu-added alloys, the high $\mu_{e}$ (1 kHz) above 20000 combined with the high $B_{10}$ of about 1.4 T is obtained in nanocrystalline state. The low core loss of 95.8 W/kg at 0.1 T and 100 kHz is confirmed for the nanocrystalline $Fe_{80}Al_{4}B_{10}Zr_{5}Cu_{1}$ alloy.

  • PDF

Magnetic and Photo-catalytic Properties of Nanocrystalline Fe Doped $TiO_2$ Powder Synthesized by Mechanical Alloying

  • Uhm, Y.R.;Woo, S.H.;Lee, M.K.;Rhee, C.K.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.955-956
    • /
    • 2006
  • Fe-doped $TiO_2$ nanopowders were prepared by mechanical alloying (MA) varying Fe contents up to 8.0 wt.%. The UV-vis absorption showed that the UV absorption for the Fe-doped powder shifted to a longer wavelength (red shift). The absorption threshold depends on the concentration of nano-size Fe dopant. As the Fe concentration increased up to 4 wt.%, the UV-vis absorption and the magnetization were increased. The benefical effect of Fe doping for photocatalysis and ferromagnetism had the critical dopant concentration of 4 wt.%. Based on the UV absorption and magnetization, the dopant level is localized to the valence band of $TiO_2$.

  • PDF

나노결정 FeMnNiC합금의 오스테나이트 안정성 (Austenite Stability of Nanocrystalline FeMnNiC Alloy)

  • 오승진;전준협;손인진;이석재
    • 한국분말재료학회지
    • /
    • 제26권5호
    • /
    • pp.389-394
    • /
    • 2019
  • In the present study, we have investigated the effect of sintering process conditions on the stability of the austenite phase in the nanocrystalline Fe-5wt.%Mn-0.2wt.%C alloy. The stability and volume fraction of the austenite phase are the key factors that determine the mechanical properties of FeMnC alloys, because strain-induced austenite-martensite transformation occurs under the application of an external stress at room temperature. Nanocrystalline Fe-5wt.%Mn-0.2wt.%C samples are fabricated using the spark plasma sintering method. The stability of the austenite phase in the sintered samples is evaluated by X-ray diffraction analysis and hardness test. The volume fraction of austenite at room temperature increases as the sample is held for 10 min at the sintering temperature, because of carbon diffusion in austenite. Moreover, water quenching effectively prevents the formation of cementite during cooling, resulting in a higher volume fraction of austenite. Furthermore, it is found that the hardness is influenced by both the austenite carbon content and volume fraction.

Microstructural Change and Magnetic Properties of Nanocrystalline Fe-Si-B-Nb-Cu Based Alloys Containing Minor Elements

  • Nam, Seul-Ki;Moon, Sun-Gyu;Sohn, Keun Yong;Park, Won-Wook
    • Journal of Magnetics
    • /
    • 제19권4호
    • /
    • pp.327-332
    • /
    • 2014
  • The effect of minor element additions (Ca, Al) on microstructural change and magnetic properties of Fe-Nb-Cu-Si-B alloy has been investigated, in this paper. The Fe-Si-B-Nb-Cu(-Ca-Al) alloys were prepared by arc melting in argon gas atmosphere. The alloy ribbons were fabricated by melt-spinning, and heat-treated under a nitrogen atmosphere at $520-570^{\circ}C$ for 1 h. The soft magnetic properties of the ribbon core were analyzed using the AC B-H meter. A differential scanning calorimetry (DSC) was used to examine the crystallization behavior of the amorphous alloy ribbon. The microstructure was observed by X-ray diffraction (XRD), transmission electron microscope (TEM) and scanning electron microscope (SEM). The addition of Ca increased the electrical resistivity to reduce the eddy current loss. And the addition of Al decreased the intrinsic magnetocrystalline anisotropy $K_1$ resulting in the increased permeability. The reduction in the size of the ${\alpha}$-Fe precipitates was observed in the alloys containing of Ca and Al. Based on the results, it can be concluded that the additions of Ca and Al notably improved the soft magnetic properties such as permeability, coercivity and core loss in the Fe-Nb-Cu-Si-B base nanocrystalline alloys.

INFLUENCE OF B AND Nd CONTENT ON THE MAGNETIC PROPERTIES OF ${\alpha}-Fe$ BASED NdFeB MAGNETS WITH ULTRAFINE GRAINS

  • Cho, Y.S.;Kim, Y.B.;Park, W.S.;Kim, C.S.;Kim, T.K.
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.427-431
    • /
    • 1995
  • The influence of Nd and B contents on the magnetic properties and structures of ${\alpha}-Fe$ based Nd-(Fe,Co)-B-Mo-Cu alloys was investigated. $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ and $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ amorphous alloys prepared by rapid solidification process were crystallized to form nanocrystalline structure. The increase of B content in $Nd_{4}{(Fe_{0.9}Co_{0.1})}_{92-x}B_{x}Mo_{3}Cu_{1}$ nanocrystalline resulted in the change of stucture of soft phase in the sequence of ${\alpha}-Fe$->${\alpha}-Fe+Fe_{3}B$->$Fe_{3}B$. The coercivitis of the alloys were increased with increasing B content and was 263 kA/m at x=18. On the contrary, the remanence has shown an opposite trends. The increase of Nd content in $Nd_{x}{(Fe_{0.9}Co_{0.1})}_{86-x}B_{10}Mo_{3}Cu_{1}$ nanocrystalline containing ${\alpha}-Fe$ as main phase had no effect on the structure and improved coercivity up to 256 kA/m. However, the remanence was decreased from 1.4 T to 1.15 T according to the increase of Nd content.

  • PDF

Dynamic Magnetostriction Characteristics of an Fe-Based Nanocrystalline FeCuNbSiB Alloy

  • Chen, Lei;Li, Ping;Wen, Yumei
    • Journal of Magnetics
    • /
    • 제16권3호
    • /
    • pp.211-215
    • /
    • 2011
  • The dynamic magnetostriction characteristics of an Fe-based nanocrystalline FeCuNbSiB alloy are investigated as a function of the dc bias magnetic field. The experimental results show that the piezomagnetic coefficient of FeCuNbSiB is about 2.1 times higher than that of Terfenol-D at the low dc magnetic bias $H_{dc}$ = 46 Oe. Moreover, FeCuNbSiB has a large resonant dynamic strain coefficient at quite low Hdc due to a high mechanical quality factor, which is 3-5 times greater than that of Terfenol-D at the same low $H_{dc}$. Based on such magnetostriction characteristics, we fabricate a new type of transducer with FeCuNbSiB/PZT-8/FeCuNbSiB. Its maximum resonant magnetoelectric voltage coefficient achieves ~10 V/Oe. The ME output power reaches 331.8 ${\mu}W$ at an optimum load resistance of 7 $k{\Omega}$ under 0.4 Oe ac magnetic field, which is 50 times higher than that of the previous ultrasonic-horn-substrate composite transducer and it decreases the size by nearly 86%. The performance indicate that the FeCuNbSiB/PZT-8/FeCuNbSiB transducer is promising for application in highly efficient magnetoelectric energy conversion.

Fe-Ni 합금 극박재 제조를 위한 전주성형기술 및 극박재 특성 (Electroforming and Properties of Fe-Ni alloy thin foil)

  • 임태홍;이흥렬
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.188-191
    • /
    • 2004
  • Electroforming is a process that employs technology similar to that used for electroplating but which is used for manufacturing metallic articles, rather than as a means of producing surface coatings. Electroforming provides a cost-effective means of producing alloys and fully dense nanocrystalline metals as foils, sheets and complex shapes. It was able to make Fe-Ni foil with $5{\mu}m$ thickness by electroforming. Electroformed Fe-Ni alloy was nanocrystalline and the yield strength was in the range $2000{\sim}2800\;MPa$. The magnetic permeability at high frequency of electroformed Fe-Ni foil was higher than that of thicker foils.

  • PDF