• 제목/요약/키워드: Microstructure properties

검색결과 4,066건 처리시간 0.04초

Microstructure and Tensile Properties of Tungsten Heavy Alloys

  • Islam, S.H.;Qu, X.H.;Akhtar, F.;Feng, P.Z.;Hea, X.B.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.547-548
    • /
    • 2006
  • The main object of this research was to examine the effect of sintering conditions on the microstructure of tungsten heavy alloys and how the resulting modification of the microstructure can be used to optimize their mechanical properties. Alloys composed of 88%, 93% and 95% wt. of tungsten and the balance is Ni: Fe in the ratio of 7:3 were sintered at different temperatures for different sintering holding times in hydrogen atmosphere. It was shown that the mechanical properties of the alloys, and especially their ductility, are harmed when tungsten grains are contiguous.

  • PDF

유도결합 플라즈마 파워가 NbN 코팅막의 미세구조, 결정구조 및 기계적 특성에 미치는 영향에 관한 연구 (Effect of Inductively Coupled Plasma on the Microstructure, Structure and Mechanical Properties of NbN Coatings)

  • 전성용
    • 한국표면공학회지
    • /
    • 제48권5호
    • /
    • pp.205-210
    • /
    • 2015
  • NbN coatings were prepared by ICP (inductively coupled plasma) assisted magnetron sputtering from a Nb metal target in $Ar+N_2$ atmosphere at various ICP powers. Effect of ICP on the microstructure, crystalline structure and mechanical properties of NbN coatings was investigated by field emission electron microscopy, X-ray diffraction, atomic force microscopy and nanoindentation measurements. The results show that ICP power has a significant influence on coating microstructure, structure and mechanical properties of NbN coatings. With the increasing of ICP power, coating microstructure evolves from the columnar structure of DC process to a highly dense one. Crystalline structure of NbN coatings were changed from cubic ${\delta}$-NbN to hexagonal ${\beta}-Nb_2N$ with increase of ICP power. The maximum nano hardness of 25.4 GPa with Ra roughness of 0.5 nm was obtained from the NbN coating sputtered at ICP power of 200 W.

유도결합 플라즈마 파워가 VN 코팅막의 미세구조, 결정구조 및 기계적 특성에 미치는 영향에 관한 연구 (Effect of Inductively Coupled Plasma on the Microstructure, Structure and Mechanical Properties of VN Coatings)

  • 전성용;이소연
    • 한국표면공학회지
    • /
    • 제49권4호
    • /
    • pp.376-381
    • /
    • 2016
  • The effects of ICP (Inductively Coupled Plasma) power, ranging from 0 to 200 W, on the crystal structure, microstructure, surface roughness and mechanical properties of magnetron sputtered VN coatings were systematically investigated with FE-SEM, AFM, XRD and nanoindentation. The results show that ICP power has a significant influence on coating microstructure and mechanical properties of VN coatings. With the increasing of ICP power, coating microstructure evolves from a porous columnar structure to a highly dense one. Average crystal grain size of single phase cubic fcc VN coatings was decreased from 10.1 nm to 4.0 nm with increase of ICP power. The maximum hardness of 28.2 GPa was obtained for the coatings deposited at ICP power of 200 W. The smoothest surface morphology with Ra roughness of 1.7 nm was obtained from the VN coating sputtered at ICP power of 200 W.

이주속압연된 Cu-Fe-P 동합금 판재의 조직 및 기계적 성질 (Microstructure and Mechanical Properties of a Cu-Fe-P Copper Alloy Sheet Processed by Differential Speed Rolling)

  • 이성희;임정윤;宇都宮裕;어광준;한승전
    • 대한금속재료학회지
    • /
    • 제48권10호
    • /
    • pp.942-950
    • /
    • 2010
  • The microstructure and mechanical properties of a Cu-Fe-P copper alloy processed by differential speed rolling (DSR) were investigated in detail. The copper alloy, with a thickness of 3 mm, was rolled to 50% reduction at ambient temperature without lubrication with a differential speed ratio of 2.0:1 and then annealed for 0.5h at various temperatures ranging from 100 to $800^{\circ}C$. Conventional rolling was performed under the same rolling conditions for comparison. The shear strain introduced by the conventional rolling process showed positive values at the positions of the upper roll side and negative values at the positions of the lower roll side. However, the result was zero or positive values at all positions for samples rolled by DSR. The effects of DSR on the microstructure and mechanical properties of the as-rolled and subsequently annealed samples are discussed.

Mo 첨가 및 시편 방향에 따른 API X70 라인파이프강의 미세조직과 기계적 특성 (Effect of Molybdenum Addition and Specimen Orientation on Microstructure and Mechanical Properties of API X70 Linepipe Steels)

  • 오동규;신승혁;황병철
    • 한국재료학회지
    • /
    • 제33권6호
    • /
    • pp.251-256
    • /
    • 2023
  • This study aims to examine the correlation between microstructures and the mechanical properties of two high-strength API X70 linepipe steels with different specimen directions and Moaddition. The microstructure of the Mo-added steel has an irregularly shaped AF, GB matrix with pearlite because of the relatively large deformation in the non-recrystallization temperature region, while that of the Mo-free steel shows a PF matrix with bainitic microstructure. In the Mo-added steel, the M/A (martensite-austenite) in granular bainite (GB) and pearlite act as crack initiation sites with decreased upper shelf energy and an increased ductile to brittle transition temperature (DBTT). Regardless of Mo addition, all of the steels demonstrate higher strength and lower elongation in the T direction than in the L direction because of the short dislocation glide path and ease of pile-up at grain boundaries. In addition, the impact test specimens with T-L direction had a lower impact absorbed energy and higher DBTT than those with the L-T direction because the former exhibit shorter unit crack path compared to the latter.

격자식 미세구조 성장 모델을 이용한 다결정 박막 소재의 유한 요소 해석 (Lattice based Microstructure Evolution Model for Monte Carlo Finite Element Analysis of Polycrystalline Materials)

  • 최재환;김한성;이준기;나경환
    • 소성∙가공
    • /
    • 제13권3호
    • /
    • pp.248-252
    • /
    • 2004
  • The mechanical properties of polycrystalline thin-films, critical for Micro-Electro-Mechanical Systems (MEMS) components, are known to have the size effect and the scatter in the length scale of microns by the numbers of intensive investigation by experiments and simulations. So, the consideration of the microstructure is essential to cover these length scale effects. The lattice based stochastic model for the microstructure evolution is used to simulate the actual microstructure, and the fast and reliable algorithm is described in this paper. The kinetics parameters, which are the key parameters for the microstructure evolution based on the nucleation and growth mechanism, are extracted from the given micrograph of a polycrystalline material by an inverse method. And the method is verified by the comparison of the quantitative measures, the number of grains and the grain size distribution, for the actual and simulated microstructures. Finite element mesh is then generated on this lattice based microstructure by the developed code. And the statistical finite element analysis is accomplished for selected microstructure.

인발공정에 의해 강소성 가공된 AA1070선재의 미세조직 및 기계적 특성 (Microstructure and Mechanical Properties of an AA1070 Wire Severely Deformed by Drawing Process)

  • 정대한;이성희
    • 한국재료학회지
    • /
    • 제30권6호
    • /
    • pp.308-314
    • /
    • 2020
  • A commercial AA1070 alloy for electrical wire is severely deformed by drawing process in which a rod with an initial diameter of 9mm into is reduced to a wire of 2mm diameter. The drawn AA1070 wire is then annealed at various temperatures from 200 to 450 ℃ for 2h. Changes in microstructure, mechanical properties and electrical properties of the specimens with annealing temperature are investigated in detail. The specimen begins partially to recrystallize at 250 ℃; above 300 ℃ it is covered with equiaxed recrystallized grains over all regions. Fiber textures of {110}<111> and {112}<111> components are mainly developed, and {110}<001> texture is partially developed as well. The tensile strength tends to decrease with annealing temperature due to the occurrence of recovery or/and recrystallization. On the other hand, the elongation of the annealed wire increases with the annealing temperature, and reaches a maximum value of 33.3 % at 300 ℃. Electric conductivity of the specimens increases with annealing temperature, and reaches a maximum value of 62.6 %IACS after annealing at 450 ℃. These results are discussed in comparison with those for the other aluminum alloy.

Kinetic Spray 공정을 이용한 벌크형 탄탈륨 소재의 제조 및 미세조직/물성 (Fabrication and Microstructure/Properties of Bulk-type Tantalum Material by a Kinetic Spray Process)

  • 이지혜;김지원;이기안
    • 한국분말재료학회지
    • /
    • 제23권1호
    • /
    • pp.8-14
    • /
    • 2016
  • A bulk-type Ta material is fabricated using the kinetic spray process and its microstructure and physical properties are investigated. Ta powder with an angular size in the range $9-37{\mu}m$ (purity 99.95%) is sprayed on a Cu plate to form a coating layer. As a result, ~7 mm-sized bulk-type high-density material capable of being used as a sputter material is fabricated. In order to assess the physical properties of the thick coating layer at different locations, the coating material is observed at three different locations (surface, center, and interface). Furthermore, a vacuum heat treatment is applied to the coating material to reduce the variation of physical properties at different locations of the coating material and improve the density. OM, Vickers hardness test, SEM, XRD, and EBSD are implemented for analyzing the microstructure and physical properties. The fabricated Ta coating material produces porosity of 0.11~0.12%, hardness of 311~327 Hv, and minor variations at different locations. In addition, a decrease in the porosity and hardness is observed at different locations upon heat treatment.

Recent Advances in Microstructural Tailoring of Silicon Nitride Ceramics and the Effects on Thermal Conductivity and Fracture Properties

  • Becher Paul F.
    • 한국세라믹학회지
    • /
    • 제42권8호
    • /
    • pp.525-531
    • /
    • 2005
  • Tailoring the microstructure and the composition of silicon nitride ceramics can have profound effects on their properties. Here it is shown that the grain growth behavior, in particular its anisotropy, is a function of the specific additives, which allow one to tune the microstructure from one consisting of more equiaxed grains to one with very elongated grains. Recent studies are discussed that provide an understanding of the atomic level processes by which these additives influence grain shapes. Next the microstructural (and compositional) parameters are discussed that can be used to modify the thermal conductivity, as well as fracture toughness of silicon nitride ceramics. As a result of the open <0001> channels in $\beta-Si_3N_4$, the c-axis conductivity can be exceptionally high. Thus, the formation of elongated c-axis grains, particularly when aligned can result in conductivity values approaching those of AlN ceramics. In addition, the controlled formation of elongated grains can also be used to significantly enhance the fracture toughness. At the same time, both properties are shown to be affected by the composition of the densification additives. Utilizing such understanding, one will be able to tailor the ceramics to achieve the properties desired for specific applications.

겹치기 마찰교반접합된 Invar 42/SS 400 합금의 미세조직과 기계적 특성 발달 (Development of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Invar 42/SS 400)

  • 송국현
    • Journal of Welding and Joining
    • /
    • 제30권5호
    • /
    • pp.34-39
    • /
    • 2012
  • This study was conducted to investigate the microstructure and mechanical properties of friction stir lap joints. Invar 42 and SS 400 were selected as the experimental materials, and friction stir welding was carried out at a tool rotation speed of 200 rpm and welding speed of 100 mm/min. The application of friction stir welding to Invar 42 effectively reduced the grain size in the stir zone; the average grain size of Invar 42 was reduced from $11.5{\mu}m$ in the base material to $6.4{\mu}m$ in the stir zone, which resulted in an improvement in the mechanical properties of the stir zone. The joint interface between Invar 42 and SS 400 showed a relatively sound weld without voids and cracks, and the intermetallic compounds with $L1_2$ type in lap jointed interface were partially formed with size of 100 nm. Moreover, the hook in the advancing side of Invar 42 was formed from SS 400, which contributed to maintenance of the tensile strength. The evolution of microstructures and mechanical properties of friction stir lap jointed Invar 42 and SS 400 are also discussed herein.