MgO(100)기판에 성장시킨 Bi2212 에피택셜 박막의 R-T특성 (R-T characteristic of Bi2212 Epitaxial thin films by growth in MgO(100) substrate)

  • 양승호;임중관;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.537-538
    • /
    • 2006
  • BSCCO thin films have been fabricated by epitaxy growth at an ultra-low growth rate. The growth rates of the films was set in the region from 0.17 to 0.27 nm/min. MgO(100) was used as a substrate. In order to appreciate stable existing region of Bi 2212 phase with temperature and ozone pressure, the substrate temperature was varied between 650 and $720^{\circ}C$ and the highly condensed ozone gas pressure ($PO_3$) in vacuum chamber was varied between $2.0{\times}10^{-6}$ and $2.3{\times}10^{-5}\;Torr$.

  • PDF

유도 결합 플라즈마를 이용한 MgO 박막의 식각특성 (The etching properties of MgO thin films in $Cl_2/Ar$ gas chemistry)

  • 구성모;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.734-737
    • /
    • 2004
  • The metal-ferroelectric-semiconductor (MFS) structure is widely studied for nondestructive readout (NDRO) memory devices, but conventional MFS structure has a critical problem. It is difficult to obtain ferroelectric films like PZT on Si substrate without interdiffusion of impurities such as Pb, Ti and other elements. In order to solve these problems, the metal-ferroelectric-insulator-semiconductor (MFIS) structure has been proposed with a buffer layer of high dielectric constant such as MgO, $Y_2O_3$, and $CeO_2$. In this study, the etching characteristics (etch rate, selectivity) of MgO thin films were etched using $Cl_2/Ar$ plasma. The maximum etch rate of 85 nm/min for MgO thin films was obtained at $Cl_2$(30%)/Ar(70%) gas mixing ratio. Also, the etch rate was measured by varying the etching parameters such as ICP rf power, dc-bias voltage, and chamber pressure. Plasma diagnostics was performed by Langmuir probe (LP) and optical emission spectroscopy (OES).

  • PDF

Si기판상에 제작된 박막형 백금 측온저항체 온도센서의 특성 (Characteristics of Thin-film Type Pt-RTD's Fabricated on Si Wafers)

  • 홍석우;노상수;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.354-357
    • /
    • 1999
  • This paper describes on the electrical and physical charateristics thin-film type Pt-RTD\\`s on Si wafers, in which MgO thin-films were used as medium layer in order to improve adhesion of Pt thin-films to SiO$_2$ layer. The MgO medium layer had the properties of improving Pt adhesion to SiO$_2$ and insulation without chemical reaction to Pt thin-films and the resistivity of Pt thin-films was improved. In the analysis of properties of Pt-RTD, TCR value had 3927 ppm/$^{\circ}C$ and liner in the temperature range of room temperature to 40$0^{\circ}C$

  • PDF

증착 온도가 Eu3+ 이온이 도핑된 MgMoO4 형광체 박막의 특성에 미치는 영향 (Effect of Deposition Temperature on the Properties of Eu3+-doped MgMoO4 Phosphor Thin Films)

  • 강동균;조신호
    • 한국표면공학회지
    • /
    • 제49권1호
    • /
    • pp.81-86
    • /
    • 2016
  • $Eu^{3+}$-doped $MgMoO_4$ phosphor thin films were deposited on quartz substrates by radio frequency magnetron sputtering with changing various growth temperatures. The effects of growth temperature on the structure, transmittance, optical band gap, and luminescence of the phosphor thin films were characterized. All the phosphor thin films, irrespective of growth temperature, showed a monoclinic structure with a main (220) diffraction peak. The thin film deposited at a growth temperature of $400^{\circ}C$ indicated an average transmittance of 90% in the wavelength range of 500 ~ 1100 nm and band gap energy of 4.81 eV. The excitation spectra of the phosphor thin films consisted of a broad charge transfer band peaked at 284 nm in the range of 230 ~ 330 nm and two weak peaks located at 368 and 461 nm, respectively. The emission spectra under ultraviolet excitation at 284 nm exhibited a sharp emission peak at 614 nm and several weak bands. All the phosphor thin films showed high asymmetry ratio values, indicating that $Eu^{3+}$ ions incorporated into the host lattice occupied at the non-inversion symmetry sites. The results suggest that the growth temperature plays an important role in growing high-quality phosphor thin films.

Evaluation of the MgO Protective Layer Deposited by Oxygen Ion-Beam-Assisted-Deposition Method in ac PDPs

  • Li, Zhao-Hui;Cho, Eou-Sik;Hong, Seong-Jae;Kwon, Sang-Jik
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권2호
    • /
    • pp.1372-1375
    • /
    • 2007
  • MgO thin films were deposited by $O^+$ IBAD method and results showed assisting oxygen ion beam energy plays a significant role in characteristics of MgO thin films. The lowest firing inception voltage, the highest brightness and the highest luminous efficiency were obtained when oxygen ion beam energy was 300 eV.

  • PDF

The discharge characteristic of Li ion doped MgO film in a flat fluorescent lamp structure

  • Ryu, Si-Hong;Lee, Seong-Eui;Ahn, Sung-Il;Choi, Kyung-Cheol
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권2호
    • /
    • pp.1388-1390
    • /
    • 2007
  • This paper investigates how various concentrations of lithium ion influence on crystallization of MgO in thin films formed by spin coating and an the discharge characteristic in a flat fluorescent lamp structure. The XRD results indicate $Li^+$ ion enhances the growth of MgO crystal in a spin coated thin film. The discharge property with the $Li^+$ ion doped MgO films show the lithium ion in MgO film clearly reduce the initial discharge voltages of test devices. Interestingly, the test panels with various doped MgO film have somewhat higher static memory margin of than that of pure-MgO owing probably to the pore structure of spin coated MgO films. The CL spectra, which confirm that the doping creates defects energy levels in the band gap of MgO, show the $F^+$ center is the main defects in doped MgO films.

  • PDF

Atmosphere Effects in Low Temperature Pyrolysis of Chemical Solution Derived Pb(Zr, Ti) O3 Films

  • Hwang, Kyu-Seog;Lee, Hyung-Min;Kim, Byung-Hoon
    • The Korean Journal of Ceramics
    • /
    • 제4권3호
    • /
    • pp.199-203
    • /
    • 1998
  • $Pb(Zr, Ti)O_3$ (Pb:Zr:Ti=1:0.52:0.48) thin films were prepared on single crystal MgO(100) substrates by dipping-pyrolysis process using a solution of constituent metal naphthenates as starting materials. The solution was spin-coated onto substrate and the precursor films were pyrolyzed at $200^{\circ}C$ in air or at $200^{\circ}C$ in argon for 1, 2, 5 and 24h, followed by final heat treatment at $750^{\circ}C$. For all the films, highly (h00)/(00l)-oriented Pb$Pb(Zr, Ti)O_3$ thin films with smooth surfaces and crack-free were obtained, whereas thin film pyrolyzed in air for 24 h exhibited polycrystalline character. According to the pole-figure analysis, epitaxy of the product films was found to depend on pyrolysis atmosphere.

  • PDF

스퍼터링 증착에 의한 $PbTiO_3$ 박막제조시 증착변수의 영향 (Effects of Deposition Parameters on Sputter Deposition of Lead Titanate Thin Films)

  • 김상섭;강영민;백성기
    • 한국세라믹학회지
    • /
    • 제30권7호
    • /
    • pp.578-588
    • /
    • 1993
  • Highly c-axis oriented ferroelectric PbTiO3 thin films were deposited on MgO single crystal substrates by RF magnetron sputtering. We have studied the effects of substrate temperature, RF input power, gas comosition, gas pressure and deposition rate on the chemical and structural characteristics of PbTiO3 thin films. The epitaxy relationship of c-axis oriented films was found to be PbTiO3{100}//MgO(100) and their microstructures were highly mosaic. It was found that the most important parameter to achieve epitaxial PbTiO3 films was the substrate temperature. The activation energy for the epitaxy formation was about 0.92eV. Lower gas pressure and RF input power were favorable for the formation of epitaxial c-axis orientation. It was also found that the optimum oxygen content in Ar gas was 10% to obtain the stoichiometric PbTiO3 composition.

  • PDF

Effects of Chamber Pressure on Dielectric Properties of Sputtered MgTiO3 Films for Multilayer Ceramic Capacitors

  • Park, Sang-Shik
    • 한국재료학회지
    • /
    • 제20권7호
    • /
    • pp.374-378
    • /
    • 2010
  • $MgTiO_3$ thin films were prepared by r.f. magnetron sputtering in order to prepare miniaturized NPO type MLCCs. $MgTiO_3$ films showed a polycrystalline structure of ilmenite characterized by the appearance of (110) and (202) peaks. The intensity of the peaks decreased with an increase in the chamber pressure due to the decrease of crystallinity which resulted from the decrease of kinetic energy of the sputtered atoms. The films annealed at $600^{\circ}C$ for 60min. showed a fine grained microstructure without micro-cracks. The grain size and roughness of the $MgTiO_3$ films decreased with the increase of chamber pressure. The average surface roughness was 1.425~0.313 nm for $MgTiO_3$ films prepared at 10~70 mTorr. $MgTiO_3$ films showed a dielectric constant of 17~19.7 and a dissipation factor of 2.1~4.9% at 1MHz. The dielectric constant of the films is similar to that of bulk ceramics. The dielectric constant and the dissipation factor decreased with the increase of the chamber pressure due to the decrease of grain size and crystallinity. The leakage current density was $10^{-5}\sim10^{-7}A/cm^2$ at 200kV/cm and this value decreased with the increase of the chamber pressure. The small grain size and smooth surface microstructure of the films deposited at high chamber pressure resulted in a low leakage current density. $MgTiO_3$ films showed a near zero temperature coefficient and satisfied the specifications for NPO type materials. The dielectric properties of the $MgTiO_3$ thin films prepared by sputtering suggest the feasibility of their application for MLCCs.

RF 마그네트론 스퍼터를 이용하여 제작한 MGZO 박막의 구조적 및 전기적, 광학적 특성에 미치는 스퍼터링 전력의 영향 (Effect of Sputtering Powers on Mg and Ga Co-Doped ZnO Thin Films with Transparent Conducting Characteristics)

  • 김인영;신승욱;김민성;윤재호;허기석;정채환;문종하;이정용;김진혁
    • 한국재료학회지
    • /
    • 제23권3호
    • /
    • pp.155-160
    • /
    • 2013
  • ZnO thin films co-doped with Mg and Ga (MxGyZzO, x + y + z = 1, x = 0.05, y = 0.02 and z = 0.93) were prepared on glass substrates by RF magnetron sputtering with different sputtering powers ranging from 100W to 200W at a substrate temperature of $350^{\circ}C$. The effects of the sputtering power on the structural, morphological, electrical, and optical properties of MGZO thin films were investigated. The X-ray diffraction patterns showed that all the MGZO thin films were grown as a hexagonal wurtzite phase with the preferred orientation on the c-axis without secondary phases such as MgO, $Ga_2O_3$, or $ZnGa_2O_4$. The intensity of the diffraction peak from the (0002) plane of the MGZO thin films was enhanced as the sputtering power increased. The (0002) peak positions of the MGZO thin films was shifted toward, a high diffraction angle as the sputtering power increased. Cross-sectional field emission scanning electron microscopy images of the MGZO thin films showed that all of these films had a columnar structure and their thickness increased with an increase in the sputtering power. MGZO thin film deposited at the sputtering power of 200W showed the best electrical characteristics in terms of the carrier concentration ($4.71{\times}10^{20}cm^{-3}$), charge carrier mobility ($10.2cm^2V^{-1}s^{-1}$) and a minimum resistivity ($1.3{\times}10^{-3}{\Omega}cm$). A UV-visible spectroscopy assessment showed that the MGZO thin films had high transmittance of more than 80 % in the visible region and that the absorption edges of MGZO thin films were very sharp and shifted toward the higher wavelength side, from 270 nm to 340 nm, with an increase in the sputtering power. The band-gap energy of MGZO thin films was widened from 3.74 eV to 3.92 eV with the change in the sputtering power.