• Title/Summary/Keyword: Metal framework

Search Result 261, Processing Time 0.021 seconds

Evaluation of marginal adaptation in three-unit frameworks fabricated with conventional and powder-free digital impression techniques

  • Kocaagaoglu, Hasan;Albayrak, Haydar;Sahin, Sezgi Cinel;Gurbulak, Aysegul Guleryuz
    • The Journal of Advanced Prosthodontics
    • /
    • v.11 no.5
    • /
    • pp.262-270
    • /
    • 2019
  • PURPOSE. The purpose of this in vitro study was to evaluate the marginal misfits of three-unit frameworks fabricated with conventional and digital impressions techniques. MATERIALS AND METHODS. Thirty brass canine and second premolar abutment preparations were fabricated by using a computer numerical control machine and were randomly divided into 3 groups (n=10) as follows: conventional impression group (Group Ci), Cerec Omnicam (Group Cdi), and 3shape TRIOS-3 (Group Tdi) digital impression groups. The laser-sintered metal frameworks were designed and fabricated with conventional and digital impressions. The marginal adaptation was assessed with a stereomicroscope at ${\times}30$ magnification. The data were analyzed with 1-way analysis of variances (ANOVAs) and the independent simple t tests. RESULTS. A statistically significant difference was found between the frameworks fabricated by conventional methods and those fabricated by digital impression methods. Multiple comparison results revealed that the frameworks in Group Ci (average, $98.8{\pm}16.43{\mu}m$; canine, $93.59{\pm}16.82{\mu}m$; premolar, $104.10{\pm}15.02{\mu}m$) had larger marginal misfit values than those in Group Cdi (average, $63.78{\pm}14.05{\mu}m$; canine, $62.73{\pm}13.71{\mu}m$; premolar, $64.84{\pm}15.06{\mu}m$) and Group Tdi (average, $65.14{\pm}18.05{\mu}m$; canine, $70.64{\pm}19.02{\mu}m$; premolar, $59.64{\pm}16.10{\mu}m$) (P=.000 for average; P=.001 for canine; P<.001 for premolar). No statistical difference was found between the marginal misfits of canine and premolar abutment teeth within the same groups (P>.05). CONCLUSION. The three-unit frameworks fabricated with digital impression techniques showed better marginal fit compared to conventional impression techniques. All marginal misfit values were clinically acceptable.

Full mouth rehabilitation utilizing computer guided implant surgery and CAD/CAM (Computer guided implant surgery와 CAD/CAM을 활용한 전악 수복 증례)

  • Kim, Sungjin;Han, Jung-Suk;Kim, Sung-Hun;Yoon, Hyung-In;Yeo, In-Sung Luke
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.1
    • /
    • pp.57-65
    • /
    • 2019
  • Computer aided design and manufacturing and implant surgery using a guide template improve restoration-driven implant treatment procedures. This case utilized those digital technologies to make definitive prostheses for a patient. According to the work flow of digital dentistry, cone beam computed tomography established the treatment plan, which was followed to make the guide template for implant placement. The template guided the implants to be installed as planned. The customized abutments and surveyed fixed restorations were digitally designed and made. The metal framework of the removable partial denture was cast from resin pattern using an additive manufacturing technique, and the artificial resin teeth were replaced with the zirconia onlays for occlusal stability. These full mouth rehabilitation procedures provided functionally and aesthetically satisfactory results for the patient.

Implant-assisted removable partial denture for severely atrophied mandible (심한 하악 치조제 흡수를 가진 환자에서 임플란트를 이용한 가철성 국소의치로 수복한 증례)

  • Choi, Bada;Kim, Yeun Ju;Lee, Jae Hoon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.2
    • /
    • pp.171-175
    • /
    • 2019
  • Mandible with severe alveolar bone atrophy poses a significant challenge in terms of reproducing clinically acceptable anatomy for a removable prosthesis. To overcome this potential complication, altered cast impression technique is often recommended to capture accurate and functional gingiva tissues. It becomes possible to get proper anchors functional impression by placing 2 implants crowns which were impossible in previous implant overdenture impression technique. In this case, an 80-year old female patient with severe mandibular ridge atrophy was treated with an implant-assisted removable partial denture with two implant crowns on the canine area. An altered cast impression was taken with an individual tray on a metal framework of removable partial denture on both posterior edentulous areas. The patient was satisfied with the final prosthesis after failure of 2 previous prostheses. Clinician had a difficult time to manage disabled patient and patient were suffered with ill-fitting denture due to inaccurate impression in conventional overdenture condition. The oral rehabilitation was completed with placing 2 implants as proper anchor.

Zirconia resin-bonded fixed partial denture in maxillary single-tooth edentulous area: A case report (상악 전치부 단일치 상실 환자에서 지르코니아 레진접착성 고정성 국소의치를 이용한 수복 증례)

  • Rojee Oh;Hee-Won Jang;Na-Hong Kim;Joo-Hyuk Bang;Keun-Woo Lee;Yong-Sang Lee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.61 no.2
    • /
    • pp.135-142
    • /
    • 2023
  • Resin-bonded fixed partial denture (RBFPD)as known as Maryland bridge is is a well-known conservative method for its minimized invasion of the teeth for an anterior single tooth edentulous area. Despite of its various advantages, RBFPD was not widespread because of its high debonding rates, non-esthetic look or weak structure for material property. Currently, with the introduction of zirconia to dental material for RBFPD, Maryland bridge entered upon a new phase. Zirconia surmounts poor esthetics of metal framework, having proper strength, and overcomes ceramic's structural weakness, being sufficiently esthetic. In this case, edentulous area of maxillary left lateral incisor was restored using zirconia resin-bonded fixed partial denture. Restoration of missing tooth in anterior area was achieved using non-invasive and esthetic prosthesis, then we report this case as satisfactory results were obtained for both the operator and the patient.

Highly catalysis Zinc MOF-loaded nanogold coupled with aptamer to assay trace carbendazim by SERS

  • Jinling Shi;Jingjing Li;Aihui Liang;Zhiliang Jiang
    • Advances in nano research
    • /
    • v.14 no.4
    • /
    • pp.313-327
    • /
    • 2023
  • Zinc metal organic framework (MOFZn)-loaded goad nanoparticles (AuNPs) sol (Au@MOFZn), which was characterized by TEM, Mapping, FTIR, XRD, and molecular spectrum, was prepared conveniently by solvothermal method. The results indicated that Au@MOFZn had a very strong catalytic effect with the nanoreaction of AuNPs formation between sodium oxalate (SO) and HAuCl4. AuNPs in the new indicator reaction had a strong resonance Rayleigh scattering (RRS) signal at 370 nm. The indicator AuNPs generated by this reaction, which had the most intense surface enhanced Raman scattering (SERS) peak at 1621 cm -1. The new SERS/RRS indicator reaction in combination with specific aptamer (Apt) to fabricate a sensitive and selective Au@MOFZn catalytic amplification-aptamer SERS/RRS assay platform for carbendazim (CBZ), with SERS/RRS linear range of 0.025-0.5 ng/mL. The detection limit was 0.02 ng/mL. Similarly, this assay platform has been also utilized to detect oxytetracycline (OTC) and profenofos (PF).

Development of dental zirconia (치과용 지르코니아의 발전)

  • Kim Sung-Hun
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.32 no.1
    • /
    • pp.4-7
    • /
    • 2023
  • Since the end of the 1990s, zirconia, which has been applied to dental prostheses, has been used in the form of coping or framework. The prostheses made in this way have been successfully used in the anterior teeth because they have no metal components as a structure. But in the posterior teeth, its use was limited due to the fracture or chipping of the veneering porcelain during the function. Later, as a solution to this shortcoming, a monolithic zirconia restoration was proposed in which a strong coping material was used in the form of a complete prosthesis. But, this resulted in some unesthetic results due to the characteristics of zirconia, which has excellent resistance to strong forces but is very white and opaque. However, now, due to technological advances in increasing the translucency of zirconia, it is possible to produce strong and esthetic zirconia restorations not only in the posterior region but also in the anterior region. In this article, the structural characteristics of various types of zirconia materials that have been developed so far, were discussed, and where the zirconia products actually in use belong to was explained.

The effect of screw tightening techniques on the detorque value in internal connection implant superstructure (내부연결 임플란트 상부구조물에서 나사조임술식이 풀림토크값에 미치는 영향)

  • Choi, Jung-Han
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.4
    • /
    • pp.243-250
    • /
    • 2010
  • Purpose: This study evaluated the effect of different screw tightening sequences and methods on detorque values in a well-fitting implant superstructure. Materials and methods: A fully edentulous mandibular master model and a metal framework directly connected to four parallel implants (Astra Tech) with a passive fit to each other were fabricated. Six stone casts were made with a splinted impression technique to represent a 'well-fitting' situation with the metal framework. Detorque values were measured twice after screw tightening using 20 Ncm. Detorque values and minimum detorque values for three screw tightening sequences (1-2-3-4, 2-4-3-1, and 2-3-1-4) and for two tightening methods (two-step and one-step) were analyzed using multi-way analysis of variance and two-way analysis of variance, respectively, at a .05 level of significance. Results: The mean detorque values for screw tightening sequences ranged from 12.8 Ncm (2-4-3-1) to 13.1 Ncm (2-3-1-4), and for screw tightening methods were 13.1 Ncm (two-step) and 11.8 Ncm (one-step). The mean of mimimum detorque values for screw tightening sequences were 11.1 Ncm (1-2-3-4) and 11.2 Ncm (2-4-3-1 and 2-3-1-4), and for screw tightening methods were 11.2 Ncm (two-step) and 9.9 Ncm (one-step). No statistically significant differences among three screw tightening sequences were found for detorque values and for mimimum detorque values. But, statistically significant differences between two screw tightening methods were found for two values. Two-step screw tightening method showed higher detorque value (P = .0003) and higher minimum detorque value (P = .0035) than one-step method. Conclusion: Within the limitations of this study, the screw tightening sequence was not a critical factor for the detorque values in a well-fitting implant superstructure by the splinted impression technique. But, two-step screw tightening method showed greater detorque values than one-step method.

Detorque values of abutment screws in a multiple implant-supported prosthesis (다수 임플란트 지지 보철물에서 지대주 나사의 풀림 토크값에 대한 연구)

  • Lee, Ju-Ri;Lee, Dong-Hwan;Hwang, Jae-Woong;Choi, Jung-Han
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.4
    • /
    • pp.280-286
    • /
    • 2010
  • Purpose: This study evaluated the detorque values of screws in a multiple implant-supported superstructure using stone casts made with 2 different impression techniques. Material and methods: A fully edentulous mandibular master model and a metal framework directly connected to four implants (Br${\aa}$nemark $System^{(R)}$; Nobel Biocare AB) with a passive fit to each other were fabricated. Six experimental stone casts (Group 1) were made with 6 non-splinted impressions on a master cast and another 6 experimental casts (Group 2) were made with 6 acrylic resin splinted impressions. The detorque values of screws ($TorqTite^{(R)}$ GoldAdapt Abutment Screw; Nobel Biocare AB) were measured twice after the metal framework was fastened onto each experimental stone cast with 20 Ncm torque. Detorque values were analyzed using the mixed model with the fixed effect of screw and reading and the random effect of model for the repeated measured data at a .05 level of ignificance. Results: The mean detorque values were 7.9 Ncm (Group 1) and 8.1 Ncm (Group 2), and the mean of minimum detorque values were 6.1 Ncm (Group 1) and 6.5 Ncm (Group 2). No statistically significant differences between 2 groups were found and no statistically significant differences among 4 screws were found for detorque values. No statistically significant differences between 2 groups were also found for minimum detorque values. Conclusion: In a multiple external hexagon implant-supported prosthesis, no significant differences between 2 groups were found for detorque values and for minimum detorque values. There seems to be no significant differences in screw joint stability between 2 stone cast groups made with 2 different impression techniques.

Prosthetic rehabilitation of a patient with tongue cancer using palatal augmentation prosthesis and mandibular implant-retained overdenture: A case report (구개 증대 보철물과 임플란트 피개의치를 이용한 설암 환자의 보철수복 증례)

  • Kim, Ye-Jin;Lee, Young-Hoon;Ko, Kyung-Ho;Park, Chan-Jin;Cho, Lee-Ra;Huh, Yoon-Hyuk
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.56 no.4
    • /
    • pp.317-322
    • /
    • 2018
  • The tongue, especially its lateral part, is the most common site of oral tumors. Patients who undergo glossectomy for the treatment of tongue cancer may experience difficulty in proper functioning for pronunciation, chewing, swallowing, and oral hygiene maintenance; therefore, a palatal augmentation prosthesis can be used to restore function of the tongue. In this case, an implant overdenture was used in a patient who had residual ridge resorption and obliteration of alveololingual sulcus after undergoing glossectomy for tongue cancer treatment. In addition, a palatal augmentation prosthesis with a metal framework, support, and retention part was fabricated. The palatal vault was reduced, so that even with limited tongue movement, adequate tongue-palate contact could be achieved. After placement of the definitive prostheses, the patient showed improvement in the functions of chewing, swallowing, and pronunciation.

Fracture Strength of All-Ceramic 3-Unit Fixed Partial Dentures Manufactured by CAD/CAM and Copy-Milling Systems (CAD/CAM 및 카피밀링 시스템을 이용하여 제작한 구치부 3-유닛 고정성 국소의치의 파절강도)

  • Kang, Hoo-Won;Kim, Hee-Jin;Kim, Jang-Ju;Ko, Myung-Won
    • Journal of Technologic Dentistry
    • /
    • v.34 no.2
    • /
    • pp.95-103
    • /
    • 2012
  • Purpose: Fracture strength of all-ceramic 3-unit fixed partial dentures manufactured by CAD/CAM and copy-milling systems were evaluated. Methods: Zirconia cores were made by milling the pre-sintered zirconia block by CAD/CAM or copy milling method followed by subsequent sintering. By building-up the corresponding porcelains on the core, all-ceramic bridges were fabricated, and those were evaluated in comparison with PFM fixed partial denture. Results: During the flexural test of the 3-unit PFM bridge, the porcelain started to chip or break at 507.28(${\pm}62.82$)kgf and the metal framework did not break until the maximum load level of 800kgf which was set in the testing instrument of this study. However, among all-ceramic restoration test groups, Everest(EV) group showed a peeling off or breakage of the porcelain from 365.64(${\pm}64.96$)kgf and the core was broken at 491.77(${\pm}55.62$)kgf. Those values of Zirkonzahn(ZR) were 431.03(${\pm}58.47$)kgf and 602.74(${\pm}48.44$)kgf, respectively. The break strength of the porcelain of PFM(PM) group was significantly higher than that of EV (p<0.05) group and there was no significant difference when comparing to that of ZR (p>0.05). ZR group showed higher break strength than that of EV group however there was no significant difference (p>0.05). The break strength of cores were in the increasing order of EV < ZR < PM (p<0.05). Conclusion: We could find that even though the PM group fractured at much higher value than all-ceramic cores, the breakage values of the porcelain of PM group with crack formation or delamination, which will be regarded as clinical failure, was significantly higher than that of EV group and not significantly higher than that of ZR group at p-values of 0.05. The break strength of ZR group was higher than that of EV group at an insignificant level(p>0.05).