FeCrMnN 계 스테인리스강의 일반부식 및 공식부식 거동에 미치는 고용 탄소의 영향 (Effects of Alloyed Carbon on the General Corrosion and the Pitting Corrosion Behavior of FeCrMnN Stainless Steels)

  • 하헌영;이태호;김성준
    • 대한금속재료학회지
    • /
    • 제49권10호
    • /
    • pp.780-789
    • /
    • 2011
  • The effects of alloyed carbon on the pitting corrosion, the general corrosion, and the passivity behavior of Fe18Cr10Mn0.4NxC (x=0~0.38 wt%) alloys were investigated by various electrochemical methods and XPS analysis. The alloyed carbon increased the general corrosion resistance of the FeCrMnN matrix. Carbon enhanced the corrosion potential, reduced the metal dissolution rate, and accelerated the hydrogen evolution reaction rate in various acidic solutions. In addition, carbon promoted the pitting corrosion resistance of the matrix in a chloride solution. The alloyed carbon in the matrix increased the chromium content in the passive film, and thus the passive film became more protective.

알루미늄 주조용 SKD61 금형강의 표면처리 방법에 따른 특성 평가 (Characteristic Evaluation According to the Surface Treatment Method of SKD61 Mold Steel for Aluminum Casting)

  • 최세원;김철우;김용호;유효상
    • 열처리공학회지
    • /
    • 제34권6호
    • /
    • pp.281-286
    • /
    • 2021
  • Arc ion plating (AIP), laser cladding, and nitriding are methods that can prevent mold damage or repair and create cracks and breakages on the die surface. The dissolution and soldering behavior of coated SKD61 by using arc ion plating, laser cladding, and nitriding was investigated. The structure of the coating was investigated as a function of deposition conditions by X-ray diffraction and the crystallographic orientation was determined using the texture factor. The TiAlN film deposited with AIP showed excellent corrosion resistance in the molten aluminum alloy at 680℃. In this paper, we have detailed the corrosion and mass loss phenomena associated with these steel-cast metal interactions.

Characterion of Calcium Phosphate Films Grown on Surgicl Ti-6AI-4V By Ion Beam Assisted Deposition

  • Lee, I-S.;Song, J-S.;Choi, J-M;Kim, H-E.
    • 한국진공학회지
    • /
    • 제7권s1호
    • /
    • pp.30-36
    • /
    • 1998
  • The plasma-spray technique is currently the most frequently used method to produce calcium phosphate coatings. Hydroxyapatite(HAp), one form of calcium phosphate, is preferred by its ability to form a direct bond with living bone, resulting in improvements of implant fixation and faster bone healing. Recently, concerns have been raised regarding the viable use and long-term stability of plasma-spray HAp coatings due to its nature of comparatively thick, porous, and poor bonding strength to metal implants. Thin layers (maximum of few microns) of calcium phosphate were formed by an e-beam evaporation with and without ion bombardments. The Ca/P ration of film was controlled by either using the evaporants having the different ration of Ca/P with addition of CaO, or adjusting the ion beam assist current. The Ca/P ration had great effects on the structure formation after heat treatment and the dissolution bahavior. The calcium phosphate films produced by IBAD exhibited high adhesion strength.

  • PDF

Determination of the pH of Iso-Selectivity of the Interfacial Diffusion Layer of Fe

  • Ha, Heon Young;Kwon, Hyuk Sang
    • Corrosion Science and Technology
    • /
    • 제7권1호
    • /
    • pp.40-44
    • /
    • 2008
  • Passive metal forms an interfacial diffuse layer on the surface of passive film by its reaction with $H^+$ or $OH^-$ ions in solution depending on solution pH. There is a critical pH, called pH point of iso-selectivity ($pH_{pis}$) at which the nature of the diffuse layer is changed from the anion-permeable at pH<$pH_{pis}$ to the cation-permeable at pH>$pH_{pis}$. The $pH_{pis}$ for a passivated Fe was determined by examining the effects of pH on the thickness of passive film and on the dissolution reaction occurring on the passive film under a gavanostatic reduction in borate-phosphate buffer solutions at various pH of 7~11. The steady-state thickness of passive film formed on Fe showed the maximum at pH 8.5~9, and further the nature of film dissolution reaction was changed from a reaction producing $Fe^{3+}$ ion at $pH\leq8.5$ to that producing $FeO_2{^-}$ at $pH\geq9$, suggesting that the $pH_{pis}$ of Fe is about pH 8.5~9. In addition, the passive film formed at pH 8.5~9, $pH_{pis}$, was found to be the most protective with the lowest defect density as confirmed by the Mott-Schottky analysis. Pitting potential was decreased with increasing $Cl^-$ concentration at $pH\leq8.5$ due probably to the formation of anion permeable diffuse layer, but it was almost constant at $pH\geq9$ irrespective of $Cl^-$ concentration due primarily to the formation of cation permeable diffuse layer on the film, confirming again that $pH_{pis}$ of Fe is 8.5~9.

커피박을 활용한 탄재 혼합 조건에 따른 용강 내 탄소의 농도 및 용해 효율 측정 (Measurement of Carbon Concentration and Dissolution Ratio in Molten Steel by the Mixing Conditions of Carbon Materials Using Coffee Grounds)

  • 김규완;류근용;김선중
    • 자원리싸이클링
    • /
    • 제30권1호
    • /
    • pp.77-82
    • /
    • 2021
  • 철강 산업에 있어서 CO2 배출량 감소는 중요한 이슈이며, CO2 배출 감소를 위해 코크스를 일부 대체할 수 있는 탄재 연료의 연구는 필요하다. 한편, 바이오매스 연료는 고정 탄소를 일부 함유하고 있으며, 반탄화 공정을 통해 연료내 탄소의 함량을 증가시킬 수 있다. 바이오매스 연료 중 커피박은 약 55 mass%의 탄소를 함유하고 있으며, 국내에서 연간 약 27만 ton이 매립 또는 소각되고 있다. 또한, 연간 커피 소비량의 증가로 인한 재활용 공정에 관한 연구가 필요하다. 본 연구에서는 반탄화 공정을 통한 커피박 내 고정 탄소의 농도에 미치는 온도의 영향을 연구하였다. 또한, 반탄화 커피박의 용해 실험을 통해 금속 샘플 내 탄소 농도와 용해 효율에 대한 코크스와 혼합비의 영향을 조사하였다.

Mineralogical studies and extraction of some valuable elements from sulfide deposits of Abu Gurdi area, South Eastern Desert, Egypt

  • Ibrahim A. Salem;Gaafar A. El Bahariya;Bothina T. El Dosuky;Eman F. Refaey;Ahmed H. Ibrahim;Amr B. ElDeeb
    • 분석과학
    • /
    • 제37권1호
    • /
    • pp.47-62
    • /
    • 2024
  • Abu Gurdi area is located in the South-eastern Desert of Egypt which considered as volcanic massive sulfide deposits (VMS). The present work aims at investigating the ore mineralogy of Abu Gurdi region in addition to the effectiveness of the hydrometallurgical route for processing these ores using alkaline leaching for the extraction of Zn, Cu, and Pb in the presence of hydrogen peroxide, has been investigated. The factors affecting the efficiency of the alkaline leaching of the used ore including the reagent composition, reagent concentration, leaching temperature, leaching time, and Solid /Liquid ratio, have been investigated. It was noted that the sulfide mineralization consists mainly of chalcopyrite, sphalerite, pyrite, galena and bornite. Gold is detected as rare, disseminated crystals within the gangue minerals. Under supergene conditions, secondary copper minerals (covellite, malachite, chrysocolla and atacamite) were formed. The maximum dissolution efficiencies of Cu, Zn, and Pb at the optimum leaching conditions i.e., 250 g/L NaCO3 - NaHCO3 alkali concentration, for 3 hr., at 250 ℃, and 1/5 Solid/liquid (S/L) ratio, were 99.48 %, 96.70 % and 99.11 %, respectively. An apparent activation energy for Zn, Cu and Pb dissolution were 21.599, 21.779 and 23.761 kJ.mol-1, respectively, which were between those of a typical diffusion-controlled process and a chemical reaction-controlled process. Hence, the diffusion of the solid product layer contributed more than the chemical reaction to control the rate of the leaching process. High pure Cu(OH)2, Pb(OH)2, and ZnCl2 were obtained from the finally obtained leach liquor at the optimum leaching conditions by precipitation at different pH. Finally, highly pure Au metal was separated from the mineralized massive sulfide via using adsorption method.

논토양의 환원환경에서 비소 및 중금속의 용출특성과 제강슬래그의 처리효과 (Leaching Behavior of Arsenic and Heavy-Metals and Treatment Effects of Steel Refining Slag in a Reducing Environment of Paddy Soil)

  • 윤성욱;유찬;윤용철;강동현;이시영;손진관;김동현
    • 한국농공학회논문집
    • /
    • 제58권3호
    • /
    • pp.29-38
    • /
    • 2016
  • There have been only a few studies focused on the stabilization of metal (loid)s in anaerobic soils such as paddy soils. In this study, laboratory-scale column tests were conducted to artificially manipulate anoxic conditions in submerged paddy fields and we observed the release behavior of As, Cd, Pb, and Zn, as well as to examine the stabilization effect of steel refining slag (SRS) on the metal(loid)s. The leachate samples were collected and chemical parameters were monitored during the test period. Results suggest that anoxic conditions were developed during submersion, and that As or heavy metals (particularly Cd) fractions bound to ferrous (Fe) /manganese (Mn) oxides were easily dissociated. Moreover, As is also reduced by itself to a trivalent form with higher mobility in the reducing environment of rice paddy soil. However, it was also shown that SRS significantly decreased the dissolution of Zn, Pb, Cd, and As in the the leachates; their removal rates in the SRS-treated soil were 66 %, 45 %, 24 %, and 84 %, respectively, of those in the control soil.

석회석과 제강슬래그를 이용한 오염토양 안정화에 따른 비소 및 중금속의 식물체 전이도 평가 (Assessment on the Transition of Arsenic and Heavy Metal from Soil to Plant according to Stabilization Process using Limestone and Steelmaking Slag)

  • 고일하;이상환;이원석;장윤영
    • 한국지하수토양환경학회지:지하수토양환경
    • /
    • 제18권7호
    • /
    • pp.63-72
    • /
    • 2013
  • This study estimated stabilization efficiency of As and heavy metal contaminated agricultural soil in abandoned mine through pot experiment. Also contaminants uptake of plant (lettuce) was compared as function of amendment (limestone, steelmaking slag and the mixture of these) addition. In soil solution analysis, concentration of contaminants in soil solutions which added limestone or steelmaking slag were lower than that of the mixture. Especially in As analysis, concentration with 5% (wt) addition of steelmaking slag showed the lowest value among those with other amendments. This seems that As stabilization happens through Fe adsorption during precipitation of Fe by pH increasing. Leachability of As in stabilized soil by TCLP was represented similar result with soil solution analysis. However leachability of heavy metals in stabilized soil was similar with that of non-stabilized soil due to dissolution of alkali precipitant by weak acid. Contaminants uptake rate by plant was also lower when limestone or steelmaking slag was used. However this study revealed that concentration of contaminants in soil solution didn't affect to the uptake rate of plant directly. Because lower $R^2$ (coefficient of determination) was represented in linear regression analysis between soil solution and plant.

일방향응고 Ni기초내열합금 GTD-111의 천이액상확산접합(II) -접합공정에서 모재조직의 변화- (Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(II) -Microstructural Change of Base Metal during Bonding Process -)

  • 강정윤;황형철;김인배;김대업;우인수
    • Journal of Welding and Joining
    • /
    • 제21권2호
    • /
    • pp.89-96
    • /
    • 2003
  • The change of microstructures in the base metal during transient liquid phase bonding process of directionally Ni base superalloy, GTD-111 was investigated. Bonds were fabricated using a series of holding times(0-7.2ks) at three different temperatures(1403, 1418 and 1453K) under a vacuum of 13.3mPa. In raw material, ${\gamma}$- ${\gamma}$' eutectic phases, platelet η phases, MC carbide and PFZ were seen in interdendritic regions or near grain boundary and size of primary ${\gamma}$' precipitates near interdendritic regions were bigger than core region. The primary ${\gamma}$' precipitates in dendrite core were dissolved early in bonding process, but ${\gamma}$' precipitates near interdendritic regions were dissolved partially and shape changed. The dissolution rate increased with increasing temperature. Phases in interdendritic regions or near pain boundary continually changed with time at the bonding temperature. In the bonding temperature of 1403K, eutectic phases had not significantly changed, but η phases had transformed from platelet shape to needle morphology and PFZ region had widened with time. The interdendritic region and near pain boundary were liquated partially at 1423k and fully at 1453k by reaction of η phases and PFZ. In the bonding temperature of 1453K, interdendritic region and near pain boundary were liquated and then new phases which mixed with η phases, PFZ and MC carbide crystallized during cooling. Crystallized η phases transformed from rod shape to platelet shape with increasing holding time.

Effects of Fertilizer and Sewage Sludge Treatments on Germination and Growth of Woody Plants in Metal Mine Tailings

  • Lee, Sul-Ki;Cho, Do-Soon
    • The Korean Journal of Ecology
    • /
    • 제23권6호
    • /
    • pp.445-452
    • /
    • 2000
  • The effects of sludge and fertilizer application on germination and seedling growth of woody plants on heavy metal mine tailings were evaluated by greenhouse experiment. Two different mine tailings (Lead-zinc mine tailings from Kwangmyong, Kyonggi-do and tungsten mine tailings from Sangdong. Kangwon-do). four fertilizer treatments (N +P +K: 20, 40, 60, and 80 kg/m$^3$), and four sewage sludge treatments (5.5, 11, 22.5, and 45 Mg/m$^3$) were used in the experiment. Tested plants were Pinus densiflora, Larix leptolepis, Amorpha fruticosa, and Alnus hirsuta. There were three replicates for each treatment. In addition, vermiculite was used instead of mine tailings to determine the effect of physical amendments. Fifty seeds of a species were sown in a pot (upper diameter 13.5 cm, depth 10 cm) and seedling emergence were recorded daily for 30 days. The highest germination rate was 53% for all treatments. Germination rate of Larix leptolepis was lowest among the four species studied. One month later after seeding, seedlings were thinned and only 5 seedling were left in each pot, and fertilizer and sewage sludge were applied once again. Growth of seedlings were determined for 10 weeks since then. Most plants grew very poorly or died within 5 weeks on lead/zinc mine tailings from Kwangmyong. The analysis of heavy metal contents by the total dissolution method showed that heavy metals generally increased in the order of tungsten mine tailings from Sangdong < sewage sludge from Puchon < lead/zinc mine tailings from Kwangmyong. Growth of woody plants was improved significantly by the fertilizer treatments on tungsten mine tailings. In contrast. survival and growth of woody plants were not affected significantly by the sewage sludge treatment on both tailings. This study shows that fertilizer applied to established seeded stands may provide some benefits in terms of increased ground cover in the field. It is suggested that reclamation should be proceeded by the study of the physico-chemical and biological characteristics of mine tailings.