• Title/Summary/Keyword: Maximum Size of Aggregate

Search Result 130, Processing Time 0.024 seconds

A Study on the Gradation Effect of the Property of Roller Compacted Concrete Pavement (골재 입도분포가 도로포장용 롤러전압 콘크리트에 미치는 영향 연구)

  • Song, Si Hoon;Lee, Seung Woo
    • International Journal of Highway Engineering
    • /
    • v.17 no.3
    • /
    • pp.49-58
    • /
    • 2015
  • PURPOSES : The use of environmentally friendly construction methods has been recently encouraged to reduce fuel consumption and the effects of global warming. For this purpose, the roller compacted concrete pavement (RCCP) construction method has been developed. RCCP is more environmentally friendly and economically efficient than general concrete by reducing the amount of CO2 generated through the application of a smaller amount of cement. RCCP has a number of advantages such as an easy construction method, low cost, high structural hydration performance, and aggregate interlocking. However, mix design standards and construction guidelines of RCCP are required for domestic application. In addition, a study on aggregate selection, which has an effect on the characteristics of RCCP, is necessary owing to a limited number of researches. Thus, the aggregate effect on the performance of RCCP in securing the required strength and workability was evaluated in consideration of domestic construction. METHODS : Sand and coarse aggregates of both 19mm and 13mm in maximum size were used in this study. Four types of aggregate gradations (s/a = 30%, 58%, and 70% for the sand and coarse aggregate of 19mm in maximum size, and s/a = 50% for a combination of the three types of aggregates) were set up to investigate the effects of the PCA band on the RCC characteristics. The conditions of s/a = 30% and 70% were evaluated to check the gradation effect outside of the recommended band. The conditions of s/a = 58% and 50% were used because they are the optimum combination of the two and three types of aggregates, respectively. RCCP gradation band was suggested gradation with a proper construction method of RCCP by synthetically comparing and analyzing the correlation of optimum water content, maximum dry density, and strength of requirements through its consistency and compaction test. RESULTS : The lower and upper limit lines are insufficient to secure a relatively strong development and workability compared to an aggregate gradation in the RCCP gradation band region. On the other hand, the line in the RCCP gradation band and the 0.45 power curve in the RCCP gradation band region were satisfactory, ensuring the required strength and workability. CONCLUSIONS : The suitable aggregate gradation on RCCP process should meet the RCCP gradation band area; however, fine particles passing through a #60 sieve do not need to be within the recommended gradation band because the influence of this region on such fine particles is small.

FRACTAL SURFACE ROUGHNESS OF CONCRETE

  • Roh Y.S.;Xi Yunping;Chung L.
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.11a
    • /
    • pp.595-602
    • /
    • 2004
  • In this study, the roughness of fracture surfaces in cementitious material has been characterized by roughness number (RN). A systematic experimental investigation was carried out to examine the dependency of fracture parameters on the aggregate sizes as well as the loading rates. Three aggregate sizes (0.1875 in, 0.5 in, and 0.75 in) and two loading rates (slow and fast loading rate) were used. A total of 52 compression tests and 53 tension tests were performed. All fracture parameters exhibited an increase, to varying degrees, when aggregates were added to the mortar matrix. The fracture surfaces of the specimens were digitized and analyzed. Fracture roughness was monotonically increased as maximum aggregate sizes increase.

  • PDF

Engineering Properties of Concrete Using Recycled Aggregate Manufactured by Bar-Crusher (봉파쇄기에 의해 제조된 재생굵은골재를 사용한 콘크리트의 공학적 특성)

  • Baek, Dae-Hyun;Han, Dong-Yeob;Yu, Myoung-Youl;Lee, Gun-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2006.11a
    • /
    • pp.83-86
    • /
    • 2006
  • This study investigates engineering properties of concrete using recycled coarse aggregated manufactured by bar-crusher. Test showed that Bar-crusher(S) had more effective results at fresh state than cone-crusher(C) and impact-crusher(I). In case of specimens manufactured by S, increase of spindle velocity, incorporating ratio of recycled aggregate and maximum size of aggregate inclined fluidity. As for the hardened concrete, compressive strength of specimens by C or I exhibited lower value than that of S. In addition, specimens using recycled aggregate manufactured by 400rpm and 500rpm of spindle velocity showed less than 10% reduction rate of strength, which is not significant reducing value. It is found that 500rpm of the spindle velocity had the best strength performance, while 600rpm was the worst. Strength value of specimens decreased as incorporating ratio of recycled aggregate inclined, but the strength value of most specimens exhibited less than 10% of reducing rate, assuming favorable result, only at less than 25% incorporating ratio of recycled aggregate.

  • PDF

Polyvinyl-alcohol fiber-reinforced concrete with coarse aggregate in beam elements

  • Leonardo M. Massone;Jaime Reveco;Alejandro Arenas;Fabian Rojas
    • Advances in Computational Design
    • /
    • v.8 no.2
    • /
    • pp.113-131
    • /
    • 2023
  • The use of fibers has been commonly considered in engineered cementitious composites, but their behavior with coarse aggregate in concrete has not been studied significantly, which is needed to meet structural performance objectives for design, such as ductility. This research analyzes the behavior of fiber-reinforced concrete with coarse aggregate with 0.62%, 1.23%, and 2% PVA (Polyvinyl-alcohol) content, varying the maximum aggregate size. Tensile (direct and indirect) and compressive concrete tests were performed. The PVA fiber addition in coarse aggregate concrete increased the ductility in compression, especially for the fiber with a larger aspect ratio, with a minor impact on strength. In addition, the tensile tests showed that the PVA fiber increased the tensile strength of concrete with coarse aggregate and, more significantly, improved the ductility. A selected mixture was used to build short and slender reinforced concrete beams to assess the behavior of structural members. PVA fiber addition in short beams changed the failure mode from shear to flexure, increasing the deflection capacity. On the other hand, the slender beam tests revealed negligible impact with the use of PVA.

Fracture Behavior and Crack Growth of Concrete by The Nonlinear Fracture Mechanics (비선형 파괴역학에 의한 콘크리트의 파괴거동과 균열성장에 관한 연구)

  • 배주성;나의균
    • Magazine of the Korea Concrete Institute
    • /
    • v.2 no.2
    • /
    • pp.81-92
    • /
    • 1990
  • Concrete, a mixed material, has heterogeniety, anisotrophy and nonlinearity. Therefore, in its 'racture analysis, it is more reasonable to evaluate its fracture toughness by applying the concept of 'racture mechanics rather than the strength concept. Up to the present the concepts of fracture mechanics which were applied to concrete have been divided into two main classes. The one is the concept of linear elastic fracture mechanics and the other is the concept of elastic-plastic fracture mechanics. But it has been pointed out that there are many problems and irrationalities in applying the concept of linear elastic fracture mechanics to concrete. In this study, the J -integral method and the COD method mainly used in the analysis of nonlinear fracture mechanics, were introduced and the three point bending test was carried out for investigating the effects of the variation of the maximum aggregate size and notch depth on the fracture behavior and the crack growth of concrete, and the relationships of fracture energy and crack opening displacement. According to the results of this study the more the maximum aggregate size and the notch depth increased, the more the nonlinearity of load-deflection behavior was remarkable. The increase of the coarse aggregate size created the more ductility of concrete. Thus concrete showed the more stable fracture. As for the path of the crack growth, the more the coarse aggregate size increased, the more it was irregulary deviated from the straight line but it was not almost affected by the variation of the notch depth. Also, the fracture energy increased according as the coarse aggregate size increased and the notch depth decreased.

Effect of Maximum Size and Contents Method of Recycled Aggregate Powder on Engineering Properties of the Cement Mortar (순환골재 미분말의 최대입경 및 치환방법이 시멘트 모르터의 공학적 특성에 미치는 영향)

  • Han, Min-Cheol;Jeon, Kyu-Nam
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.4
    • /
    • pp.129-136
    • /
    • 2010
  • This study is to investigate experimentally the engineering characteristics of cement mortar according to the replacement method and contents of recycled aggregate powder (RP) by collecting the recycled aggregate powder with the maximum size of below 0.08 mm and 0.15 mm. then, the results of the study can be summarized as follows. The flow of flesh mortar represented a trend in decreasing while the recycled aggregate powder was substituted as it is compared with that of plain. In addition, in case of correlation between tests, it appeared that the correlation between flow and ring flow is big. In the case of the characteristics of hardened mortar, the strength showed more improvements as the RP was substituted to aggregate than the case, which is substituted to aggregate. In addition, it was verified that the results in which the RP was substituted to aggregate by 5% represented similar values to that of the plain according to the passage of age.

  • PDF

Property Evaluation of the Concrete Replacing 5-13mm Recycled Coarse Aggregates (5~13mm 입도분급 순환 굵은 골재 혼합사용에 따른 콘크리트의 특성평가)

  • Han, Min-Cheol;Song, Young-Wo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.1
    • /
    • pp.55-61
    • /
    • 2017
  • This paper is to investigate experimentally the effect of substitution of recycled coarse aggregate(RCA) under 13mm on the engineering properties of the concrete using gap graded coarse aggregates. Concretes with 0.4 of water to cement ratio(W/C) were fabricated to achieve 30MPa of design strength with coarse aggregate over 13mm in size with the maximum size of 25mm. RCA was substituted for coarse aggregate over 13mm from 10% to 50% and crushed coarse aggregate under 13mm was also substituted for coarse aggregate over 13mm from 20% to 40%, respectively. Test results indicated that the replacement of RCA up to 20% resulted in an increase of fluidity and strength. It also caused a decrease in the drying shrinkage due to dense packing effect by achieving continuous grading of mixed aggregates. For practical application of RCA, when properly substituted, the use of RCA enabled the concrete to reduce water contents and sand to aggregate ratio in mixing design stage of the concrete. And, it can also enhance the compressive strength of the concrete.

An Experimental Study on the Structural Characteristics of Reinforced Concrete Beams Containing Oyster Shells (굴패각을 사용한 철근콘크리트 보의 특성에 관한 실험적 연구)

  • Lee, Sang-cheol;Woo, Song-gyu;An, Yong-deok;Jun, Hak-su;Koo, Hae-shik
    • KIEAE Journal
    • /
    • v.7 no.5
    • /
    • pp.135-142
    • /
    • 2007
  • This is an experimental study on the structural characteristics of reinforced concrete beams using of the oyster shells as a substitute fine aggregate of concrete. In this study, the main factors consist of the grain sizes and the percentage of substitution of oyster shells to fine aggregate in the equal water cement ratio. The results of the study showed as followed. The initial load value of them represented similar constant within 10% of the maximum load value in each test beam. But the maximum load value and the ultimate load value decreased with increased grain size and the rate of substitution. As the grain size of oyster shells became smaller, the load values of them were somewhat higher. The deflection among deformation properties of reinforced concrete beams with oyster shells represented typical curves like that of normal reinforced concrete. In the deformation of steel and concrete, the deformation was proportionated to the load till yield point and from yield point until approaching the ultimate load point. One type was typical curve of the load and the deformation and the other type irregularly was changed to very small deformation for the load increase centering around load axis. After the analyzing structural behaviors and the properties of reinforced concrete test beams with oyster shells, the most excellent grain size of oyster shells represented 1.0mm and less or 5.0mm and less with taking uniformly, and the percentage of practicable substitution of them to fine aggregate was about 30%.

Expansion behavior of concrete containing different steel slag aggregate sizes under heat curing

  • Shu, Chun-Ya;Kuo, Wen-Ten
    • Computers and Concrete
    • /
    • v.16 no.3
    • /
    • pp.487-502
    • /
    • 2015
  • This study investigated particle expansion in basic oxygen furnace slag (BOF) and desulfurization slag (DSS) after heat curing by using the volume method. Concrete hydration was accelerated by heat curing. The compressive strength, ultrasonic pulse velocity, and resistivity of the concrete were analyzed. Maximum expansion occurred in the BOF and DSS samples containing 0.30-0.60 mm and 0.60-1.18 mm particles, respectively. Deterioration was more severe in the BOF samples. In the slag aggregates for the complete replacement of fine aggregate, severe fractures occurred in both the BOF and DSS samples. Scanning electron microscopy revealed excess CH after curing, which caused peripheral hydration products to become extruded, resulting in fracture.

The effects of limestone powder and fly ash as an addition on fresh, elastic, inelastic and strength properties of self-compacting concrete

  • Hilmioglu, Hayati;Sengul, Cengiz;Ozkul, M. Hulusi
    • Advances in concrete construction
    • /
    • v.14 no.2
    • /
    • pp.93-102
    • /
    • 2022
  • In this study, limestone powder (LS) and fly ash (FA) were used as powder materials in self-compacting concrete (SCC) in increasing quantities in addition to cement, so that the two powders commonly used in the production of SCC could be compared in the same study. Considering the reduction of the maximum aggregate size in SCC, 10 mm or 16 mm was selected as the coarse aggregate size. The properties of fresh concrete were determined by slump flow (including T500 time), V-funnel and J-ring experiments. The experimental results showed that as the amount of both LS and FA increased, the slump flow also increased. The increase in powder material had a negative effect on V-funnel flow times, causing it to increase; however, the increase in FA concretes was smaller compared to LS ones. The increase in the powder content reduced the amount of blockage in the J-ring test for both aggregate sizes. As the hardened concrete properties, the compressive and splitting strengths as well as the modulus of elasticity were determined. Longitudinal and transverse deformations were measured by attaching a special frame to the cylindrical specimens and the values of Poisson's ratio, initiation and critical stresses were obtained. Despite having a similar W/C ratio, all SCC exhibited higher compressive strength than NVC. Compressive strength increased with increasing powder content for both LS and FA; however, the increase of the FA was higher than the LS due to the pozzolanic effect. SCC with a coarse aggregate size of 16 mm showed higher strength than 10 mm for both powders. Similarly, the modulus of elasticity increased with the amount of powder material. Inelastic properties, which are rarely found in the literature for SCC, were determined by measuring the initial and critical stresses. Crack formation in SCC begins under lower stresses (corresponding to lower initial stresses) than in normal concretes, while critical stresses indicate a more brittle behavior by taking higher values.