• Title/Summary/Keyword: Magnetic nanoparticle silica

검색결과 13건 처리시간 0.029초

Polyamine Group Assembled Silica Coated Ferrite Nanoparticle for Lambda DNA Detection

  • Park, Moo-Eon;Chang, Jeong-Ho
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1193-1194
    • /
    • 2006
  • The magnetic ferrite nanoparticles were synthesized and coated by silica precursor in controlling the coating thicknesses and sizeses. The surface modification was performed with amino-functionalized organic silanes on silica coated magnetic nanoparticles. The use of functionalized self-assembled magnetic ferrite nanoparticles for nucleic acid separation process give a lot of advantages rather than the conventional silica based process.

  • PDF

아미노실란화 철산화물 나노입자를 이용한 Human DNA의 초고속 자성분리 (High Throughput Magnetic Separation for Human DNA by Aminosilanized Iron Oxide Nanoparticles)

  • 강기호;장정호
    • 한국세라믹학회지
    • /
    • 제45권10호
    • /
    • pp.605-609
    • /
    • 2008
  • This work describes the preparation of functionalized magnetic nanoparticles(MNPs) and their bioapplication to human DNA separation. Silica coated MNPs were prepared by changing the volume ratio of tetraethyl orthosilicate(TEOS) for controlled coating thickness on the original nanoparticle of MNPs. The sol-gel process in silica coating on MNPs surface was adapted for relatively mild reaction condition, low-cost, and surfactant-free. And then amino functionalized magnetic nanoparticles were synthesized using amine groups as surface modifiers. The result of adsorption efficiency for human DNA with amino-functionalized silica coated MNPs was calculated as a function of the number of amine groups.

소수성의 실리카 나노입자가 충진된 치아수복용 고분자 복합체 제조 (Synthesis of Polymeric Dental Restorative Composite Filled with Hydrophobic Silica Nanoparticle)

  • 한상혁;서기택;마승재;임상명;김오영
    • 공업화학
    • /
    • 제17권4호
    • /
    • pp.403-408
    • /
    • 2006
  • 가시광선 중합형의 고분자계 치아수복재의 고기능화를 위해 충전제로 사용된 친수성의 실리카 나노입자 표면을 $\gamma$-methacryloxypropyltrimethoxysilane ($\gamma$-MPS) 결합제로 소수성 처리하여 치아수복용 고분자 복합체를 제조하였다. 처리된 실리카의 구조적 물성과 복합체 내에서의 분산도 및 복합체의 중합 특성 등을 실리카의 소수화도와 비교하여 고찰하였다. 그 결과, 사용된 $\gamma$-MPS의 양이 40 wt%까지 증가함에 따라 실리카의 소수화도가 증가하였으며 그 이상에서는 큰 변화가 없었다. 또한 소수화도가 향상됨에 따라 복합체 내에서의 충전제 분산도가 양호하였으며 광중합 후 미반응 단량체는 핵자기공명 분석 결과 거의 남아 있지 않아 중합 특성이 우수함을 확인하였다.

난류 확산화염에서 체류시간이 실리카 나노입자의 생성에 미치는 영향 (The Effect of Residence Time on the Generation of Silica Nanoparticles in a Turbulent Diffusion Flame)

  • 곽인재;배수호;신현동
    • 한국연소학회:학술대회논문집
    • /
    • 한국연소학회 2006년도 제33회 KOSCO SYMPOSIUM 논문집
    • /
    • pp.196-201
    • /
    • 2006
  • Silica(SiO2) nanoparticles are used as additives in plastics and rubbers to improve mechanical, electrical, magnetic properties and optical material. Silica nanoparticles were synthesized by the gas phase thermal oxidation of several kinds of precursors in many types of reactor. Diffusion flame reactor has some advantages compared with other types of reactors. In this study, we investigated the generation of silica nanoparticles on the effect of residence time by tetraethylothosilicate(TEOS) in a turbulent diffusion flame reactor controlled by providing reactant flowrate and reactor geometry affect particle morphology, particle size and particle size distribution. To determine the flame residence time, flame length should be determined which was examined by ICCD image. Particle size, distribution and morphology were performed with TEM.

  • PDF

실란 커플링제에 의해 표면이 개질된 실리카 나노입자의 분광학적 분석 (Spectroscopic Analysis of Silica Nanoparticles Modified with Silane Coupling Agent)

  • 송성규;김정혜;황기섭;하기룡
    • Korean Chemical Engineering Research
    • /
    • 제49권2호
    • /
    • pp.181-186
    • /
    • 2011
  • 본 연구에서는 실리카 나노 입자의 표면 개질을 위해 실란 커플링제인 3-(trimethoxysilyl)propylmethacrylate(MPS) 를 사용하여 표면 개질 반응을 수행하였다. 용매의 pH, MPS의 가수 분해 반응시간, 표면 개질 반응시간 및 실리카 표면의 실라놀기(Si-OH)에 대한 MPS의 몰 비를 변화하여 각각의 반응조건이 실리카 표면개질 반응에 미치는 영향을 연구하였다. 개질반응 후 Fourier Transform Infrared Spectroscopy(FTIR), 원소분석(EA) 및 고체 상태 cross-polarization magic angle spinning(CP/MAS) Nuclear Magnetic Resonance Spectroscopy(NMR)법을 사용하여 표면이 개질된 실리카 입자들의 분석을 수행하였다. 연구 결과 용매의 pH가 4.5일 때 MPS가 단량체 형태로 실리카 표면의 실라놀기와 반응하고 이외의 pH에서는 MPS가 이량체, 삼량체 혹은 사량체의 올리고머 형태로 실리카의 실라놀기와 반응함이 우세함을 나타내었다. 가수분해반응 시간을 30분에서 90분으로 증가시키면 MPS가 올리고머 형태로 실리카 표면의 실라놀기와 반응하는 것이 우세하고, 투입한 MPS 몰 비의 증가도 MPS가 올리고머 형태로 실리카 표면의 실라놀기와 반응하는 것이 우세함을 나타내었다.

실리카 나노입자 표면에 결합된 아미노기와 Glycidyl Methacrylate의 반응에 관한 분광학적 연구 (Spectroscopic Studies on the Reaction between Amino Groups on Silica Nanoparticle Surface and Glycidyl Methacrylate)

  • 이상미;하기룡
    • 폴리머
    • /
    • 제37권6호
    • /
    • pp.777-783
    • /
    • 2013
  • 본 연구에서는 실리카 나노입자를 dipodal 형태의 bis[3-(trimethoxysilyl)propyl]amine(BTMA) 실란 커플링제로 실리카 표면을 개질한 후, glycidyl methacrylate(GMA)로 표면 처리를 하여 실리카에 결합된 BTMA의 N-H기와 GMA의 epoxide기의 개환 반응에 의하여 실리카 표면에 중합용 methacrylate기를 도입하는 연구를 수행하였다. 반응시간, 반응온도 및 투입하는 GMA의 농도 변화가 BTMA의 N-H기와 GMA의 epoxide기 사이의 반응에 미치는 영향을 Fourier transform infrared spectroscopy(FTIR), elemental analysis(EA) 및 고체상태 $^{13}C$ cross-polarization magic angle spinning(CP/MAS), nuclear magnetic resonance spectroscopy(NMR)법을 사용하여 분석하였다. BTMA로 개질된 실리카를 GMA로 처리하면 실리카 입자에 결합되어 있는 BTMA의 N-H기와 GMA의 epoxide기가 열리면서 상호 반응이 일어났으며, 실험한 조건에서는 반응시간, 반응온도 및 투입하는 GMA 농도가 증가할수록 실리카 표면에 도입되는 methacrylate기가 증가함을 확인하였다.

Utilization of functionalized magnetic nanoparticles for high throughput DNA separation

  • 장정호
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2009년도 추계학술발표대회
    • /
    • pp.12.2-12.2
    • /
    • 2009
  • The work describes anoptimized process to highly efficient and convenient preparation in highthroughput magnetic human DNA separation with chemically functionalizedsilica-coated magnetic nanoparticles. The effect of nanoparticle's size and the surface's hydrophilicity change were studied for magnetic DNA separation process, inwhich the optimum efficiency was explored via the function of the amino-groupnumbers, particle size, the amount of the nanoparticles used, and theconcentration of NaCl salt. The DNA adsorption yields were high in terms of theamount of triamino-functionalized nanoparticles used, and the average particlesize was 25 nm. The adsorption efficiency of aminofunctionalized nanoparticleswas the 4-5 times (80-100%) higher compared to silica-coated nanoparticles only(10-20%). DNA desorption efficiency showed an optimum level of over 0.7 M ofthe NaCl concentration. To elucidate the agglomeration of nanoparticles afterelectrostatic interaction, the Guinier plots were calculated from small angleX-ray diffractions in a comparison of the results of electron diffraction TEM,and confocal laser scanning microscopy. Additionally, the direct separation ofhuman genomic DNA was achieved from human saliva and whole blood with highefficiency.

  • PDF

Cytotoxicity and DNA Damage Induced by Magnetic Nanoparticle Silica in L5178Y Cell

  • Kang, Jin-Seok;Yum, Young-Na;Park, Sue-Nie
    • Biomolecules & Therapeutics
    • /
    • 제19권2호
    • /
    • pp.261-266
    • /
    • 2011
  • As recent reports suggest that nanoparticles may penetrate into cell membrane and effect DNA condition, it is necessary to assay possible cytotoxic and genotoxic risk. Three different sizes of magnetic nanoparticle silica (MNP@$SiO_2$) (50, 100 and 200 nm diameter) were tested for cytotoxicity and DNA damage using L5178Y cell. MNP@$SiO_2$ had constant physicochemical characteristics confirmed by transmission electron microscope, electron spin resonance spectrometer and inductively coupled plasma-atomic emission spectrometer for 48 h. Treatment of MNP@$SiO_2$ induced dose and time dependent cytotoxicity. At 6 h, 50, 100 or 200 nm MNP@$SiO_2$ decreased significantly cell viability over the concentration of 125 ${\mu}g/ml$ compared to vehicle control (p<0.05 or p<0.01). Moreover, at 24 h, 50 or 100 nm MNP@$SiO_2$ decreased significantly cell viability over the concentration of 125 ${\mu}g/ml$(p<0.01). And treatment of 200 nm MNP@$SiO_2$ decreased significantly cell viability at the concentration of 62.5 ${\mu}g/ml$ (p<0.05) and of 125, 250, 500 ${\mu}g/ml$ (p<0.01, respectively). Furthermore, at 48 h, 50, 100 or 200 nm MNP@$SiO_2$ decreased significantly cell viability at the concentration of 62.5 ${\mu}g/ml$ (p<0.05) and of 125, 250, 500 ${\mu}g/ml$ (p<0.01, respectively). Cellular location detected by confocal microscope represented they were existed in cytoplasm, mainly around cell membrane at 2 h after treatment of MNP@$SiO_2$. Treatment of 50 nm MNP@$SiO_2$ significantly increased DNA damage at middle and high dose (p<0.01), and treatment of 100 nm or 200 nm significantly increased DNA damage in all dose compared to control (p<0.01). Taken together, treatment of MNP@$SiO_2$ induced cytotoxicity and enhanced DNA damage in L5178Y cell.

Ionic liquid coated magnetic core/shell CoFe2O4@SiO2 nanoparticles for the separation/analysis of trace gold in water sample

  • Zeng, Yanxia;Zhu, Xiashi;Xie, Jiliang;Chen, Li
    • Advances in nano research
    • /
    • 제10권3호
    • /
    • pp.295-312
    • /
    • 2021
  • A new ionic liquid functionalized magnetic silica nanoparticle was synthesized and characterized and tested as an adsorbent. The adsorbent was used for magnetic solid phase extraction on ICP-MS method. Simultaneous determination of precious metal Au has been addressed. The method is simple and fast and has been applied to standard water and surface water analysis. A new method for separation/analysis of trace precious metal Au by Magnetron Solid Phase Extraction (MSPE) combined with ICP-MS. The element to be tested is rapidly adsorbed on CoFe2O4@SiO2@[BMIM]PF6 composite nano-adsorbent and eluted with thiourea. The method has a preconcentration factor of 9.5-fold. This method has been successfully applied to the determination of gold in actual water samples. Hydrophobic Ionic Liquids (ILs) 1-butyl-3-methylimidazole hexafluorophosphate ([BMIM]PF6) coated CoFe2O4@SiO2 nanoparticles with core-shell structure to prepare magnetic solid phase extraction agent (CoFe2O4@SiO2@ILs) and establish a new method of MSPE coupled with inductively coupled plasma mass spectrometry for separation/analysis of trace gold. The results showed that trace gold was adsorbed rapidly by CoFe2O4@SiO2@[BMIM]PF6 and eluanted by thiourea. Under the optimal conditions, preconcentration factor of the proposed method was 9.5-fold. The linear range, detection limit, correlation coefficient (R) and relative standard deviation (RSD) were found to be 0.01~1000.00 ng·mL-1, 0.001 ng·mL-1, 0.9990 and 3.4% (n = 11, c = 4.5 ng·mL-1). The CoFe2O4@SiO2 nanoparticles could be used repeatedly for 8 times. This proposed method has been successfully applied to the determination of trace gold in water samples.

Characterizations of Modified Silica Nanoparticles(I)

  • Min, Seong-Kee;Park, Chan-Young;Lee, Won-Ki;Seul, Soo-Duk
    • 한국재료학회지
    • /
    • 제22권6호
    • /
    • pp.275-279
    • /
    • 2012
  • (3-mercaptopropyl)trimethoxysilane (MPTMS) was used as a silylation agent, and modified silica nanoparticles were prepared by solution polymerization. 2.0 g of silica nanoparticles, 150 ml of toluene, and 20 ml of MPTMS were put into a 300 ml flask, and these mixtures were dispersed with ultrasonic vibration for 60 min. 0.2 g of hydroquinone as an inhibitor and 1 to 2 drops of 2,6-dimethylpyridine as a catalyst were added into the mixture. The mixture was then stirred with a magnetic stirrer for 8 hrs. at room temperature. After the reaction, the mixture was centrifuged for 1 hr. at 6000rpm. After precipitation, 150 ml of ethanol was added, and ultrasonic vibration was applied for 30 min. After the ultrasonic vibration, centrifugation was carried out again for 1 hr. at 6000rpm. Organo-modification of silica nanoparticles with a ${\gamma}$-methacryloxypropyl functional group was successfully achieved by solution polymerization in the ethanol solution. The characteristics of the ${\gamma}$-mercaptopropyl modified silica nanoparticles (MPSN) were examined using X-ray photoelectron spectroscopy (XPS, THERMO VG SCIENTIFIC, MultiLab 2000), a laser scattering system (LSS, TOPCON Co., GLS-1000), Fourier transform infrared spectroscopy (FTIR, JASCO INTERNATIONL CO., FT/IR-4200), scanning electron microscopy (SEM, HITACHI, S-2400), an elemental analysis (EA, Elementar, Vario macro/micro) and a thermogravimetric analysis (TGA, Perkin Elmer, TGA 7, Pyris 1). From the analysis results, the content of the methacryloxypropyl group was 0.98 mmol/g and the conversion rate of acrylamide monomer was 93%. SEM analysis results showed that the organo-modification of ultra-fine particles effectively prevented their agglomeration and improved their dispensability.