• 제목/요약/키워드: MN9D

검색결과 211건 처리시간 0.021초

Involvement of Corticotropin-releasing Factor Receptor 2β in Differentiation of Dopaminergic MN9D Cells

  • Jin, Tae-Eun;Jang, Miae;Kim, Hyunjung;Choi, Yu Mi;Cho, Hana;Chung, Sungkwon;Park, Myoung Kyu
    • Molecules and Cells
    • /
    • 제26권3호
    • /
    • pp.243-249
    • /
    • 2008
  • Corticotropin releasing factor (CRF) mediates various responses to stress through CRF receptors 1 and 2. CRF receptor 2 has two forms, $2{\alpha}$ and $2{\beta}$ each of which appears to have distinct roles. Here we used dopaminergic neuron-derived MN9D cells to investigate the function of CRF receptor 2 in dopamine neurons. We found that n-butyrate, a histone deacetylase inhibitor, induced MN9D cell differentiation and increased gene expression of all CRF receptors. CRF receptor $2{\beta}$ was minimally expressed in MN9D cells; however, its expression dramatically increased during differentiation. CRF receptor $2{\beta}$ expression levels appeared to correlate with neurite outgrowth, suggesting CRF receptor $2{\beta}$ involvement in neuronal differentiation. To validate this statement, we made a CRF receptor $2{\beta}$-overexpressing $MN9D/CRFR2{\beta}$ stable cell line. This cell line showed robust neurite outgrowth and GAP43 overexpression, together with MEK and ERK activation, suggesting MN9D cell neuronal differentiation. From these results, we conclude that CRF receptor $2{\beta}$ plays an important role in MN9D cell differentiation by activating the MEK/ERK signaling pathway.

Oxidation of Fe-(5.3-29.8)%Mn-(1.1-1.9)%Al-0.45%C Alloys at 550-650 ℃

  • Park, Soon Yong;Xiao, Xiao;Kim, Min Ji;Lee, Geun Taek;Hwang, Dae Ho;Woo, Young Ho;Lee, Dong Bok
    • Corrosion Science and Technology
    • /
    • 제21권1호
    • /
    • pp.53-61
    • /
    • 2022
  • Alloys of Fe-(5.3-29.8)%Mn-(1.1-1.9)%Al-(0.4-0.5)%C were oxidized at 550 ℃ to 650 ℃ for 20 h to understand effects of alloying elements on oxidation. Their oxidation resistance increased with increasing Mn level to a small extent. Their oxidation kinetics changed from parabolic to linear when Mn content was decreased and temperature was increasing. Oxide scales primarily consisted of Fe2O3, Mn2O3, and MnFe2O4 without any protective Al-bearing oxides. During oxidation, Fe, Mn, and a lesser amount of Al diffused outward, while oxygen diffused inward to form internal oxides. Both oxide scales and internal oxides consisted of Fe, Mn, and a small amount of Al. The oxidation of Mn and carbon transformed γ-matrix to α-matrix in the subscale. The oxidation led to the formation of relatively thick oxide scales due to inherently inferior oxidation resistance of alloys and the formation of voids and cracks due to evaporation of manganese, decarburization, and outward diffusion of cations across oxides.

Figure of merit and bending characteristics of Mn-SnO2/Ag/Mn-SnO2 tri-layer film (Mn-SnO2/Ag/Mn-SnO2 3중 다층막의 성능지수와 밴딩 특성)

  • Cho, Youngsoo;Jang, Guneik
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • 제31권4호
    • /
    • pp.190-195
    • /
    • 2021
  • Typical Mn-SnO2/Ag/Mn-SnO2 tri-layer films were prepared on a PET substrate by RF/DC magnetron sputtering method at room temperature. Based on EMP simulation, the thicknesses of the top and bottom Mn-doped SnO2 layers were kept at 40 nm and the Ag layer was maintained at 13 nm for continuous electrical conduction. The experimentally measured optical transmittances at 550 nm wavelength were ranged from 82.9 to 88.1 % and sheet resistances were varied from 5.9 to 6.9 Ω/☐. The highest value of figure of merit, ϕTC was 48.1 × 10-3 Ω-1. Based on bending test under 4 and 5 mm of inner and outer curvature radius condition, tri-layer film resistance varies only by approximately 1.5 % after 10,000 bending cycles, showing excellent mechanical flexibility.

Mutual Solubility of Mn and Fe in AZ91 Alloy Melts and Its Application to Composition Control of AZ91D Recycled Ingots (AZ91 합금 용탕내 Mn과 Fe의 상호용해도 측정 및 AZ91D 재생지금의 성분조정에의 활용)

  • Kwon, Soon-Il;Byun, Ji-Young;Kim, Seon-Jin;Shim, Jae-Dong
    • Korean Journal of Materials Research
    • /
    • 제13권9호
    • /
    • pp.619-624
    • /
    • 2003
  • This paper describes a method to control Mn and Fe contents in recycled AZ91D ingots, based on the mutual solubility of Mn and Fe in AZ91 alloy melts. For this purpose, Fe solubility with the change of Mn content and temperature was investigated in the homogenized and re-precipitated liquid AZ91 alloy. The increase of the amount of Mn added to the melt resulted in the decrease of Fe content. The data obtained in this study was adopted to the pilot plant for recycling of the scrap. As a result, Mn and Fe contents measured in the recycled ingot were in good agreement with ASTM B93 standard.

Sintering and the Optical Properties of Mn3O4-added Al2O3 (Mn3O4를 첨가한 Al2O3 세라믹스의 소결 및 광학 특성)

  • Kim, Jin-Ho;Baik, Seung-Woo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • 제29권9호
    • /
    • pp.539-545
    • /
    • 2016
  • Alumina added with Mn3O4 up to 7.5 cat% of Mn was prepared by conventional ceramic processing, and the sintering behavior and the optical properties of which were studied as functions of Mn content. Densification and grain growth of alumina were enhanced by Mn addition up to 0.75 cat% but was leveled off at higher concentrations. XRD revealed that $Al_2MnO_4$(galaxite) was formed as a second phase in the specimens with more than 0.75 cat% of Mn. Thus it is believed that either the solid solution effect of Mn or the Zener effect of $Al_2MnO_4$ becomes predominant in the sintering of Mn-added $Al_2O_3$ according to the additive concentration. UV-VIS reflectivity(SCI) spectra of Mn-added $Al_2O_3$ consisted of smooth bottoms in 300~550 nm wavelength range and plateaus at wavelengths longer than 650 nm. The reflectivity spectrum continuously moved downward, and the specimen color became darker and thicker with increasing Mn content. The CIELAB color change with respect to standard white was also dependent on the amount of Mn added: ${\Delta}L^*$(D65) negatively increased and ${\Delta}E_{ab}^*$(D65) positively increased with increasing Mn content, probably due to Mn substitution to Al and/or the mixing effect of black $Al_2MnO_4$ as a second phase.

Structural and optical properties of Ni-substituted spinel $LiMn_2O_4$ thin films (니켈 치환된 스피넬 LiMn2O4 박막의 구조적, 광학적 성질)

  • Lee, Jung-Han;Kim, Kwang-Joo
    • Journal of the Korean Vacuum Society
    • /
    • 제15권5호
    • /
    • pp.527-533
    • /
    • 2006
  • Spinel $LiNi_xMn_{2-x}O_4$ thin films were synthesized up to x = 0.9 by a sol-gel method employing spin-coating. The Ni-substituted films were found to maintain cubic structure at low x but to exhibit tetragonal structure for $x{\geq}0.6$. Such cubic-tetragonal phase transition indicates that $Ni^{3+}(d7)$ ions with low-spin $(t_{2g}^6,e_g^1)$ state occupy the octahedral sites of the compound, thus being subject to the Jahn-Teller distortion. By x-ray photoelectron spectroscopy both $Ni^{2+}$ and $Ni^{3+}$ ions were detected. Optical properties of the $LiNi_xMn_{2-x}O_4$ films were investigated by spectroscopic ellipsometry (SE) in the visible?ultraviolet range. The measured dielectric function spectra by SE mainly consist of broad absorption structures attributed to charge-transfer (CT) transitions, $O^{2-}(2p){\rightarrow}Mn^{4+}(3d)$ for 1.9 $(t_{2g})$ and $2.8{\sim}3.0$ eV $(e_g)$ structures and $O^{2-}(2p){\rightarrow}Mn^{3+}(3d)$ for 2.3 $(t_{2g})$ and $3.4{\sim}3.6$ eV $(e_g)$ structures. Also, sharp absorption structures were observed at about 1.6, 1.7, and 1.9 eV, interpreted as due to d-d crystal-field transitions within the octahedral $Mn^{3+}$ ion. The strengths of these absorption structures are reduced by the Ni substitution. Rapid reduction of the CT transition strength involving the eg states for x = 0.6 is attributed to the reduced wavefunction overlap between the $e_g$ and the $O^{2-}(2p)$ states due to the tetragonal extension of the lattice constant by the Jahn-Teller effect.

A study on Dielectric Properties usig PMN Ceramics with $MnO_2$ substitution ($MnO_2$치환된 PMN계 세라믹스의 유전특성)

  • Ji, S.H.;You, D.H.;Lee, Y.H.;Kim, Y.I.;Park, K.H.;Lee, D.C.
    • Proceedings of the KIEE Conference
    • /
    • 대한전기학회 1997년도 하계학술대회 논문집 C
    • /
    • pp.1537-1539
    • /
    • 1997
  • In this study, the dielectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$ Ceramics have been investigated as a addition of the amount of $MnO_2(0{\leq}x{\leq}0.9wt%)$. The Temperature-dependant dielectric characteristics of 0.9PMN-0.1PT relaxor ferroelectric system were improved by enhencing the extent of the diffuse phase transition(DPT). The maximum dielectric permittivity decreased by substitution $MnO_2$ and the dielectric loss decreased with increasing $MnO_2$ substitution amount. It is expected decreasing in inner heat energy for temperature with increasing $MnO_2$ substitution.

  • PDF

Plasma Concentrations of Fe, Cu, Mn, and Cr of Maternal and Umbilical Cord Blood during Pregnancy

  • Lee, Jong-Im;Lim, Hyeon-Sook;Cho, Young-Sook
    • Preventive Nutrition and Food Science
    • /
    • 제7권3호
    • /
    • pp.282-286
    • /
    • 2002
  • Anemia is prevalent among pregnant women in Korea, and Fe deficiency anemia is a major nutritional problem throughout the world. Because studies of Cu, Mn, and Cr levels excluding Fe are rare, we were interested in changes in the nutritional status of these trace minerals and their relationship to hematogenesis. Accordingly, we determined the changes in plasma Fe, Cu, Mn, and Cr concentrations of maternal and umbilical cord blood during pregnancy, and evaluated the relationships between them at different time points during pregnancy. A total of 81 women participated in the study: 26 subjects in the first trimester, 23 in the second, and 32 in the third trimester. Plasma Fe levels were lower significantly (p<0.05) in the third trimester. Plasma Cu level ($\mu\textrm{g}$/dL) in each trimester were 86.6$\pm$13.8, 111.6$\pm$27.9, and 114.0$\pm$29.7, respectively; with significant increases (p<0.()5) in the second and third trimester. Plasma Mn concentrations (pg/dL) in each trimester were 212.6$\pm$89.0, 234.0$\pm$140.0, and 240.3$\pm$166.0, respectively and tended to increase, though not significantly, as the pregnancies progressed. The plasma concentrations of Cr (pg/dL) in each trimester were 3.7$\pm$2.0, 3.1$\pm$1.0, and 2.4$\pm$1.2, respectively; and was significantly lower (p<0.05) in the third trimester. In umbilical cord blood, the plasma level of Fe was 194.8$\pm$74.6 $\mu\textrm{g}$/dL, Cu was 57.5$\pm$10.9 $\mu\textrm{g}$/dL, Mn was 482.4$\pm$111.1 pg/dL, and Cr was 9.3$\pm$2.8 pg/dL. Plasma concentrations of Fe, Cu, Mn, and Cr of cord blood were 300 %, 50 %, 200 %, and 370% as compared to those of maternal blood in the third trimester. These results suggest that an active transport mechanism for the transport of Fe, Mn, and Cr from mother to fetus may exist, whereas, for Cu, the placenta appears to have a blocking effect on the transport from mother to baby.

Ruminal Solubility of Trace Elements from Selected Philippine Forages

  • Serra, S.D.;Serra, A.B.;Ichinohe, T.;Fujihara, T.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제10권4호
    • /
    • pp.378-384
    • /
    • 1997
  • The ruminal solubility of copper (Cu), manganese (Mn), molybdenum (Mo), and zinc (Zn) in eight Philippine forages was studied. These forages were: 1) grasses: paragrass (Brachiaria mutica (Forsk.) Stapf), stargrass (Cynodon plectostachyum Pilger), and napiergrass (Pennisetum purpureum Schumach.); 2) creeping legumes: calopogonium or calopo (Calopogonium muconoides Desv.) and centrocema (Centrocema pubescens Benth.); 3) tree lequmes: gliricidia or kakawate (Gliricidia sepium (Jacq.) Walp.), leucaena or ipil-ipil (Leucaena leucocephala (Lam.) de Wit.), and sesbania or katuray (Sesbania grandiflora (L.) Poir). Nylon bags with samples were incubated for 0, 3, 6, 12, 24, 48 and 72h in three rumen cannulated sheep fed with timothy hay (Phleum pratense L.) at 2% body weight/d. The 0-h bags were washed with deionized water. There were species differences (p < 0.05) on the different solubilities of trace elements. At O-h incubation, the trend of solubility was Mo (54%) > Zn (43%) > Cu (38.7%) > Mn (29.5%). At 3-h incubation, all the elements except Mn had an average solubility above 50%. Combining particulate passage rate (1.9%/h) and various trace elements disappearance rates, the effective ruminal solubilization (ERS) of trace elements were computed. The ERS across species ranged from 44.6 to 89.9% for Cu, 29.9 to 84% for Mn, 66 to 95.1% for Mo, and 30.1 to 82.3% for Zn resulting to a trend of Mo > Zn > Cu > Mn.

Color Tuning of a Mn4+ Doped Phosphor : Sr1-xBaxGe4O9:MnMn4+0.005 (0.00 ≤ x ≤ 1.00) (Mn4+ 도핑된 형광체, Sr1-xBaxGe4O9:MnMn4+0.005 (0.00 ≤ x ≤ 1.00)의 Color Tuning)

  • Park, Woon Bae
    • Journal of the Korean Chemical Society
    • /
    • 제61권4호
    • /
    • pp.163-167
    • /
    • 2017
  • Along with the progress of white LED technology, red phosphors have become increasingly important in industry and academia, and a more specific demand has steadily increased in the market. Red phosphors are used in high efficiency and high rendering LED lightings. However, using red phosphors with $Eu^{2+}$ activators caused color rewarming and reduced emission intensity in white LED chips due to strong reabsorption in the green or yellow wavelength range caused by the 4f-5d transition. $Mn^{4+}$ doped phosphors which have no such drawbacks and which can further improve the color rendering index (CRI) are now of great interest. However, $Mn^{4+}$-doped phosphors have a disadvantage in that the emission wavelength is determined depending on the host due to the $^2E_g{\rightarrow}^4A_2$ transition. In this study, the $SrO-BaO-GeO_2$ solid-solution was selected, and $Sr_{1-x}B_axGe_4O_9:Mn^{4+}{_{0.005}}$ ($0{\leq}x{\leq}1$) phosphors were synthesized and characterized. This led to a versatile color tuning in LED technology.