• Title/Summary/Keyword: MAXIMUM STRENGTH

Search Result 3,770, Processing Time 0.033 seconds

Studies on the Effect of Water Content, Curing Temperature and Grain Size Distribution of Soils on Unconfined Compressive Strength of Soil-Cement Mixtures. (함수비, 양생온도 및 흙의 입도가 Soil-Cement의 압축강도에 미치는 영향에 관한 연구(I))

  • 김재영;강신업
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.19 no.1
    • /
    • pp.4312-4322
    • /
    • 1977
  • In order to investigate the effect of the water content and the accelerated curing on the strength of the soil-cement mixtures, laboratory test of soil cement mixtures was performed at five levels of water content, four levels of accelerated curing temperatures, three levels of normal curing periods, and six levels of accelerated curing time. Also this study was carried out to investigate the effect of grain size distribution of 21 types of soils on the strength of soil-cement mixtures at four levels of cement content and three levels of curing time. The results are summarized as follows: 1. Optimum moisture content increased with increase of the cement content, but maximum dry density was changed ununiformly with cement content. Water content corresponding to the maximum strength was a little higher than the optimum moisture content along the increase of cement content. 2. In molding the specimens with the optimum moisture content, the maximum strength appeared at the wet side of the optimum moisture content. 3. According to increase of curing temperature as 30, 40, 50, and 60$^{\circ}C$, unconiiend compressive strength of soil-cement mixtures increased, the rate of increase at the early curing period was large, and approximately 120 hours was suifficient to harden soil-cement mixtures completely. 4. The strength of soil-cement mixtures at the curing temperature of 10$^{\circ}C$ decreased at the rate of 30 to 50 percent than at the curing temperature of 20$^{\circ}C$, and the strength of soil-cement mixtures at the curing temperature of 0$^{\circ}C$ increased a little with increase of curing time. 5. Although the strength of soil-cement mixtures seemed to be a little affected by the temperature difference between day time and night, it was recommended that reasonable working period was the duration from July to August of which average maximum temperature of Korea was approximately 30$^{\circ}C$. 6. Accelerated curing time corresponding to the normal curing time of 28-day was shorten with increase of curing temperature, also it was a little affected by the cement. Accelerated curing time that the strength of soil-cement mixtures for the cement of 9 percent and the curing temperature of 60was shorten with increase of curing temperature, also it was a little affected by the cement. Accelerated curing time that the strength of soil-cement mix- tures for the cement of 9 percent and the curing temperature of 60$^{\circ}C$ was 45 hours at the KY sample, 50 hours at the MH, 40 hours at the SS, and 34 hours at the JJ respectively. 7. Accelerated curing time was depended upon the grain size distribution of soil, it decreased with increase the percent passing of No. 200 sieve. 8. Relationship between the normal curing times and the accelerated curing times showed that there was a linear relationship between them, its slope decreased with increase of curing temperature. 9. The most reasonable soil of the soil-cement mixtures was the sandy loam which was a well graded soil. Assuming the base of road requiring 7-day strength of 21 kg/$\textrm{cm}^2$ being used, the soil-cement mixtures could be obtained with adding 6 percent of cement in such a sails S-7, S-8, S-9, S-10, S-11, S-12, S-13. 10. The regression equation between the 28-day and the 7-day strength was obtained as follow; q28=1.12q7,+6.5(r=0.96).

  • PDF

Concurrent flexural strength and deformability design of high-performance concrete beams

  • Ho, J.C.M.;Zhou, K.J.H.
    • Structural Engineering and Mechanics
    • /
    • v.40 no.4
    • /
    • pp.541-562
    • /
    • 2011
  • In the design of earthquake resistant reinforced concrete (RC) structures, both flexural strength and deformability need to be considered. However, in almost all existing RC design codes, the design of flexural strength and deformability of RC beams are separated and independent on each other. Therefore, the pros and cons of using high-performance materials on the flexural performance of RC beams are not revealed. From the theoretical results obtained in a previous study on flexural deformability of RC beams, it is seen that the critical design factors such as degree of reinforcement, concrete/steel yield strength and confining pressure would simultaneously affect the flexural strength and deformability. To study the effects of these factors, the previous theoretical results are presented in various charts plotting flexural strength against deformability. Using these charts, a "concurrent flexural strength and deformability design" that would allow structural engineers to consider simultaneously both strength and deformability requirements is developed. For application in real construction practice where concrete strength is usually prescribed, a simpler method of determining the maximum and minimum limits of degree of reinforcement for a particular pair of strength and deformability demand is proposed. Numerical examples are presented to illustrate the application of both design methods.

THE EFFECTS OF HEAT TREATMENT OF ORTHODONTIC WIRES (교정용 강선재의 열처리 효과에 관한 실험적 연구)

  • Lee, Myeung-Suck;Sohn, Byung-Hwa
    • The korean journal of orthodontics
    • /
    • v.22 no.3 s.38
    • /
    • pp.591-602
    • /
    • 1992
  • The purpose of this study was to evaluate the effect of heat treatment on physical properties of 0.016' and 0.016' x 0.022' stainless steel wires. Temperature of heat treatment had intervals of $50^{\circ}C$ from $400^{\circ}C$ to $700^{\circ}C$, and time of heat treatment were 3, 6 and 9 minutes. Tensile tests were measured by ultimate tensile strength and yield strength. Bending tests were assessed by maximum bending force, recovery force, and stiffness. Torsion test was evaluated by torsion cycle until wires were fractured. The results were as follows: 1. In round wires, the highest value of ultimate tensile strength and yield strength were recorded of heat treatment at $500^{\circ}C$. In rectangular wires, the highest value of ultimate tensile strength were after 9 minutes at $400^{\circ}C,\;450^{\circ}C$ and 3, 6 minutes of heat treatment at $50^{\circ}C$, yield strength were the highest value after 3, 6 minutes of heat treatment at $500^{\circ}C$. 2. In both round and rectangular wires, maximum bending force and recovery force were the highest values after 6 minutes of heat treatment at $500^{\circ}C$. In round wires, highest value of stiffness were formed after 9 minutes at heat treatment at $500^{\circ}C$. In rectangular wires, the highest value of stiffness were for 6 minutes in $500^{\circ}C$. 3. In rectangular wires, torsion cycle was minimum after 6 minutes of heat treatment at $500^{\circ}C$. 4. In all of tension, bending, and torsion tests, the heat treated wires were softened over at $700^{\circ}C$. 5. In all of tension, bending, and torsion tests, physical properties of the wires were more influenced by the temperatures than the duration of the heat treatment.

  • PDF

EFFECTS OF HYDROFLUORIC ACID CONCENTRATION & ETCHING TIME ON THE SHEAR BOND STRENGTH BETWEEN LITHIUM DISILICATE CERAMIC AND RESIN CEMENT (불산 식각 농도 및 시간이 lithium disilicate 도재와 레진시멘트의 전단결합강도에 미치는 영향)

  • Seo, Jae-Min;Park, Charn-Woon;Ahn, Seung-Geun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.4
    • /
    • pp.407-418
    • /
    • 2007
  • Purpose: The objective of this study was to evaluate the effects of hydrofluoric acid concentration & etching time on the shear bond strength between IPS Empress 2 ceramic and resin cement. Material and methods: Thirty three rectangular shape ceramic specimens($20{\times}12{\times}5mm$ size, IPS Empress 2 core materials) were used for this study. The ceramic specimens divided into ten experimental groups with three specimens in each group and were etched with hydrofluoric acid(4%, 9%) according to different etching times(30s, 60s, 90s, 120s, 180s). Etched surfaces of ceramic specimens were bonded with resin cement(Rely X Unicorn) using acrylic glass tube. All cemented specimens were tested under shear loading until fracture on universal testing machine at a crosshead speed of 0.5mm/min and the maximum load at fracture(kg) was recorded. Collected shear bond strength data were analyzed with one way ANOVA and Duncan tests. All etched ceramic surfaces were examined morphologically using SEM(scanning electron microscopy). Results: Shear bond strength of etching group$(35.89{\sim}68.01MPa)$ had four to seven times greater than no-etching group$(9.53{\pm}2.29MPa)$. The ceramic specimen etched with 4% hydrofluoric acid for 60s showed the maximum shear bond strength$(68.01{\pm}11.78MPa)$. Ceramic surface etched with 4% hydrofluoric acid for 60s showed most retentive surface texture. Conclusion: It is considered that 60s etching with 4% hydrofluoric acid is optimal etching methods for IPS Empress 2 ceramic bonding.

Effect of Enzyme Stabilization on Hardening of Clay-rock Brick (점토-골재 벽돌 경화에 있어 효소 사용의 효과)

  • Mitikie, Bahiru Bewket;Lee, Tai-Sik
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.4
    • /
    • pp.366-374
    • /
    • 2017
  • This study investigates enzyme stabilization in clay-rock bricks through mechanical tests and image processing. Appropriate soil mixtures were designed using clay/crushed rock with ratios of 70/30, 60/40, 50/50, 40/60, and 30/70 by weight to verify the strength of the enzyme brick and soil compaction. The maximum compressive and flexural strengths in the 60/40 ratio mixture were found to be 5MPa and 1.25MPa, respectively; however, the maximum dry unit weight of $2.073g/cm^3$ was found in the 50/50 clay/gravel ratio mixture. Generally, the strength of the enzyme brick was improved by 27%. The paper concludes that in order to achieve optimal strength, soils should be mixed with the 60/40 clay/gravel ratio, which provides an adequate strength, while 50/50 ratio should be used for achieving more compaction. The SEM-EDX observation and Matlab image processing verified how the bond structure appeared after enzyme stabilization. It was found that enzymes created bond with the clay soil and the crushed rock for rendering strength and stability.

Improvement and Analysis of Stacking Durability of Corrugated Fiberboard Boxes for Agricultural Products -Moisture Absorption Properties and Compressive Strength Reduction- (농산물 포장용 골판지상자의 층적내구성의 분석과 향상에 관한 연구(I) -수분흡습특성과 압축강도열화-)

  • Park, J.M.;Kwon, S.H.;Kwon, S.G.;Kim, M.S.
    • Journal of Biosystems Engineering
    • /
    • v.19 no.4
    • /
    • pp.358-368
    • /
    • 1994
  • Major factors in reducing the stacking strength of corrugated fiberboard boxes in cold storage or transport conditions are high relative humidity, causing elevated moisture absorption by the boxes. The bottom boxes in a stack will deform to the critical deflection causing agricultural products damage there, and eventually additional deflection will cause box collapse and finally toppling of the stack. The study was conducted to determine the water absorption characteristics and the compressive strength of the corrugated fiberboard boxes being widely used in packaging agricultural products in Korea. The sample boxes for the study were selected from the regular slotted containers (RSC) types, and one was the box used in apple packaging (Box A), another one was the box used in pear packaging (Box B). The corrugated shipping containers were made from a large portion of recycled fibers in Korea, and comparing with Box B, Box A was fabricated from fiberboard which contained more percentage of old corrugated containers (OCC) imported from foreign countries than domestic waste paper. The results obtained from the study were summarized as follows ; 1. Equilibrium moisture content (EMC) of the sample boxes was established after about 20 hours, and the EMC by absorption was lower than that by desorption. The EMC increased with the increasing of relative humidity and with the decreasing of temperature, and the rate of increasing was much higher above the relative humidity of 50%. 2. The maximum compressive strength of Box A was about 100 kgf greater than that of Box B on the same enviromental conditions. The strength of the sample boxes decreased rapidly with the increasing of relative humidity. The effect of relative humidity on the strength was a little higher than that of temperature. 3. As the applied load was progressively increased and a level was reached, the vertical side panels ($L{\times}D$) deflected laterally inwards or outwards. The panels deflected laterally inwards at higher relative humidity. 4. The maximum compressive deflection ratio and the critical deflection ratio of the sample boxes were increased linearly with the increasing of relative hunidity, but trends for its ratios showed inconsistant response to temperature.

  • PDF

Comparison of the Isokinetic Strength of the Knee and Ankle and Isometric Strength of the Lumbar Extensor in Female Collegiate Dancers and Controls (무용전공 여대생들과 일반 여대생들의 무릎과 발목 등속성 최대우력과 허리폄근 등척성 최대우력 비교)

  • Won, Jong-Im
    • Physical Therapy Korea
    • /
    • v.16 no.1
    • /
    • pp.25-33
    • /
    • 2009
  • In dancers, intact muscular coordination is a well balanced antagonist, which could be a decisive factor in protection against injury as dancers often have hypermobile joints and their ankle joints often bear their full body weight in extreme positions. The purposes of this study were to identify the isokinetic strength to the knee and ankle and the isometric strength of the trunk in female collegiate dancers and controls. Furthermore, the study aimed to investigate the peak torque ratio of knee extension to flexion, ankle plantarflexion (PF) to dorsiflexion (DF), and dominant legs to nondominant. Twenty-one female collegiate dancers (20.0 years of age) and twenty-one female collegiate students (19.3 years of age) performed isokinetic maximum efforts of the knee extensors and flexors at $60^{\circ}/sec$ and $120^{\circ}/sec$, the ankle plantarflexors and dorsiflexors at $30^{\circ}/sec$ and $120^{\circ}/sec$ and isometric maximum efforts of the lumbar extensors at $0^{\circ}$, $12^{\circ}$, $24^{\circ}$, $36^{\circ}$, $48^{\circ}$, $60^{\circ}$, and $72^{\circ}$. The results were as follows: The isokinetic peak torque of the knee extensors and the ratio of knee extensors to flexors of dancers were significantly higher than those of controls (p<.01). However, the isometric peak torque of the back extensors (p<.01) and isokinetic peak torque of the ankle plantarflexors and dorsiflexors (p<.05) of dancers were significantly lower than those of controls. Further studies are needed to identify the difference in proprioception of the joints between dancers and controls.

  • PDF

An Fundamental Study on the Earth Wall Material Development by using of Lime Composition and Earth (석회복합체와 흙을 이용한 흙벽체 재료 개발에 관한 기초적 연구)

  • Hwang, Hey zoo;Kang, Nam Yi
    • KIEAE Journal
    • /
    • v.10 no.5
    • /
    • pp.115-121
    • /
    • 2010
  • Lime was the solidifier mostly used at the fields of construction and civil works in the past. however, the development of Portland cement remarkably reduced the use of it. Recently as the concernment on circumstances gets higher, lime wined attention again as an eco-friendly material and was used at earth-using construction. This study examined the physical and chemical capacity of lime complexes with lime capacity improved, and performed fundamental study on the way to concretize by mixing it with earth. As a result, lime complex pressure strength was lower than cement pressure strength but it showed the possibility that its strength was improved by W/B control. The measurement of XRD after paste formation confirmed a compound generated by the reaction of Ca2+ion and Si, Al, and Fe from pozzolan reaction. A earth wall experiment by using lime complexes and earth showed that the higher, WB or the lower the quantity of unit combined materials, the lower the pressure strength was. The maximum pressure strength was maximum 11MPa when the quantity of unit combined materials was 450. It is because the composed earth particles had a high content of micro powder less than silt, so a lot of combination are demanded to secure fluidity. As a result of peptization experiment, after hardening, the material was not dissolved, which informed of the possibility of use as an outer subsidiary material. If the material is hardened by mold formation method, natural hardening crack appears. Cast expresses smart surface quality and enables to design for multiple purpose. The result shows the possibility of construction of low-story structures by using earth wall made of lime complexes and earth.

Study on Structural Strength Analysis of Automotive Seat Frame (자동차 시트 프레임의 구조 강도 해석에 관한 연구)

  • Kim, Key-Sun;Kim, Sung-Soo;Kim, Sei-Hwan;Cho, Jae-Ung
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.1
    • /
    • pp.39-44
    • /
    • 2013
  • Seat is the part relevant to comfortableness and safety among automotive parts directly. It also should have sufficient stiffness and strength to satisfy these conditions and ensure the safety of passenger. Automotive seat is modelled with 3D and is simulated with structural analyses about three kinds of experiments by before and after gap, side gap, before and after moment strength. As analysis result, deformation angles of $0.038^{\circ}$ and $0.04^{\circ}$ are respectively shown at before and after gap test, side gap test. Through before and after the moment strength test, maximum total deformations of 0.18946mm and 3.2482mm are respectively shown at front and rear loads. By the study result of no excessive deformation and no fracture at automotive seat frame, the sufficient rigidity and strength to guarantee the safety of passenger can be verified.

Experimental investigations on performance of concrete incorporating Precious Slag Balls (PS Balls) as fine aggregates

  • Sharath, S.;Gayana, B.C.;Reddy, Krishna R.;Chandar, K. Ram
    • Advances in concrete construction
    • /
    • v.8 no.3
    • /
    • pp.239-246
    • /
    • 2019
  • Substitution of natural fine aggregates with industrial by-products like precious slag balls (PS Balls) offers various advantages like technical, economic and environmental which are very important in the present era of sustainability in construction industry. PS balls are manufactured by subjecting steel slag to slag atomizing Technology (SAT) which imparts them the desirable characteristics of fine aggregates. The main objective of this research paper is to assess the feasibility of producing good quality concrete by using PS balls, to identify the potential benefits by their incorporation and to provide solution for increasing their utilization in concrete applications. The study investigates the effect of PS balls as partial replacement of fine aggregates in various percentages (20%, 40%, 60%, 80% and 100%) on mechanical properties of concrete such as compressive strength, splitting tensile strength, and flexural strength. The optimum mix was found to be at 40% replacement of PS balls with maximum strength of 62.89 MPa at 28 days curing. Permeability of concrete was performed and it resulted in a more durable concrete with replacement of PS balls at 40% and 100% as fine aggregates. These two specific values were considered as optimum replacement is 40% and also the maximum possible replacement is 100%. Scanning electron microscope (SEM) analysis was done and it was found that the PS balls in concrete were unaffected and with optimum percentage of PS balls as fine aggregates in concrete resulted in good strength and less cracks. Hence, it is possible to produce good workable concrete with low water to cement ratio and higher strength concrete by incorporating PS balls.